• 제목/요약/키워드: Borosilicate glasses

검색결과 47건 처리시간 0.022초

Characteristics of Carbon Tetrafluoride Plasma Resistance of Various Glasses

  • Choi, Jae Ho;Han, Yoon Soo;Lee, Sung Min;Park, Hyung Bin;Choi, Sung Churl;Kim, Hyeong Jun
    • 한국세라믹학회지
    • /
    • 제53권6호
    • /
    • pp.700-706
    • /
    • 2016
  • Etch rate, surface roughness and microstructure as plasma resistance were evaluated for six kinds of oxide glass with different compositions. Borosilicate glass (BS) was found to be etched at the highest etch rate and zinc aluminum phosphate glass (ZAP) showed a relatively lower etch rate than borosilicate. On the other hand, the etching rate of calcium aluminosilicate glass (CAS) was measured to be similar to that of sintered alumina while yttrium aluminosilicate glass (YAS) showed the lowest etch rate. Such different etch rates by mixture plasma as a function of glass compositions was dependent on whether or not fluoride compounds were formed on glass and sublimated in high vacuum. Especially, in view that $CaF_2$ and $YF_3$ with high sublimation points were formed on the surface of CAS and YAS glasses, both CAS and YAS glasses were considered to be a good candidate for protective coating materials on the damaged polycrystalline ceramics parts in semi-conductor and display processes.

분광계에 의한 Borosilicate계 글라스의 조성 및 온도의존성 평가 (Composition and Temperature Dependence of Structural Changes in Borosilicate Glasses by Spectrometer)

  • 박성제;류봉기
    • 한국재료학회지
    • /
    • 제15권12호
    • /
    • pp.786-790
    • /
    • 2005
  • We investigated the particularity of temperature and composition changes in $xNa_2O{\cdot}(52.5-x)B_2O_3{\cdot}47.5SiO_2$ glasses by use of FT-IR, $^{11}B$ NMR, Raman spectrometer. From FT-IR and $^{11}B$ NMR spectrometer, we thought that tetrahedral boron, $BO_4$ units are created $N_4$ increasing tendency generated near $600^{\circ}C$. It's expected that composition ana heat treatment directly contributed to structural changes, this changes are following to $Na_2O$ increasing or decreasing. caused by $N_4\;and\;BO_4$ units are caused by relatively increasing or decreasing in the glasses' structure. Particularly, $BO_4$ units are converted to $BO_3$ units after $600^{\circ}C$ heat treatment for 50h in the composition of $x<18(R<0.5,\;R=Na_2O/B_2O_3\;mol\%)$. On the order hand, $BO_3$ units are converted to, $BO_4$ units after $600^{\circ}C$ heat treatment for 50h in the composition of $x{\geq}18\;(R>0.5)$. This particularity of composition and temperature dependence of structural changes are similarly represented by Raman analysis results.

Effect of SiO2/B2O3 ratio on Li ion conductivity of a Li2O-B2O3-SiO2 glass electrolyte

  • Kim, Young Han;Yoon, Mi Young;Lee, Eun Jung;Hwang, Hae Jin
    • Journal of Ceramic Processing Research
    • /
    • 제13권spc1호
    • /
    • pp.37-41
    • /
    • 2012
  • A lithium ion conducting borosilicate glass was fabricated by a conventional melt quenching technique from a mixture of Li2CO3, B2O3 and SiO2 powders. The Li ion conductivity of the lithium borosilicate glasses was evaluated in terms of the SiO2/B2O3 ratio. In the Li2O-B2O3-SiO2 ternary glass, the glass forming region decreases with an increasing Li2O content. At the same Li2O, the crystallization tendency of the glass samples increases with the SiO2/B2O3 ratio, resulting in a reduced glass forming region in the Li2O-B2O3-SiO2 ternary glass. The electrical conductivity moderately depends on the SiO2/B2O3 ratio in the Li2O-B2O3-SiO2 ternary glass. The conductivity of the glasses slightly increases with the SiO2/B2O3 ratio. The observed phenomenon can be explained by the modification of the glass structure as a function of the SiO2 content.

$Tb^{3+}$를 첨가한 Borosilicate 유리속에서 일어나는 에너지 전달과 Cross-Relaxation (Energy Transfer and Cross-Relaxation in $Tb^{3+}$-doped Borosilicate Glasses)

  • 김중환;문병기;오학태;김학수;윤수인;서효진;설정식
    • 한국광학회지
    • /
    • 제1권2호
    • /
    • pp.149-154
    • /
    • 1990
  • $Tb^{3+}$이온을 첨가한 borosilicate 유리속에서 일어나는 에너지전달을 연구하기 위하여 $Tb^{3+}$이온의 농도에 따른 형광방출의 세기 및 $^5D_3$$^5D_4$ 준위의 형광수명시간을 측정.분석하였다. $Tb^{3+}$이온농도가 증가하면 cross-relaxation에 의해 $^5D_3$ 준위의 상태밀도가 줄어드는 대신에 $^5D_4$ 준위의 상태밀도가 증가했다. 그리고 이 상호작용은 전기 쌍극자-전기쌍극자 상호작용이며 임계작용거리는 13$\AA$이었다. 또 5D4 형광방출을 소광시키는 원인이 되는 $^5D_4$$\longrightarrow$$^5D_4$형의 에너지전달은 그 임계작용거리가 3.5$\AA$으로 나타났다.

  • PDF

귀금속(금, 은)-유리계의 젖음성과 부착성 (Wettability and Adhesion of Noble Metal (Au, Ag)-Glass Systems)

  • 김종희
    • 한국세라믹학회지
    • /
    • 제32권4호
    • /
    • pp.405-412
    • /
    • 1995
  • In order to estimate the wettability of the borosilicate glasses with different composition on the noble metals of gold and silver, the measurements of the contact angle between the solid and the liquid were made at various temperatures and holding times using the sessil-drop method. The wetting behavior and the adhesion of the phases were strongly influenced by the thermal or the physical characteristics of the materials. The dependence of wetting angle ($\theta$) on the holding time (t) could be represented by the relation of $\theta$=a.tb, whereby the wettability of the systems was quantitatively compared. Also with increasing content of borosilicate glass in the glass-gold matrix composite, the tensile strength was decreased whereas the elastic modulus was increased.

  • PDF

핵폐기용 모의글라스의 조성변화에 따른 용출특성에 관한 연구 (Study on the Leaching Characteristics of Simulated Nuclear Waste Glass with variable Composition)

  • 한호현;이승한;류수착;류봉기
    • 한국표면공학회지
    • /
    • 제28권5호
    • /
    • pp.259-266
    • /
    • 1995
  • In order to manufacture an attractive waste glass for the permanent and secure disposal of high-level radioactive waste, the complex composition of the simulated nuclear waste glass PNL-7668 was simplified to a composition of sodium borosilicate glass. The substitutions of $Fe_2O_3$ and $Al_2O_3$ were added to examine on the leaching characteristics of simulated nuclear waste glass with variable composition. The leach tests for these glasses were performed according to 'MCC-1, Static Leach Test Procedure' in acid and basic solution. In this study, for the $Al_2O_3$-containing glasses, Na ion release from these glasses was higher in acid solution than in basic solution. As the content of $Fe_2O_3$ was increased in glasses, Na ion release was increased in acid solution, in spite of decrease of amount of total mass diminution.

  • PDF

산화알루미늄의 치환에 따른 붕규산 유리의 분상 미 이온교환성에 관한 연구 (Ion Exchange Capacity and Phase Separation of Alkali Borosilicate Glass by Substituting $Al_2O_3$)

  • 김병호;유영문
    • 한국세라믹학회지
    • /
    • 제21권1호
    • /
    • pp.41-50
    • /
    • 1984
  • The ion-exchange porous glasses were prepared by heat treating and subsequently acid treating the (95-y) $SiO_2$.$yB_2O_3$.$5Na_2O+xAl_2O_3$ glasses with y=55, 45, 35, 25. mole% and x=0, 2, 5, 9 mole% It was then investigated how the cation exchange capacity was affected by the phase separation in these glasses. For that matter such quantities as alkali extraction amount pore volume and specific surface area of the glasses were measured. The phase separation in these glasses was in general suppressed by the addition of $Al_2O_3$ maximally around the composition of 5 mole% $Al_2O_3$ This may be because the micro-phase separation prevailed in the glass of that composition over the macro-phase separation increasing thereby the specific surface area as well as the residual amount Al of after acid-treatment and accordingly the cation exchange capacity. The maximum values of the cation exchange capacity was observed to be about 150meq/100g for the glasses of (40-50) $SiO_2$ (55~45)$yB_2O_3$. $5Na_2O+5Al_2O_3$.

  • PDF

Zinc borosilicate 유리의 CaO 첨가에 따른 항균력 개선 효과 검증 (Effect of CaO on the antibacterial property of zinc borosilicate glasses)

  • 황민성;정재엽
    • 한국결정성장학회지
    • /
    • 제33권5호
    • /
    • pp.187-190
    • /
    • 2023
  • 본 연구에서는 ZnO-Na2O-B2O3-SiO2 계 유리에 CaO의 첨가에 따른 유리의 열적, 화학적 특성, 표면 제타전위 및 항균특성을 분석하였다. 유리 조성에 따른 열적 특성은 DTA 분석을 통해 확인하였고, 30ZnO-xCaO-20Na2O-30B2O3-(20-x)SiO2 (x = 0, 2, 4, 6, 8, 10 mol%)계 유리에서 CaO 함량이 증가함에 따라 유리전이온도가 줄어드는 것을 확인하였다. CaO 함량이 늘어날수록 유리 구조가 약화됨에 따라 더 많은 Zn2+ 이온이 용출되었고, 알칼리 및 알칼리 토류의 초기 급속한 용출로 인해 유리의 표면 제타전위가 증가함을 확인하였다. 이러한 이유로 유리의 항균활성 또한 급격하게 개선됨을 확인하였으며, 대장균(gram negative)과 황색포도상구균(gram positive) 모두에 대해 99.9 % 항균 활성을 갖는 항균 유리를 개발할 수 있었다.

Compositional Effects on Thermal and Electrical Properties of Dielectric Glass Paste

  • Kim, Teock-Nam;Lee, Jea-Yeol;Kim, Hyung-Sun;Hu, Jeung-Soo
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2000년도 제1회 학술대회 논문집
    • /
    • pp.95-96
    • /
    • 2000
  • The effect of $Al_2O_3$ on the dielectric constant and the coefficient of thermal expansion of lead borosilicate glasses for the application of PDP glass paste was investigated. Measurements were made theoretically by using empirical equations on the composition of the of glasses in which the $PbO/Al_2O_3$, $B_2O_3/Al_2O_3$ and $SiO_2/Al_2O_3$ ratios were systematically varied. As a result, with increasing $PbO/Al_2O_3$ the thermal expansion coefficient and the dielectric constant noticeably increased, while the change of $B_2O_3/Al_2O_3$ and $SiO_2/Al_2O_3$ ratios did not affect those properties of the glasses.

  • PDF

Physicochemical Property of Borosilicate Glass for Rare Earth Waste From the PyroGreen Process

  • Young Hwan Hwang;Mi-Hyun Lee;Cheon-Woo Kim
    • 방사성폐기물학회지
    • /
    • 제21권2호
    • /
    • pp.271-281
    • /
    • 2023
  • A study was conducted on the vitrification of the rare earth oxide waste generated from the PyroGreen process. The target rare earth waste consisted of eight elements: Nd, Ce, La, Pr, Sm, Y, Gd, and Eu. The waste loading of the rare earth waste in the developed borosilicate glass system was 20wt%. The fabricated glass, processed at 1,200℃, exhibited uniform and homogeneous surface without any crystallization and precipitation. The viscosity and electrical conductivity of the melted glass at 1,200℃ were 7.2 poise and 1.1 S·cm-1, respectively, that were suitable for the operation of the vitrification facility. The calculated leaching index of Cs, Co, and Sr were 10.4, 10.6, and 9.8, respectively. The evaluated Product Consistency Test (PCT) normalized release of the glass indicated that the glass satisfied the requirements for the disposal acceptance criteria. Furthermore, the pristine, 90 days water immersed, 30 thermal cycled, and 10 MGy gamma ray irradiated glasses exhibited good compressive strength. The results indicated that the fabricated glass containing rare earth waste from the PyroGreen process was acceptable for the disposal in the repository, in terms of chemical durability and mechanical strength.