The Influence of Vanadium Addition on Fracture Behavior and Martensite Substructure in a Ni-36.5at.%Al Alloy (Ni-36.5at.%Al 합금에서 V 첨가가 파괴거동 및 마르텐사이트 내부조직에 미치는 영향)

  • Kim, Young Do;Choi, Ju;Wayman, C. Marvin
    • Analytical Science and Technology
    • /
    • v.5 no.2
    • /
    • pp.203-211
    • /
    • 1992
  • Fracture behavior and martensite substructure of Ni-36.5at.%Al alloy were investigated with the addition of vanadium which is known as scavenging element of grain boundary. The fracture surfaces were examined by scanning electron microscopy and the EDX spectrometer was applied for composition analysis of fracture surfaces. The substructure of martensite was studied by transmission electron microscopy. By addition of vanadium, fracture surfaces show mixed modes of intergranular and transgranular fracture and more Al content is found on the grain boundaries. For Ni-36.5at.%Al alloy, the planar faults observed in the martensite plates are the internal twins. By increasing the vanadium content, the modulated structure with stacking faults and dislocations dominates while the twinned martensite disappears. The stacking fault is determined to be extrinsic due to the substitution of V for Al. It is concluded that the segregation of sulfur on the high-energy state stacking fault area suppresses the intergranular fracture.

  • PDF

PERFORMANCE OF FIMS MICROCHANNEL PLATE DETECTOR SYSTEM (FIMS의 마이크로채널 플레이트 검출기 시스템의 특성)

  • Nam, U.W.;Rhee, J.G.;Kong, K.N.;Park, Y.S.;Jin, K.C.;Jin, H.;Park, J.H.;Yuk, I.S.;Seon, K.I.;Han, W.;Lee, D.H.;Ryu, K.S.;Min, K.W.;Edelstein, J.;Korpela, E.
    • Journal of Astronomy and Space Sciences
    • /
    • v.19 no.4
    • /
    • pp.273-282
    • /
    • 2002
  • We describe some performance of the detector electronics system for the FIMS (Far-ultraviolet Imaging Spectrograph) mission. The FIMS mission to map the far ultraviolet sky uses MCP (micro-channel plate) detectors with a crossed delay line anode to record photon arrival events. FIMS has two MCP detectors, each with a ~25mm$\times$25mm active area. The unconventional anode design allows for the use of a single set of position encoding electronics for both detector fields. The centroid position of the charge cloud, generated by the photon-stimulated MCP, is determined by measuring the arrival times at both ends of the anode following amplification and external delay. The temporal response of the detector electronics system determines the readout's positional resolution for the charge centroid. High temporal resolution (<$35{\times}75$ps FWHM) and low power consumption (< 6W) were achieved for the FIMS detector electronics system.

Punching Shear Strength of the Void Transfer Plate (중공 전이 슬래브의 뚫림 전단 강도)

  • Han, Sang-Whan;Park, Jin-Ah;Kim, Jun-Sam;Im, Ju-Hyeuk;Park, Young-Mi
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.3
    • /
    • pp.367-374
    • /
    • 2010
  • The transfer slab system is a structural system that transfers the loads from the upper shear wall structure to the lower columns. This is a costly system due to a very thick slab, and the relatively high cost can be mitigated by introducing voids in the slab. However, this system of flat plate containing voids is vulnerable to brittle failure caused by punching shear in vicinity of slab-column connection. Thus, the punching shear capacity of the void system is very important. However, the current code doesn't provide a clear design provision for the strength of slabs with a void section. In this study, experimental study was conducted to investigate the punching shear strength of the void slab system. The shear strength of the specimens was predicted by current code and previous researches. In result, the punching shear strength of the void system is determined as the least value calculated at critical section located a distance d/2 from the face of the column and the center of the void section using the effective area at critical section.

A study on the residual stress at the weld joint of 2.25Cr-1.6W heat resistant steel (보일러용 배관재 2.25Cr-1.6W계 내열강의 용접부 응력 해석)

  • Lee, Y.S.;Lee, K.W.;Lee, J.B.;Kim, Y.D.;Kong, B.W.;Ryu, S.H.;Kim, J.T.;Kim, B.S.;Jang, J.C.
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.62-62
    • /
    • 2009
  • 석탄화력발전소의 CO2배출량 감소와 고효율, 대용량화로 인해 초초임계압(USC:Ultra Super Critical) 화력발전소의 건설이 증가하고 있다. USC 발전소는 효율향상을 위한 증기온도와 압력의 상승 때문에 보일러 고온고압부에 기존의 소재에 비해 고온강도와 내산화성의 재료물성이 향상된 신소재 적용이 불가피하다. 특히 사용된 신소재 중에서 보일러 본체를 구성하는 수냉벽관(Water wall), 과열기와, 재열기용 튜브 및 후육부인 헤더와 배관재로 기존의 2.25Cr-1Mo강을 개량한 2.25Cr-1.6W계 내열강이 적용되고 있다. 2.25Cr-1.6W강은 SMI와 MHI가 공동개발한 소재로 1995년 튜브제품이, 1999년에 단조, 파이프재, 플레이트제품이 ASME code case로 등재되었고, 2009년 ASME code case 2199-4로 개정되어 사용 중이다. 이 소재는 2.25Cr-1Mo강에 고온강도 개선을 위해 석출강화효과가 있는 V과 Nb을 첨가하였고, 탄화물의 열적안정성과 고용강화효과 증대를 위해 W을 첨가하였다. 그리고 제작성과 용접성 및 재료의 인성 향상을 위해 B첨가와 C함량을 낮추었다. 합금성분의 첨가와 조정에 의해 고온강도는 개선되었지만, 보일러 설치 및 보수를 위한 용접과정에서 용접금속과 CGHAZ(Coarse Grain HAZ)에서 용접균열이 발생하였다. 대부분의 용접균열은 용접결함이나 고온 혹은 저온균열이 아닌 2.25Cr-1.6W계강의 강도 개선을 위해 첨가한 V과 Nb이 용접후열처리 도중 입내에 MX형태의 미세석출로 입내를 강화시킴으로서 발생한 재열균열 민감성 증대에 기인된 것으로 판단된다. 이에 본 연구에서 용접 및 후열처리 과정에서 용접금속과 HAZ에서 발생하는 용접금속의 응력분포를 전산해석을 통해 확인하고 실제 후육파이프 용접부에서 잔류응력을 측정해 비교하였다. 용접부 응력분포는 SYSWELD 프로그램을 사용해 해석을 수행하였고, 발전소 실배관재의 용접부 응력측정은 수평부 측정이 용이하도록 지그를 부착한 Potable 잔류응력측정기를 사용해 Hole Drilling Method(HDM)를 적용하여 잔류응력을 측정하였다. 해석 결과 CGHAZ부위의 잔류응력이 용접금속과 기타 부위에 비해 높은 응력분포를 나타냈으며, 이는 CGHAZ와 용접용융선 부근에서 균열이 발생하는 실제값과 일치하는 결과를 보였다. 실제 배관재 용접부에서 측정한 잔류응력값은 항복응력의 약 50% 이하 응력값을 나타냈다. 배관 구조에 기인한 시스템응력의 영향을 제거하기 위해 배관재 용접부를 중심으로 양끝단을 절단 후 용접부에서 측정한 응력은 항복응력 대비 25%수준의 낮은값을 보였다. 그러나 배관재가 장기간 고온환경에 노출되었고 용접금속 내부의 균열이 발생한 상태에서 측정하였기 때문에 용접잔류응력은 상당부분 해소되어 상대적으로 낮은 응력값이 얻어진 것으로 판단된다.

  • PDF

Numerical Study on the Effect of the Arrangement Type of Rotor Sail on Lift Formation (로터세일의 배열 형태가 양력 형성에 미치는 영향에 관한 수치해석적 연구)

  • Jung-Eun Kim;Dae-Hwan Cho;Chang-Yong Lee
    • Journal of the Korean Society of Marine Environment & Safety
    • /
    • v.29 no.2
    • /
    • pp.197-206
    • /
    • 2023
  • Recently, the international community, including the International Maritime Organization (IMO), has strengthened regulations on air pollution emissions of ships, and eco-friendly ships are actively being developed to reduce exhaust gas emissions. Among them, rotor sail (RS), a wind-assisted ship propulsion system, is attracting attention again. RS is a cylindrical device installed on the ship deck, that generates hydrodynamic lift using a magnus effect. This is a next generation eco-friendly auxiliary propulsion technology, and Enercon company, which developed RS-applied ships, announced that fuel savings of more than 30% are possible. In this study, optimal installation conditions such as RS spacing and arrangement type were selected when multiple RSs were installed on ships. AR=5.1, SR=1.0, and De/D was fixed at 2.0 according to the RS arrangement, and the wind direction was considered only for the unidirectional +y-axis. Regarding arrangement conditions, five conditions were set at 3D intervals in the +x-axis direction from 3D to 15D and five conditions in the +y-axis direction from 5D to 25D. CL, CD and aerodynamic efficiency (CL/CD) were compared according to the square(□) and diamond(◇) shape arrangements. Consequently, the effect of RS on the longitudinal distance was not significantly different. However, in the case of RS flow characteristics according to the transverse distance, the interaction effect of RS was the greatest when the two RSs almost matched the wind direction. In the case of the RS flow characteristics according to the arrangement, notably, when the wind blew in the forward (0°) direction, the diamond (◇) arrangement was least affected by the backward flow between RSs.

An effect of immediate orthodontic force on palatal endosseous appliance$(C-Palatal\;Plate^{TM})$ in beagle Dog (성견 구개부 골내고정원 장치에 가해진 즉시 교정력이 주위조직에 미치는 영향)

  • Kim, Su-Jung;Lee, Young-Jun;Chug, Kyu-Rhim
    • The korean journal of orthodontics
    • /
    • v.33 no.2 s.97
    • /
    • pp.91-102
    • /
    • 2003
  • This study was performed to investigate the effect of immediate orthodontic force on soft md hard tissues surrounding C-Palatal $Plate^{TM}$ in beagle Dog. Immediately after this appliance was implanted on the midpalate of 4 adult beagle Dogs, 400gm continuous orthodontic force was applied. Experimental animals were euthanized at 8weeks, 18weeks, and 22weeks (including post-removal healing time of 4weeks), and a control animal was euthanized at 8weeks after implantation without orthodontic force application. The appliance and the surrounding tissue were studied radiographically, macroscopically, and histologically. The results were as follows: 1. The lateral radiographs taken after euthanasia showed very slight displacement of the vortical plate in the experimental animals, compared with the control animal. Mobility test of all animals confirmed primary stability without any increase of mobility during experimental period. 2. No pathologic changes were found in the healing condition of covering soft tissue and bone-screw interface in experimental animals as well as a control animal. 3. Osseointegration was achieved in the bone-screw interface in 8weeks after implantation and the amount of osseointegration increased in 18weeks. There was little difference of osseointegration between the compression side and the tension side. 4. In the marginal bone area, slight bone apposition and resorption were found regardless of compression and tension side, while there was no change in the control animal. 5. Both 8week-animal and 18week-animal showed the new bone apposition along the surface of screws which were perforated into the nasal cavity, while the control animal showed no change. 6. After 4weeks of plate removal, the covering epithelium was repaired intactly, while the connective tissue showed loose and irregular rearrangement and the connective tissue capsule remained. The C-Palatal $Plate^{TM}$ manifested sufficient anchorage capacity in the context of histological study as well as clinical outcomes, when immediate orthodontic force was applied after implantation.

A Damage Measurement of Steel Beam using PZT Sensor (PZT센서를 이용한 철골보 손상계측)

  • Seo, Hye-Won;Park, Min-Suk;Lee, Swoo-Heon;Shin, Kyung-Jae
    • Journal of Korean Society of Steel Construction
    • /
    • v.22 no.5
    • /
    • pp.477-485
    • /
    • 2010
  • Various monitoring sensors are used to predict and detect structural damage. Smart sensors, such as glass-fiber sensors, PZT, and MEMS, among others, have replaced traditional sensors. They are now being used in many areas. This study aims to predict the damage by measuring the PZT voltage attached on the specimen by the applied impact load. In the experiment to detect damages in beam connection, simple $H-400{\times}200{\times}8{\times}13$ beams were spliced with bolts. The results of FFT between PZT sensor and accelrometer were compared to measure the sensitivity of the PZT sensor. The damage to the beam was presumed by loosening the bolt, and then the damage measurement was accompanied. Secondly, a steel $PL600{\times}65{\times}5.8$ plate beam was fabricated for the purpose of experimenting on damage measurement. Impact loading test on three different locations was carried out. Damage width varied between 6~42mm on both sides by cutting, using a steel saw. The ratio of frequencies before and after the damage was computed to quantify the damage level by using FFT, and the change in mode pattern with the increased damage was investigated to measure the damage.

Site-Specific Recombination by the Integrase MJ1 on Mammalian Cell (동물 세포 내에서 MJ1 인티그라제에 의한 부위 특이적 재조합)

  • Kim, Hye-Young;Yoon, Bo-Hyun;Chang, Hyo-Ihl
    • Microbiology and Biotechnology Letters
    • /
    • v.39 no.4
    • /
    • pp.337-344
    • /
    • 2011
  • Integrase MJ1 from the bacteriophage ${\Phi}FC1$ carries out recombination between two DNA sequences (the phage attachment site, attP and the bacterial attachment site, attB) in NIH3T3 mouse cells. In this study, the integration vector containing attP, attB and the integrase gene MJ, was constructed. The integration mediated by integrase MJ1 in Escherichia coli led to excision of LacZ. Therefore, the frequency of integration was measured by the counting of the white colony, which is detectable on X-Gal plates. The extrachromosomal integration in NIH3T3 mouse cells was monitored by the expression of the green fluorescent protein (GFP) as a reporter. To demonstrate integration mediated integrase MJ1 in NIH3T3 cells, vectors containing attP and attB were co-transfected into NIH3T3 cells. The integration was confirmed by fluorescent microscopy. The expression of GFP was induced in NIH3T3 cells expressing MJ1 without accessory factors. By contrast, the excision mediated by the MJ1 between attR and attL had no effect on the expression of GFP. These results suggest that integrase MJ1 may enable a variety of genomic modifications for research and therapeutic purposes in higher living cells.

The effect of heat input and PWHT on the mechanical properties and microstructure of HSB600 steel weldments with GMAW (HSB600강 가스메탈아크용접부에서 입열량과 용접후 열처리가 기계적 특성과 미세조직에 미치는 영향)

  • Ju, Dong-Hwi;Jang, Bok-Su;Lim, Young-Min;Koh, Jin-Hyun
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.13 no.5
    • /
    • pp.1939-1946
    • /
    • 2012
  • High performance steel for bridges requires higher performance in tensile and yield strength, toughness, weldability, etc. The purpose of this study is to investigate the weldability of HSB 600 steel. The effects of heat input (1.4~3.2kJ/mm) and postweld heat treatment (PWHT, $600^{\circ}C$, 40hr.) on the TMCP HSB600 steel weldments made by GMAW process were investigated. The tensile strength and hardness of as-welded specimens decreased with increasing heat input. Charpy V-notch impact energy did not show any significant difference by postweld heat treatment. The fine-grained acicular ferrite was mainly formed in the 2.1kJ/mm of heat input while polygonal and side plate ferrites were dominated in the high inputs. Meanwhile, tensile strength and hardness of PWHT weldments decreased due to the coarsening and globularization of ferrite microstructure and reduction of residual stresses with increasing heat inputs. However, there was no significant difference in the impact energy absorption.

단일벽 탄소나노튜브의 직경 분포에 미치는 합성 템플레이트 및 공정변수의 영향

  • Gwak, Eun-Hye;Yun, Gyeong-Byeong;Jeong, Gu-Hwan
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.08a
    • /
    • pp.250-250
    • /
    • 2013
  • 단일벽 탄소나노튜브(Single-walled nanotubes, SWNTs)는 나노스케일의 크기와 우수한 물성으로 인하여, 전자, 에너지, 바이오 분야로의 응용이 기대되고 있다. 특히 SWNTs의 직경을 제어하게 되면 튜브의 전도성 제어가 훨씬 수월하게 되어, 차세대 나노전자소자의 실현을 앞당길 수 있으며 이러한 이유로 많은 연구들이 현재 행해지고 있다. SWNTs의 직경제어 합성을 위해서는 현재 열화학기상증착법(Thermal chemical vapor deposition; TCVD)이 가장 일반적으로 이용되고 있으며, 합성 촉매와 합성되는 튜브의 직경과의 크기 연관성이 알려진 후로는, 촉매의 크기를 제어하여 SWNTs의 직경을 제어하고자 하는 연구들이 활발하게 보고되고 있다. 특히, 촉매 나노입자의 직경이 1~2 nm 이하로 감소될 경우, SWNTs의 직경 분포가 어떻게 변화할 것인지가 최근 가장 중요한 관심사로 남아 있으나, 이러한 크기의 금속입자는 나노입자의 융점저하 현상이 발현되는 영역이므로, SWNTs의 합성온도 영역에서 촉매 금속입자는 반액체(Semi-liquid) 상태로 존재할 것으로 추측하고 있다. 본 연구에서는 고온의 SWNTs 합성환경에서 금속나노촉매의 유동성을 제한하기 위하여 나노사이즈의 기공이 규칙적으로 정렬된 다공성 물질인 제올라이트를 촉매담지체로 이용하였고, 이 때 다양한 합성변수가 SWNTs의 직경에 미치는 영향을 살펴보고자 하였다. SWNTs의 합성을 위해 실리콘 산화막 기판 위에 제올라이트를 도포한 후, 합성 촉매로서 전자빔증발법을 통하여 수 ${\AA}$에서 수 nm 두께의 철 박막을 증착하였다. 합성은 메탄을 원료가스로 하여 TCVD법으로 실시하였다. 주요변수로는 제올라이트 종류, 증착하는 철 박막의 두께, 합성온도를 설정하였으며, 이에 따라 합성된 SWNTs의 합성수율 및 직경분포의 변화를 체계적으로 살펴보았다. SWNTs의 전체적인 합성수율의 변화는 SEM 관찰결과를 이용하였으며, SWNTs의 직경은 AFM 관찰 및 Raman 스펙트럼의 분석에서 도출하였다. 실험결과, 제올라이트 종류에 따라서는 명확한 튜브직경 분포의 변화 없이 비교적 좁은 직경분포를 갖는 SWNTs가 합성되었으며, 합성온도가 $850^{\circ}C$ 이하로 감소되면 합성수율이 현저히 감소되는 것을 알 수 있었다. 촉매박막의 두께가 1 nm 이상인 경우에서는 직경 5 nm 전후의 나노입자가 형성되었으며, 이때 SWNTs의 합성수율은 높았으나 다양한 직경의 튜브가 합성이 된 것을 확인할 수 있었다. 반면, 촉매입자의 크기가 2 nm 이하에서는 합성수율은 다소 저하되었으나, SWNTs의 직경분포의 폭이 상대적으로 훨씬 좁아지는 것을 알 수 있었다. 추후, 극미세 촉매와 저온합성 환경에서의 합성수율 향상을 위한 합성공정의 개량이 지속적으로 요구된다.

  • PDF