A Study on the Solidified Structures of Al-Pb Alloy Solidified by Rapid Cooling (급냉응고 시킨 Al-Pb 합금의 응고조직에 관한 연구)

  • Kim, Yong-Kil;Kim, Tong-Hoon
    • Journal of Korea Foundry Society
    • /
    • v.2 no.1
    • /
    • pp.12-18
    • /
    • 1982
  • The present investigation was made to abtain a fine distribution of Pb Particles in AL - Pb binary alloys , which have a broad miscibility gap and large specific difference, by means of rapid Cooling of the molten alloys. Al-2.4% Pb, Al-5.5wt% Pb and Al-8.0wt % Pb alloy were used. The rapid cooling operation was performed by free falling of homogeneous liquid Al-Ph alloys into the water-cooled copper mold, and thermal analysis was made. Microstructures were observed, and variations of size and number of Pb particles were analysicle analyzer. By the result of examination with the varing cooling rates 100 to $210^{\circ}C/sec$ fine distributions of Pb particles were obtained with high cooling rate. Under same cooling condition, the best rapid cooling effect was recognized in Al-5.5wt% Pb alloy.

  • PDF

Change of Secondary Dendrite Arm Spacing of Hypoeutectic Al-Si Alloys according to Si Content and Cooling Rate (아공정 Al-Si 합금에서 Si 함량과 냉각속도에 따른 제이차수지상간격의 변화)

  • Park, Kyeong-Seob;Kim, Hee-Soo
    • Journal of Korea Foundry Society
    • /
    • v.37 no.4
    • /
    • pp.108-114
    • /
    • 2017
  • In this study, we investigated the effect of the Si content on the secondary dendrite arm spacing (SDAS) of hypoeutectic Al-Si binary alloys in the range of 4~10 wt% Si. Cooling curves were measured during the solidification of the alloy cast in a step-wise mold. We compared two kinds of solidification time: the first is the total solidification time for both dendritic and eutectic growth, and the second is the solidification time for only dendritic growth. The proportional constant in the relationship between SDAS and cooling rate was estimated, as this constant represents the stability of the cast microstructure. The proportional constant decreased with the Si contents from 4 wt% to 8 wt%, and it remains relatively uniform with up to 10 wt% of Si.

Weldability of Al Alloys,Part I ;Cfacking and Porosity (알루미늄 합금의 용접특성 - part I : 균열 및 기공)

  • 이창희;장래웅
    • Journal of Welding and Joining
    • /
    • v.10 no.3
    • /
    • pp.1-12
    • /
    • 1992
  • A literature review was conducted to survey informations available on the welding metallurgy of aluminum alloys and its effect on fusion weldability, especially on solidification cracking and pore formation. Solidification cracking behavior of Al weld is a complicate matter as compared to other high alloys, where a relatively simple Fe-X(most detrimental elements S, P, B, Si, etc) binary diagram can be successfully applicable. Both additive and synergistic effects of elements should be considered together. A same element play a different role from system to system. Porosity, caused by hydrogen contamination of the weld is one of the most troublesome welding problems. The primary sources of hydrogen are believed to be an absorbed moisture on the filler metal or base metal and in the shielding gas. It is extremely important that reliable quality-control procedures be employed to eliminate all possible sources of hydrogen contamination. Selection of proper process and parameters is sometimes more important than controlling of alloying elements in order to make a defect-free weld.

  • PDF

A Study on the Recrystallization Behavior of Zr-xSn Binary Alloys (Zr-xSn 이원계 합금의 재결정에 관한 연구)

  • Lee, Myeong-Ho;Gu, Jae-Song;Jeong, Yong-Hwan;Jeong, Yeon-Ho
    • Korean Journal of Materials Research
    • /
    • v.9 no.11
    • /
    • pp.1123-1128
    • /
    • 1999
  • To investigate the effect of Sn on the recrystallization of Zr-based alloys. Zr-xSn (x=0.5, 0.8, 1.5, 2.0wt.%) alloys were manufactured to be the sheets through the defined manufacturing procedure. The specimens were annealed at $300^{\circ}C$ to $800^{\circ}C$ for 1 hour. The hardness, microstructure and precipitate of the alloys with the annealing temperature were investigated by using micro- knoop hardness tester, optical microscope(O/M) and transmission electron microscope(TEM), respectively. The cold-worked Zr-xSn alloys showed the typical behavior of the recovery. recrystallization, and grain growth. The recrystallization of Zr-xSn alloys occurred between $500^{\circ}C$ and $700^{\circ}C$. As the Sn content increased. the recrystallization temperature of the cold-worked alloys increased but their grain sizes after recrystallization decreased. It is suggested that the recrystallization of the cold- worked Zr alloys be occurred by the subgrain coalescence and growth mechanism.

  • PDF

A model for columnar-dendritic solidification of binary alloys accounting for dendrite tip undercooling (선단과냉을 고려한 이원합금의 주상 수지상응고 모델)

  • Yu, Ho-Seon
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.22 no.5
    • /
    • pp.698-707
    • /
    • 1998
  • A simplified model for predicting microsegregation during columnar-dendritic solidification of binary alloys is developed, in which back diffusion, dendrite arm coarsening and dendrite tip undercooling are simultaneously incorporated. The inclusion of tip undercooling is accomplished by modifying the initial conditions of the existing solute diffusion model, in such forms that tip undercooling depresses the beginning of solidification below the liquidus temperature, and that the secondary arm spacing evolves in accordance with the minimum undercooling theory. Sample calculations for the well-known benchmark system show that the present predictions not only consist with the extablished limiting cases, but also agree favorably with the available experimental data within a reasonable tolerance. In particular, a typical decreasing trend in the eutectic fraction at high cooling rates is successfully resolved. Comparison of the individual and combined effects of characteristic parameters in reference with the limiting cases reveals the interactions among parameters. Every parameter plays the role of reducing the eutectic fraction, and the degree of influence depends primarily on the cooling rate. Coarsening enhances the effect of tip undercooling, while suppressing that of back diffusion. A vigorous back diffusion seems to restrain the apperance of the undercooling effect. Overall, each contribution of the three parameters to microsegregation is estimated to be of the same order, which suffices to justify the present study.

Effect of Manganese Content on the Magnetic Susceptibility of Ferrous-Manganese Alloys: Correlation between Microstructure on X-Ray Diffraction and Size of the Low-Intensity Area on MRI

  • Youn, Sung Won;Kim, Moon Jung;Yi, Seounghoon;Ahn, Hyun Jin;Park, Kwan Kyu;Lee, Jongmin;Lee, Young-Cheol
    • Investigative Magnetic Resonance Imaging
    • /
    • v.19 no.2
    • /
    • pp.76-87
    • /
    • 2015
  • Purpose: There is an ongoing search for a stent material that produces a reduced susceptibility artifact. This study evaluated the effect of manganese (Mn) content on the MRI susceptibility artifact of ferrous-manganese (Fe-Mn) alloys, and investigated the correlation between MRI findings and measurements of Fe-Mn microstructure on X-ray diffraction (XRD). Materials and Methods: Fe-Mn binary alloys were prepared with Mn contents varying from 10% to 35% by weight (i.e., 10%, 15%, 20%, 25%, 30%, and 35%; designated as Fe-10Mn, Fe-15Mn, Fe-20Mn, Fe-25Mn, Fe-30Mn, and Fe-35Mn, respectively), and their microstructure was evaluated using XRD. Three-dimensional spoiled gradient echo sequences of cylindrical specimens were obtained in parallel and perpendicular to the static magnetic field (B0). In addition, T1-weighted spin echo, T2-weighted fast spin echo, and $T2^*$weighted gradient echo images were obtained. The size of the low-intensity area on MRI was measured for each of the Fe-Mn binary alloys prepared. Results: Three phases of ${\alpha}^{\prime}$-martensite, ${\gamma}$-austenite, and ${\varepsilon}$-martensite were seen on XRD, and their composition changed from ${\alpha}^{\prime}$-martensite to ${\gamma}$-austenite and/or ${\varepsilon}$-martensite, with increasing Mn content. The Fe-10Mn and Fe-15Mn specimens comprised ${\alpha}^{\prime}$-martensite, the Fe-20Mn and Fe-25Mn specimens comprised ${\gamma}+{\varepsilon}$ phases, and the Fe-30Mn and Fe-35Mn specimens exhibited a single ${\gamma}$ phase. The size of the low-intensity areas of Fe-Mn on MRI decreased relative to its microstructure on XRD with increasing Mn content. Conclusion: Based on these findings, proper conditioning of the Mn content in Fe-Mn alloys will improve its visibility on MR angiography, and a Mn content of more than 25% is recommended to reduce the magnetic susceptibility artifacts on MRI. A reduced artifact of Fe-Mn alloys on MRI is closely related to the paramagnetic constitution of ${\gamma}$-austenite and/or ${\varepsilon}$-martensite.

Electrochemical Behaviors of Binary Ti-Zr Alloys

  • Oh, M.Y.;Kim, W.G.;Choe, H.C.;Ko, Y.M.
    • Corrosion Science and Technology
    • /
    • v.8 no.2
    • /
    • pp.89-92
    • /
    • 2009
  • Pure Ti as well as Ti-6Al-4V alloy exhibit excellent properties for dental implant applications. However, for a better biocompatibility it seems important to avoid in the composition the presence of V due to the toxic effects of V ion release. Thus Al and V free and composed of non-toxic element such as Nb, Zr alloys as biomaterials have been developed. Especially, Zr contains to same family in periodic table as Ti. The addition of Zr to Ti alloy has an excellent mechanical properties, good corrosion resistance, and biocompatibility. In this study, the electrochemical characteristics of Ti-Zr alloys for biomaterials have been investigated using by electrochemical methods. Methods: Ti-Zr(10, 20, 30 and 40 wt%) alloys were prepared by arc melting and homogenized for 24 hr at $1000^{\circ}C$ in argon atmosphere. Phase constitutions and microstructure of the specimens were characterized by XRD, OM and SEM. The corrosion properties of the specimens were examined through potentiodynamic test (potential range of -1500 ~ 2000 mV), potentiostatic test (const. potential of 300 mV) in artificial saliva solution by potentiostat (EG&G Co, PARSTAT 2273. USA).