• 제목/요약/키워드: Aluminum diecasting

검색결과 21건 처리시간 0.019초

다이캐스팅 ADC12 합금의 열처리 전후의 기계적 특성변화 (Change of Mechanical Properties During Heat Treatment of Diecast ADC12 Alloy)

  • 강신욱;박경섭;오은호;심정일;김희수
    • 한국주조공학회지
    • /
    • 제36권3호
    • /
    • pp.88-94
    • /
    • 2016
  • We investigated the effect of heat treatment on an ADC12 alloy produced using diecasting. The heat treatment used in this study was a typical T6 process: a solid solution treatment followed by an artificial aging treatment. As-cast specimens were solid-solution-treated at $500^{\circ}C$ and $530^{\circ}C$ for 1-16 hr, and aged at $160^{\circ}C$ and $180^{\circ}C$ for 1-8 hr. Microstructural changes in the alloy during the heat treatment were observed. Changes in mechanical properties of the alloy were measured using a micro-Vickers hardness tester. Finally, we determined the optimal heat treatment conditions for the diecast ADC12 alloy.

알루미늄 용탕 운반용 고보온성 Ladle 설계 및 평가 (Design and Evaluation of High Insulation Ladle for Carrying Aluminum Molten Metal)

  • 박진영;최석환;윤필환;김억수
    • 한국주조공학회지
    • /
    • 제30권3호
    • /
    • pp.115-120
    • /
    • 2010
  • Recently, an advanced raw material supplying system in diecasting industry that molten metal produced by the raw material supplier can be directly delivered to the diecasting shops was proposed. It was known to have advantages of reducing melting process cost and improving working environment. However, for its successful mass production, the development of high insulation ladle is inevitable. In this study, the optimal mixing ratio of $SiO_2-Al_2O_3$ was investigated and the high insulation ladle with computer simulation result was built in a prototype and evaluated. The prototype which has refractory wall of $SiO_233%-Al_2O_3$ 35%-CaO 33% showed high insulation sufficient for carrying the Al molten metal for 138 minutes. Gas quantity result and SEM-EDS analysis on the melt poured in the ladle also showed extremely low level of 0.028 cc / 100 g and no penetration of Al molten metal into the refractory wall, satisfying the requirements for mass production.

반응고 성형법에 의해 제조된 고효율 전동기용 Cu-Rotor의 미세조직 및 결함 분석 (Analysis of Microstructures and Defects of the Thixoformed Cu rotor for High Efficiency Electrical Motors)

  • 강병무;서동우;손근용;이상용
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 추계학술대회논문집
    • /
    • pp.55-59
    • /
    • 2003
  • Rotor in small-medium induction motor has been usually manufactured by aluminum diecasting. In order to improve efficiency of induction motors, however, it is desirable that pure aluminum is replaced by high electrical conductivity copper alloy. For this purpose, a rotor is thixoformed with Cu-Ca alloy. Thermomechanical processing(TMP) is carried out to modify the semi-solid microstructure of the alloy and final microstructures and filling defects of thixoformed Cu- rotors are investigated. The characteristics of thixoformed Cu-rotor such as motor efficiency and torque are compared with those of Al rotor.

  • PDF

Al-Si 합금의 양극산화거동 및 규소화합물 제어 (Anodizing Behavior and Silicides Control in Al-Si Alloy System)

  • 박종문;김주석;김재권;김수림;박노진;오명훈
    • 열처리공학회지
    • /
    • 제31권1호
    • /
    • pp.6-11
    • /
    • 2018
  • The anodic oxidation behavior of Si-containing aluminum alloy for diecasting was investigated. Especially, the property changes during anodization both on aluminum 1050 and 9 weight percentage silicon containing aluminum (Al-9Si) alloys were analyzed by the static current test. In order to fabricate a uniform anodic oxidation film by effect of Al-Si compound, nitric acid containing hydrofluoric acid had been used as a desmutter for aluminum alloy after alkaline etching. It was found that the level of voltage of Al-9Si alloy during the static current test was almost as double as higher than aluminum 1050 through anodization. By adding hydrofluoric acid in the nitric acid electrolyte, the silicon compound on the surface was removed, and the optimum amount of added hydrofluoric acid could be derived. It was also observed that the size of silicon compound formed on the surface could be refined by heat treatment at $500^{\circ}C$ and followed water quenching.

전자기력을 이용한 알루미늄 스크랩 중의 Fe 제거에 관한 연구;Part 2. Al-Si-Cu계 합금 스크랩에서 전자기력에 따른 Fe계 금속간화합물의 이동양상 (A Study on the Elimination of Fe Elements in Aluminum Alloy by Electromagnetic Force;Part 2. The Movement of Fe-Contained Intermetallics with Electromagnetic Force in Al-Si-Cu Scrap)

  • 김정호;노정훈;박준표;윤의박
    • 한국주조공학회지
    • /
    • 제18권3호
    • /
    • pp.240-245
    • /
    • 1998
  • In the view point of the environmental conservation and the energy reduction, the recycling of metal scrap is coming as one of the global subjects in the world. In this study, the movement of intermetallics with electromagnetic force in a melt of a scrap of Al-Si-Cu alloy (JIS ADC12), which was widely used in diecasting process, was investigated in order to eliminate the Fe element, which was usually accumulated in a scrap. In this study, we applied electromagnetic method to eliminate Fe element in ADC12 aluminum alloy scrap which contains 1.64wt.% Fe and the effects of electromagnetic force on the particle movement was visualized and confirmed by water modeling and experiment. As a result, the Fe intermetallic compounds are moved to the direction opposite to that of the electromagnetic force as the force applies, thus eliminated from the bulk metal. Therefore, the content of Fe in matrix decreased from 1.64wt.% to 0.45wt.%.

  • PDF

Al 합금 다이캐스팅 용 타이타늄 기지 복합재료 슬리브의 내용손성 및 내마모성 평가 (Endurance in Al Alloy Melts and Wear Resistance of Titanium Matrix Composite Shot-Sleeve for Aluminum Alloy Die-casting)

  • 최봉재;성시영;김영직
    • 대한금속재료학회지
    • /
    • 제50권2호
    • /
    • pp.176-182
    • /
    • 2012
  • The main purpose of this study was to evaluate the endurance against Al alloy melts and wear resistance of an in-situ synthesized titanium matrix composite (TMC) sleeve for aluminum alloy die-casting. The conventional die-casting shot sleeve material was STD61 tool steel. TMCs have great thermal stability, wear and oxidation resistance. The in-situ reaction between Ti and $B_4C$ leads to two kinds of thermodynamically stable reinforcements, such as TiBw and TiCp. To evaluate the feasibility of the application to a TMCs diecasting shot sleeve, the interfacial reaction behavior was examined between Al alloys melts with TMCs and STD61 tool steel. The pin-on-disk type dry sliding wear test was also investigated for TMCs and STD61 tool steel.

반용융 성형공정의 응용 및 문제점 (Applications of Semi-Solid Forming and its Problems)

  • 강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1997년도 고액공존금속의 성형기술 심포지엄
    • /
    • pp.135-147
    • /
    • 1997
  • The production of light metal parts using aluminum is mainly performed by die casting and squeeze casting, which directly fabricate the required shape from the liquid state. However, die casting is subject to defects such as shrinkage porosity and air trapped when molten metal enters the cavity, whilst squeeze casting also has defects due to turbulent flow in the die cavity. Both diecasting and sqeeze casting have inhomogeneous mechanical property in terms of dendritic structure during solidification. Active research has been carried out on semi-solid processing, rather than on conventional process methods such as die casting, which involve various problems. Therefore in this paper, to introduce the fundamental technology for d e design, in die casting and forging process with semi-solid materials, relationship between stress and strain of semi-solid materials, and for producing parts die design has been proposed as parameters of globulization of the microstructure and gate shape. The prevention of various defects to produce sound parts are also introduced.

  • PDF

마그네슘 주조성형기술의 개발동향 (Development Trend of Magnesium Casting Technology)

  • 김현식;예대희;강민철
    • 한국주조공학회지
    • /
    • 제31권5호
    • /
    • pp.243-248
    • /
    • 2011
  • Magnesium alloys have many advantages such as light-weight, high machinability, damping capacity, etc. So magnesium alloy parts have been used in transportation, mobile phone, military industries. Because of HCP atomic structure, Magnesium is very difficult in plastic deformation process, so most of magnesium products are fabricated by casting process. Magnesium alloys have low heat-capacity, high fluidity and low Fe solubility. For these reasons it is more suitable than aluminum in mass-production by casting. And various casting technologies have been developed. So casting technologies for magnesium developed recently is discussed in this paper.

6극 전자석 전자교반 레오캐스팅에 따른 A356의 조직적 / 기계적 영향분석 (Microstructure and Mechanical Property of A356 for Rheocasting Using 6-Pole Electromagnetic Stirring Casting Process)

  • 김백규;노중석;방희재;허민;박진하;전충환
    • 한국주조공학회지
    • /
    • 제40권3호
    • /
    • pp.61-65
    • /
    • 2020
  • Rheo-diecasting with stirring has been used in many material industries. As the 4th Industrial Revolution approaches the world, eco-friendly high-strength and light-weight materials become more important. Casting methods have been studied and used for aluminum-alloy automobile parts. This study carried out the effect analysis of the micro-structure and mechanical properties, such as yield/ultimate tensile strength, elongation, and hardness, of A356 using the 6-pole EMS (electro-magnetic stirring) casting process with a high electromagnetic force. As a result, the hardness and elongation of the A356 after T6 heat-treatment show a significant improvement, respectively, by 20% and 50%.

Fabrication of Low Carbon Steel Coated with 18%Cr-2.5%Ni-Fe Powder by Laser Cladding and Its Application on Plastic Injection Mold for Aluminum Diecasting

  • Kim, Cheol-Woo;Yoo, Hyo-Sang;Cho, Kyun-Taek;Jeon, Jae-Yeol;Choi, Se-Weon;Kim, Young-Chan
    • 한국재료학회지
    • /
    • 제31권11호
    • /
    • pp.601-607
    • /
    • 2021
  • Laser cladding a surface treatment process that grants superior characteristics such as toughness, hardness, and corrosion resistance to the surface, and rebuilds cracked molds; as such, it can be a strong tool to prolong service life of mold steel. Furthermore, compared with the other similar coating processes - thermal spray, etc., laser cladding provides superior bonding strength and precision coating on a local area. In this study, surface characteristics are studied after laser cladding of low carbon steel using 18%Cr-2.5%Ni-Fe powder (Rockit404), known for its high hardness and excellent corrosion resistance. A diode laser with wavelength of 900-1070 nm is adopted as laser source under argon atmosphere; electrical power for the laser cladding process is 5, 6, and 10 kW. Fundamental surface characteristics such as crossectional microstructure and hardness profile are observed and measured, and special evaluation, such as a soldering test with molten ALDC12 alloy, is conducted to investigate the corrosion resistance characteristics. As a result of the die-soldering test by immersion of low carbon alloy steel in ALDC12 molten metal, the clad layer's soldering thickness decreases.