Diffusion coupling experiment was done to study expansion of body and soild reaction in BaCO3-TiO2 system. Specimen of BaCO3 and TiO2 was formed with Pt-mark's method. Each specimen was fired at interval of 25℃ from 900℃ to 1000℃ for 2hrs. After that, specimen was fixed with resin and polished. Product layers of specimen were observed with SEM and EDS. The result were following; 1. Diffusion component is Ba2+, which diffuse toward TiO2. 2. Large crack between layer of BaCO3 and Ba2TiO4 was generated because of difference of thermal expansion coefficient. 3. Ba2TiO4 is formed to TiO2 body by the reaction of BaTiO3 and BaO and its structure is very porous. 4. BaTiO3 changes immediately to Ba2TiO4 by the reaction of BaO. But BaTiO3 which formed by the reaction of TiO2 and Ba2TiO4 exsists as layer because the diffusion distance of Ba2+ is far.
It is hard to synthesize pure $BaTiO_3$ from $BaCO_3$ and $TiO_2$ in solid reaction for the activity of BaO and secondary phase. For this reason, the wet chemical techniques have been studied. Starting material which was used in these methods were expensive and the properties of powder which was synthesized in same defined. So, some process have been studying again to improve soild reaction method. This study which was one of those was to defin the forming mechanism of $Ba_2TiO_4$ and to control some condition of $Ba_2TiO_4$. The synthesis temperature of $BaTiO_3$ in solid reaction was near $1120^{\circ}C$. The quantity and forming temperature of $Ba_2TiO_4$ could be controlled by atmosphere heat treatment. $Ba_2TiO_4$ was related to expansion in Ba-rich region of $BaTiO_3$. $BaTiO_2O_5$ and $BaTiO_3O_7$ was reason to expand in Ti-rich region. The dielectrics of $CeAIO_3$ which was synthesized and sintered in reduction atmosphere and $BaTiO_3$ system were affected by $CeO_2$ which was formed for the decomposition of $CeAIO_3$ heat treatment in air.
Using the reverse transcription polymerase chain reaction (RT-PCR), a rapid and sensitive assay method for the detection and identification of barley yellow mosaic virus (BaYMV) and barley mild mosaic virus (BaMMV) was adapted. Two units of primers from each virus were selected and used for the determination of two different viruses. PCR fragments of BaYMV (ca. 0.9kb) and BaMMV (ca. 0.8kb) were obtained from the designed method for the assay of BaYMV and BaMMV coat protein. PT-PCR fragments were cloned using vector pT7 Blue and the sequences of the selected clones were analyzed. coat protein of BaYMV and that of BaMMV consisted of 297 amino acids (891 nucleotides) and 251 amino acids (753 nucleotides), respectively. The snalysis of coat protein genes from these two viruses showed that 45.6% of nucleotides sequence ad 34.9% of amino acid in BaYMV were homologous to those in BaMMV.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.19
no.5
/
pp.223-227
/
2009
$BaCO_3$ crystals with various morphology were prepared using precipitation, hydrothermal and ligand-assisted methods. An irregular structure of $BaCO_3$ microparticle was obtained by simple precipitation method from $Ba(NO_3)_2$ and $Na_2CO_3$ in aqueous solution. Hexagonal pyramidals of $BaCO_3$ were synthesized using a hydrothermal method between $Ba(NO_3)_2$ and urea. Hexagonal rods of $BaCO_3$ were also synthesized using the ligand-assisted hydrothermal method. The aspect ratio of $BaCO_3$ hexagonal rods was increased with the concentration of ligand.
Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
/
v.14
no.2
/
pp.101-112
/
2016
This study investigated the removal of Sr, which was one of the high radioactive nuclides, by adsorption with Barium (Ba) impregnated 4A zeolite (BaA) from high-radioactive seawater waste (HSW). Adsorption of Sr by BaA (BaA-Sr), in the impregnated Ba concentration of above 20.2wt%, was decreased by increasing the impregnated Ba concentration, and the impregnated Ba concentration was suitable at 20.2wt%. The BaA-Sr adsorption was added to the co-precipitation of Sr with $BaSO_4$ precipitation in the adsorption of Sr by 4A (4A-Sr) within BaA. Thus, it was possible to remove Sr more than 99% at m/V (adsorbent weight/solution volume)=5 g/L for BaA and m/V >20 g/L for 4A, respectively, in the Sr concentration of less than 0.2 mg/L (actual concentration level of Sr in HSW). It shows that BaA-Sr adsorption is better than 4A-Sr adsorption in for the removal capacity of Sr per unit gram of adsorbent, and the reduction of the secondary solid waste generation (spent adsorbent etc.). Also, BaA-Sr adsorption was more excellent removal capacity of Sr in the seawater waste than distilled water. Therefore, it seems to be effective for the direct removal of Sr from HSW. On the other hand, the adsorption of Cs by BaA (BaA-Cs) was mainly performed by 4A within BaA. Accordingly, it seems to be little effect of impregnated Ba into BaA. Meanwhile, BaA-Sr adsorption kinetics could be expressed the pseudo-second order rate equation. By increasing the initial Sr concentrations and the ratios of V/m, the adsorption rate constants ($k_2$) were decreased, but the equilibrium adsorption capacities ($q_e$) were increasing. However, with increasing the temperature of solution, $k_2$ was conversely increased, and $q_e$ was decreased. The activation energy of BaA-Sr adsorption was 38 kJ/mol. Thus, the chemical adsorption seems to be dominant rather than physical adsorption, although it is not a chemisorption with strong bonding form.
YBa2Cu3O7-$\delta$, Y2BaCuO5, and binary compounds in the Ba-Cu-O system with the nominal composition of Ba2CuO3, BaCuO2, Ba3Cu4O7, Ba3Cu5O8 were synthesized to investigate the heat evolutions and crystalline phases in the hydration reaction of orthorhombic YBa2Cu3O7-$\delta$ phase. The observed crystalline phases were YBa2Cu3O7-$\delta$, Y2BaCuO5, and BaCuO2, or Ba2Cu3O5+x, and some amount of noncrystalline phase in the Ba-Cu system comounds. In contact with distilled water, YBa2Cu3O7-$\delta$ and Y2BaCuO5 did not have considerable heat liberation, but in the binary compounds of the Ba-Cu-O system, the amount of total heat liberation was increased with respect to the Cu content. It might be that the reaction of high temperature superconductor YBa2Cu3O7-$\delta$ with water and/or moisture originated from the unusual oxidation state of Cu ion and the presence of amorphous Ba-Cu oxide compound. The degradation of high Tc superconductor by moisture and water could be controlled by restricting the heterogeneous distribution of Tc comlposition and the formation of second phase, such as stable Y2BaCuO5, and the resulting unstable Ba-Cu oxide compound.
Journal of the Korea Organic Resources Recycling Association
/
v.26
no.1
/
pp.39-45
/
2018
Research on FA(Fly ash) is actively carried out, while the research on BA(Bottom ash) is not so, and research on BA recycling field is urgently required. Therefore, in this study, we investigated the lightweight and thermal insulation characteristics of BA mortar by comparing BA mortar made with porous dry BA(air-cooled) and general mortar. To investigate the lightweight of BA, density test, unit volume mass test and SEM(Scanning Electron Microscope) test were performed. BA mortar and general mortar molds were prepared for the thermal insulation test at room temperature and humidity environment determined by KS A 0006 and they were dried at the temperature of $105{\pm}2^{\circ}C$ until the weight became constant. As a result of the lightweight test, the lightweight of BA mortar is about 30% lighter than the general mortar. Therefore, BA is expected to contribute to reduce the building load when used as building material. As a result of thermal insulation test, the thermal conductivity of BA mortar is about 30% better than that of general mortar.
The two viruses of barley yellow mosaic(BaYMV) and barley mild mosaic virus (BaMMV) were detected by ELISA from barley plants with virus-like symptoms which were collected from 16 locations in southern Korea, during 1995 and 1996. Both viruses occurred in southern Korea. Barley plants at Chongdo and Koseong were infected with BaMMV, while those infected with BaYMV were at Kurye and Taegu. After sowing 50 barley cultivars at habitually infected fields in 10 locations, the susceptibility and resistance to BaYMV and BaMMV were screened with antiserum tests. The cultivars of Albori, Alchanbori, Daejinbori, Jokangbori, Milyangbori, Boeunkwamek, Naehanssalbori, Olssalbori, Weossalbori, Dusan 29 and Deogndohyangchonkwa showed positive reaction to BaYMV antiserum, while Saeolbori, Chalbori, Jinjukwa and Baegjinkwa showed positive reaction to BaMMV. Nonsankwa 1-6 and wheat cultivars of Chongkeymil, Dahongmil, Grumil, Urimil, Jochonhomil, Sinkeyhomil showed negative reactions to both viruses. The rest cultivars were infected both with BaYMV and BaMMV. Sap inoculations to barleyplants with the two viruses of BaYMV isolated in Haenam and BaMMV isolated at National Honam Agricultural Station, expressed lower infection rate than those grown in the virus-infected fields.
The three different composition of BaTi4O9, Ba2Ti9O20 and BaTi5O11 were prepared by coprecipitation process, and then the dielectric properties of these compounds were measured at low microwave frequencies. The powder showing high level of purity was synthesised by the coprecipition reaction of BaCl2 and TiCl4 where (NH4)2CO3 and NH4OH were used as a deflocculent. Followings are the result of this study: 1. The sintering temperature increased with increasing TiO2 content. 2. BaTi4O9 powder were synthesized as a single phase by this processing technique, but the resultant Ba2Ti9O20 and BaTi5O11 phase existed with Ba2Ti9O20 and BaTi5O11 phases. 3. Single phase BaTi4O9 showed high dielectric constant value of 35, high Q value of 8100.
The crystal structure of Ba46-X, Ba46Al92Si100O384 [a= 25.297(1) Å], has been determined by single-crystal X-ray diffraction techniques in the cubic space group Fd&bar{3}at 21(1) ℃. The crystal was prepared by ion exchange in flowing stream of 0.05 M Ba(OH)2 aqueous solution for 5 days. The crystal was then dehydrated at 380 ℃ and 2 × 10-6 Torr for 2 days. The structure was refined to the final error indices R1= 0.051 and Rw= 0.054 with 369 reflections for which I > 3σ(I). In this structure, all Ba2+ ions are located at the three different crystallographic sites: fourteen Ba2+ ions are located at site Ⅰ, the centers of the double six rings, two Ba2+ ions lie at site Ⅰ', in the sodalite cavity opposite double six rings(D6R's) and another thirty Ba2+ ions are located at site Ⅱ in the supercage. Two Ba2+ ions are recessed ca. 0.27 Å into the sodalite cavity from their three O(3) oxygen plane and thirty Ba2+ ions are recessed ca. 1.11 Å into the supercage from their three O(2) oxygen planes, respectively (Ba(1)-O(3) = 2.76(1) Å, O(3)-Ba(1)-O(3) = 180(0)°, Ba(2)-O(3) = 2.45(1) Å, O(3)-Ba(2)-O(3) = 108(1)°, Ba(3)-O(2)=2.65(1) Å, and O(2)-Ba(3)-O(2)=103.9(4)°).
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.