Hydration Mechanism of Alkali Activated Slag Cement

  • Jong Cheol Kim;Keun Ho Auh;Sung Yun Hong
    • The Korean Journal of Ceramics
    • /
    • v.5 no.1
    • /
    • pp.35-39
    • /
    • 1999
  • For many years, alkali activated blast furnace slag cement containing no ordinary portland cement has received much attention in the view of energy saving and its many excellent properties. We examined the structural change of slag glass which was activated by alkali metal compounds using IR spectroscopy. The properties of hydrated products and unhydrated slag grains was characterized by XRD and micro-conduction calorimeter. Ion concentration change in the liquid during the hydration of blast furnace slag was also studied to investigated the hydration mechanism.

  • PDF

Estimation of Strength and Pore Structure of Alkali-Activated Fire Protection Materials at High Temperature (고온에서의 알칼리 활성화 내화성 결합재의 강도 및 공극구조 평가)

  • Song, Hun;Kim, Young-Ho;Kim, Wan-Ki;So, Hyung-Suk
    • Journal of The Korean Digital Architecture Interior Association
    • /
    • v.12 no.4
    • /
    • pp.59-66
    • /
    • 2012
  • This study is interested in identifying the effectiveness of alkali-activated fire protection material compounds including the alkali-activator such as potassium hydroxide, sodium silicate and fly ash as the fire resistant finishing materials. Also, this paper is concerned with change in compressive strength and pore structure of the alkali-activated fire protection material at high temperatures. The testing methods of fire protection materials in high temperature properties are make use of TG-DSC and mercury intrusion porosimetry measurements. This study results show that compressive strength is rapidly degraded depending on a rise of heating temperature. Porosity showed a tendency to increase irrespective of specimen types. This is due to both the outbreak of collapse of gel comprising the cement and a micro crack by heating. However, alkali-activated fire protection material composed of potassium hydroxide, sodium silicate and fly ash has the thermal stability of the slight decrease of compressive strength and porosity at high temperature. These thermal stability is caused by the ceramic binding capacity induced by alkali activation reaction by the reason of the thermal analysis result not showing the decomposition of calcium hydrate.

The Compressive Strength Development of Briquette Ash by Alkali Activated Reaction (알칼리 활성반응에 의한 Briquette ash의 강도 발현 특성)

  • Seo, Myeong-Deok;Lee, Su-Jeong;Park, Hyun-Hye;Kim, Yun-Jong;Lee, Su-Ok;Kim, Taik-Nam;Cho, Sung-Baek
    • Korean Journal of Materials Research
    • /
    • v.18 no.9
    • /
    • pp.463-469
    • /
    • 2008
  • Non-sintering cement was manufactured with briquette ash. Alkali activator for compression bodies used a NaOH solution. In order to apply alkali-activated briquette ash and the non-sintering cement to concrete, several experimental studies were performed. It was necessary to study the binder obtained by means of a substitute for the cement. This study concentrated on strength development according to the concentration of NaOH solution, the curing temperature, and the curing time. The highest compressive strength of compression bodies appeared as $353kgf/cm^2$ cured at $80^{\circ}C$ for 28 days. This result indicates that a higher curing temperature is needed to get a higher strength body. Also, geopolymerization was examined by SEM and XRD analysis after the curing of compression bodies. According to SEM and XRD, the main reaction product in the alkali activated briquette ash is aluminosilicate crystal.

Analysis of Internal Structure in Alkali-Activated Fire Protection Materials Using Fly ash (플라이애시를 활용한 알칼리 활성화 내화성 마감재의 내부구조 분석)

  • Song, Hun;Chu, Yong-Sik;Lee, Jong-Kyu
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.4
    • /
    • pp.104-112
    • /
    • 2012
  • This study involves investigating the correlation between variation of internal structure and heating temperature of alkali-activated fire protection materials using fly ash. Dehydration and micro crack thermal expansion occur in cement hydrates of cementitious materials heated by fire. Internal structure difference due to both the dehydration of cement hydrates and pore solution causes and influences changes in the properties of materials. Also, this study is concerned with change in microstructure and dehydration of the alkali-activated fire protection materials at high temperatures. The testing methods of alkali-activated fire protection materials in high temperature properties are make use of TG-DSC and mercury intrusion porosimetry measurements. The study results show that the alkali-activated fire resistant finishing material composed of potassium hydroxide, sodium silicate and fly ash has the high temperature thermal stability. These thermal stability is caused by the ceramic binding capacity induced by alkali activation reaction.

  • PDF

A Preliminary Study on Alkali Activation of Waste Concrete Powder

  • Sasui, Sasui;Kim, Gyu-Yong;Eu, Ha-Min;Lee, Yae-Chan;Phyeon, Su-Jeong;Nam, Jeong-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2023.05a
    • /
    • pp.303-304
    • /
    • 2023
  • In this study, the effects of NaOH and KOH alkali activators of various concentrations on the performance of alkali activated waste concrete powder (WCP) was discussed. The samples activated by alkaline solutions were cured for up to 28 days and then compressive strength test was performed. These samples were also characterized using various techniques to explore the phase evolution, and microstructural changes. Results showed superior performance of NaOH-activated WCP. Additionally, activation of WCP by 8M concentrated alkali solutions improved the strength, reactivity and microstructure of alkali activated WCP binder sample.

  • PDF

Evaluation of Absorbent-Pervious Alkali-Activated Block Using Recycled Aggregate (순환골재를 이용한 보투수성 알칼리 결합재 블록의 성능평가)

  • Park, Kwang-Min;Kim, Hyung-Suk;Cho, Young-Keun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.2
    • /
    • pp.160-167
    • /
    • 2017
  • The purpose of this study is to identify the possibility of developing the 100% Recycled-resources Absorbent-Pervious Alkali-activated Blocks using both the alkalli-binder and the recycled aggregate. In addition, It established a test method such as Void ratio, compressive strength, coefficient permeability, absorption, and evaporation. As a result, an alkali-activated using recycled aggregate block was able to manufacture an 24 MPa class absorbent-pervious blocks with a liquid type sodium silicate and early high temperature curing. In this case, water-holding capacity, absorption and relative absorption were more effective than the natural aggregates. In conclusion, Absorbent-pervious alkali-activated Block Using recycled aggregate has a surface temperature reducing effect of approximately 10 % compared to ordinary concrete block.

Isothermal Conduction Calorimetry Analysis of Alkali Activated Slag Binder (알칼리 활성 슬래그 결합재의 미소수화열 분석)

  • Choi, Young-Cheol;Cho, Hyun-Woo;Oh, Sung-Woo;Moon, Gyu-Don
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.3
    • /
    • pp.237-243
    • /
    • 2015
  • In this research, isothermal conduction calorimetry analysis has been conducted to investigate the reactivity of alkali activated slag binders. In order to secure the reactivity and workability of alkali activated slag binders, experiences with various types and concentrations of alkali activators were performed. Isothermal conduction calorimetry were measured with different alkali activators and mass ratio of $SO_3$ to binders as variables, and sodium tripolyphosphate ($Na_2P_3O_{10}$) and hydrated sodium borate ($Na_2B_4O_710H_2O$) were used to control setting time. As a results, alkali activated slag binders required alkali activators with 4 to 5 percent of concentration to accelerate the formation of calcium silicate hydrate(C-S-H) by alkali-activation, and overall heat generation rate delayed as accumulated heat decreased due to the high $SO_3$ contents. Moreover, the use of hydrated sodium borate as setting retarder causes elongated setting time due to delaying heat generation, so it can be considered that setting retarder played an important role in delaying total heat generation rate.

A Study on the Alkali-Silica Reaction of Geopolymer Mortar (지오폴리머 모르타르의 알칼리-실리카반응에 관한 연구)

  • Kim, Sung-Hoon;Kim, Young-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2015.11a
    • /
    • pp.7-8
    • /
    • 2015
  • The purpose of this study is to investigate the expansion of alkali-activated geopolymer mortar containing reactive aggregate due to alkali-silica reaction. In addition, this study is particularly concerned with the behavior of these alkaline materials in the presence of reactive aggregates. The test method included expansion measurement of the mortar bar specimens and geopolymer compressive strength test. Major results that alkali-activated geopolymer mortars showed expansion due to the alkali-silica reaction. geopolymer mortars is safety for the expansion exhibited less than 0.2% at 14 day.

  • PDF

Microstructural, Mechanical, and Durability Related Similarities in Concretes Based on OPC and Alkali-Activated Slag Binders

  • Vance, Kirk;Aguayo, Matthew;Dakhane, Akash;Ravikumar, Deepak;Jain, Jitendra;Neithalath, Narayanan
    • International Journal of Concrete Structures and Materials
    • /
    • v.8 no.4
    • /
    • pp.289-299
    • /
    • 2014
  • Alkali-activated slag concretes are being extensively researched because of its potential sustainability-related benefits. For such concretes to be implemented in large scale concrete applications such as infrastructural and building elements, it is essential to understand its early and long-term performance characteristics vis-a'-vis conventional ordinary portland cement (OPC) based concretes. This paper presents a comprehensive study of the property and performance features including early-age isothermal calorimetric response, compressive strength development with time, microstructural features such as the pore volume and representative pore size, and accelerated chloride transport resistance of OPC and alkali-activated binder systems. Slag mixtures activated using sodium silicate solution ($SiO_2$-to-$Na_2O$ ratio or $M_s$ of 1-2) to provide a total alkalinity of 0.05 ($Na_2O$-to-binder ratio) are compared with OPC mixtures with and without partial cement replacement with Class F fly ash (20 % by mass) or silica fume (6 % by mass). Major similarities are noted between these binder systems for: (1) calorimetric response with respect to the presence of features even though the locations and peaks vary based on $M_s$, (2) compressive strength and its development, (3) total porosity and pore size, and (4) rapid chloride permeability and non-steady state migration coefficients. Moreover, electrical impedance based circuit models are used to bring out the microstructural features (resistance of the connected pores, and capacitances of the solid phase and pore-solid interface) that are similar in conventional OPC and alkali-activated slag concretes. This study thus demonstrates that performance-equivalent alkali-activated slag systems that are more sustainable from energy and environmental standpoints can be proportioned.

An Experimental Study on Alkali-Silica Reaction of Alkali-Activated Ground Granulated Blast Furnace Slag Mortars (알칼리 활성 고로슬래그 미분말 모르터의 알칼리-실리카 반응에 관한 실험적 연구)

  • Kim, Young-Soo;Moon, Dong-Il;Lee, Dong-Woon
    • Journal of the Korea Institute of Building Construction
    • /
    • v.11 no.4
    • /
    • pp.345-352
    • /
    • 2011
  • The purpose of this study was to investigate the expansion of alkali-activated mortar based on ground granulated blast furnace slag containing reactive aggregate due to alkali-silica reaction. In addition, this study was particularly concerned with the behavior of these alkaline materials in the presence of reactive aggregates. The experimental program included expansion measurement of the mortar bar specimens, as well as the determination of the morphology and composition of the alkali-silica reaction products by using scanning electron microscopy(SEM), and energy dispersive x-ray(EDX). The experiment showed that while alkali-activated ground granulated blast furnace slag mortars showed expansion due to the alkali-silica reaction, the expansion was 0.1% at Curing Day 14, showing that it is safe. After the accelerated test, SEM and BEM analysis showed the presence of alkali-silica gel and rim around the aggregate and cement paste. According to the EDX, the reaction products decreased markedly as alkali-activated ground granulated blast furnace slag was used. In addition, for the substitutive materials of mineral admixture, a further study on improving the quality of alkali-activated ground granulated blast furnace slag is needed to assure of the durability properties of concrete.