Texture and Plastic deformation of the Severe Ecaped and Heatreated AA 1050 Aluminum Alloy Sheet (심한 전단변형(ECAP)과 열처리한 알루미늄 AA 1050 합금 판재의 소성변형비와 집합조직)

  • Akramov Saidmurod;Lee M. K.;Kim I.;Park B. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2005.05a
    • /
    • pp.148-151
    • /
    • 2005
  • A study on the microstructure and the texture of the samples after ECAP and subsequent heat treatment has been carried out. The specimens after ECAP showed a very fine grain size, a decrease of <100> // ND, and an increase of <111> // ND textures. The $\{111\}<112>,\;\{123\}<634>,\;\{110\}<001>,\;\{112\}<111>,\;\{110\}<111>,\;and\;\{013\}<231>$ texture components were increased in the specimens after the ECAP and subsequent heat-treatment at $400^{\circ}C$ for 1 hour. One of the most important properties in sheet metals is formability. The r-value or plastic strain ratio has been used as a parameter that expresses the formability of sheet metals. The change of the plastic strain ratios after the ECAP and subsequent heat-treatment conditions has been investigated and it was found that they were two times higher than those of the initial Al sheets. This could be attributed to the formation above texture components through the ECAP and subsequent heat-treatment.

  • PDF

The Study on Coatings to Improve the Radiative Heat Dissipation of Aluminum Alloy (알루미늄 합금의 복사방열향상을 위한 코팅연구)

  • Seo, Mihui;Kim, Donghyun;Lee, Junghoon;Chung, Wonsub
    • Journal of the Korean institute of surface engineering
    • /
    • v.46 no.5
    • /
    • pp.208-215
    • /
    • 2013
  • The aim of the present study was to improve the radiative heat dissipation of aluminum alloy, Al 1050. Resin/CuO coating and Cu/CuO composite plating were applied on aluminum alloy to improve the radiative heat dissipation. Resin/CuO coating was made using thermosetting silicon resin and Cu/CuO composite plating was made in pyrophosphate copper plating bath. Radiant heat flux($W/m^2$) was measured by self-produced radiant heat measurement device to compare each specimen. The cross section of specimen and chemical bonding of surface were analyzed by FE-SEM, XPS and FT-IR. As a result, radiant heat of Resin/CuO coating was higher than Cu/CuO composite plating due to the adhesion with aluminum plate and the difference in chemical bonding. But, Both of them were higher than aluminum alloy. In order to confirm the result of experiment, aluminum plate, Resin/CuO coating and Cu/CuO composite plating sample were applied LED and measured the LED temperature. As a result, LED temperature of samples were matched previous results and confirmed coated samples were lower about 10 degrees than the aluminum alloy.

A Development of Optimizing Tools for Friction Stir Welding with 2 mm Thick Aluminum Alloy using a Milling Machine (밀링을 이용한 AI합금의 마찰 교반용접용 최적공구형상 및 치수개발에 관한 연구)

  • 장석기;신상현
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.25 no.4
    • /
    • pp.791-796
    • /
    • 2001
  • Friction stir welding is a solid phase welding process that does not melt the metal when welding. The FSW is the most remarkable and potentially useful new welding technique that is still in development. Friction stir butt welding process on 2 mm thick Al 1050 plates by utilizing a milling machine was experimentally studied. With the optimized heat generating tool welds could be achieved that are void and crack free. It was found that the friction stir welded tensile test specimens failed in the HAZ outside of the weld metal, and that the tensile strength was above 90% of that of the base metal.

  • PDF

Effects of phase changes on mechanical properties of Ti-Nb alloys (Ti-Nb계 합금의 상변화가 기계적 성질에 미치는 영향)

  • Park, Hyo-Byeong
    • Journal of Technologic Dentistry
    • /
    • v.27 no.1
    • /
    • pp.9-17
    • /
    • 2005
  • The use of titanium alloys as biomaterials is increasing due to their superior biocompatibility and enhanced corrosion resistance compared to conventional stainless steels and cobalt-based alloys. Ti-6Al-4V ($\alpha+\beta$type) alloy instead of pure titanium ($\alpha$type) is being widely used as biomaterials has some characteristics such as high fatigue strength, tensile strength and corrosion resistance. But it has been reported recently that the vanadium element expresses cytotoxicity and the aluminium element is related with dementia of Alzheimer type and neurotoxicity. In order to overcome their detrimental effects, $\beta$-phase stabilizer Nb was chosen in the present study. This paper was described the influence of phase changes of Ti-Nb alloys on mechanical properties. Ti-3wt.%Nb($\alpha$type),Ti-20wt.%Nb($\alpha+\beta$type) and Ti-40wt.%Nb($\beta$type) alloys were melted by vacuum arc furnace. The specimens were homogenized at 1050$^{\circ}C$ for 24hr and were then hot rolled to 50% reduction. Each alloys were solution heat treated at $\beta$ zone and $\alpha+\beta$ zone after homogenization and then were aged. The mechanical properties of Ti alloys were analysed by hardness test, tensile test, elongation test and SEM test. The results can be summarized as follows: 1) The higher hardness value of $\alpha+\beta$type alloy was obtained compared to the, $\alpha,\beta$type alloys. 2) The aged treated showed better hardness compared to the solution heat treated, homogenized. 3) In the case of solution and aging treatment at $\beta$region, the $\alpha+\beta$type alloy showed the most highest tensile strength and $\beta$type alloy showed the best elongation.

  • PDF

Effect of process conditions on crystal structure of Al PEO coating. I. Unipolar pulse and coating time (알루미늄 PEO 코팅의 결정상에 미치는 공정 조건에 대한 연구 I. Unipolar 펄스와 코팅시간)

  • Kim, Bae-Yeon;Ham, Jae-Ho;Lee, Deuk Yong;Kim, Yong-Nam;Jeon, Min-Seok;Kim, Kiyoon;Choi, Ji-Won;Kim, Sung Youp;Kim, Kwang Youp
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.24 no.2
    • /
    • pp.59-64
    • /
    • 2014
  • Crystallographic phases of Plasma electrolytic oxidized Al alloy, A1050, were investigated. The electrolyte of PEO was $Na_2Si_2O_3$ and KOH. Unipolar pulse, $ 2000{\mu}sec$ with $400{\mu}sec+420V$ impulse, were applied for 2 min, 5 min, 15 min, and 30 min. ${\gamma}-Alumina$, as well as ${\alpha}-alumina$, was main crystal phase. ${\gamma}-Alumina$ was appeared in the beginning, then the amount of ${\alpha}-alumina$ was increased with time, but the amount of ${\gamma}-Alumina$ remained constant without any increasing. So, it is concluded that plasma gas produce ${\gamma}-Alumina$ at the first, and then ${\gamma}-Alumina$ transform ${\alpha}-alumina$ finally. During the transformation, high temperature of micro plasma gives transformation energy.

Morphology of RF-sputtered Mn-Coatings for Ti-29Nb-xHf Alloys after Micro-Pore Form by PEO

  • Park, Min-Gyu;Park, Seon-Yeong;Choe, Han-Cheol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.197-197
    • /
    • 2016
  • Commercially pure titanium (CP Ti) and Ti-6Al-4V alloys have been widely used for biomedical applications. However, the use of the Ti-6Al-4V alloy in biomaterial is then a subject of controversy because aluminum ions and vanadium oxide have potential detrimental influence on the human body due to vanadium and aluminum. Hence, recent works showed that the synthesis of new Ti-based alloys for implant application involves more biocompatible metallic alloying element, such as, Nb, Hf, Zr and Mo. In particular, Nb and Hf are one of the most effective Ti ${\beta}-stabilizer$ and reducing the elastic modulus. Plasma electrolyte oxidation (PEO) is known as excellent method in the biocompatibility of biomaterial due to quickly coating time and controlled coating condition. The anodized oxide layer and diameter modulation of Ti alloys can be obtained function of improvement of cell adhesion. Manganese(Mn) plays very important roles in essential for normal growth and metabolism of skeletal tissue in vertebrates and can be detected as minor constituents in teeth and bone. Radio frequency(RF) magnetron sputtering in the various PVD methods has high deposition rates, high-purity films, extremely high adhesion of films, and excellent uniform layers for depositing a wide range of materials, including metals, alloys and ceramics like a hydroxyapatite. The aim of this study is to research the Mn coatings on the micro-pore formed Ti-29Nb-xHf alloys by RF-magnetron sputtering for dental applications. Ti-29Nb-xHf (x= 0, 3, 7 and 15wt%, mass fraction) alloys were prepared Ti-29Nb-xHf alloys of containing Hf up from 0 wt% to 15 wt% were melted by using a vacuum furnace. Ti-29Nb-xHf alloys were homogenized for 2 hr at $1050^{\circ}C$. Each alloy was anodized in solution containing typically 0.15 M calcium acetate monohydrate + 0.02 M calcium glycerophosphate at room temperature. A direct current power source was used for the process of anodization. Anodized alloys was prepared using 270V~300V anodization voltage at room. Mn coatings was produced by RF-magnetron sputtering system. RF power of 100W was applied to the target for 1h at room temperature. The microstructure, phase and composition of Mn coated oxide surface of Ti-29Nb-xHf alloys were examined by FE-SEM, EDS, and XRD.

  • PDF

Microstructure and Abnormal Grain Coarsening Behavior of Nb-microalloyed Steel (Nb 첨가 합금강의 미세조직과 결정립 조대화 거동)

  • Sungjin Kim;Jeonghu Choi;Minhee Kim;Minhwan Ryu;Jaehyun Park;Jaehyeok Sin;Woochul Shin;Minwook Kim;Jae-Gil Jung;Seok-Jae Lee
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.37 no.4
    • /
    • pp.155-162
    • /
    • 2024
  • SCr420H steel which is commonly utilized for automotive components requires the carburizing heat treatment process. Abnormal grain growth during this treatment significantly affects the mechanical properties of the steel parts. Consequently, a process designed to prevent abnormal grain growth at certain elevated temperatures is essential. For enhanced grain refinement, we considered the addition of Nb in SCr420H steel. The experimental condition of the carburizing heat treatment involved reheating the steel sample to temperatures between 940℃ and 1080℃. Using scanning electron microscopy, we examined the microstructure of specimens treated with the secondary solution, revealing an organization of bainite and ferrite. Transmission electron microscopy was utilized to determine the type, shape, and size of the carbonitrides, showing a high fraction of AlN at the secondary solution treatment temperature of approximately 1050℃ and of (Nb,Ti)(C,N) around 1200℃. AlN particles measured about 100 nm and (Nb,Ti)(C,N) about 50 nm. Optical microscopy was utilized to assess grain size variations at different secondary solution treatment temperatures. It is noted that the temperature at which abnormal grain coarsening occurred rose with increasing secondary solution treatment temperatures, indicating a greater influence of (Nb,Ti)(C,N) with higher heat treatment temperatures. This research provides reference data for preventing abnormal grain growth in Nb-added low alloy steels undergoing carburizing heat treatment.

Si and Mg Coatings on the Hydroxyapatite Film Formed Ti-29Nb-xHf Alloys by Plasma Electrolyte Oxidation

  • Park, Seon-Yeong;Choe, Han-Cheol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.152-152
    • /
    • 2017
  • Titanium and its alloys have been widely used for biomedical applications. However, the use of the Ti-6Al-4V alloy in biomaterial is then a subject of controversy because aluminum ions and vanadium oxide have potential detrimental influence on the human body due to vanadium and aluminum. Hence, recent works showed that the synthesis of new Ti-based alloys for implant application involves more biocompatible metallic alloying element,such as, Nb, Hf, Zr and Mo. In particular, Nb and Hf are one of the most effective Ti ${\beta}$-stabilizer and reducing the elastic modulus. Plasma electrolyte oxidation (PEO) is known as excellent method in the biocompatibility of biomaterial due to quickly coating time and controlled coating condition. The anodized oxide layer and diameter modulation of Ti alloys can be obtained function of improvement of cell adhesion. Silicon (Si) and magnesium (Mg) has a beneficial effect on bone. Si in particular has been found to be essential for normal bone and cartilage growth and development. In vitro studies have shown that Mg plays very important roles in essential for normal growth and metabolism of skeletal tissue in vertebrates and can be detected as minor constituents in teeth and bone. Therefore, in this study, Si and Mg coatings on the hydroxyapatite film formed Ti-29Nb-xHf alloys by plasma electrolyte oxidation has been investigated using several experimental techniques. Ti-29Nb-xHf (x= 0, 3, 7 and 15wt%, mass fraction) alloys were prepared Ti-29Nb-xHf alloys of containing Hf up from 0 wt% to 15 wt% were melted by using a vacuum furnace. Ti-29Nb-xHf alloys were homogenized for 2 hr at $1050^{\circ}C$. The electrolyte was Si and Mg ions containing calcium acetate monohydrate + calcium glycerophosphate at room temperature. The microstructure, phase and composition of Si and Mg coated oxide surface of Ti-29Nb-xHf alloys were examined by FE-SEM, EDS, and XRD.