• 제목/요약/키워드: BiSI

검색결과 522건 처리시간 0.034초

(Bi2O3)0.85.(Nb2O5)0.15-6Bi2O3.SiO2계 복합다결정체의 미세구조와 광학적 특성 (Microstructures and Optical Properties of Composite Crystals in the System (Bi2O3)0.85.(Nb2O5)0.15-6Bi2O3.SiO2)

  • 김호건
    • 한국세라믹학회지
    • /
    • 제26권1호
    • /
    • pp.139-145
    • /
    • 1989
  • An eutectic melt in the system(Bi2O3)0.85·(Nb2O5)0.15-6Bi2O3·SiO2 was unidirectionally solidfield at a rate of 0.5mm/h under a thermal gradient of 100℃/cm. Double crucibles and seed crystal plate were used in order to botain the composite crystals which had uniform microstructure throughout the ingot. The obtained composite crystals showed uniform microstructure, in which needle-like δ-(Bi2O3)0.85·(Nb2O5)0.15 crystals were arrayed in parallel in a matrix of γ-6Bi2O3·SiO2 single crystal. It was found that the <110> direction of δ-(Bi2O3)0.85·(Nb2O5)0.15 crystal was essentially parallel to the <111> direction of γ-6Bi2O3·SiO2 crystal in the composite crystals. A transverse thin plate of the composite crystals showed a high resolution optical transmission like an optical fiber array, and sharp chatoyancy was observed in the cabochon shaped composite crystals. Then, this may be useful for applications such as screen of a cathode ray tube or artificial cat's eye gem stones.

  • PDF

Bi-materials of Al-Mg Alloy Reinforced with/without SiC and Al2O3 Particles; Processing and Mechanical Properties

  • Chang, Si-Young;Cho, Han-Gyoung;Kim, Yang-Do
    • 한국분말재료학회지
    • /
    • 제14권6호
    • /
    • pp.354-361
    • /
    • 2007
  • The bi-materials with Al-Mg alloy and its composites reinforced with SiC and $Al_2O_3$ particles were prepared by conventional powder metallurgy method. The A1-5 wt%Mg and composite mixtures were compacted under $150{\sim}450\;MPa$, and then the mixtures compacted under 400 MPa were sintered at $773{\sim}1173K$ for 5h. The obtained bi-materials with Al-Mg/SiCp composite showed the higher relative density than those with $Al-Mg/Al_2O_3$ composite after compaction and sintering. Based on the results, the bi-materials compacted under 400 MPa and sintered at 873K for 5h were used for mechanical tests. In the composite side of bi-materials, the SiC particles were densely distributed compared to the $Al_2O_3$ particles. The bi-materials with Al-Mg/SiC composite showed the higher micro-hardness than those with $Al-Mg/Al_2O_3$ composite. The mechanical properties were evaluated by the compressive test. The bi-materials revealed almost the same value of 0.2% proof stress with Al-Mg alloy. Their compressive strength was lower than that of Al-Mg alloy. Moreover, impact absorbed energy of bi-materials was smaller than that of composite. However, the bi-materials with Al-Mg/SiCp composite particularly showed almost similar impact absorbed energy to $Al-Mg/Al_2O_3$ composite. From the observation of microstructure, it was deduced that the bi-materials was preferentially fractured through micro-interface between matrix and composite in the vicinity of macro-interface.

분말야금법을 이용한 Bi-materials의 제조 (Preparation of Bi-materials by Powder Metallurgy Method)

  • 이인규;이광식;장시영
    • 한국분말재료학회지
    • /
    • 제11권6호
    • /
    • pp.462-466
    • /
    • 2004
  • The bi-materials composed of $Al-5wt{\%}Mg$ and its composite reinforced with SiC particles were prepared by ball-milling and subsequent sintering process. The size of powder in Al-Mg/SiCp mixture decreased with increasing ball-milling time, it was saturated above 30 h when the ball and powder was in the ratio of 30 to 1. Both $Al-5wt{\%}Mg$ powders mixture and $Al-5wt{\%}Mg/SiCp$ mixture were compacted under a pressure of 350MPa and were bonded by sintering at temperatures ranging from 873K to 1173K for 1-5h. At 873k, the sound bi-mate-rials could not be obtained. In contrast, the bi-materials with the macroscopically well-bonded interface were obtained at higher temperatures than 873K. The length of well-bonded interface became longer with increasing temperature and time, indicating the improved contact in the interface between unreinforced Al-Mg part and Al-Mg/SiCp composite part. The relative density in the bi-materials increased as the sintering temperature and time increased, and the bi-materials sintered at 1173K for 5h showed the highest density.

${\gamma}$-$6Bi_2O_3$.$SiO_2$ 결정을 포함하는 복합다결정체의 작성 (Preparation of Composite Polycrystals Including ${\gamma}$-$6Bi_2O_3$.$SiO_2$)

  • 김호건
    • 한국세라믹학회지
    • /
    • 제23권2호
    • /
    • pp.13-20
    • /
    • 1986
  • Composite polycrystals including ${\gamma}$-$6Bi_2O_3$.$SiO_2$ crystal which have needlelike regular structure are useful for the high resolution optical devices. For the purpose of obtaining the composite polycrystals described above the melts of eutectic composition in the three eutectic systems including $6Bi_2O_3$.$SiO_2$ composition were unidirectionally solidified at a rate of 0.05 and 0.25 cm/h under a thermal gradient of 10$0^{\circ}C$/m. Composite polycrystals of relatively regular structure in which needlelike ${\gamma}$-$6Bi_2O_3$.$SiO_2$ crystals were arrayed in parallel with $2Bi_2O_3$.$B_2O_3$ crystal matrix were obtained when the eutectic melt of $6Bi_2O_3$.$SiO_2 -2Bi_2O_3$.$B_2O_3$ system was solidified at a rate of 0.25 cm/h. Partial structural irregularity however was found in the obtained composite polycrystals.

  • PDF

실리콘-게르마늄 바이시모스 공정에서의 실리콘-게르마늄 이종접합 바이폴라 트랜지스터 열화 현상 (Degradation of the SiGe hetero-junction bipolar transistor in SiGe BiCMOS process)

  • 김상훈;이승윤;박찬우;강진영
    • 한국진공학회지
    • /
    • 제14권1호
    • /
    • pp.29-34
    • /
    • 2005
  • 실리콘-게르마늄 바이시모스(SiGe BiCMOS) 소자 제작시 발생하는 실리콘-게르마늄 이종접합 바이폴라 트랜지스터(SiGe HBT) 열화 현상에 대하여 고찰하였다. 독립적으로 제작된 소자에 비해 SiGe BiCMOS 공정에서의 SiGe HBT소자는 얼리 전압(Early voltage), 콜렉터-에미터 항복전압 및 전류이득등의 DC특성이 열화되고 상당한 크기의 베이스 누설전류가 존재한다는 것을 알 수 있었다. 또한 AC 특성인 차단주파수(f/sub T/) 및 최대 진동주파수(f/sub max/)도 1/2이하로 현저하게 저하되는 것을 확인하였다. 이는 고온의 소오스-드레인 열처리에 의한 붕소의 농도분포 변화가 에미터-베이스 및 콜렉터-베이스 접합 위치에 변화를 주고, 결국 실리콘-게르마늄 내에서의 접합 형성이 이루어지지 않아 전류 이득이 감소하고 기생 장벽이 형성되어서 발생한 현상이다.

Fabrication and Characteristics Study of $n-Bi_2O_3$/n-Si Heterojunction

  • Ismail, Raid A.
    • JSTS:Journal of Semiconductor Technology and Science
    • /
    • 제6권2호
    • /
    • pp.119-123
    • /
    • 2006
  • This work presents the fabrication and characteristics of $Bi_2O_3/Si$ heterojunction prepared by rapid thermal oxidation technique without any postdeposition annealing condition. The bismuth trioxide film was deposited onto monocrystalline Si and glass substrates by rapid thermal oxidation of bismuth film with aid of halogen lamp at $500^{\circ}C/\;45$ s in static air. The structural, optical and electrical properties of $Bi_2O_3$ film were investigated and compared with other published results. The structural investigation showed that the grown films are polycrystalline and multiphase (${\alpha}-Bi_2O_3$ and ${\beta}-Bi_2O_3$). Optical properties revealed that these films having direct optical band gap of 2.55 eV at 300 K with high transparency in visible and NIR regions. Dark and illuminated I-V, CV, and spectral responsivity of $Bi_2O_3/Si$ heterojunction were investigated and discussed.

Photoferroelectric 반도체의 광학적 특성 연구 III.($SbS_{1-x}Se_xI,\;BiS_{1-x}Se_xI,\;Sb_{1-x}Bi_xSI,\;Sb_{1-x}Bi_xSeI,\;SbS_{1-x}Se_xI:Co,\;BiS_{1-x}Se_xI:Co,\;Sb_{1-x}Bi_xSI:Co$, 및 $Sb_{1-x}Bi_xSeI:Co$ 단결정의 광학적 특성에 관한 연구) (Optical Properties of Photoferroelectric Semiconductors III.(Optical Properties of $SbS_{1-x}Se_xI,\;BiS_{1-x}Se_xI,\;Sb_{1-x}Bi_xSI,\;Sb_{1-x}Bi_xSeI,\;SbS_{1-x}Se_xI:Co,\;BiS_{1-x}Se_xI:Co,\;Sb_{1-x}Bi_xSI:Co\;and\;Sb_{1-x}Bi_xSeI:Co$ Single Crystals))

  • 현승철;오석균;윤상현;김화택;김형곤;최성휴;김창대;윤창선;권숙일
    • 한국진공학회지
    • /
    • 제2권2호
    • /
    • pp.227-235
    • /
    • 1993
  • $SbS_{1-x}Se_xI,\;BiS_{1-x}Se_xI,\;Sb_{1-x}Bi_xSI,\;Sb_{1-x}Bi_xSeI,\;SbS_{1-x}Se_xI:Co,\;BiS_{1-x}Se_xI:Co,\;Sb_{1-x}Bi_xSI:Co$, and $Sb_{1-x}Bi_xSeI:Co$ single crystals were grown by the vertical Bridgman method using the ingots. It has been found that these single crystals have an orthorhombic structure and indirect optical transition. The composition dependences of energy gaps are given by $E_g(x)=E_g(0)-Ax+Bx^2$. The impurity optical absorption peaks due to cobalt deped with impurity are attributed to the electron transitions between the split energy levels of $Co^{2+}$ and $Co^{3+}$ ions sited at $T_d$symmetry of the host lattice.

  • PDF

Si(100)기판에 $SrBi_2Ta_2O_9$ 박막증착 시 $Bi_2O_3$ 후열처리에 따른 유전특성 (Dielectric properties of SBT($SrBi_2Ta_2O_9$) on $Bi_2O_3$/Pt/Ti/$SiO_2$/Si substrate accordiing to various substrate temperature of $Bi_2O_3$ buffer layer)

  • 윤지언;차원효;이철수;손영국
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.200-201
    • /
    • 2007
  • The SBT($SrBi_2Ta_2O_9$) thin films with $Bi_2O_3$ buffer layer were deposited on Pt/Ti/$SiO_2$/Si substrate by R.F. magnetron sputtering method in order to improve the ferroelectric characteristics. In SBT thin films, the deficiency of bismuth during the process due to its volatility results in an obvious non stoichiometry of the films and the presence of secondary phases. $Bi_2O_3$ buffer layer was found to be effective to achieve the low temperature crystallization and improve the ferroelectric properties of SBT thin films. Ferroelectric properties and crystallinities of SBT thin films with various post annealing of $Bi_2O_3$ buffer layer were observed as various annealing temperature, using X-Ray Diffraction (XRD), scanning electron microscopy (SEM), Keithley 237 and HP 4192A Impedance Analyzer.

  • PDF