Degradation and mineralization of violet-3B dye using C-N-codoped TiO2 photocatalyst

  • Putri, Reza Audina;Safni, Safni;Jamarun, Novesar;Septiani, Upita;Kim, Moon-Kyung;Zoh, Kyung-Duk
    • Environmental Engineering Research
    • /
    • 제25권4호
    • /
    • pp.529-535
    • /
    • 2020
  • The present study investigated the photodegradation of synthetic organic dye; violet-3B, without and with the addition of C-N-codoped TiO2 catalyst using a visible halogen-lamp as a light source. The catalyst was synthesized by using a peroxo sol-gel method with free-organic solvent. The effects of initial dye concentration, catalyst dosage, and pH solution on the photodegradation of violet-3B were examined. The efficiency of the photodegradation process for violet-3B dye was higher at neutral to less acidic pH. The kinetics reaction rate of photodegradation of violet-3B dye with the addition of C-N-codoped TiO2 followed pseudo-first order kinetics represented by the Langmuir-Hinshelwood model, and increasing the initial concentration of dyes decreased rate constants of photodegradation. Photodegradation of 5 mg L-1 violet-3B dye achieved 96% color removal within 240 min of irradiation in the presence of C-N-codoped TiO2 catalyst, and approximately 44% TOC was removed as a result of the mineralization.

반도성 $BaTiO_3$ 세라믹스의 미세구조 및 PTCR 특성에 미치는 $Si_3N_4$ 첨가효과 (Effect of $Si_3N_4$ Addition on the Microstructure and PTCR Characteristics in Semiconducting $BaTiO_3$ Ceramics)

  • 김준수;정윤해;이병하
    • 한국세라믹학회지
    • /
    • 제31권10호
    • /
    • pp.1089-1098
    • /
    • 1994
  • The effect of Si3N4 addition on the microstructure and PTCR characteristics of BaTiO3 was studied. When 0.1 mol% Sb2O3-doped BaTiO3 codoped with Si3N4 (0.1, 0.25, 0.5, 0.75, and 1 wt%, respectively) were sintered, their microstructures were changed by the amount of the liquid phase as a result of eutectic reaction at 126$0^{\circ}C$. By these microstructural changes, the specific resistivity ratio($\rho$max/$\rho$min) with Si3N4 content variation of 0.1 mol% Sb2O3-doped BaTiO3 ceramics sintered at 130$0^{\circ}C$ for 1 hour varied between 3.70$\times$102(0.1 wt% Si3N4) to 1.16$\times$103 (1wt% Si3N4).