In the lamination process of multi-layer ceramic modules, the occurrence of delamination comes into repeatedly. To completely improve the lamination process of LTCC sheets, a binder film was introduced between the layers. The binder film did not originate the delamination until the thickness under $40{\mu}m$. After lamination, the thickness of the binder film was determined by the infilteraion of binder by the pressure, and after the bake-out, was dependent on the decomposition of binder resin. Any detectable defect was not observed in the multilayer structure with Ag inner electrodes.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2006.11a
/
pp.230-231
/
2006
In this paper, we examined effects by the binder in manufacturing titanium dioxide film for dye sensitized solar cell. Binder(PEG and PEO) was added the amount of 10-40wt% to commercial $TiO_2$ (P25), Respectively. All of $TiO_2$ film was showed porous structure owing to the addition of binders. But the difference of film's porosity could not be confirmed. The transmittance of $TiO_2$ film was decreased with the increase of binder's amount, generally. In case of 20wt%, however. The transmittance of $TiO_2$ films was showed the highest value.
Park, Jung-Cheul;Chu, Soon-Nam;Lee, Hyeon-Seok;Kwon, Jung-Youl;Lee, Heon-Yong;Ahn, Sang-Yong
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2007.06a
/
pp.117-118
/
2007
In this paper, we examined an effect by the binder in titanium dioxide film for dye sensitized solar cell. Binder(PEG and PEO) was added the quantity of 10- 40wt% to commercial $TiO_2$ (P25), Respectively. All of $TiO_2$ film was showed porous structure. but difference of film's porosity could not be confirm. Transmittances of $TiO_2$ film was decreased with the increase of binder's quantity, generally. In case of 20wt%, however, Transmittances of $TiO_2$ film was recoded the highest value. and it measured 1.77 of energy-conversion efficiency.
To improve the adhesion properties between the conductive paste and PET film, the PET film was chemically treated using acids and bases and physically treated through corona discharge. A paste using ethylcellulose, which is used in actual industrial manufacturing and silane-treated CNF, as a binder was manufactured and coated on PET film to compare the adhesive properties. The specimen coated with a paste containing silane-treated CNF as a binder on a corona discharge-treated PET film showed the highest level of adhesion, 5B. On the other hand, it was confirmed that when PET film was chemically treated with acid/base, there was no improvement in adhesive properties.
Journal of the Korean institute of surface engineering
/
v.46
no.6
/
pp.277-282
/
2013
This study is an experimental attempt to confirm the binder effect of zeolite coating on glass plate by heat treatment. As a result, zeolite was successfully formed with low concentratios of pressure, whose concentration was effective in 10% or more for thin film zeolite coating. And as the content of the binder (TEOS) in mixed coating solution was higher, the zeolite was fastened better on the surface. Above 5% content of the binder in the coating solution, TEOS hindered zeolite synthesis of the precursor and brought to zeolite capacity decrease. Furthermore, when the concentration of the precursor, sedimentation rate of the precursor was higher and the coating efficiency is reduced thereby. Therefore, the most effective concentrations of the precursor and TEOS in the coating solution was 10% and 5%, respectively. It was concluded that zeolite coating is produced by heat treatment method after dipping without hydrothermal synthesis.
Kim, Seok Jun;Park, Wan-Su;Hwang, Jung Seok;Pak, Na Young;Choi, Young Ju;Chung, Dae-won
Applied Chemistry for Engineering
/
v.26
no.4
/
pp.458-462
/
2015
It is essential to employ a binder to prepare transparent films from conductive polymer such as poly(3,4-ethylenedioxythiophene)-poly(styrene sulfonate) (PEDOT/PSS). In this paper, poly(vinyl alcohol) (PVA), poly(vinyl pyrrolidone) (PVP), and PSS were selected as a binder, and their effects were investigated. The formation of the film was found to be primarily dependent on the surface tension of coating solution including PEDOT/PSS and a binder. When PSS was used as a binder, the film was not formed. In case of using PVP, it was easily peeled off from the substrate. However, when using the PVA or the mixtures of PVA and PSS or PVA and PVP as a binder, films with good transparency and uniform surface resistances were produced. Based on adhesion and long-term stability tests, we concluded that the mixture of PVA and PSS is the best binder for preparing antistatic films of PEDOT/PSS.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.13
no.1
/
pp.52-59
/
2000
In order to develop the transparent anti-static film with higher than 80% transparency to visible light, organic conductive compounds, N-methyl phenazinium 7,7,8,8-tetracyanoquinonedimethane (TCNQ) com-plex salts was synthesized and bar-coated on the polythylene terephthalate (PET) film using polymer binders. The best surface properties were obtained when acrylic binder was used. A single layer of TCNQ made of a acrylic binder showed a surface resistance of 10\ulcorner $\Omega$/ , a conductivity of 10\ulcorner S/cm, and a transparency of 75%. An optical microscopic examination revealed that the binder was first solidi-fied on the surface of PET film over which the needle-shaped TCNQ crystals were grown. An acrylic polyol coating over the TCNQ layer improved the transparency to 87%, becuase the acrylic polyol covers the surface of TCNQ crystals to reduce the surface roughness. This conductive material has thermal stability at room temperature and 4$0^{\circ}C$ over 4,000 h.
In this work, the effects of binder materials on the tribological behavior were experimentally evaluated for air curable MoS$_2$bonded film lubricants. The binders tested were basically alkyd and acryl based resins, and also were modified by nitro-cellulose in various weight percentages. Effects on the binder ratio to solid lubricants and the molecular weight of binders were also investigated in all aspects of the tribological behavior. For the tests, LFW-1 and Falex tester were used to measure mainly the endurance life and load carrying capacity of bonded lubricants. Results showed that lubricants of methacrylic resin has the better performance than those of other resins, and also the properties of lubricants both of alkyd and acrylic resins could be improved by modification with nitro-cellulose. It was also shown that the optimum ratio of nitro-cellulose related closely to the binder material and the testing machine.
This study was performed to develop an antibacterial film that can be dried at room temperature. A nanosized TiO$_2$ particle-dispersed solution was prepared by the hydrothermal treatment of peroxo-titanic acid at 160${^{\circ}C}$ for 4h. The binder was synthesized through the hydrolysis and condensation reactions of TEOS (10cc) and GPTS (3.5cc) in the mixture of H$_2$O (30cc) and EtOH (30cc). The synthesized binder was mixed with 0.1 M of TiO$_2$ solution in a volume ratio of binder/TiO$_2$ solution=0.25~0.5. The glass substrate was coated after using the dip coating method, which was then followed by drying for over 2h at room temperature. Although the TiO$_2$ particles did not chemically-bond to the binder, the coating layer strongly adhered to the substrate and displayed good antibacterial properties.
The objective of this paper is to evaluate the performance of low $CO_2$ asphalt binder properties using LEADCAP$^{(R)}$(Low Energy and Carbon Asphalt Pavement) additive as function of various aging methods such as RTFO(Rolling thin film oven), Ultraviolet(UV) lay. In order to simulate the short-term aging of asphalt binder that occurs during the hot-mixing asphalt process, the Rolling Thin Film Oven(RTFO) was used. Asphalt binder using LEADCAP$^{(R)}$ is prepared by addition of a photoinitiator activated by ultraviolet lay. The mechanical and rheological properties of the asphalt binder were estimated using UTM(Universal Testing Machine) and DSR(Dynamic Shear Rheometer). The test results showed that the asphalt binder using LEADCAP$^{(R)}$ additive was improved the rutting resistance at testing temperature ($70^{\circ}C$) and increased tensile strength at low temperature. Also, Thermal analysis shows that the Melting Point(Tm) of asphalt binder using LEADCAP$^{(R)}$ additive was constant although the asphalt binder was aged by Ultraviolet.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.