• Title/Summary/Keyword: Bending Strength Test

Search Result 1,044, Processing Time 0.03 seconds

Change of Ice Resistance of Ice-Breaking Tanker According to Frictional Coefficient (빙마찰계수에 따른 쇄빙탱커의 빙저항 변화)

  • Cho, Seong-Rak;Lee, Sungsu;Lee, Yong-Chul;Yum, Jong-Gil;Jang, Jinho
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.58 no.3
    • /
    • pp.175-181
    • /
    • 2021
  • This study describes the model tests in ice according to the frictional coefficient of an ice-breaking ship and the change in ice resistance by the analysis method for each component of ice resistances. The target vessel is a 90K DWT ice-breaking tanker capable of operating in ARC7 ice conditions in the Arctic Ocean, and twin POD propellers are fitted. The hull was specially painted with four different frictional coefficients on the same ship model. The total ice resistance can be separated by ice breaking, ice buoyancy, ice clearing resistances through the tests in level ice, pre-sawn ice and creep test in pre-sawn ice under sea ice thickness of 1.2 m and 1.7 m. Ice resistance was analyzed by correcting the thickness and bending strength of model ice by the ITTC correction method. As the frictional coefficient between the hull and ice increases, ice buoyancy and clearing resistances increase significantly. When the surface of the hull is rough, it is considered that the broken ice pieces do not slip easily to the side, resulting in an increase in ice buoyancy resistance. Also, the frictional coefficient was found to have a great influence on the ice clearing resistance as the ice thickness became thicker.

Flexural Behavior of Layered RC Slabs, which Bio-Mimics the Interface of Shell Layers, Produced by Using 3D Printable Highly Ductile Cement Composite (3D 프린팅용 고연성 시멘트 복합체를 활용한 패류 껍질층 경계면 모방형 적층 RC 슬래브의 휨 거동)

  • Chang-Jin Hyun;Ki-Seong Kwon;Ji-Seok Seo;Yun-Yong Kim
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.28 no.1
    • /
    • pp.90-97
    • /
    • 2024
  • In this study, we employed Highly Ductile Cement Composite (HDCC) to evaluate the flexural performance of a RC slab that simulates the laminating structure of a seashell. To evaluate flexural performance, we produced conventional RC slab specimens, HDCC slab specimens, and HDCC-M slab specimens which biomimics a seashell's layered structure by inserting PE mesh inside the slab made of HDCC. A series of 4-point bending tests were conducted. Experimental results shows the flexural strength of the HDCC-M slab specimen was 1.7 times and 1.2 times higher than that of the RC and HDCC slab specimens, respectively. Furthermore, the ductility was evaluated using the ratio of yield deflection to maximum deflection, and it was confirmed that the HDCC slab test specimen exhibited the best ductility. This is most likely due to the fact that the inserted PE mesh separates the layers and increases ductility, while the HDCC passing through the mesh prevents the loss of load carrying capacity due to layer separation.

Bond strength of fiber reinforced composite after repair (섬유 강화 컴포지트의 수리 후 접합 강도)

  • Kim, Min-Jung;Kim, Kyung-Ho;Choy, Kwang-Chul
    • The korean journal of orthodontics
    • /
    • v.36 no.3 s.116
    • /
    • pp.188-197
    • /
    • 2006
  • Fiber reinforced composite (FRC) is usually used as a connector joining a few teeth into one unit in orthodontics. However, fracture often occurs during the two to three years of the orthodontic treatment period due to repeated occlusal loading or water sorption in the oral environment. We simulated the repair by overlapping and attaching portions of two FRC strips in the middle and performed a three-point bending test to investigate the changes of the repair strength among the different FRC groups. The specimens were grouped according to the overlapping lengths of the two FRC strips, which were 1, 2, 3 and 4 mm (group E1, E2, E3 and E4, respectively) and the control group consisted of unrepaired, intact FRC strips. Each group consisted of 6 specimens and were cured with a light emitting diode curing unit. Group E4 showed the highest maximum loads of 2.67 N, then the control group (2.39 N), group E3 (2.35 N), E2 (2.10 N), and E1 (1.75 N) in decreasing order. Group E4 also showed the highest stiffness, which was 2.32 N/mm, however, the stiffness of group E3 (2.06N/mm) was higher than that of the control group (1.88 N/mm). According to the visual examination, the specimens tended to be bent rather than being fractured into two pieces with an increased length of overlapping portions. The above results suggest that a minimum overlapping length of 3 mm was necessary to obtain an adequate repair of a 10 mm length of FRC connector. In addition, the critical section adjacent to the joint area, where the thickness decreased abruptly, should be reinforced with flowable resin to minimize the bending tendency.

Effect of Therapeutic Gymnastic Ball Exercise in Patients With Chronic Low Back Pain (만성 요통환자의 치료를 위한 치료용 볼 운동의 효과)

  • Lee, Eun-Young;Bang, Yoo-Soon;Ko, Ja-Kyung
    • Physical Therapy Korea
    • /
    • v.10 no.3
    • /
    • pp.109-126
    • /
    • 2003
  • This study was designed 10 investigate the effects of therapeutic gymnastic ball exercise on pain, flexibility, lumbar disability level and daily activity levels in male patients of the armed forces medical hospital who complain of chronic low back pain. Twenty-three males were placed in the experimental group and twenty-nine males were placed in the control group. All of the subjects were chosen on the basis of availability among in-patients who were diagnosed with low back pain. The control patients were matched to the experimental group and they were selected considering gender, pain duration and age. Gymnastic ball exercise therapy was developed by the author with the assistance of a rehabilitation specialist. Gymnastic ball exercise therapy includes muscle relaxation, flexibility, muscle strength and posture development exercises. The gymnastic ball exercise therapy was carried out by the experimental group three times a week for eight weeks. Before and after the experiments, the intensity of pain, the lumbar joint mobility (flexibility), the lumbar disability levels, and the daily activity levels of the subjects were measured, respectively. The intensity of pain and the lumbar disability levels were measured by the Visual Analogue Scale, the level of flexibility by a measurement ruler, and the level of disability by the Oswestry Low Back Pain Disability Scale. Data were analysed using a t-test, a paired t-test and an unpaired t-test. The results were as follows: 1. The intensity of pain in the lumbar spine in the experimental group was significantly decreased compared with that of the control group during the 4th week and 8th week. 2. The flexibility of the lumbar spine in the experimental group was significantly increased compared with that of the control group during the 4th week and 8 week. 3. The level of pain caused by anterior, posterior, left lateral and right lateral bending and by rotation in experimental group was significantly decreased compared with that of the control group. 4. The Oswestry Disability score of the experimental group was significantly increased compared with that of control group. These findings indicate that gymnastic ball exercise therapy could be effective in decreasing pain and lumbar disability, and increasing the daily activity levels and lumbar flexibility in patients with chronic low back pain. The study also suggests that gymnastic ball exercise therapy could be an essential factor for effective nursing intervention for patients suffering from chronic low back pain.

  • PDF

Lap Details Using Headed Bars and Hooked Bars for Flexural Members with Different Depths (확대머리 철근과 갈고리 철근을 이용한 단차가 있는 휨부재의 겹침이음상세)

  • Lee, Kyu-Seon;Jin, Se-Hoon;Kim, Seung-Hun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.20 no.4
    • /
    • pp.144-152
    • /
    • 2016
  • This paper focuses on the experimental study for investigating the performance for lap splice of hooked or headed reinforcement in beam with different depths. In the experiment, seven specimens, with its variables as the lap length of headed or hooked bar, the existence of stirrups, etc., was manufactured. Bending test was conducted. Lap strengths by test were compared with the theoretical model based on KCI2012. The result showed that the cracks at failure mode occurred along the axial direction to a headed bar. The initial stiffness and the stiffness after initial crack were similar for all specimens. For HS series specimens without stirrups, a 25% increase in lap length was increased 11.8~18.1% maximum strengths. For HH series specimens without stirrups, a increase in lap length did not affect the maximum strengths because of the pryout failure of headed bar. For HS series specimens, the theoretical lap strengths based on KCI2012 considering the B grade lap and the reduction factor for stirrup were evaluated. They are smaller than the test strengths and can ensure the safety in terms of strength capacity. For HH series specimens, the stirrups in the lap zone are needed to prevent the pryout behaviour of headed bar.

An Experimental Study on the Performance of RC Beam according to the Rapid Freezing and Thawing Test Method in the Air (기중 급속 동결 융해 시험 방법에 따른 철근콘크리트 보의 성능 실험 연구)

  • Kim, Sang-Woo;Lee, Dong-Ju;Kim, Kyeong-Min;Kim, Jin-Sup
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.25 no.4
    • /
    • pp.46-55
    • /
    • 2021
  • Concrete structures can cause various problems as the number of common years increases when exposed to external extreme climate conditions. Among these problems, freezing and thawing occur due to the action of extreme climate factors such as heavy rain and heavy snow, which have become the most problematic in recent years. In this study, we present a rapid freezing and thawing test method of concrete in the air, referring to KS F 2456, as Seoul exhibits very dry weather during the period of freezing and thawing. Concrete test specimens and RC beams were fabricated to perform rapid freezing and thawing of 0, 100, 200, and 300 cycles, and the performance evaluation confirmed the degradation of each subject in material and member units. The design strength of 24 MPa, which performs rapid freezing and thawing in the air up to 300 cycles, decreases by 5.24 MPa (21%), and as rapid freezing and thawing in the air increases the stress burden on reinforced concrete bending members, reducing the energy absorption (dissipation) ability of structures due to earthquakes.

Mechanical Modeling of Pen Drop Test for Protection of Ultra-Thin Glass Layer (초박형 유리층 보호를 위한 펜 낙하 시험의 기계적 모델링)

  • Oh, Eun Sung;Oh, Seung Jin;Lee, Sun-Woo;Jeon, Seung-Min;Kim, Taek-Soo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.29 no.3
    • /
    • pp.49-53
    • /
    • 2022
  • Ultra-thin glass (UTG) has been widely used in foldable display as a cover window for the protection of display and has a great potential for rollable display and various flexible electronics. The foldable display is under impact loading by bending and touch pen and exposed to other external impact loads such as drop while people are using it. These external impact loads can cause cracks or fracture to UTG because it is very thin under 100 ㎛ as well as brittle. Cracking and fracture lead to severe reliability problems for foldable smartphone. Thus, this study constructs finite element analysis (FEA) model for the pen drop test which can measure the impact resistance of UTG and conducts mechanical modeling to improve the reliability of UTG under impact loading. When a protective layer is placed to an upper layer or lower layer of UTG layer, stress mechanism which is applied to the UTG layer by pen drop is analyzed and an optimized structure is suggested for reliability improvement of UTG layer. Furthermore, maximum principal stress values applied at the UTG layer are analyzed according to pen drop height to obtain maximum pen drop height based on the strength of UTG.

A Study on the Fabrication of the Laminated Wood Composed of Poplar and Larch (포푸라와 일본잎갈나무의 집성재 제조에 관한 연구)

  • Jo, Jae-Myeong;Kang, Sun-Goo;Kim, Ki-Hyeon;Chung, Byeong-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.2 no.2
    • /
    • pp.25-31
    • /
    • 1974
  • 1. Various gluing qualities applying Resorcinol Plyophen #6000 were studied on aiming the strength relationships of laminated woods resulted by single species [poplar (Populus deltoides), larch(Larix leptolepis)], mixed species of (poplar and larch), preservatives, treated poplar the scarf joint with mixed species of poplar and larch and the scarf joint treated with preservatives. 1. 1 On the block shear and on the DVL tension test, the mean wood failure ratio showed an excellent value i.e., above 65% and the tangential strength for larch was higher than that of radial, but it was reversed for poplar as shown in Tables 1 and 2. 1. 2 The lamina treated with Na-PCP reduced slightly the strength but the limited strength allowed for manufacturing laminated wood was not influenced by treating Na-PCP as shown in Tables 3 and 4. 1. 3 The safe scarf ratio in the plane scarf joint was above 1/12 for larch and 1/6 for poplar regard less of the chemical treatment or untreatment as shown in Tables. 5, 6, 7 and 8. 2. In the normal and boiled state, the gluing quality of the laminated wood composed of single[poplar (Populus deltoides), larch (Larix leptolepis)] and double species (poplar and larch) glued with Resorcinol Plyophen #6000 were measured as follow, and also represented the delamination of the same laminated wood. 2.1 The normal block shear strength of the straight and curved laminated wood (in life size) were more than three times of the standards adhesion strength. And, the value of the boiled stock was decreased to one half of the standard shear adhesion strength, but it was more than twice the standard strength for the boiled stock. Thus, it was recognized that the water resistance of the Resorcinol Plyophen #6000 was very high as shown in Tables 9 and 10. 2. 2 The delamination ratio of the straight and curved laminated woods in respect of their composition were decraesed, in turn, in the following order i. e., larch, mixed stock (larch+poplar) and poplar. The maximum value represented by the larch was 3.5% but it was below the limited value as shown in Table 11. 3. The various strengthes i.e., compressive, bending and adhesion obtainted by the straight laminaced wood which were constructed by five plies of single and double species of lamina i. e., larch (Larix leptolepis) and poplar (Populus euramericana), glued with urea resin were shown as follows: 3. 1 If desired a higher strength of architectural laminated wood composed of poplar (P) and larch (L), the combination of the laminas should be arranged as follows, L+P+L+P+L as shown in Table 12. 3.2 The strength of laminated wood composed of laminas which included pith and knots was conside rably decreased than that of clear lamina as shown Table 13. 3.3 The shear strength of the FPL block of the straight laminated wood constructed by the same species which were glued with urea adhesives was more than twice the limited adhesion strength, thus it makes possible to use it for interior constructional stock.

  • PDF

The Effect of Exercise Program on Chronic Low Back Pain in Female Teachers of Elementary School (만성요통 여교사에 대한 운동프로그램의 효과 - 근력, 근지구력, 유연성, 통증, 기능장애, 우울 및 생활만족도를 중심으로 -)

  • Choi, Soon-Young
    • Women's Health Nursing
    • /
    • v.7 no.2
    • /
    • pp.169-187
    • /
    • 2001
  • This study was performed to probe the effect of exercise program on muscle strength, endurance, flexibility, pain, disability level and life satisfaction in female teachers of elementary school who complain of low back pain. For this study, 44 female teachers aged 30-50 years with mechanical low back pain of 6 months' duration, who had the structural normalities in the lumbar spine, were recruited from April 1 to July 10 1999. Twenty three out of them were assigned to the experimental group and twenty one to the control group. The exercise program consisted of education on right postures, the etiology and diagnosis of low back pain, and exercise intervention such as muscle relaxation, elongation and strengthening. With 8 weeks program, the subjects received two sessions of education and six sessions of group exercise in the 1st week, while three sessions of group exercise and four sessions of individual exercise weekly and two sessions of education during the later 7 weeks. The muscle strength and endurance were measured by Cybex 770, the flexibility by flexibility measurement machine, the intensity of pain by Visual Analogue Scale (VAS), the level of disability by Oswestry low back pain disability scale, depression by Beck depression inventory (BDI), and life satisfaction by Life satisfaction index-Z. Study measurements were taken before and after 8 weeks exercise program. Data were analyzed using paired t-test, t-test, and ANCOVA. The results were as follows ; 1. The flexors and extensors peak torque and flexors peak torque per body weight of experimental group were significantly increased at test velocities $30^{\circ}$/sec, $60^{\circ}$/sec compared with those of control group. There was no significant difference in extensors peak torque per flexors peak torque at $30^{\circ}/sec$, $60^{\circ}/sec$ between experimental and control group. 2. The flexors and extensors total work and flexors total work per body weight of experimental group were significantly increased at $120^{\circ}/sec$, compared with those of control group. 3.The flexibility of lumbar spine in experimental group was significantly increased compared with that of control group. The pains in anterior, posterior, left lateral and right lateral bending and in rotation of experimental group were significantly increased compared with those of control group. 4. The Oswestry disability scores of experimental and control group were significantly decreased, and there was no difference in the Oswestry disability score change between experimental and control group. 5. The scores of BDI of experimental group were significantly decreased compared with those of control group. Life satisfaction index-Z scores of experimental group were not changed, but those of control group were significantly decreased. There was no difference in the score change of Life satisfaction index-Z between experimental and control group. 6. ANCOVA analysis for the data variables of inhomogeneous baseline represented that there was no significant difference in extensors peak torque and extensors total work at $120^{\circ}/sec$ and extensor total work per body weight at $120^{\circ}/sec$ change between experimental group and control group. These findings indicate that the exercise program could be effective in increasing the muscle strength, endurance, flexibility and decreasing pain, improving depression in female teachers of elementary school with chronic low back pain. It is suggested that the exercise program could be an essential factor for the effective nursing intervention to the patients suffered from chronic low back pain.

  • PDF

A comparative study of electroplating and electroless plating for diameter increase of orthodontic wire (교정용 선재의 직경 증가를 위한 전기도금법과 무전해도금법의 비교연구)

  • Kim, Jae-Nam;Cho, Jin-Hyoung;Sung, Young-Eun;Lee, Ki-Heon;Hwang, Hyeon-Shik
    • The korean journal of orthodontics
    • /
    • v.36 no.2 s.115
    • /
    • pp.145-152
    • /
    • 2006
  • The purpose of this study was to evaluate electroless plating as a method of increasing the diameter of an orthodontic wire in comparison with eletroplating. After pretreatment plating of the 0.016 inch stainless steel orthodontic wire, electroless plating was performed at $90^{\circ}C$ until the diameter of the wire was increased to 0.018 inch. During the process of electroless plating, the diameter of the wire was measured every 5 minutes to examine the increasing ratio of the wire's diameter per time unit. And to examine the uniformity, the diameter at 3 points on the electroless-plated orthodontic wire was measured. An X-ray diffraction test for analyzing the nature of the plated metal and a 3-point bending test for analyzing the physical property were performed. The electroless-plated wire group showed a increased tendency for stiffness, yield strength, and ultimate strength than the electroplated wire group. And there was a statistically significant difference between the two groups for stiffness and ultimate strength. In the electroless-plated wire group, the increasing ratio of the diameter was $0.00461{\pm}0.00003mm/5min$ (0.00092 mm/min). In the electroplated wire group, it was $0.00821{\pm}0.00015mm/min$. The results of the uniformity test showed a tendency for uniformity in both the plating methods. The results of this study suggest that electroless plating of the wire is closer to the ready-made wire than electroplating wire in terms of the physical property. However, the length of plating time needs further consideration for the clinical application of electroless plating.