Recently the use of ferritic stainless steels for automotive exhaust system has been increased dramatically. A detailed knowledge of material behavior of ferritic stainless steel is important for successful manufacturing of exhaust systems. To achieve this goal, numerical study of square cup deep drawing for ferritic stainless steel sheet, type 409L was conducted with Yld2000-24. Uniaxial tensile test and hydraulic bulge test were performed to characterize plastic material behavior. Finite element simulation of square cup deep drawing was performed successfully.
A modified Mukerjee's model considering the microstructural evolution was developed to study the superplastic bulge forming process of Ti-6Al-4V alloy. Through the microstructual observation after deformation, it was found that the grain growth rate of uniaxially tested specimens was different from that of biaxially deformed specimens. From this result, bulge forming experiments with and without back pressure were performed to examine the grain growth behavior and to compare the results of biaxial test with those of triaxial test. Good agreement between the prediction by a modified Mukerjee's model and the experimental measurements was obtained for bulge profile and thickness distribution.
A bulge testing system was developed to measure mechanical properties of thin film materials. A bulge pressure test system for pressurizing the bulge window of the film and a micro out-of-plane ESPI(Electronic Speckle Pattern Interferometric) system for measuring deflection of the film were included in the testing system developed. For the out-of-plane ESPI system, whole field speckle fringe pattern, corresponding to the out-of-plane deflection of the bulged film, was 3-dimensionally visualized using 4-bucket phase shifting algorithm and least square phase unwrapping algorithm. The bulge pressure for loading and unloading was controlled at a constant rate. From the pressure-deflection curve measured by this testing system, ain-plane stress-strain curve could be determined. In this study, elastic modulus of an electrolytic copper film 18 ${\mu}m$ was determined. The modulus was calculated from determining the plain-strain biaxial elastic modulus at the respective unloading slopes of the stress-strain curve and for the Poisson's ratio of 0.34.
Superplastic formability depends on flow parameters such as temperature, strain rate, strain and stress, microstructures. Usually, superplastic properties of materials are characterized with using a uni-axial tension testing. However, superplastic sheet is formed under mutiaxial loading condition in most forming practices. In the present study, superplastic characteristics of A15083 alloys were determined with using both a uni-axial and biaxial bulging tests. Specially, cone-type die was used to achieve constant strain rate under constant pressure condition. Even though constant strain rate under a certain pressure was achieved only approximately, a cone-type bulging test was found to be quite beneficial to get a multiaxial formability of superplastic materials.
In the present study, blow forming characteristics of commercially roiled AZ31 alloy sheets were investigated. Two different kinds of AZ31 sheets were originally fabricated by using direct casting and strip casting methods respectively. Both sheets have similar grain sizes of about $7{\mu}m$ with a relatively equiaxed structure after rolling. A series of tensile tests were carried out to get flow behavior in terms of temperature and strain rate. Also, grain size effect was investigated by annealing as-received sheet at elevated temperatures. Elongation increased with temperature increment as well expected. However, the differences in tensile test condition did not give much difference in elongation even at the temperature range where a large elongation would be expected with such as fine grain of $7{\mu}m$. Blow forming experiments showed that forming condition did not result in higher difference in dome height. However, the interesting feature from this study was that formability of this AZ31 alloy got different with stress condition. Firstly, biaxial stress condition might result in lower temperature and strain rate dependencies compared to uniaxial tension results for both DC and SC sheets. Secondly, DC showed slower grain growth in uniaxial tension than in biaxial stress state while SC has much higher grain growth rage in uniaxial tension than in bulging.
박막의 탄성 특성을 평가하는 방법으로 nano-indentation, Brillouin light scattering measurement, ultrasonic surface wave measurement, bulge test, vibration membrane method 등 여러 가지가 제시되어 왔다. 이러한 방법들은 필름의 두께가 일정 두께 이상이 되어야 정확한 측정이 가능한 방법으로 매우 얇은 박막에서도 탄성특성을 평가할 수 있는 freehang, bridge 방법이 제시되었으며, 이 방법은 간단한 식각 공정을 통해 매우 얇은 박막에도 적용시킬 수 있다는 장점을 가지고 있다. 본 연구에서는 아주 얇은 박막에서도 탄성특성을 평가할 수 있는 freehang 방법을 이용하여 순수한 Diamond-like carbon (DLC) 필름과 Sidl 첨가된 DLC 필름의 탄성 특성을 평가하고자 한다. 실험에서 사용한 필름은 rf-PACVD 장비를 이용하여 증착하였다. 이때 전극과 플라즈마 사이의 바이어스 음전압은 -400 Vb로 합성압력은 10mTorr로 고정하였다. 사용한 반응 가스는 벤젠(C6H6), 그리고 벤젠과 희석된 실렌(SiH4 : H2 = 10 : 90)이며, 희석된 실렌의 첨가량을 조절하여 필름 내에 일정량의 Si을 함유시켰다. 각각의 조건에서 증착시간을 조절하여 필름의 두께를 변화시켰으며, KOH(5.6mol) 용액을 이용하여 습식 식각을 함으로써 freehang을 제작하였다. 이때 식각액에 의한 DLC 필름의 손상은 관찰되지 않았다. 필름의 잔류 응력을 측정하기 위해 200$\pm$10 혹은 100$\pm$5$\mu\textrm{m}$ 두께의 얇은 (100) Si wafer를 5$\times$50 mm2의 strip 형태로 절단하여 사용하였다. 필름의 압축 잔류 응력에 의해 발생한 필름/기판 복합체의 곡률은 laser 반사법과 $\alpha$-step profiler를 이용하여 측정하였으며, 이 결과를 Brenner 등에 유도된 식을 이용하여 잔류 응력을 계산하였다. 또한 제작된 frddhang은 광학 현미경과 전자주사현미경에 의해 관찰되었다. 이렇게 제작된 freehang을 이용하여 필름이 기판에 부착되기 위해 필요한 변형률을 측정하고, 독립적으로 측정된 필름의 잔류 응력을 박막의 응력-변형률 관계식에 적용하여 biaxial elastic modulus, E/(1-v)를 구할 수 있었다. 측정 결과 필름의 잔류 응력과 biaxial elastic modulus는 필름의 두께가 감소함에 따라 감소하는 경향을 나타냈으며, 같은 두께의 필름인 경우, 식각 깊이에 따른 biaxial elastic modulus 의 변화를 통해 최적의 식각 깊이를 알 수 있었다.
Although the bulge forming technique is currently employed in commercial superplastic forming processes, the uniaxial tensile test is still the most commonly used method for the evaluation of the superplasticity of materials due to its simplicity in testing. However, the results obtained from the uniaxial tensile test can not be applied in analyzing the characteristics of the real parts formed in multi-axial stress state. In this paper, using the tensile test specimen obtained from the square cup manufactured by superplastic forming, tensile strength and elongation have been investigated according to the strain and cavity volume fraction. From the result of experiment, tensile strength and elongation are decreased according to the strain and cavity in Al-6%Cu-0.4%Zr alloy. On condition of uniaxial stress, cavity volume fraction is increased on linear according to the increasement of thickness strain. However, on condition of biaxial stress there are critical point( E t=1.5-1.6) that the slope, the ratio of cavity volume fraction and strain, have been changed. Therefore, cavity volume fraction is different with respect to stress condition, although the same strain.
박막의 탄성특성을 평가하는 방법으로 nano-indentation, Brillouin light scattering measurement, ultrasonic surface wave measurement, bulge test, vibration membrane method 등 여러 가지가 제시되어 왔다. 최근에는 탄성특성을 평가할 수 있는 간단한 방법으로 기판 식각 기법을 이용한 freehang, bridge 방법이 제시되었다. 이중에서 bridge 방법은 간단한 식각 기법을 이용하여 얇은 박막에서도 탄성 특성을 평가할 수 있는 방법으로 제시되었다. 그러나 식각 과정에서 발생하는 patch 부분의 under-cut으로 인해 정확한 bridge의 길이를 측정할 수 없게 되어 오차가 발생하고 있다. 본 연구에서는 bridge 방법에서 발생하는 오차를 줄이기 위한 방법으로, patch 부분에 etch-stop을 제작해 줌으로서 식각 과정에서 발생하는 under-cut을 효과적으로 제거시켰다. Etch-stop은 2장의 mask를 align key를 이용하여 제작하였다. 먼저 산화막이 형성되어 있는 Si 기판위에 mask 1을 이용하여 patch 부분을 lithography 작업하고, 습식 식각 공정을 한 뒤 DLC 필름을 증착시킨다. 다음으로 mask 2를 이용하여 bridge pattern을 제작하고, DLC 필름을 증착시킨 후 lift-off 기술과 산화막 등방식각 공정을 통해 bridge를 제작하였다. 이렇게 제작된 bridge를 통해 필름이 기판에 부착되기 위해 필요한 변형률을 측정하고, 독립적으로 측정된 필름의 잔류응력과 함께 박막의 응력-변형률 관계식에 적용시켜 biaxial elastic modulus, E/(1-v)를 구할 수 있었다. Sidl 첨가된 DLC 필름은 rf-PACVD 장비를 이용하여 증착하였다. 이때 전극과 플라즈마 사이의 바이어스 음전압은 -400V로 합성압력은 10mTorr로 고정하였다. 사용한 반응가스는 벤젠(C6H6)과 희석된 실렌(SiH4:2H=10:90)이며, 희석된 실렌의 첨가량을 조절하여 필름 내에 함유된 Si의 양을 조절하였다. 각각의 조건에서 증착시간을 조절하여 필름의 두께를 조절하였다. 필름의 잔류응력은 압축잔류 응력에 의해 발생한 필름/기판 복합체의 곡률을 laser 반사법을 이용하여 측정하고, 이 결과를 Brenner 등에 의해 유도된 식을 대입하여 계산하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.