• Title/Summary/Keyword: Aluminum borate

Search Result 24, Processing Time 0.02 seconds

Effect of the Slag Former on the Metal Melting and Radionuclides Distribution in an Electric Arc Furnace

  • Song Song-Pyung;Min Byung-Youn;Choi Wang-Kyu;Chung Chong-Hun;Oh Won-zin
    • Proceedings of the Korean Radioactive Waste Society Conference
    • /
    • 2005.11a
    • /
    • pp.32-37
    • /
    • 2005
  • The characteristics of the metal melting and radionuclide distribution of the radioactive has been investigated in a lab-scale arc furnace. The slag former based on the constituents of silica, calcium oxide, aluminum oxide, borate and calcium fluoride additions was used for melting of the stainless and carbon steel. In the melting of the stainless steel, the amount of slag formation increased with an increase of the concentration of the slag former. But the effects of the slag basicity on the amount of stag formation showed a local maximum value of the slag formation with an increase of the basicity index in the melting of the stainless steel as well as in the melting of the carbon steel. With an increase of the amount of slag former addition, the trends of the cobalt distribution into the ingot and the stag depended on the kind of slag former used in the melting of the stainless steel while the effect of the slag basicity on the distribution of the cobalt was not clarified in the melting of carbon steel. Tn the melting of the carbon steel, the strontium was captured at up to $50\%$ into the slag phase. Cesium was completely eliminated from the melt of the stainless steel as well as the carbon steel and distributed to the dust phase.

  • PDF

Fracture Toughness and Slinding Wear Properties of ABOw/AC4CH by Binder Additives (ABOw/AC4CH의 바인더 종류에 따른 파괴인성 및 미끄럼마모 특성)

  • Park, Won-Jo;Jung, Jae-Wook;Choi, Yong-Bum;Lee, Kwung-Young
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2002.10a
    • /
    • pp.373-378
    • /
    • 2002
  • Metal matrix composites have a great interest in recent years because high specific strength, high specific stiffness characteristics, and application ranges of the composites are extend to variety industry. In this paper, an investigation was performed on the plane strain fracture toughness and slinding wear properties of AC4CH alloy(Al-Si-Mg line) reinforced with 20wt% aluminum borate whisker expect one, which contained a inorganic binder($TiO_2$). the binder led to the formation of strengthen the whisker each other. The test of fracture toughness was using CT(half size) specimen of thickness 12.5mm, width 25mm. and test of slinding wear of using tribo a pin-on-disk machine and lubricant is used without paraffine 8.2CST at room temperature. As results, Fracture toughness $K_{IC}$ is $8.7MPa-m^{05}$ for ABOw/AC4CH, $9.28MPa-m^{05}$ for ABOw/AC4CH added $TiO_2$. but AC4CH alloy was violated the critical stipulated by ASTM standard for valid measurement of $K_{IC}$. In case of, it was performed $J_{IC}$ test instead of $K_{IC}$ based on ASTM E 1820.

  • PDF

Effect of an Aging Treatment on the Interfacial Reaction and Mechanical Properties of an AS52+Sr/Al18B4O33 Magnesium Matrix Composite (AS52+Sr/Al18B4O33 복합재료 계면반응 및 기계적 특성에 미치는 시효 열처리의 영향)

  • Park, YongHa;Park, YongHo;Park, IkMin;Cho, KyungMox
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.10
    • /
    • pp.957-963
    • /
    • 2010
  • The aging behavior of aluminum borate whisker ($Al_{18}B_4O_{33}$) reinforced AS52+Sr magnesium matrix composites was investigated with Vickers hardness measurements, bending tests, scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Experimental results showed that aging is accelerated in the $AS52+Sr/Al_{18}B_4O_{33}$ composite compared with an unreinforced AS52+Sr alloy. The hardness of the alloy and composite increases monotonically as a function of the aging time before reaching its peak hardness and then gradually decreases. The composite reaches its peak hardness in 10 h, whereas the matrix alloy requires 30h, indicating accelerated age-hardening in the $AS52+Sr/Al_{18}B_4O_{33}$ composite compared with the unreinforced AS52+Sr alloy at $170^{\circ}C$. The interfacial reaction of $AS52+Sr/Al_{18}B_4O_{33}$ magnesium matrix composite is considered to play a dominant role in the strengthening mechanism, ultimately affecting the mechanical properties of the composite.

Analysis of Effective Elastic Modulus and Interfacial Bond Strength of Aluminum Borate Whisker Reinforced Mg Matrix Composite by Using Three Dimensional Unit Cell Model (3차원 Unit Cell 모델을 이용한 알루미늄 보레이트 휘스커 강화 Mg 복합재료의 유효 탄성계수 및 계면강도의 분석)

  • Son, Jae Hyoung;Lee, Wook Jin;Park, Yong Ha;Park, Yong Ho;Park, Ik Min
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.5
    • /
    • pp.469-475
    • /
    • 2010
  • In this study, the interfacial bond strength of a squeeze infiltrated $Al_{18}B_{4}O_{33}$/AS52 Mg composite was investigated by using a finite element method. Three types of Mg composites with volume fractions of 15, 25 and 35% were fabricated. Three-dimensional models of the composite were developed by using a unit cell model in order to determine the effective elastic modulus of the metal matrix composite and the interfacial bond strength between the whisker and magnesium matrix. After modeling, numerical results were compared with the experimental tensile test results of $Al_{18}B_{4}O_{33}$/AS52 Mg composites. The results showed that the effective modulus of the composite strongly depended on the interfacial strength between the matrix and reinforcement. Based on the numerical and experimental findings, it was found that the strong interfacial bond was achieved by the interfacial reaction product of 30 nm thick MgO, which led to an improvement in the mechanical properties of the $Al_{18}B_{4}O_{33}$/AS52 Mg composites.