Aqueous alkali-developable Photosensitive Barrier Rib Paste for PDP and Photolithographic Process

  • Park, Lee-Soon;Jeong, Seung-Won;Kim, Soon-Hak;Tae, Heung-Sik
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2000.01a
    • /
    • pp.177-179
    • /
    • 2000
  • Barrier rib for the plasma display panel (PDP) was made by photolithographic process utilizing photosensitive barrier rib paste. The barrier rib paste was prepared by first dissolving poly(MMA-co-MAA) binder polymer in butyl carbitol(BC) solvent at 15 wt% concentration. To this solution were added a mixture of functional monomers , Irgacure 651 photoinitiator, and barrier rib power and then the whole mixture was dispersed in the three roll mill for 2 hour. The effect of component and concentration of photosensitive barrier rib paste was studied. After optimization of the paste formulation and photolithographic process, barrier rib could be obtained with good resolution up to 110-120 ${\mu}m$ height and 80-90 ${\mu}m$ width.

  • PDF

Photosensitive Barrier Rib Paste for PDP and Photolithographic Process (Plasma Display Panel용 감광성 격벽 재료 및 Photolithography 공정 성질)

  • Park, Lee Soon;Jeong, Seung Won;Oh, Hyun Shik;Kim, Soon Hak;Song, Sang Moo
    • Applied Chemistry for Engineering
    • /
    • v.10 no.8
    • /
    • pp.1114-1118
    • /
    • 1999
  • Barrier rib for the plasma display panel(PDP) was made by photolithographic process utilizing photosensitive barrier rib paste. The barrier rib paste was prepared by first dissolving ethylcellulose(binder polymer) in butyl carbitol(BC)/butyl carbitol acetate(BCA) =30/70 wt % mixture solvent at 15 wt % concentration. To this solution a mixture of functional monomers consisted of tripropyleneglycol diacrylate/ pentaerythritol triacrylate = 50/50 wt %, Irgacur 651 photoinitiator, and barrier rib powder were added and then the whole mixture was mixed in the three roll mill for 2 hr. The effect of component and concentration of photosensitive barrier paste on the photolithographic process was studied. After optimization of the paste formulation and photolithographic process, barrier rib could be obtained with good resolution up to $100{\mu}m$ height.

  • PDF

Patterning Barrier Ribs of PDP by Transparent Soft Mold

  • Paek, Sin-Hye;Choi, Hyung-Suk;Park, Lee-Soon
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2002.08a
    • /
    • pp.639-642
    • /
    • 2002
  • A new PDP barrier rib formation technique was investigated utilizing transparent soft maid made of silicon resin. Transparent soft mold was fabricated by pouring a silicone resin into the base mold made with photosensitive glass. The photosensitive barrier rib paste was coated on the glass substrate and dried in a 90 $^{\circ}C$ convection oven for 20min. The transparent soft mold was pressed on top of the semi-dry barrier rib layer and then irradiated with a UV lamp to a total dose of $900{\sim}1000mJ/cm^2$ The soft maid was then removed from the pressed barrier rib by winding up and fine pattern of barrier rib was obtained. The photosensitive barrier rib paste makes the demolding easy due to reduced interfacial forces and shrinking of paste materials.

  • PDF

Photosensitive Barrier Rib Paste and Materials and Process

  • Park, Lee-Soon;Kim, Soon-Hak;Jang, Dong-Gyu;Kim, Duck-Gon;Hur, Young-June;Tawfik, Ayman
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2005.07b
    • /
    • pp.823-827
    • /
    • 2005
  • Barrier ribs in the plasma display panel (PDP) function to maintain the discharge space between the glass plates as well as to prevent optical crosstalk. Patterning of barrier ribs is one of unique processes for making PDP. Barrier ribs could be formed by screen-printing, sand blasting, etching, and photolithographic process. In this work photosensitive barrier rib pastes were prepared by incorporating binder polymer, solvent, functional monomers photoinitiator, and barrier rib powder of which surface was treated with fumed silica particles. Studies on the function of materials for the barrier rib paste were undertaken. After optimization of paste formulation and photolithographic process, it was applied to the photosensitive barrier rib green sheet and was found that photolithographic patterning of barrier ribs could be formed with good resolution up to $110{\mu}m$ height and $60{\mu}m$ width after sintering.

  • PDF

Photolithographic Method of Patterning Barrier Ribs for PDP by Green Sheet

  • Park, Lee-Soon;Jang, Dong-Gyu;Hur, Young-June;Lee, Sung-Ho;Kim, Duck-Gon;Kwon, Young-Hwan
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2005.07b
    • /
    • pp.1225-1228
    • /
    • 2005
  • Barrier ribs in the plasma display panel(PDP) function to maintain the discharge space between the glass plates as well as to prevent optical crosstalk. Patterning of barrier ribs is one of unique processes for making PDP. In this work photosensitive barrier rib pastes were prepared by incorporating binder polymer, solvent, functional monomers photoinitiator, and barrier rib powder of which surface was treated with fumed silica particles. Study on the function of materials for the barrier rib paste were undertaken. After optimization of paste formulation and photolithographic process, it was found that photolithographic patterning of barrier ribs with photosensitive barrier rib green sheet could be used in the fabrication of high resolution PDP.

  • PDF

Barrier Rib Patterning Technology for Cost Effective High Resolution PDP

  • Park, Lee-Soon;Paek, Sin-Hye;Yun, Sang-Won;Choi, Hyung-Suk
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2002.08a
    • /
    • pp.989-993
    • /
    • 2002
  • Barrier ribs in the color plasma display panel(PDP) function to maintain the discharge space between to glass plates as well as to prevent optical crosstalk. Patterning of barrier ribs is one of unique processes for making PDP. In this work photosensitive barrier rib pastes were prepared by incorporating binder polymer, solvent, functional monomers photoinitiator, mid barrier rib powder. Study on the function of materials for the barrier rib paste were undertaken. After optimization of paste formulation, both photolithographic and transparent soft molding method resulted in fine pattern of barrier ribs with high aspect ratio.

  • PDF

Material Design for the Fabrication of Barrier Ribs with High Aspect Ratio of Plasma Display Panel by X-ray Lithography

  • Ryu, Seung-Min;Yang, Dong-Yol;So, Jae-Yong;Park, Lee-Soon
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2008.10a
    • /
    • pp.989-992
    • /
    • 2008
  • X-ray lithography is one of the most powerful processes in the fabrication of nano/micro structures with a high aspect ratio. This process enables the fabrication of ultra-thin barrier ribs for PDP using X-ray sensitive paste. In this paper, organic material including photo-monomers, photo-oligomers, binder polymer and additives as well as inorganic powders with different size were optimized to fabricate high aspect ratio barrier rib pattern for PDP.

  • PDF

Effect of Binder Polymer on the Photolithographic Patterning of PDP Barrier Rib

  • Kim, Dong-Ju;Kim, Duck-Gon;Woo, Chang-Min;Ryu, Sueng-Min;Yang, Dong-Yol;Kim, Soon-Hak;Park, Lee-Soon
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2007.08b
    • /
    • pp.1364-1367
    • /
    • 2007
  • In this study, the effect of binder polymer on the photolithographic patterning of barrier ribs was studied from view point of polymer structure and barrier rib pattern.

  • PDF

Processing of Barrier Ribs of PDP Using an UV-curable Paste (광경화성 페이스트를 이용한 PDP 격벽 형성 연구)

  • Kim Yoo-Seong;Koh Tae-Gum;Kim Yong-Seog
    • Journal of Powder Materials
    • /
    • v.13 no.3 s.56
    • /
    • pp.211-216
    • /
    • 2006
  • In an attempt to reduce processing cost and to improve resolution of PDPs, micro mold transfer processing route for barrier ribs of plasma display panel was attempted. In this study, the parameters that may cause defects during the process were identified, which include the shrinkage during UV curing process, stress due to evaporation of organic components, and sintering shrinkage. Considering such parameters, UV curable paste was developed and barrier ribs of PDPs were successfully processed via the process. This work demonstrated the possibility of build-up route in manufacturing barrier ribs of PDP.

Etching of the PDP barrier rib material using laser beam (레이저빔에 의한 PDP 격벽 재료의 식각)

  • Ahn, Min-Young;Lee, Kyoung-Cheol;Lee, Hong-Kyu;Lee, Sang-Don;Lee, Cheon
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.13 no.6
    • /
    • pp.526-532
    • /
    • 2000
  • The paste on the glass or fabrication of the PDP(Plasma Display Panel) barrier rib was selectively etched using focused A $r_{+}$ laser(λ=514 nm) and Nd:YAG(λ=532, 266 nm) laser irradiation. The depth of the etched grooves increase with increasing a laser fluence and decreasing a laser beam scan speed. Using second harmonic of Nd:YAG laser(532 nm) the etching threshold laser fluence was 6.5 mJ/c $m^2$ for the sample of PDP barrier rib. The thickness of 180 ${\mu}{\textrm}{m}$ of the sample on the glass was clearly removed without any damage on the glass substrate by fluence of 19.5J/c $m^2$beam scan speed of 20${\mu}{\textrm}{m}$ /s. In order to increase the etch rate of the barrier rib material barrier rib samples heated by a resistive heater during laser irradiation. The heated sample has many defects and becomes to be fragile. This imperfection of the structure compared to the sample without heat treatment allows the effective etching by the focused laser beam. The etch rates were 65${\mu}{\textrm}{m}$/s and 270 ${\mu}{\textrm}{m}$/s at room temperature and 20$0^{\circ}C$, respectively.y.