• Title/Summary/Keyword: Bi content

Search Result 342, Processing Time 0.031 seconds

A study on the sintering and Dielectric Characteristics of Low Temperature Sinterable $SiO_2-TiO_2-Bi_2O_3-RO$ System (RO:BaO-CaO-SrO) Glass/Ceramic Dielectrics as a Function of $AI_2O_3$ Content (저온 소성용 $SiO_2-TiO_2-Bi_2O_3-RO$계 (RO;BaO-CaO-SrO) Glass/Ceramic 유전체의 $AI_2O_3$ 함량에 따른 소결 및 유전 특성의 변화)

  • Yun, Jang-Seok;Lee, In-Gyu;Lim, Uk;Cho, Hyun-Min;Park, Chong-Chol
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.12
    • /
    • pp.1350-1355
    • /
    • 1999
  • Sintering characteristics and dielectric properties of low temperature sinterable Glass/Ceramic dielectric materials were investigated. The dielectric materials which were developed for microwave frequency applications consist of SiO2-TiO2-Bi2O3-RO system(RO:BaO-CaO-SrO) crystallizable glass and Al2O3 as a ceramic filler. Sintering experiments showed that no more densification occurred above 80$0^{\circ}C$ and bulk density and shrinkage depended on Al2O3 content only. Results of dielectric measurements showed that $\varepsilon$r Q$\times$f and $\tau$f of the material containing 30wt% Al2O3 were 17.3, 600 and +23 ppm respectively. Those values for 45 and 60wt% Al2O3 samples were 11.6, 1400, +0.7 ppm and 7.2, 2000, -8.5 ppm, repectively. The results clearly showed that the Glas/Ceramic materials of present experiment decreased in $\varepsilon$r and increased in $\times$f value and changed from positive to negative value in $\tau$f value with the increasement of Al2O3 content.

  • PDF

Significance and Application of Digital Breast Tomosynthesis for the BI-RADS Classification of Breast Cancer

  • Cai, Si-Qing;Yan, Jian-Xiang;Chen, Qing-Shi;Huang, Mei-Ling;Cai, Dong-Lu
    • Asian Pacific Journal of Cancer Prevention
    • /
    • v.16 no.9
    • /
    • pp.4109-4114
    • /
    • 2015
  • Background: Full-field digital mammography (FFDM) with dense breasts has a high rate of missed diagnosis, and digital breast tomosynthesis (DBT) could reduce organization overlapping and provide more reliable images for BI-RADS classification. This study aims to explore application of COMBO (FFDM+DBT) for effect and significance of BI-RADS classification of breast cancer. Materials and Methods: In this study, we selected 832 patients who had been treated from May 2013 to November 2013. Classify FFDM and COMBO examination according to BI-RADS separately and compare the differences for glands in the image of the same patient in judgment, mass characteristics display and indirect signs. Employ Paired Wilcoxon rank sum test was used in 79 breast cancer patients to find differences between two examine methods. Results: The results indicated that COMBO pattern is able to observe more details in distribution of glands when estimating content. Paired Wilcoxon rank sum test showed that overall classification level of COMBO is higher significantly compared to FFDM to BI-RADS diagnosis and classification of breast (P<0.05). The area under FFDM ROC curve is 0.805, while that is 0.941 in COMBO pattern. COMBO shows relation of mass with the surrounding tissues, the calcification in the mass, and multiple foci clearly in breast cancer tissues. The optimal sensitivity of cut-off value in COMBO pattern is 82.9%, which is higher than that in FFDM (60%). They share the same specificity which is both 93.2%. Conclusions: Digital Breast Tomosynthesis (DBT) could be used for the BI-RADS classification in breast cancer in clinical.

Effect of Processing Variables on Microstructure and Critical Current Density of BSCCO Superconductors Tape (BSCCO 초전도 선재의 미세조직 및 임계전류밀도에 미치는 공정변수 효과)

  • 지봉기;김태우;주진호;김원주;이희균;홍계원
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.11
    • /
    • pp.1014-1021
    • /
    • 1998
  • We evaluated the effect of processing variables on microstructural evolution interface irregularity between Ag sheath and superconductor core and resultant critical current density(J$_{c}$) of (Bi,Pb)$_2$Sr$_2$Ca$_2$Cu$_3$O$_{x}$(2223) superconductor tape. The value of J$_{c}$ was significantly influenced by the interface irregularity, degree of texturing and relative 2223 content. The interface became more irregular(sausage effect), while the degree of texturing gradually improved as the dimension of tape decreased during forming process. As the dimension of wire/tape were changed from diameter of 3.25 mm to thickness of 0.20 mm, J$_{c}$ value was observed to be increased by 10 times. In addition, optimum sintering temperature for improved J$_{c}$ was observed to be 835$^{\circ}C$ in a ambient atmosphere probably due to combined effect of both improved texturing and high 2223 content. Microstructural investigation showed the degree of texturing was degraded by the existence of both second phases and interface irregularity. It was observed that larger grain size and better texturing was developed near relatively flat interface compared to those inside superconducting core.ting core.

  • PDF

Phase Transformation Behavior of Bi2O3-ZnO-Nb2O5 Ceramics sintered at low Temperature

  • Shiao, Fu-Thang;Ke, Han-Chou;Lee, Ying-Chieh
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1232-1233
    • /
    • 2006
  • To co-fire with commercial LTCC (Low Temperature Co-fired Ceramic) materials at $850^{\circ}C{\sim}880^{\circ}C$, different contents of $B_2O_3$ were added to the $Bi_2O_3-ZnO-Nb_2O_5$ (BZN) ceramics. According to the test results, the cubic phase of BZN was transformed into orthorhombic in all the test materials. $BiNbO_4$ phase was formed in test materials with $2{\sim}5wt%$ of $B_2O_3$ addition. The phase transformation of cubic BZN was controlled during the synthesis process with excess ZnO content. The Cubic and orthorhombic phases of BZN could coexist and be sintered densely at $850^{\circ}C/2hr$.

  • PDF

Effect of CdO addition on the microwave dielectric properties of BiNbO$_4$ceramics using mobile communication (이동통신용 BiNbO$_4$세라믹스의 CdO 첨가량에 따른 고주파 유전 특성)

  • 윤중락;이헌용
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1997.11a
    • /
    • pp.405-408
    • /
    • 1997
  • The microwave dielectric properties of CuO and CdO addition of BiNbO$_4$ceramics were investigated. As the content of CdO increased, sintered density and quality factor is decreased. With increase in sintering temperature, the dielectric constant and quality factor is increased. In case of specimen sintered at 96$0^{\circ}C$ with 0.03 wt% CuO and CdO, the microwave dielectric properties obtained were dielectric constant of 41.2, quality factor (Q$\times$f) of 6, 500, temperature coefficient of resonant frequency of ppm/$^{\circ}C$.

  • PDF

Permanent Mold Casting of Copper-Base Alloys for Plumbing Applications

  • Sahoo, M.;Sadayappan, M.;Fasoyinu, F.A.
    • Journal of Korea Foundry Society
    • /
    • v.20 no.1
    • /
    • pp.3-12
    • /
    • 2000
  • The lead content of drinking water has been restricted to less than 15 ppb by Environmental Protection Agency (EPA) in USA. This has led to extensive research and development work at the Materials Technology Laboratory (MTL) of CANMET, a Canadian Government research laboratory, on the development of low-lead and lead-free copper alloys for plumbing applications. Attentionhas also been focused on the environmentally friendly and energy efficient permanent mold casting process to minimize the disposal of foundry sand contaminated by lead due to the use of leaded alloys in the non-ferrous foundries. A new series of alloys called SeBiLOY contaning Bi and Se been introduced to replace lead in the leaded alloys. This paper addresses some important casting characteristics such as fluidity, hot tear resistance, mechanical properties and microstructure of lead-free alloys such as SeBiLOY III and low-lead alloys such as silicon brass, silicon bronze and yellow brass in gravity permanent mold casting.

  • PDF

Corn Growth and Development influenced by Potential CO2 Leakage from Carbon Capture and Storage (CCS) Site (지중저장 이산화탄소의 잠재적 누출 모사에 따른 옥수수 초기 반응 및 생장 연구)

  • Kim, You Jin;Chen, Xuanlin;He, Wenmei;Yoo, Gayoung
    • Journal of Climate Change Research
    • /
    • v.8 no.3
    • /
    • pp.257-264
    • /
    • 2017
  • Carbon capture and storage (CCS) technology has been suggested as an ultimate strategy for mitigating climate change. However, potential leakage of $CO_2$ from the CCS facilities could lead to serious damage to environment. Plants can be a bio-indicator for $CO_2$ leakage as a cost-effective way, although plants' responses vary with plant species. In this study, a greenhouse experiment was conducted to investigate the relation between the $CO_2$ tolerance of corn species and the initial physiological responses to the elevated soil $CO_2$ concentration. Treatment groups included CI (99.99% $CO_2$ gas injection) and BI (no gas injection). Mean soil $CO_2$ concentration for the CI treatment was 19.5~39.4%, and mean $O_2$ concentration was 6.6~18.4%. The soil gas concentrations in the BI treatment were at the ambient levels. In the CI treatment, chlorophyll content was not decreased until the $13^{th}$ day of the $CO_2$ injection. On the $15^{th}$ day, leaf starch content and stomatal conductance were increased by 89% and 25% in the CI treatment compared to the BI treatment, respectively. This might be due to the compensatory reaction of corn to avoid high soil $CO_2$ stress. However, the prolonged $CO_2$ injection decreased chlorophyll content after 13 days. After $CO_2$ injection, plant biomass was reduced by 25% in the CI treatment compared to the BI treatment. Due to the inhibited root growth, leaf phosphorous and potassium contents were decreased by 54% on average in the CI treatment. This study indicates that corn has a high tolerance to soil $CO_2$ concentration of 30% for 2 weeks by its compensatory reactions such as an maintenance of chlorophyll content and an increase in stomatal conductance.

A Study on the Phase Change of Cubic Bi1.5Zn1.0Nb1.5O7(c-BZN) and the Corresponding Change in Dielectric Properties According to the Addition of Li2CO3 (Li2CO3 첨가에 따른 입방정 Bi1.5Zn1.0Nb1.5O7(c-BZN)의 상 변화 및 그에 따른 유전특성 변화 연구)

  • Yuseon Lee;Yunseok Kim;Seulwon Choi;Seongmin Han;Kyoungho Lee
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.30 no.4
    • /
    • pp.79-85
    • /
    • 2023
  • A novel low-temperature co-fired ceramic (LTCC) dielectric, composed of (1-4x)Bi1.5Zn1.0Nb1.5O7-3xBi2Zn2/3Nb4/3O7-2xLiZnNbO4 (x=0.03-0.21), was synthesized through reactive liquid phase sintering of Bi1.5Zn1.0Nb1.5O7-xLi2CO3 ceramic at temperatures ranging from 850℃ to 920℃ for 4 hours. During sintering, Li2CO3 reacted with Bi1.5Zn1.0Nb1.5O7, resulting in the formation of Bi2Zn2/3Nb4/3O7, and LiZnNbO4. The resulting sintered body exhibited a relative sintering density exceeding 96% of the theoretical density. By altering the initial Li2CO3 content (x) and consequently modulating the volume fraction of Bi1.5Zn1.0Nb1.5O7, Bi2Zn2/3Nb4/3O7, and LiZnNbO4 in the final sintered body, a sample with high dielectric constant (εr), low dielectric loss (tan δ), and the temperature coefficient of dielectric constant (TCε) characterized by NP0 specification (TCε ≤ ±30 ppm/℃) was achieved. As the Li2CO3 content increased from x=0.03 mol to x=0.15 mol, the volume fraction of Bi2Zn2/3Nb4/3O7 and LiZnNbO4 in the composite increased, while the volume fraction of Bi1.5Zn1.0Nb1.5O7 decreased. Consequently, the dielectric constant (εr) of the composite materials varied from 148.38 to 126.99, the dielectric loss (tan δ) shifted from 5.29×10-4 to 3.31×10-4, and the temperature coefficient of dielectric constant (TCε) transitioned from -340.35 ppm/℃ to 299.67 ppm/℃. A dielectric exhibiting NP0 characteristics was achieved at x=0.09 for Li2CO3, with a dielectric constant (εr) of 143.06, a dielectric loss (tan δ) value of 4.31×10-4, and a temperature coefficient of dielectric constant (TCε) value of -9.98 ppm/℃. Chemical compatibility experiment with Ag electrode revealed that the developed composite material exhibited no reactivity with the Ag electrode during the co-firing process.

Orientation Control of $SrBi_2Ta_2O_9$ Thin Films on Pt (111) Substrates

  • Lee, Si-Hyung;Lee, Jeon-Kook;Choelhwyi Bae;Jung, Hyung-Jin;Yoon, Ki-Hyun
    • The Korean Journal of Ceramics
    • /
    • v.6 no.2
    • /
    • pp.116-119
    • /
    • 2000
  • The a-axis and c-axis prefer oriented SBT thin films could be deposited on Pt(111)/Ti/$SiO_2$$650^{\circ}C$). The c-axis preferred orientation of SBT film can be obtained by Sr deficiency and high compressive stress. However, the a-axis-oriented grains can be formed under stoichiometric Sr content and nearly stress-free state.

  • PDF

Magnetic and Electric Properties of Multiferroic Ni-doped BiFeO3

  • Yu, Yeong-Jun;Hwang, Ji-Seop;Park, Jeong-Su;Lee, Ju-Yeol;Gang, Ji-Hun;Kim, Gi-Won;Lee, Gwang-Hun;Lee, Bo-Hwa;Lee, Yeong-Baek
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2014.02a
    • /
    • pp.182-182
    • /
    • 2014
  • Multiferroic materials have attracted much attention due to their own fascinating fundamental physical properties and potential technological applications to magnetic/ferroelectric data storage systems, quantum electromagnets, spintronics, and sensor devices. Among single-phase multiferroic materials, $BiFeO_3$, in particular, has received considerable attention because the enhanced ferromagnetism was found by the Fe-site ion substitution with magnetic ions. The structural, the magnetic and the ferroelectric properties of polycrystalline $BiFe_{1-x}Ni_xO_3$ (x=0, 0.01, 0.02, 0.03 and 0.05), which were prepared by the solid-state reaction and the rapid-sintering method, have been investigated. The x-ray diffraction patterns reveal that all the samples are in single phase and show rhombohedral structure with R3c space group. The magnetic properties are enhanced according to the doping content. The Ni-doped $BiFeO_3$ samples exhibit lossy P-E loop due to the oxygen vacancy. The leakage current density of Ni-doped samples (x=0.01 and 0.02) is increased by four orders of magnitude. On the other hand, the x=0.03 and 0.05 samples show the relative reduction of the leakage current.

  • PDF