• Title/Summary/Keyword: Brazing alloy

Search Result 106, Processing Time 0.023 seconds

Friction Welding of Dissimilar Hot Die Punch Materials and Its Creep Prediction and Quality Evaluation by AE(I) - FRW and AE+ (열간 금형펀치 제작을 위한 이종재 마찰용접과 고온크리프 실시간 예측 및 AE에 의한 품질평가(Ⅰ) -마찰용접과 AE)

  • Park, Il-Dong;Oh, Sae-Kyoo;Kim, Ji-Su
    • Journal of Ocean Engineering and Technology
    • /
    • v.13 no.3 s.33
    • /
    • pp.77-82
    • /
    • 1999
  • The compleete joining method for dissimilar hot die punch materials and its real-time evaluation method are not available at present. Brazing method has been used for joining them, but it is known that the welded joint by the brazing has the lower bonding efficiency and reliability than the diffusion welding. The friction wleding with a diffusion mechanism in bonding was applied in this study. So, this work was carried out to determine the optimal friction welding conditions and to analyze mechanical properties of friction welded joints of hot die punch materials (STD61 for the blade part of hot die punch) to alloy steel (SCM440 for the shank park of hot die punch) such as plunger. In addition, acoustic emission test was carried out during friction welding to evaluate the weld quality.

  • PDF

Effects of Drawing Parameters on Mechanical Properties of BAS121 Alloy Tubes for Heat-exchangers by High Frequency Induction Welding (고주파유도용접된 열교환기용 BAS121합금튜브의 기계적 특성에 미치는 인발조건의 영향)

  • Han Sang-Woo;Kim Byung-Il;Lee Hyun-Woo;Chon Woo-Young;Gook Jin-Seon
    • Korean Journal of Materials Research
    • /
    • v.14 no.12
    • /
    • pp.851-856
    • /
    • 2004
  • The aim of this study is to investigate the optimum drawing parameter for BAS121 welded tubes. The BAS121 aluminium alloy tubes with 25 mm in external diameter and 1.3 mm in thickness for heat-exchangers were manufactured by high frequency induction welding with the V shaped convergence angle $6.5^{\circ}$ and power input 55 kW. With increasing the reduction of area ($13,\;21\%$) by drawing, tensile strength was increased and elongation was decreased. With increasing the reduction of area by drawing, hardness in weld metal increased rapidly, while that of base metal increased slowly. In the specimen with the outer diameter smaller than 22 mm, hardness of weld metal was higher than that of base metal. The optimum drawing parameter of area reduction in BAS121 alloys was estimated about $13\%$ because of the work hardening of welds.

Brazing characteristics of $ZrO_2$ and Ti-6Al-4V brazed joints with increasing temperature (브레이징 온도 변화에 따른 $ZrO_2$와 Ti-6Al-4V의 접합 특성)

  • Kee, Se-Ho;Park, Sang-Yoon;Heo, Young-Ku;Jung, Jae-Pil;Kim, Won-Joong
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.50 no.3
    • /
    • pp.169-175
    • /
    • 2012
  • Purpose: In this study, brazing characteristics of $ZrO_2$ and Ti-6Al-4V brazed joints with increasing temperature were investigated. Materials and methods: The sample size of the $ZrO_2$ was $3mm{\times}3mm{\times}3mm$ (thickness), and Ti-6Al-4V was $10mm(diameter){\times}5mm(thickness)$. The filler metal consisted of Ag-Cu-Sn-Ti was prepared in powder form. The brazing sample was heated in a vacuum furnace under $5{\times}10^{-6}$ torr atmosphere, while the brazing temperature was changed from 700 to $800^{\circ}C$ for 30 min. Results: The experimental results shows that brazed joint of $ZrO_2$ and Ti-6Al-4V occurred at $700-800^{\circ}C$. Brazed joint consisted of Ag-rich matrix and Cu-rich phase. A Cu-Ti intermetallic compounds and a Ti-Sn-Cu-Ag alloy were produced along the Ti-6Al-4V bonded interface. Thickness of the reacted layer along the Ti-6Al-4V bonded interface was increased with brazing temperature. Defect ratios of $ZrO_2$ and Ti-6Al-4V bonded interfaces decreased with brazing temperature. Conclusion: Thickness and defect ratio of brazed joints were decreased with increasing temperature. Zirconia was not wetting with filler metal, because the reaction between $ZrO_2$ and Ti did not occur enough.

Effect of Sn Addition on Microstructure of Al Alloy Powder for Brazing Process (브레이징용 Al 합금 분말의 미세조직에 미치는 Sn 함량의 영향)

  • Kim, Yong-Ho;Yoo, Hyo-Sang;Na, Sang-Su;Son, Hyeon-Taek
    • Journal of Powder Materials
    • /
    • v.27 no.2
    • /
    • pp.139-145
    • /
    • 2020
  • The powder manufacturing process using the gas atomizer process is easy for mass production, has a fine powder particle size, and has excellent mechanical properties compared to the existing casting process, so it can be applied to various industries such as automobiles, electronic devices, aviation, and 3D printers. In this study, a modified A4032-xSn (x = 0, 1, 3, 5, and 10 wt.%) alloy with low melting point properties is investigated. After maintaining an argon (Ar) gas atmosphere, the main crucible is tilted; containing molten metal at 1,000℃ by melting the master alloy at a high frequency, and Ar gas is sprayed at 10 bar gas pressure after the molten metal inflow to the tundish crucible, which is maintained at 800℃. The manufactured powder is measured using a particle size analyzer, and FESEM is used to observe the shape and surface of the alloy powder. DSC is performed to investigate the change in shape, according to the melting point and temperature change. The microstructure of added tin (Sn) was observed by heat treatment at 575℃ for 10 min. As the content of Sn increased, the volume fraction increased to 1.1, 3.1, 6.4, and 10.9%.

The Metallization of Diamond Grits

  • Sung, James-C.;Hu, Shao-Chung;Chang, Yen-Shuo
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1134-1135
    • /
    • 2006
  • A revolutionary "Active Braze Coated Diamond" (ABCD) has been developed for bonding diamond grits firmly in the metal matrix. The molten braze is wetted and reacted with diamond to form strong chemical bond at the interface so that the diamond does not become knocked out of tools. The ABC is a nickel alloy that can form metallurgical diffusion bondswith the metal matrix. In essence, ABCD turns diamond into a metal grain so that the diamond tools can be made by conventional powder metallurgical process without being concerned about the poor bonding between matrix metal powder and the diamond as before.

  • PDF

Analysis of the Fume Generation Rates in the Flux Cored Arc welding

  • Chae, H.B.;Kim, J.H.;Yang, S.C.
    • International Journal of Korean Welding Society
    • /
    • v.1 no.1
    • /
    • pp.71-77
    • /
    • 2001
  • The characteristics of the fume generation in a flux cored arc welding were investigated using the fume collection chamber developed. The Korean Standard concerning the method for the evaluation of the fume generation rate(FGR) was updated by the evaluation method obtained through this study. It was found that the effect of humidity in the test environment should be considered and the automatic welding method had to be employed for the purpose of the exact evaluation of the fume generation rate. The results showed that the fume generation rate was influenced by the welding parameters. The important factors were the welding current arc voltage, travel speed, and contact tip to work distance(CTWD) that affected the heat input as well as the torch angle and the shielding gas flow rate that influenced the shielding effect. The fume generation rate increased as the heat input increased and the shielding effect decreased. It was also observed that the effect of the welding current is much grater than the other welding parameters.

  • PDF

Design Study of a Brazed Plate Heat Exchanger Condenser Through Two-Phase Flow Analysis (이상유동 해석을 통한 브레이징 판형 응축기 설계 연구)

  • Hwang, Dae-jung;Oh, Cheol;Park, Sang-kyun;Jee, Jae-hoon;Bang, Eun-shin;Lee, Byeong-gil
    • New & Renewable Energy
    • /
    • v.18 no.2
    • /
    • pp.73-81
    • /
    • 2022
  • This study was aimed at designing a condenser, as a component of the organic Rankine cycle system for ships. The condenser was manufactured through press molding to achieve a bent shape to enhance the heat transfer performance, considering the shape of the heat transfer plate used in a brazing plate heat exchanger. The heat transfer plate was made of copper-nickel alloy. The required heat transfer rate for the condenser was 110 kW, and the maximum number of layers was set as 25, considering the characteristics of high-temperature brazing. Computational fluid dynamics techniques were used to perform the thermal fluid analysis, based on the ANSYS CFX (v.18.1) commercial program. The heat transfer rate of the condenser was 4.96 kW for one layer (width and length of 0.224 and 0.7 m, respectively) of the heat transfer exchanger. The fin efficiency pertaining to the heat transfer plate was approximately 20%. The heat flow analysis for one layer of the heat exchanger plate indicated that the condenser with 25 layers of heat transfer plates could achieve a heat transfer rate of 110 kW.

A Study on the Characteristics for High Frequency Induction Heating of Ti Alloy Groove Wire (안경테용 Ti 합금 홈선의 고주파유도가열처리에 따른 특성 변화에 관한 연구)

  • Park, Jeong-Sik;Jang, Woo-Yeong;Lee, Jeong-Yeong
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.12 no.3
    • /
    • pp.55-58
    • /
    • 2007
  • Titanum and its alloys have been used as the important materials of eyewear frame due to its light weight, mechanical strength and corrosion resistance. This study investigates hardness and microstructures of titanum alloy groove wires in according with heating time by high frequency induction heating. Because of increase of grain size by the growth of heating time, hardness of ${\beta}-Ti$ has reduced. Hardness of Ti-325 reduced until 2 sec and rapidly increased at 3 sec by high frequency induction heating. It is observed that hardness of Ti-325 reduces by the increase of the grain size until 2 sec and suddenly increased by the development of the detailed ${\alpha}+{\beta}$ lamella at 3 sec.

  • PDF

Structure design of regenerative cooling chamber of liquid rocket thrust chamber (액체로켓 연소기 재생냉각 챔버 구조설계)

  • Ryu, Chul-Sung;Choi, Hwan-Seok;Lee, Dong-Ju
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.33 no.12
    • /
    • pp.109-116
    • /
    • 2005
  • Elastic-plastic structural analysis for regenerative cooling chamber of liquid rocket thrust chamber is performed. Uniaxial tension test is also conducted for the copper alloy in order to get material data necessary for the structure analysis. The results of uniaxial tension test reveal that copper alloy become ductile after brazing process and flow stress becomes lower as temperature becomes higher. As a result of structural analysis using the material data, the deformation of cooling channel is more increased by thermal load than by internal pressure of cooling fluid. Therefore, the results of analysis show that structural stability and cooling performance of combustion thrust chamber which is designed to endure mechanical load and minimized a channel thickness are improved by decreased thermal load as possible.

Properties of Friction Welding of Dissimilar Metals WCu-Cu Weld for Electrical Contact Device (전기접점용 이종금속 WCu-Cu 접합재의 마찰압점 특성)

  • An, Yong-Ho;Yun, Gi-Gap;Min, Taek-Gi;Han, Byeong-Seong
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.49 no.4
    • /
    • pp.239-245
    • /
    • 2000
  • A copper-tungsten sintered alloy(WCu) has been friction-welded to a tough pitch copper (Cu) in order to investigate friction weldability. The maximum tensile strength of the SWu-Cu friction welded joints had cp to 96% of those of the Cu base metal under the condition of friction time 0.6sec, friction pressure 45MPa, upset pressure 125MPa and upset time 5.0sec. And it is confirmed that the tensile strength of friction welded joints are influenced highly by upset pressure rather than friction time. And it is considered that mixed layer was formed in the Cu adjacent side to the weld interface, W particles included in mixed layer induced fracture in the Cu adjacent side to the weld interface and also, thickness of mixed layer was reduced as upset pressure increase.

  • PDF