Ball Screw Cutting of Hardned Steel (고경도강의 나사선삭)

  • 황동환;박철우;김대은;이상조
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1993.10a
    • /
    • pp.37-41
    • /
    • 1993
  • ball screw is a critical machine component which dictates the precison of a given machine tool. The conventional manufacturing method requires the heat treated ball screw to be ground to its final dimensions. This study looks into the the feasibility of replacing the grinding process with a simpler process, namely threading on NC lathe. The purpose is to reduce the capital investment as well as production time in the manufacture of ball screws. Ceramics and CBN cutting tools are compared with respect to their ability to machine hardened steel. It is shown that CBN tools can be successfully utilized to machine precision ball screws with superior suface qualities.

  • PDF

Machining Characteristics of Ni-based Heat Resisting Alloy (니켈기 초내열합금의 절삭성에 관한 연구)

  • 강신호;김대은
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.15 no.4
    • /
    • pp.27-35
    • /
    • 1998
  • Ni-based heat resisting alloys are commonly used for high temperature applications such as in aircraft engines and gas turbines. In this work, the machinability of Nimonic 263 alloy is investigated with respect to optimum tool type and cutting conditions for both continuous and discontinuous machining as well as weld region. Among the five types of tools tested, K25 tool experienced the least of damage in machining the weld region. Furthermore, despite their superior high temperature hardness, Si-Al-O-N and CBN tools peformed poorly in machining Nimonic 263.

  • PDF

Analysis of Thermal Displacement of PCBN Tool Holder for Machining Accuracy in Hard Turning (하드터닝에서 CBN 공구홀더의 열변형이 가공정밀도에 미치는 영향)

  • 노승국;이찬홍;하재용
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.363-366
    • /
    • 2003
  • The hard turning is a turning operation performed in high strength alloy steels (HRC>30) in order to reach surface roughness close to those obtained in grinding. This is possible because of availability of improved tool materials (polycrystalline cubic boron nitride. PCBN), ad more rigid machine tools. According to many previous work of hard turning mechanism, the maximum temperature of cutting can be raised up to 100$0^{\circ}C$. As the heat generation rate is very high, the thermal displacement of tool holder cannot be negligible. Therefore, the aim of this paper is to analyze effects of high heat generation at CBN tool tip to the thermal displacement of a tool holder in hard turning and finally geometric accuracy. The thermal behavior of a CBN tool holder is investigated by numerical simulation and experiment, and the result shows thermal elongation of microns order is possible during hard turning process.

  • PDF

A study on the surface integrity of machined surface layer in machining hardened STD11 steel (경화처리된 합금공구강의 절삭에서 가공 표면층의 표면성상에 관한 연구)

  • Noh, Sang-Lai;An, Sang-Ook
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.11 no.5
    • /
    • pp.153-160
    • /
    • 1994
  • In this study, residual stress and surface roughness were investigated experimentally to evaluate surface integrity on surface layer machined by CBN, ceramics and WC cutting tools. When machining difficult-to-cut material (hardened STD11 steel $H_{R}$C 60), residual stresses remaining in machined surface layer were mainly compressive. The increase of flank wear caused a shift of the compressive residual stress maximum to greater workpiece depths, but the changes did not penetrate the workpiece beneath a depth of 300 .mu. m. Surface roughness was influenced considerably by variations of the cutting speed and feed. In machining hard material, CBN and A1$_{2}$ $O_{3}$ ceramics cutting tool materials proved significantly superior to mixed ceramics A1$_{2}$ $O_{3}$-TiC and WC in evaluation of surface integrity.y.

  • PDF

Machinability of ceramic and WC-Co green compacts (세라믹 및 초경합금 성형체의 피절삭성)

  • Lee, Jae-Woo
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.21 no.9
    • /
    • pp.1520-1530
    • /
    • 1997
  • Machining pressed compacts of ceramic and WC-Co materials can be the most cost effective way of forming the bodies prior to sintering when the required number of pieces is small. In this study, in order to clarify the machinability for turning, the $Si_3N_4$ and the WC-Co green compacts unsintered were machined under different cutting conditions with various tools. Absorbing chips by vacuum hose decreases tool wear. The tool wear becomes larger in the order of the ceramic, CBN and cemented carbide tools in machining the $Si_3N_4$ green compacts. In machining the WC-Co green compacts, the tool wear becomes larger in the order of the ceramic, cemented carbide and CBN tools. The land of cutting edge does not affect tool wear. When machining with cemented carbide tool, the tool wear i equal cutting length is nearly identical in spite of the increase of cutting spee, and the roughness of machined surface was the best in the cutting speed of 90 m/min. The tool wear decreases with the increase of rake angle and relief angle and with the decrease of nose radius. The machined surfaces become worse with the increase of feed rate and depth of cut, and with the decrease of rake angle and relief angle. The tool wear is not affected by the feed and depth of cut.

A Study on the Coated Characteristics of Ceramic Tools (세라믹공구 재료의 피복특성에 관한 연구)

  • Lee, Myeong-Je;Im, Hong-Seop;Yu, Bong-Hwan
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.4 s.175
    • /
    • pp.900-906
    • /
    • 2000
  • Ceramic, PCD and CBN tools are available for the difficult-to-cut-materials such as hardened carbon tool steel, stainless steel, Inconel 718 and etc. Ceramic tools are likely to be chipped and abruptly broken before the appearance of normal wear in turning. Ceramic tools are suitable for continuous in turning, not for intermittent in milling. In this study, TiN/TiCN multi-layer coated ceramic tools were found to restrain the chipping, breaking and early fracture and to increase the critical cutting speed owing to TiN/TiCN multi-layer coating in Arc Ion Plating of PVD method.

Comparative Study on the Ceramic and the TiN Coated Ceramic Tools for the Early Fracture (세라믹공구와 TiN피복 세라믹 공구의 초기파손에 관한 비교연구)

  • 이명재
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.7 no.4
    • /
    • pp.123-129
    • /
    • 1998
  • Ceramic and CBN tools are available for the difficult-to -cut-materials such as hardened carbon tool steel. stainless steel and etc. Ceramic tools are suitable for continuous turning cut, not for intermittent milling cut. Ceramic tools are likely to be chipped and abruptly broken before the appearance of normal wear in turning. In this study, TiN coated ceramic tools were found to restrain the chipping, breaking and early fracture and to increase the critical cutting velocity owing to TiN coating in PVD method.

  • PDF

Fracture Characteristics of Cutting Tools in Machining of Hardened Alloy Steel (열처리한 합금공구강의 절삭에서 공구파손의 특성)

  • Noh, S.L.;An, S.O.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.7 no.3
    • /
    • pp.199-205
    • /
    • 1994
  • The fracture characteristics and tool life of ceramics and WC, CBN cutting tool when turning heat treated steel STD11($H_RC$ 60) were investigated experimentally to clarify the machinability and optimum tool materials in cutting of difficult-to-cut material with high hardness. Forthermore, the behaviors of the tool wear and failure were examined with regard to cutting force. The hardened steel wore the cutting tool edge rapidily and increased the cutting forces, especially radial force. The tool was worn by the abrasive action. Flank Weat of $Al_2O_3-TiC$ ceramic and WC tool become relatively large and CBN & $Al_2O_3$, ceramic tool had a long life among the tool materials tested. The tool fracture patterns were just like minor cutting wear, flank wear, crater wear, notch wear, chipping. Flank wear rate was accelerated by occurrence of chipping. During the proceeding of machining, it was possible to foresee the catastrophic fracture of tool by abrupt increase of radial force.

  • PDF

A Study on the Coated Characteristics of Ceramic Tools (코팅공구의 절삭성능에 관한 연구)

  • 유봉환
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.9 no.1
    • /
    • pp.96-101
    • /
    • 2000
  • Ceramic, PCD and CBN tools are available for the difficult-to-cut-materials such as hardened carbon tool steel, stainless steel, Inconel 718 and etc.. Ceramic toolsare likely to be chipped and abruptly broken before the appearance of normal wear in turning. Ther2efore ceramic tools are suitable for continuous cut in turning not for intermittent in milling. In this study, TiN/TiCN multi-layer coated ceramic tools were found to restrain the chipping, breaking and early fracture and to increase the critical cutting speed owing to TiN/TiCN multi-layer coating in Arc Ion Plating of PVD method.

  • PDF

Machinability of Presintered $Al_2O_3$ ceramics (알루미나 세라믹 예비소결제의 피절삭성)

  • Kim, Sung-Chung;Lee, Jae-Woo
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.21 no.6
    • /
    • pp.1002-1012
    • /
    • 1997
  • When the presintered ceramics are machined with ceramic tool, the tool life becomes extremely short. The CBN tool exhibits the best performance in dry machining of the ceramics presintered at $1450^{\circ}C$ among all cutting tests. The roughness of the machined surface of the ceramics presintered below $1350^{\circ}C$ is smaller than that of the ceramics presintered at $1450^{\circ}C$ While the performance of the cemented carbide and CBN tools is better in dry than in wet machining, the diamond tool shows adverse tendency. The tool life is not affected by the feed rate and depth of cut. During the following full-sintering after the machining of the presintered ceramics, the surface roughness decreases up to 62%. The finished surface in machining the presintered ceramics is much better than that in machining the full-sintered ceramic.