• 제목/요약/키워드: C-Cl activation

검색결과 203건 처리시간 0.021초

${\alpha}$-셀룰로오즈의 열분해에 관한 연구(I) - 산촉매 NaCl의 영향 - (Kinetics of Pyrolysis Degradation of on ${\alpha}-Cellulose$. - Effect of Acid Catalysts NaCl-)

  • 나상도;황준호;최경선;설수덕;손진언
    • Elastomers and Composites
    • /
    • 제31권2호
    • /
    • pp.122-129
    • /
    • 1996
  • The Thermal decomposition of the ${\alpha}-Cellulose$ and NaCl was studied using a thermal analysis technique in the steam of nitrogen gas with 30ml/min at various heating ranges from 4 to $20^{\circ}C/min$. The Derivative and Integral method used to be obtained values of activation energy of decomposition reaction. 1. The values of activation energy evaluated by Derivative and Intergral method were consistent with each other very well. 2. The maximum value of heat of decomposition evalated by DSC method was ${\alpha}-Cellulose/NaCl= 90/10$. 3. The thermogravimetric trace curve agreed with the theoretical equation.

  • PDF

Geometries and Energies of S$_N$2 Transition States$^\dag$

  • Lee, Ik-Choon;Kim, Chan-Kyung;Song, Chang-Hyun
    • Bulletin of the Korean Chemical Society
    • /
    • 제7권5호
    • /
    • pp.391-395
    • /
    • 1986
  • MNDO calculations were carried out to determine reactant complexes and transition states of the $S_N2$ reactions of $CH_3X\;+\;Y^-\;{\to}\;CH_3Y\;+\;X^-$ where X = F, Cl, CN and Y = CN, OH, F, Cl. The leaving group ability was found to vary inversely with the activation barrier, which in turn was mainly ascribable to the deformation energies accompanied with bond stretching of C-X bond and inversion of $CH_3$ group. The nucleophilicity was shown to be in the order $Cl^->F^->OH^->CN^-$ but the effect on the activation barrier was relatively small compared with that of the leaving group. The bond breaking and bond formation indices and energy decomposition analysis showed that the TS for the reaction of $CH_3$Cl occurs in the early stage of the reaction coordinate relative to that of $CH_3$F. It has been shown that the potential energy surface (PES) diagrams approach can only accommodate thermodynamic effects but fails to correlate intrinsic kinetic effects on the TS structure.

$K_2CoCl_4$ 단결정의 성장과 물리적 성질 (The crystal growth and physical properties of the single crystal $K_2CoCl_4$)

  • 김용근;안호영;정희태;정세영
    • 한국결정성장학회지
    • /
    • 제7권3호
    • /
    • pp.359-365
    • /
    • 1997
  • $K_2CoCl_4$ 단결정을 Ar분위기에서 Czochralski법으로 육성하였다. 육성된 결정의 물리적 성질의 조사로서 먼저 유전적 특성을 조사하여 commensurate-incommensurate(C-INC) 상전이에서 유전율의 thermal hysteresis가 $5^{\circ}C$ 이하의 값을 가짐을 보였고, incommensurate(INC) 상에서 $K^+$ 이온에 의한 ionic hopping mechanism으로 전도도를 해석하였으며 이때 activation energy는 0.62 eV 이었다. 각각의 결정축으로 열팽창을 조사하여 c축으로 가장 큰 열팽창을 보였으며 열팽창계수를 계산하였다. 광학적 특성의 조사로서 200 nm~ 3000 nm 영역에서 흡수 스펙트럼을 측정하여 나타나는 흡수 peak을 결정장내의 에너지 준위의 분리에 따른 전이 에너지로 해석하였으며, 800 nm~ 1200 nm 영역의 투과특성으로 optical band filter로서의 가능성을 제시하였다.

  • PDF

커피폐기물을 이용한 활성탄의 제조: ZnCl2-활성화 (The Preparation of Activated Carbon from Coffee Waste: ZnCl2-Activation)

  • 유상희;김학희
    • 공업화학
    • /
    • 제9권4호
    • /
    • pp.509-515
    • /
    • 1998
  • 커피폐기물을 원료로 하여 염화아연으로 화학적 활성화시켜 커피활성탄 (activated coffee char)을 제조하였다. 이 연구는 roasting과정, 탄화과정, 활성화, 그리고 수세 및 건조의 공정으로 수행되었다. Roasting 과정은 $300{\sim}400^{\circ}C$에서 10분간 수행되었다. 탄화과정의 적절한 조건은 $650^{\circ}C$에서 1시간인 것으로 나타났다. 화학적 활성화에 있어서 가장 중요한 parameter는 활성화제와 coffee char의 화학비인 것을 알 수 있었다. $N_2$ gas를 이용하여 77K에서 제조된 커피활성탄의 BET 비표면적과 BJH 세공용적을 측정하였다. 염화아연에 의해 활성화되어 제조된 coffee char의 비표면적이 $1110{\sim}1580m^2/g$로 분석되었으며 세공용적은 $0.51{\sim}0.81cm^3/g$로 각각 분석되었다. SEM은 세공과 coffee char의 표면관찰에 이용되었다. 분석결과, 활성화 표면과 많은 세공이 형성되어 있는 것을 보였다. 커피폐기물을 이용한 activated coffee char의 제조가 성공적으로 수행되었으며, 이는 폐기물을 이용한 자원 개발의 가능성을 보여주었다.

  • PDF

Kinetics and Mechanism of Substitution Reaction of $PPN^+(\eta^n-MeCp)Mn(CO)_2\;Cl^-$ with $PR_3$(R=Me, Et, OEt, $C_6H_5$)

  • 박용광;이용구;김규식
    • Bulletin of the Korean Chemical Society
    • /
    • 제17권2호
    • /
    • pp.138-142
    • /
    • 1996
  • The transition metal carbonylate, PPN+(${\eta}^5-MeCp)Mn(CO)_2Cl^-$ undergoes a novel ligand substitution reaction with PR3 (R=Me, Et, OEt, $C_6H_5$ in THF at elevated temperatures (40 $^{\circ}C$ up to 60 $^{\circ}C)$ under the pseudo-first-order reaction conditions (usually 20-fold excess of PR3 with respect to metal carbonylate concentrations) where chloride is displaced by PR3. The reaction follows overall first order dependence on [(${\eta}^5-MeCp)Mn(CO)_2Cl^-$]; however, the negative entropy changes of activation (${\Delta}S^{\neq}$=-19.3 e.u. for $P(OEt)_3$; ${\Delta}S^{\neq}$=-16.4 e.u. for $PPh_3$) suggest the existence of the intermediate, ((η3-MeCp)Mn(CO)2(THF)Cl-, which eventually transforms to the product (${\eta}^5-MeCp)Mn(CO)_2(PR_3)$.

무화과 펙틴에스테라제의 부분 정제 및 in situ 상태에서의 활성 특성 (Partial Purification of Fig Pectinesterase and Characterization of its in situ Activity)

  • 허원녕;김명화;고은경
    • 한국식품과학회지
    • /
    • 제30권5호
    • /
    • pp.1169-1178
    • /
    • 1998
  • 무화과 PE를 추출하여 ammonium sulfate로 분획 투석한 후 Q-Sepharose column 및 CM-cation exchanger column을 이용한 chromatography와 HPLC에 의해 1개의 음이온성 PE와 2개의 양이온성 PE로 분리되었으며, 이들은 모두 전기영동상에 분자량 27,000정도의 밀접한 두 개의 band로 나타난 부분 정제된 단백질이었다. 이 효소 단백질들은 보관 중에 활성을 급격히 상실되므로 현실적인 이용성을 고려하여 분말화한 시료 현탁액을 이용한 in situ PE의 특성을 조사하였다. 그 결과 분말 시료는 냉동 저장뿐 만 아니라 $5^{\circ}C$에서도 장기간 저장할 수 있었으며, 최적 pH는 8.5, 최적온도는 $50^{\circ}C$이였고, 활성화 에너지는 7,671 cal $mol^{-1}\;K^{-1}$ 이었으며 $55^{\circ}C$까지는 열 안정성을 유지하였다. 또한 $0.2{\sim}0.4$ M NaCl에서 활성이 촉진되었으며 PE의 용출은 0.8 M 이상의 NaCl 에서 효과적이였고 $0{\sim}1.0$ M NaCl까지의 범위에서는 특별히 안정성에 영향을 미치지 않았다.

  • PDF

중성염이 견의 반응염색에 미치는 영향(I) - 양이온의 영향- (Effect of Neutral Salts on the Reactive Dyeing of Silk(I) -Effect of Cations-)

  • 도성국;박찬헌;권지윤
    • 한국염색가공학회지
    • /
    • 제12권6호
    • /
    • pp.372-379
    • /
    • 2000
  • Four kinds of neutral salts with different cations, LiCl, NaCl, KCl, and CsCl, were added to the dye bath to accurately understand the effect of cations on the reactive dyeing of silk with C. I. Reactive Black 5. The cations of salts added lowered the negative surface potential of the silk, improving equilibrium adsorption and the accessibility of the dyestuff to the fiber greatly and speeding up the dyeing rate in the order of $Li^+>Na^+>K^+>Cs^+$. The activation energy$(E_a)$ for the dyeing was in the order of$Li^+>Na^+>K^+>Cs^+$ but the activation free energy$(\Delta{G}^*)$, or the real energy barrier for the reaction, was in the order of $Li^+>Na^+>K^+>Cs^+$ because the degree of the contribution of E$^{a}$ to the activation entropy$(\Delta{S}^*)$ was $Li^+>Na^+>K^+>Cs^+$. It was found from this result that LiCl had the strongest lowering effect on the negative surface potential of silk. The decrease in $\Delta{S}^*$ should be attributed to the loosely bonded activated complex of dyestufffs, cations and fiber molecules at transition state. It was clarified from the Bronsted equation that salts had the ionic strength effect and the specific salt effect on the reactive dyeing.

  • PDF

Cp-Ti와 Ti-6Al-4V 합금으로 제조된 치과용 임플란트의 부식특성에 관한 블라스팅과 산세처리의 영향 (Effects of Blasting and Acidic Treatment on the Corrosion Characteristics of Dental Implant Fabricated with Cp-Ti and Ti-6Al-4V Alloy)

  • 문영필;최한철;박수정;김원기;고영무
    • 한국표면공학회지
    • /
    • 제39권4호
    • /
    • pp.190-197
    • /
    • 2006
  • The effects of blasting and acidic treatment on the corrosion characteristics of dental implant fabricated with Cp-Ti and Ti-6Al-4V alloy have been researched by using electrochemical methods. The fabricated implants were cleaned and sandblasted by $Al_2O_3$ powder and then acidic treatment was carried out in nitric acid solution. The surface morphology were observed using scanning electron microscope. The corrosion behaviors were investigated using potentiosat and EIS in 0.9% NaCl solution at $36.5{\pm}1^{\circ}C$. The potentio-dynamic test in 0.9% NaCl indicated that the corrosion potential of blasting and acidic treated implant was lower than that of non treated implant, but current density was higher than that of non treated implant. From the cyclic potentiodynamic test results of Ti implant, the passivation current density of blasting and acidic treated implant slightly higher than that of non treated implant. From A.C. impedance test results in 0.9% NaCl solution, polarization resistance($R_p$) value of blasting and acidic treated implant was lower than that of non treated implant. In case of blasting and acidic treated implant surface, the pits were observed in valley and crest of implant surface.

마그네슘의 금속염 환원에 의한 초미립 탄화티탄 분말 합성거동 (Synthesis and kinetic of ultrafine titanium carbide particles by Mg-thermal reduction of liquid metal chlorides)

  • 이동원;백진호;김병기
    • 한국분말재료학회지
    • /
    • 제11권4호
    • /
    • pp.322-327
    • /
    • 2004
  • Ultrafine titanium carbide particles were synthesized by the reaction of liquid-magnesium and vaporized TiCl$_{4}$+C$_{x}$Cl$_{4}$(x = 1 and 2) solution. Fine titanium carbide particles with about 50 nm were successfully produced by combining Ti and C atoms released by chloride reduction of magnesium, and vacuum was then used to remove the residual phases of MgCl$_{2}$ and excess Mg. Small amounts of impurities such as O, Fe, Mg and Cl were detected in the product, but such problem can be solved by more precise process control. The lattice parameter of the product was 0.43267 nm, near the standard value. With respect to the reaction kinetics, the activation energy for the reactions of TiCl$_{4}$+C$_{2}$Cl$_{4}$and Mg was found to 69 kJ/mole, which was about half value against the use of TiCl$_{4}$+CCl$_{4}$, and such higher reactivity of the former contributed to increase the stoichiometry until the level of TiC$_{0.96}$ and decrease the free carbon content below 0.3 wt.%.

폐감귤박으로 제조한 활성탄에 의한 아세톤, 벤젠 및 메틸메르캅탄의 흡착특성 (Adsorption Characteristics of Acetone, Benzene, and Metylmercaptan by Activated Carbon Prepared from Waste Citrus Peel)

  • 감상규;강경호;이민규
    • 공업화학
    • /
    • 제28권6호
    • /
    • pp.663-669
    • /
    • 2017
  • 활성화제로 KOH, NaOH 및 $ZnCl_2$를 사용하여 폐감귤박으로부터 활성탄을 제조하였다. 최적조건(활성화제의 침적비율 300%, 활성화 온도 : KOH의 경우 $900^{\circ}C$, NaOH의 경우 $700^{\circ}C$, $ZnCl_2$의 경우 $600^{\circ}C$, 활성화 시간 1.5 h)에서 제조한 활성탄을 각각 ACK, ACN 및 ACZ로 명명하였다. 이들 활성탄을 사용하여 회분식 반응기에서 아세톤, 벤젠 및 메틸메르캅탄(MM) 등의 3가지 대상가스에 대한 흡착 특성을 검토하였다. 이들 활성탄에 의한 3가지 대상 가스의 흡착은 Langmuir 모델식보다는 Freundlich 모델식에 더 부합되는 것으로 나타났다. 그리고 흡착 속도실험결과는 유사 1차 속도식보다는 유사 2차 속도식에 잘 부합하였으며, 입자 내 확산 모델 결과는 흡착 과정에서 외부물질전달과 입자확산이 동시에 일어나는 것을 시사해 주었다.