• Title/Summary/Keyword: Aluminum Alloy 7075

Search Result 95, Processing Time 0.024 seconds

A Study on the Influence of Ceramic Coating on Characteristics of Friction and Abrasion of Aluminum Alloy(7075 T6) Used in Mechanical Casting (세라믹 코팅이 기계 주조용 알루미늄합금(7075 T6)의 마찰ㆍ마모특성에 미치는 영향에 관한 연구)

  • Lyu, Sung-Ki;Jung, Kwang-Jo;Lu, Long
    • Journal of the Korean Society of Safety
    • /
    • v.18 no.3
    • /
    • pp.14-21
    • /
    • 2003
  • This study deals with the influence of ceramic coating on characteristics of friction and abrasion of aluminum allot(7075 T6) used in mechanical casting. In this research, frictional wear characteristic of ceramic coating materials such as $A1_2O_3$, $Si_3N_4$, SiC was investigated using aluminum alloy(7075 T6) and stainless 403 cast iron under room temperature and normal air pressure. The coating layer was observed using SEM. The conclusions are as follows: 1) Friction coefficients of $A1_2O_3$, SiC and $Si_3N_4$ are obtained 0.63 0.56 and 0.54 respectively. 2) Abrasion resistance of stainless 403 cast iron with $Si_3N_4$ is the best among the ceramic coating materials. 3) Abrasion mechanism of aluminum alloy(7075 T6) coaled with ceramic material and stainless 403 cast iron is caused by brittle fracture. 4) Coating the ceramic material on the aluminum alloy(7075 T6) can effectively increase the antiwear, impact properties, and corrosion resistance.

Experimental Investigation of Fatigue Crack Growth Behavior in Friction Stir Welded 7075-T651 Aluminum Alloy Joints under Constant Stress Intensity Factor Range Control Testing (For LT Orientation Specimen) (일정 응력확대계수범위 제어 시험하의 마찰교반용접된 7075-T651 알루미늄 합금 용접부의 피로균열전파 거동의 실험적 고찰 (LT 방향의 시험편에 대하여))

  • Jeong, Yeui Han;Kim, Seon Jin
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.37 no.6
    • /
    • pp.775-782
    • /
    • 2013
  • In this study, as a series of studies aimed at investigating the spatial randomness of fatigue crack growth for friction stir welded (FSWed) 7075-T651 aluminum alloy joints, the fatigue crack growth behavior of FSWed 7075-T651 aluminum alloy joints was investigated for LT orientation specimens. Fatigue crack growth tests were conducted under constant stress intensity factor range (SIFR) control for 5 specimens of the FSWed 7075-T651 aluminum alloy, including base metal (BM), heat affected zone (HAZ), and weld metal (WM) specimens. The mean fatigue crack growth rate of WM specimens was found to be the highest, whereas that of HAZ and WM specimens was the lowest. Furthermore, the variability of fatigue crack growth rate was found to be the highest in WM specimens and lowest in BM specimens.

Thixo-extrusion of Semi Solid 7075 Aluminum Alloys and Mechanical Properties of The Extrudates (반응고 7075 알루미늄 합금의 반용융 압출 및 압출재의 기계적 특성)

  • Choi, Tae-Young;Kim, Dae-Hwan;Kim, Soo-Bae;Shim, Sung-Young;Lim, Su-Gun
    • Journal of Korea Foundry Society
    • /
    • v.34 no.3
    • /
    • pp.87-93
    • /
    • 2014
  • Thixo-extrusion of semi-solid 7075 aluminum alloy and the mechanical properties of its extrudates were investigated. The semisolid alloy was prepared by a cooling slope cast. In other to perform thixo-extrusion, semi-solid 7075 aluminum alloy billets were reheated at the reheating conditions reported in a previous study. The maximum extrusion pressure in thixo-extrusion was 615MPa. This was lower than that of conventional hot extrusion ($P_{max}=940MPa$) at the same extrusion conditions due to the increased fluidity of the alloy billet in the semi-solid state. The values of Rockwell hardness (scale B) at the extrusion direction of the as thixoextruded bar were 48~53HRB and the difference in Rockwell hardness between the transverse direction and the extrusion direction was 5HRB or less. The results show that thxio-extrusion of semi-solid 7075 Al alloy improves the workability and anisotropic with the extrusion direction compared with hot extrusion of the conventional alloy.

Effect of Heat Treatment History in Fabrication of Hybrid Center Pillar on Tensile Strength of 7075 Aluminum Alloy Sheet (하이브리드 센터필러 제조 시 열처리 이력이 7075 알루미늄 합금 판재의 인장강도에 미치는 영향)

  • Yoo, D.;Kim, J.H.;Park, S.;Jang, H.K.;Kim, D.
    • Transactions of Materials Processing
    • /
    • v.30 no.2
    • /
    • pp.61-68
    • /
    • 2021
  • As part of efforts to reduce the weight of automotive body-in-white, a hybrid center pillar with high strength 7075 aluminum alloy (AA7075) sheet and carbon fiber reinforced plastic (CFRP) has been recently studied. In the fabrication of the AA7075-CFRP hybrid center pillar, the AA7075 sheet might go through heating-forming-in-die quenching (HFQ), artificial aging, hybridizing, and then paint baking processes. In this study, we investigate the effects of the heat treatment history associated with each process on the tensile strength of the AA7075 sheet. Typical heat treatment conditions are HFQ for 20 minutes at 480℃ and then cooling down with die, artificial aging of T6 temper for 24 hours at 120℃, hybridizing for 10 minutes at 150℃, and paint baking for 20 minutes at 180℃. The tensile strength of the AA7075 sheet is continuously increased by a series of heat treatments of hybridizing and paint baking and is expected to have yield stress above 500MPa without artificial aging of T6 temper.

A Study on the Compressive Properties of Thixo-Extruded 7075 Aluminum Alloy (7075 알루미늄 합금 반용융 압출재의 압축특성)

  • Kim, Dae-Hwan;Jung, Hyun-Ju;Lim, Su-Gun
    • Journal of Korea Foundry Society
    • /
    • v.37 no.2
    • /
    • pp.38-44
    • /
    • 2017
  • Given that the conventional extrusion of high-strength Al alloys such as 7075 aluminum alloys is difficult due to their very low extrudability as compared to that of 6061 aluminum alloys, thixo-extrusion can be used to obtain a high-strength material easily at a lower extrusion pressure as compared to conventional extrusion. In this study, hot- and thixo-extruded 7075 aluminum alloys are prepared by a vertical forward extrusion process and their microstructures, hardness levels, and compressive properties are investigated. Hot-extruded alloy bars are assessed to obtain a microstructure elongated in the extrusion direction, whereas with thixo-extruded alloy bars, it was possible to obtain a microstructure having fine and equiaxed grains by dynamic recrystallization. The resulting isotropy and improved formability at the hot deformation temperature of the thixo-extruded alloy were attributed to the fine and equiaxed grains formed by the thixo-extrusion process.

Marco and Microscopic Observations of Fatigue Crack Growth in Friction Stir Welded 7075-T651 Aluminum Alloy Plates (마찰교반용접된 7075-T651 알루미늄 판재의 피로균열전파의 거시적 및 미시적 관찰)

  • Kong, Yu-Sik;Kim, Seon-Jin
    • Journal of Power System Engineering
    • /
    • v.18 no.2
    • /
    • pp.62-69
    • /
    • 2014
  • In this paper, in order to investigate the effects of marco and microscopic observations of fatigue crack growth in friction stir welded (FSWed) 7075-T651 aluminum alloy plates, fatigue crack growth tests were performed under constant amplitude loading condition at room temperature with three different pre-cack locations, namely base metal (BM-CL) and two kinds of pre-crack locations in welded joints, weld metal (WM-CL) and heat affected zone (HAZ-CL) specimens. The fatigue crack growth behavior of FSWed 7075-T651 aluminum alloy plates were discussed based on the marco and microscopic fractographic observations. The marcoscopic aspects of surface crack growth path for BM-CL and HAZ-CL specimens indicate relatively straight lines, however, the crack growth paths of WM-CL specimens grow first straight and by followed toward the TMAZ and HAZ. The microscopic aspects of fatigue fracture for BM-CL and HAZ-CL specimens indicate typical fatigue striation, but WM-CL showed intergranular fracture pattern by micro structural changes of FSW process.

Microstructural Control of AA7075 Alloy for Thixoextrusion (반용융 압출을 위한 AA7075 합금의 조직제어)

  • Yoon, Young-Ok;Kim, Young-Jig;Kim, Shae-K.;Jo, Hyung-Ho
    • Journal of Korea Foundry Society
    • /
    • v.25 no.6
    • /
    • pp.249-253
    • /
    • 2005
  • The present study focuses on 7075 aluminum wrought alloy to investigate the potential industrial applications of thixoextrusion process. The microstructural evolution of 7075 aluminum wrought alloy for thixoextrusion has been investigated as a function of isothermal holding temperature and time in the partially remelted semisolid state. The results showed that the liquid fraction increased with increasing isothermal holding temperature and time while the average grain size was inversely proportional to isothermal holding temperature and time up to 5min. However, there was no big change of liquid fraction and average grain size with respect to isothermal holding temperature and time. The important fact that the liquid fraction and average grain size were almost uniform after 5 min holding time is considered very useful for thixoextrusion in terms of process control.

A Study on the properties of aluminum nitride films on the Al7075 deposited by pulsed DC reactive magnetron sputtering

  • Kim, Jung-hyo;Cha, Byung-Chul;Lee, Keun-Hak;Park, Won-Wook
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2012.11a
    • /
    • pp.179-180
    • /
    • 2012
  • Aluminum alloys are widely known as non-ferrous metal with light weight and high strength. Consequently, these materials take center stage in the aircraft and automobile industry. The Al7075 aluminum alloy is based on the Al-Zn-Mg-Cu and one of the strongest wrought aluminum alloys. Aluminum nitride has ten times higher thermal conductivity($319W/m{\cdot}K$) than Al2O3 and also has outstanding electric insulation($1{\times}1014{\Omega}{\cdot}cm$). Furthermore, it has high mechanical property (430 MPa) even though its co-efficient of thermal expansion is less than alumina For these reasons, it has great possibilities to be used for not only the field which needs high strength lightweight but also electronic material field because of its suitability to be applied to the insulator film of PCB or wafer of ceramic with high heat conduction. This paper investigates the mechanical properties and corrosion behavior of aluminum alloy Al7075 deposited with aluminum nitride thin films To improve the surface properties of Al7075 with respect to hardness, and resistance to corrosion, aluminum nitride thin films have been deposited by pulsed DC reactive magnetron sputtering. The pulsed DC power provides arc-free deposition of insulating films.

  • PDF

Estimation of Machinability Turning Process for Al7075-T6 by Cryogenic Heat Treatment (극저온 열처리된 Al7075-T6의 선삭특성 분석)

  • Lim, Hak Jin;Oh, Jeong Kyu;Kim, Pyeong Ho;Lee, Jong Hwan;Kim, Jeong Suk
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.22 no.5
    • /
    • pp.865-870
    • /
    • 2013
  • In recent years, aluminum processing has been increasing in the aerospace, vehicle, airplane industries etc., because aluminum has abundant resources and has a high specific strength. Aluminum alloys have a high coefficient of thermal expansion therefore, it is necessary to consider the temperature problem in the cutting process. The objective of this research is to investigate the machinability of a hardened aluminum alloy Al7075-T6 by using cryogenic heat treatment. The machining test is conducted by comparing the cutting force and surface roughness, corresponding to various cutting conditions of depth of cut, cutting speed, and feed rate, with those of Al7075-T0.

The Effect of Cooling Rate on the Solidification Behavior and Segregation of 7075 and 7050 Aluminum Alloys (7075 및 7050 알루미늄 합금의 응고 거동 및 편석에 미치는 냉각 속도의 영향)

  • Choi, Jeong-Yun;Kwon, Young-Dong;Lee, Joo-Won;Lee, Zin-Hyoung
    • Journal of Korea Foundry Society
    • /
    • v.21 no.6
    • /
    • pp.343-349
    • /
    • 2001
  • The effect of cooling rate on the solidification microstructure and segregation behavior of 7075 and 7050 aluminum alloy was investigated. Samples were solidified with cooling rates from 0.3 to $17^{\circ}K/sec$. Using the cooling curves of each sample, liquidus, eutectic and intermetallic reaction temperatures were estimated. The microstructures were characterized in terms of dendrite arm spacing and eutectic volume fraction. The segregation behavior of each alloying element of these alloys in various cooling rates was discussed.

  • PDF