다양한 온도에서 염소가스 반응에 의해 표면 개질된 SiC의 트라이볼로지 특성평가 (Estimation of Tribological Properties on Surface Modified SiC by Chlorine Gas Reaction at Various Temperatures)

  • 배흥택;정지훈;최현주;임대순
    • 한국세라믹학회지
    • /
    • 제46권5호
    • /
    • pp.515-519
    • /
    • 2009
  • Carbon layers were fabricated on silicon carbide by chlorination reaction at temperatures between $1000^{\circ}C$ and $1500^{\circ}C$ with $Cl_2/H_2$ gas mixtures. The effect of reaction temperature on the micro-structures and tribological behavior of SiC derived carbon layer was investigated. Tribological tests were carried out ball-on-disk type wear tester. Carbon layers were characterized by X-ray diffractometer, Raman spectroscopy and surface profilometer. Both friction coefficients and wear rates were maintained low values at reaction temperature up to $1300^{\circ}C$ but increased suddenly above this temperature. Variation of surface roughness as a function of reaction temperature was dominant factor affecting tribological transition behavior of carbon layer derived from silicon carbide at high temperature.

TiC표면개질에서 $Cl_2$ 가스농도가 tribology 특성에 미치는 효과 (Effect of $Cl_2$ Gas Concentration of the Surface Modified TiC on the Tribological Properties)

  • 배흥택;임대순;나병철
    • Tribology and Lubricants
    • /
    • 제23권6호
    • /
    • pp.261-265
    • /
    • 2007
  • Carbide-derived carbon coating has been synthesized by low temperature treatment of TiC disk with $H_2/Cl_2$ mixture gases. A variety of physical measurements indicated that Ti was extracted and carbon layer was formed by exposure of $Cl_2$ gas. The $I_D/I_G$ ratio increased with increasing $Cl_2$ gas concentration. Wear coefficient and frictional coefficient varied with $Cl_2$ gas concentration. When the $Cl_2$ gas concentration decreased to 3.3 vol%, the friction coefficient approach a minimum. The results showed that degree of graphite crystallinity and variation of porosity due to the $Cl_2$ gas content were responsible for different tribology performance.

염소가스 반응시간에 따른 TiC표면 탄소막의 Tribology 특성 (Dependence of $Cl_2$ Gas Reaction Time on Tribological Properties of TiC Derived Carbon Layer)

  • 임대순;배흥택;정지훈;나병철
    • Tribology and Lubricants
    • /
    • 제25권1호
    • /
    • pp.20-24
    • /
    • 2009
  • TiC-derived carbon coatings have been synthesized at $600^{\circ}C$ temperature treatment with $H_2/Cl_2$ mixture gases. From Raman spectroscopy measurements, the modified layer was covered with carbon and the thick-ness of the layer was increased with increasing reaction time. And $I_D/I_G$ ratio was decreased with increasing reaction time. The superior tribological property was obtained from TiC reacted with $Cl_2$ gas for 2 hrs. And the tribological property measurements indicate that TiC-derived carbon layer has $0.9{\times}10_{-6}mm^3/Nm$ in wear coefficient and 0.13 in friction coefficient.