• 제목/요약/키워드: Basal Texture

검색결과 66건 처리시간 0.127초

마그네슘의 결정립 성장과 집합조직: 상장모델 계산 (Grain Growth and Texture Evolution of Mg: Phase Field Modeling)

  • 김동욱;차필령
    • 한국분말재료학회지
    • /
    • 제18권2호
    • /
    • pp.168-171
    • /
    • 2011
  • We investigate grain growth behavior of poly-crystalline Mg sheet having strong basal fiber texture using phase field model for grain growth and micro-elasticity. Strong initial basal texture was maintained when external load was not imposed, but was weaken when external biaxial strain was imposed. Elastic interaction between elastic anisotropy of Mg grain and external load is the reason why texture evolution occurs.

결정립크기와 집합조직제어를 통한 마그네슘 합금의 기계적 성질 개선 (Improvement of Mechanical Properties of Mg alloys through Control of Grain Size and Texture)

  • 김우진;이종범;김우영;정하국;박종덕
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.57-58
    • /
    • 2006
  • The effects of lowering ECAP temperature during ECAP process and Post-ECAP annealing on microstructure, texture and mechanical properties of the AZ31 alloys have been investigated in the present study. The as-extruded materials were ECAP processed to 2 passes at 553K prior to subsequent pressing up to 6 passes at 523K or 493K. When this method of lowering ECAP temperature during ECAP was used, the rods could be successfully deformed up to 6 passes without any surface cracking. Grain refinement during ECAP process at 553K might have helped the material to endure further straining at lower deformation temperatures probably by increasing the strain accommodation effect by grain boundary sliding, causing stress relaxation. Texture modification during ECAP has a great influence on the strength of Mg alloys because HCP metals have limited number of slip systems. As slip is most prone to take place on basal planes in Mg at room temperature, the rotation of high fraction of basal planes to the directions favorable for slip as in ECAP decreases the yield stress appreciably. The strength of AZ31 Mg alloys increases with decrease of grain size if the texture is constant though ECAP deformation history is different. A standard positive strength dependence on the grain size for Mg alloys with the similar texture (Fig. 1) supports that the softening of ECAPed Mg alloys (a negative slope) typically observed despite the significant grain refinement is due to the texture modification where the rotation of basal planes occurs towards the orientation for easier slip. It could be predicted that if the original fiber texture is restored after ECAP treatment yielding marked grain refinement, yield stress as high as 500 MPa will be obtained at the grain size of ${\sim}1{\mu}m$. Differential speed rolling (DSR) with a high speed ratio between the upper and lower rolls was applied to alter the microstructure and texture of the AZ31 sheets. Significant grain refinement took place during the rolling owing to introduction of large shear deformation. Grain size as small as $1.4{\mu}m$ could be obtained at 423K after DSR. There was a good correlation between the (0002) pole intensity and tensile elongation. This result indicates that tensile ductility improvement in the asymmetrically rolled AZ31 Mg alloys is closely related to the weakening of basal texture during DSR. Further basal texture weakening occurred during annealing after DSR. According to Hall-Petch relation shown in Fig. 1, the strength of the asymmetrically rolled AZ31 is lower than that of the symmetrically rolled one when compared at the same grain size. This result was attributed to weakening of fiber texture during DSR. The DSRed AZ31, however, shows higher strength than the ECAPed AZ31 where texture has been completely replaced by a new texture associated with high Schmid factors.

  • PDF

고온변형 중의 AZ80 마그네슘 합금의 미세조직 형성 거동에 미치는 변형속도의 영향 (Effect of Strain Rate on Microstructure Formation Behaviors of AZ80 Magnesium Alloy During High-temperature Deformation)

  • 박민수;김권후
    • 열처리공학회지
    • /
    • 제33권4호
    • /
    • pp.180-184
    • /
    • 2020
  • The crystallographic texture plays an important role in both the plastic deformation and the macroscopic anisotropy of magnesium alloys. In previous study for AZ80 magnesium alloy, it was found that the main texture components of the textures vary with the deformation conditions at high temperatures. Also, the basal texture was formed at stress of more than 15-20 MPa and the non-basal texture was formed at stress of less than 15-20 MPa. Therefore, in this study, uniaxial compression deformation of AZ80 magnesium alloy was carried out at high temperature (stress of 15-20 MPa). The uniaxial compression deformation is performed at temperature of 723 K and strain rate 3.0 × 10-3s-1, with a strain range of between -0.4 and -1.3. Texture measurement was carried out on the compression planes by the Schulz reflection method using nickel filtered Cu Kα radiation. EBSD measurement was also conducted in order to observe spatial distribution of orientation. As a result of high temperature deformation, the main component of texture and its development vary depending on deformation condition of this study.

열간압연에 따른 AZ61 및 AZ80 마그네슘 합금의 미세조직 및 집합조직 발달에 대한 연구 (Development of Microstructure and Texture of AZ61 and AZ80 Magnesium Alloys by Hot Rolling)

  • 이지호;박노진
    • 열처리공학회지
    • /
    • 제33권2호
    • /
    • pp.49-56
    • /
    • 2020
  • Magnesium alloy is a metal with high specific strength and light weight, and is attracting attention as a next generation metal for environmentally friendly automobiles and transportation equipment. However, magnesium alloys have a problem of degrading formability due to the basal texture developed during processing, and their application is limited. Although active researches on the control of textures have been conducted in order to minimize this problem, there is a lack of research on the formation of microstructures and textures according to elemental differences. In this study, AZ61 and AZ80 magnesium alloys were selected to investigate the effects of aluminum addition on the microstructure development of magnesium alloys. This research has proven that the increase of the rolling rate results in the decrease of the average grain size of the two alloys, the increase of the hardness, and the increase of the fraction of twins. As shown on this research below, the basal texture developed strongly as the rolling ratio increased. On the other hand, this research also has proven that the two alloys exhibited different texture strength and distribution tendencies, which could be due to the effects of aluminum addition on work hardening, grain size, and twin behavior.

Effect of Cu-Addition and Die-Upset Temperature on Texture in Die-Upset Nd-Lean Nd-Fe-B Alloys

  • Kwon, H.W.;Yu, J.H.
    • Journal of Magnetics
    • /
    • 제15권1호
    • /
    • pp.32-35
    • /
    • 2010
  • The effects of Cu-addition and die-upset temperature on the texture in the die-upset Nd-lean $Nd_xFe_{93.5-(x+y)}-Cu_yGa_{0.5}B_6$ (x = 9-12, y = 0-2) alloys were investigated. The die-upset Cu-containing Nd-lean $Nd_{12}Fe_{81.5-y}-Cu_yGa_{0.5}B_6$ (y = 1, 2) alloys showed a considerable texture. Texture in the Nd-lean alloys developed through basal plane slip deformation. The Cu-addition reduced the melting point of grain boundary phase facilitating grain gliding during the die-upsetting, and providing a greater chance for the $Nd_2Fe_{14}B$ grains to meet the deformation conditions. Die-upsetting at higher temperature facilitated grain gliding and plastic deformation, thus enhancing texture.

AZ80 마그네슘 합금 압출재의 압축 성형조건에 따른 방위특성 분석 (Texture Evolution of Extruded AZ80 Mg Alloy under Various Compressive Forming Conditions)

  • 윤종헌;이상익;이정환;박성혁;조재형
    • 소성∙가공
    • /
    • 제21권4호
    • /
    • pp.240-245
    • /
    • 2012
  • With the increasing demand for light-weight materials to reduce fuel consumption, the automobile industry has extensively studied magnesium alloys which are light weight metals. The intrinsic poor formability and poor ductility at ambient temperature due to the hexagonal close-packed (HCP) crystal structure and the associated insufficient number of independent slip systems restricts the practical usage of these alloys. Hot working of magnesium alloys using a forging or extrusion enables net-shape manufacturing with enhanced formability and ductility since there are several operative non-basal slip systems in addition to basal slip plane, which increases the workability. In this research, the thermomechanical properties of AZ80 Mg alloy were obtained by compression testing at the various temperatures and strain rates. Optical microscopy and EBSD were used to study the microstructural behavior such as misorientation distribution and dynamic recrystallization. The results were correlated to the hardening and the softening of the alloy. The experimental data in conjunction with a physical explanation provide the optimal conditions for net-shape forging under hot or warm temperatures through control of the grain refinement and the working conditions.

Effects of Pig Skin Collagen Supplementation on Broiler Breast Meat

  • Park, Sanghun;Kim, Yun-a;Lee, Sanghun;Park, Yunhwan;Kim, Nahee;Choi, Jungseok
    • 한국축산식품학회지
    • /
    • 제41권4호
    • /
    • pp.674-686
    • /
    • 2021
  • This study aimed to enhance the quality of broiler breast meat by adding pig skin collagen to feed. A total of 50 Ross 308 broilers were classified according to the following feeding regime for two weeks: basal diet (NC), basal diet+0.1% fish collagen (PC), basal diet+0.1% pig skin collagen (T1), basal diet+0.5% pig skin collagen (T2), and basal diet+1.0% pig skin collagen (T3). The moisture content was the highest in the PC group, and the protein content was the lowest in the T1 group (p<0.05). The fat content was higher in the T1 and PC groups, whereas the ash content was higher in the T3 group (p<0.05). Drip loss was the highest in the NC group and the lowest in the T2 group (p<0.05). Lightness was low in groups T2 and T3, redness was low in groups T2 and PC, and yellowness was low in groups T1, T2, and PC (p<0.05). The collagen content of the chicken breast was the highest in the T3 group, and that of the skin was the highest in the T1 group (p<0.05). The texture characteristics of springiness, cohesiveness, chewiness, and hardness were the highest in the T3 group (p<0.05). In conclusion, the supplementation of a broiler diet with pig skin collagen was found to increase the collagen content of the breast meat, indicating the improved quality of the broiler breast meat.

AZ61 마그네슘 압출재의 압출 온도에 따른 기계적 특성 및 고주기 피로 특성 (Effect of Extrusion Temperature on Mechanical Properties and High-cycle Fatigue Properties of Extruded AZ61 Alloy)

  • 김예진;차재원;김영민;박성혁
    • 소성∙가공
    • /
    • 제31권3호
    • /
    • pp.117-123
    • /
    • 2022
  • In this study, a commercial AZ61 magnesium alloy is extruded at 300 ℃ and 400 ℃ and the microstructures, mechanical properties, and high-cycle fatigue properties of the extruded materials are investigated. Both extruded materials have a fully recrystallized microstructure with no Mg17Al12 precipitates. The average grain size and maximum basal texture intensity of the extruded material increase with increasing extrusion temperature. The material extruded at 400 ℃ (AZ61-400) has higher tensile yield strength and lower compressive yield strength than the material extruded at 300 ℃ (AZ61-300) because of the stronger basal texture of the former. Because of coarser grain size, the tensile elongation of AZ61-400 is lower than that of AZ61-300. Despite the differences in microstructures and tensile/compressive properties, the two extruded materials have the same fatigue strength of 110 MPa. This is because the finer grain size of AZ61-300 causes an increase in fatigue strength, but its weaker texture causes a decrease in fatigue strength. In both extruded materials, fatigue cracks initiate at the surface of fatigue specimens at all stress amplitudes tested.

AZ31Mg 합금의 집합조직과 벤딩 특성 (AZ3l Mg alloy Texture and Bending Characteristics)

  • 김인수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 추계학술대회 논문집
    • /
    • pp.75-76
    • /
    • 2008
  • In this study, texture development and bending characteristics of strong {0002} textured were observed. AZ31 Mg alloy sheets were prepared along the angle of 0 and 12.5 degrees to the lolling direction or {0002} texture. Prepared samples with different angles to the rolling direction were rolled at room temperature condition and after subsequent heat treatment to investigate texture with x-ray diffractometer, respectively The specimen having along the angles of 0 degree to rolling direction shows the highest load and 12.5 degrees specimen shows the highest displacement among any other specimens in bending test.

  • PDF

액상소결한 탄화규소의 집합조직 발달에 관한 연구 (A Study on Texture Development in Liquid-Phase Sintered Silicon Carbide)

  • 성한규;조경식;박노진;최헌진;이준근
    • 한국세라믹학회지
    • /
    • 제37권4호
    • /
    • pp.320-326
    • /
    • 2000
  • Development of texture in SiC materials by hot-pressing and subsequent annealing was studied. Crystallographic texture type was characterized by measuring X-ray pole figures on the perpendicular plane to the hot-pressing direction. Observed all pole figures were nearly axially symmetric (fiber texture). In case of ${\beta}$-SiC materials, the pole density of basal plane (0004) increased as annealing time increased, in contrast, other planes (hkil) of ${\beta}$-SiC materials and all planes of ${\alpha}$-SiC materials nearly remained unchanged. In the case of ${\beta}$-SiC materials, therefore, a weak texture of (0001) plane at the normal direction took place in the 8h annealed samples, resulting from grian growth. The fracture toughness values of ${\alpha}$-SiC materials measured in both planes parallel and perpendicular to the hot-pressing direction were very similar. However, the fracture toughness of ${\beta}$-SiC materials measured parallel to the hot-pressing direction were higher than that measured perpendicular to the hot-pressing derection, relatively, because of the texture and the microstructure anisotropy.

  • PDF