소화기용 7050 Al합금소재의 적용성 개발 (Application development of 7050Al alloy in small arms.)

  • 김헌규;최중환
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1996년도 추계학술대회 논문집
    • /
    • pp.1093-1097
    • /
    • 1996
  • The Substitution development of 7075-T6 Al alloy to 7050-T74 Al alloy in small arms to improve anti-stress corrosion cracking was processed along with mass productivity consideration. To meet 7050 Al alloy material characteristics Indirect extrusion type was adopted and local heating above recrystalization temperature in forging process had to be avoided. The T74 aging treatment was 12$0^{\circ}C$ -6hrs and 175$^{\circ}C$ -12hrs and was appropriate for both machanical and anti-cohesion properties. In accessment of field application test 7050Al alloy made parts of small arms showed equivalent or better performance than 7075 Al alloy.

  • PDF

7050 Al합금의 응력부식저항성에 미치는 2단 시효처리의 영향 (Effect of Two-Step Aging Treatment on the Stress Corossion Cracking Resistance of 7050 Al Alloy)

  • 최중환;김종기;김헌규;이상래;김인배
    • 한국재료학회지
    • /
    • 제9권7호
    • /
    • pp.695-700
    • /
    • 1999
  • 7050 Al합금의 응력부식저항성에 미치는 2단 시효처리의 영향을 미세조직관찰, 전기전도도시험 및 SCF값을 평가함으로써 조사하였다. 최대 경도 이상 과시효에 의해 주 강화상인 η'상이 η상으로 변태되었고, 입내 및 입계에 존재하는 η상의 크기와 간격이 커졌으며 그 결과 응력부식저항성이 증대되었다. 2차 시효시간의 증가에 따라 전기전도도값은 증가되었으나 항복강도의 감소로 인하여 SCF값은 감소되었는데, 이러한 결과는 응력부식저항성의 증가를 의미한다. AMS 4107규격을 기준으로 하였을 때 7050 Al합금 단조재의 적정시효조건은 1차시효가 12$0^{\circ}C$에서 6시간, 2차시효는 $175^{\circ}C$에서 12시간이었다.

  • PDF

질소이온 주입시킨 7050A1 합금의 표면 미세구조 변화의 분석 (Analyzing Surface Microstructure of 7050A1 Alloy Modified by $N^+ion$ Implantation)

  • 이창우;권숙인;한전건
    • 분석과학
    • /
    • 제7권4호
    • /
    • pp.527-540
    • /
    • 1994
  • 본 연구는 질소이온 주입시킨 7050A1 합금의 표면 미세구조 변화에 대하여 살펴보았다. 이온 주입은 이온을 가속시켜서 물리적으로 모재의 표면에 주입시키는 표면처리의 한 방법으로서, 본 연구에서는 가속 에너지를 100KeV로 하고 전류밀도는 $23.1{\mu}A/cm^2$, 주입량은 $5{\times}10^{15}ions/cm^2$, $5{\times}10^{17}ions/cm^2$과, $8{\times}10^{17}ions/cm^2$로 질소이온을 주입하였다. 이온 주입층은 EPMA, AES, XPS, TEM 등으로 분석하였으며, 그 결과를 computer simulation을 통하여 비교하여 보았다. 질소이온 주입시킨 7050A1 합금은 극 표면에서부터 약 $4000{\AA}$ 사이에서 AlN이 Gaussian 분포를 지니고 있었으며, 일정 깊이에서 이온의 주입에 의해 충격을 받은 영역을 관찰할 수 있었고 이러한 표면의 변화들은 미소경도에 영향을 미치게 되어 저하중에서 경도값의 상승을 야기했다.

  • PDF

항공기용 Al 합금 단조품의 특성 향상을 위한 단조 공정 설계 (Forging Process Design to Improve the Properties of Al Alloy Forged Part for Aerospace)

  • 이영선;이정환
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2001년도 추계학술대회 논문집
    • /
    • pp.228-232
    • /
    • 2001
  • Fatigue strength, electrical conductivity and stress-corrosion-cracking resistance are considered as important factors at aircraft Al alloys, therefore Al7050 alloy has been developed to improve such properties. However, hammer-forged Al7050 parts showed the undesirable structures such as severe local grain coarsening and inhomogeneous material flow, resulted in the degraded mechanical properties. In this paper, process conditions are investigated for elimination of the grain coarsening and improved material flow during forging process by both of experiments and FEM analysis. Particular interest has been given to understand role of preform shape on the grain coarsening behavior and magnitude of the hammer forging load The use of preform has been beneficial for reduction of the forging load and elimination of the grain coarsening. However, in the cases of as received bar and the round bar, which was machined to 2.5mm thickness in surface layer, some degree of local grain coarsening behavior has been observed. The optimized preform shape could be properly designed by applying the FEM simulation.

  • PDF

7050Al 합금의 열처리공정 개발에 관한 연구 (A study on the heat treatment processing of 7050 aluminum alloy)

  • 이효수;남태운;이병권
    • 열처리공학회지
    • /
    • 제9권2호
    • /
    • pp.139-146
    • /
    • 1996
  • The aero-industry is union industry which includes a research development type, a knowledge accumulation type and a developed country type. The aero-industry of Korea is in semi-developed type stage but departed later than that of other country such as Taiwan, Indonesia etc. Therefore, the necessity of domestic airplane material is required. This study on 7050Al extruded alloy aims to suggest an adequate heat treatment conditions of T73, T74 and T76. The results of this study show that; 1. The optimum conditions of T7x heat treatment in extruded 7050Al alloy show this; $$T73:121^{\circ}C{\times}7hr+177^{\circ}C{\times}14hr$$. $$T74:121^{\circ}C{\times}7hr+177^{\circ}C{\times}10hr$$. $$T76:121^{\circ}C{\times}7hr+163^{\circ}C{\times}21hr$$. 2. The 2nd step aging heat treatment such as T73, T74 and T76 etc. is efective in 7050Al alloy but the variation otf microstructure and mechanical property with dispersive inclusions produced for extrusion process causes some troubles. Accordingly, in order to produce a good 7050Al alloy, a careful attention is needed in manufacturing process.

  • PDF

7050 Al합금의 미세조직 및 기계적성질에 미치는 시효처리의 영향 (Effect of Aging Treatment on the Microstructures and Mechanical Properties of 7050 Al Alloy)

  • 김종기;최중환;김인배;김종기;이상래
    • 한국재료학회지
    • /
    • 제7권9호
    • /
    • pp.789-794
    • /
    • 1997
  • 7050AI합금의 미세조직 및 기계적성질에 미치는 2단시효처리의 영향을 투과전자현미경, 열분석, 경도시험 및 인장 시험을 통하여 조사하였다. 12$0^{\circ}C$에서 6시간 1차 시효처리한 후 1$65^{\circ}C$와 175$^{\circ}C$에서 2차 시효처리하였을때 1$65^{\circ}C$에서는 6시간 시효시 최대경도값 201.3Hv를 나타내었고, 175$^{\circ}C$에서는 3시간 시효처리하였을때 최대경도값 197Hv를 나타내었다.

  • PDF

Ag 첨가가 7050 Al합금의 기계적 성질에 미치는 영향 (Effect of Ag Addition on the Mechanical Properties of 7050 Al Alloy)

  • 곽서희;정영훈;권숙인;조권구;신명철
    • 열처리공학회지
    • /
    • 제12권2호
    • /
    • pp.129-135
    • /
    • 1999
  • The effects of Ag addition on the microstructures and mechanical properties of 7050 Al alloy were investigated. Various homogenizing and aging treatments were carried out to analyze the controversial effects of Ag in 7050 Al alloy. Transmission electron microscopy(TEM) was used for microstructural analysis. The hardening precipitates(${\eta}^{\prime}$) become finer with Ag addition. It suggests that Ag promotes easier nucleation of ${\eta}{\prime}$. The strength of overaged Ag bearing alloys are higher than that of Ag free alloy. Hardening precipitates(${\eta}^{\prime}$) in Ag bearing alloys are smaller than that of Ag free alloys, because the growth rate of ${\eta}^{\prime}$ during overaging stage is lower in Ag bearing alloys.

  • PDF