서브제로 처리한 오스테나이트계 STS202의 탄성파 특성 (Elastic Wave Characteristics of Austenitic STS202 with Subzero Treatment)

  • 최성원;최병철;남기우
    • 한국산업융합학회 논문집
    • /
    • 제24권3호
    • /
    • pp.295-300
    • /
    • 2021
  • This study investigated the dominant frequency of the elastic waves from the tensile test. The specimen was rolled with five different rolling degrees (10, 22, 33, 42 and 50%), which was treated subzero. The specimen was rolled at room temperature, which was transformed from austenite to martensite (only α'-martensite). The dominant frequency increased with an increase in the rolling degree regardless of the subzero temperature, and decreased after 33% of the rolling degree. On the other hand, higher frequency band was obtained at lower temperature and long time. The dominant frequency increased when the amount of α'-martensite increased and decreased with the α'-martensite amount between 50-65%. The lower subzero treatment temperature increased the amount of α'-martensite, which resulted in the higher dominant frequency. The longer treatment time at the same subzero temperature led to an increase in the amount of α'-martensite, leading to high dominant frequency.