• 제목/요약/키워드: Al-Ni composites

검색결과 80건 처리시간 0.019초

Remarkable Stability of Graphene/Ni-Al Layered Double Hydroxide Hybrid Composites for Electrochemical Capacitor Electrodes

  • Lee, Jeong Woo;In, Su-Il;Kim, Jong-Duk
    • Journal of Electrochemical Science and Technology
    • /
    • 제4권1호
    • /
    • pp.19-26
    • /
    • 2013
  • Graphene/Ni-Al layered double hydroxide (LDH) hybrid materials were synthesized by a hydrothermal reaction. Hexagonal Ni-Al LDH particles nucleated and grew on graphene sheets, thus preventing restacking of the graphene sheets and aggregation of the Ni-Al LDH nanoparticles upon drying. Electrode made from the graphene/Ni-Al LDH hybrid materials showed a substantial improvement in electrochemical capacitance relative to those made with pure Ni-Al LDH nanoparticles. In addition, the graphene/Ni-Al LDH hybrid composite materials showed remarkable stability after 4000 cycles with over 100% capacitance retention. These materials are thus very promising for use in electrochemical capacitor electrodes.

Electrodeposition of Ni-W/Al2O3 Nano-Composites and the Influence of Al2O3 Incorporation on Mechanical and Corrosion Resistance Behaviours

  • M. Ramaprakash;R. Nivethida;A. Muthukrishnan;A. Jerom Samraj;M. G. Neelavannan;N. Rajasekaran
    • Journal of Electrochemical Science and Technology
    • /
    • 제14권4호
    • /
    • pp.377-387
    • /
    • 2023
  • Ni-W/Al2O3 nano-composites were electrodeposited on mild steel substrate for mechanical and corrosion resistance applications. This study focused on the preparation of Ni-W/Al2O3 nano-composite coating with various quantity of Al2O3 incorporations. The addition of Al2O3 in the electrolytes were varied from 1-10 g/L in electrolytes and the Al2O3 incorporation in Ni-W/Al2O3 nano-composite coatings were obtained from 1.82 to 13.86 wt.%. The incorporation of Al2O3 in Ni-W alloy matrix influenced the grain size, surface morphology and structural properties were observed. The distributions of Al2O3 particle in alloy matrix were confirmed using electron microscopy (FESEM and TEM) and EDAX mapping analysis. The crystal structure informations were studied using X-ray diffraction method and it confirms that the deposits having cubic crystal structure. The better corrosion rate (0.87 mpy) and microhardness (965 HV) properties were obtained for the Ni-W/Al2O3 nano-composite coating with 13.86 wt.% of Al2O3 incorporations.

자전고온반응에 의한 금속간화합물/금속 적층복합재료의 기계적 특성 (Mechanical Properties of Intermetallic/Metal Laminated Composite by SHS Reaction)

  • 김희연;정동석;;홍순형
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2002년도 추계학술발표대회 논문집
    • /
    • pp.60-63
    • /
    • 2002
  • Metal/intermetallic laminated composites have been manufactured by SHS reactions between Ni and Al elemental metal foils. Microstructure showed that the intermetallic volume fraction was 55%, 45%, 35% in the 1:1, 2:1, 4:1 thickness ratio(Ni:Al) specimen and the main phases of the intermetallic were transformed from $Ni_2Al_3$ to NiAl when the thickness ratio was increased. Tensile strength and elongation were increased when the volume fraction of Ni metallic phase was increased. Under assumptions of isostrain condition, the tensile strength of metal/intermetallic laminated composites didn't obey the ROM due to the thermal residual stress and this was confirmed by X-ray residual stress analysis. Fracture toughness results by the SENB test showed R-curves with upward curvature based on LSB condition. Bridging stress based on LSB condition was determined by the curve fitting analysis, In-situ observed microstructure during fracture test showed that the various bridging mechanism such as crack bridging, crack branching and ductile failure of metallic layer were occurred

  • PDF

금형주조법을 이용한 TiNi/6061Al 지적복합재료의 제조 및 기계적 특성 (Fabrication and Mechanical Properties of TiNi/6061Al Smart Composite by Permanent Mold Casting)

  • 김순국;이준희;윤두표;박영철;이규창;김영희
    • 한국주조공학회지
    • /
    • 제18권6호
    • /
    • pp.534-540
    • /
    • 1998
  • 6061Al-matrix composite with TiNi shape memory fiber as reinforcement has been fabricated by Permanent Mold Casting to investigate the mechanical properties of the smart composites. The composites have showed good interface bonding as a result of the analysis of SEM and EDX. The smartness of composite is given due to the shape memory effect of the TiNi fiber which generates compressive residual stresses in the matrix material when heated after being prestrained. The tensile strength of the composites was tested at temperatures between $90^{\circ}C$ and room temperature with increasing amount of pre-strain, and it showed that the tensile strength at $90^{\circ}C$ was higher than that of the room temperature. Especially, the tensile strength of the composite increases with increasing pre-strain. It showed that hardness of matrix was higher than that of common 6061Al alloy.

  • PDF

TiNi/Al 6061 형상기억복합재료의 기계적특성에 관한 실험 및 해석적 평가 (The Evaluation of Mechanical Properties of TiNi/Al 6061 Shape Memory Composites by Using Experimental and Finite Element Analysis)

  • 박동성;박영철;이동화;이규창
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.687-691
    • /
    • 2001
  • Al alloy matrix composite with TiNi shape memory fiber as reinforcement has been fabricated by hot pressing to investigate mechanical properties. The stress-strain behavior of the composites was evaluated at temperatures between 363K and room temperature as a function of pre-strain by using experimental and finite element analysis, and both cases showed that the tensile stress at 363K was higher than that of the room temperature. Especially, the tensile stress of this composite increases with increasing the amount of pre-strain, and it also depends on the volume fraction of fiber and heat treatment. The smartness of the composite is given due to the shape memory effect of the TiNi fiber which generates compressive residual stress in the matrix material when heated after being pre-strained.

  • PDF

무전해 니켈도금된 다중벽 탄소나노튜브의 첨가가 알루미나강화 에폭시 복합재료의 열전도도 및 파괴인성에 미치는 영향 (Influence of Electroless Ni-plated MWCNTs on Thermal Conductivity and Fracture Toughness of MWCNTs/Al2O3/Epoxy Composites)

  • 최정란;이영실;박수진
    • 폴리머
    • /
    • 제37권4호
    • /
    • pp.449-454
    • /
    • 2013
  • 본 연구에서는 무전해 니켈도금에 따른 탄소나노튜브의 표면특성변화가 알루미나강화 에폭시 복합재료의 열전도도 및 파괴인성에 미치는 영향에 대하여 살펴보았다. 무전해 니켈도금된 탄소나노튜브의 표면특성은 주사전자현미경(SEM), X-선 광전자분광기(XPS), X-선 회절분석(XRD)을 통하여 알아보았다. 열전도도는 열전도율 측정 시스템으로 측정하였고, 파괴인성은 만능시험기(UTM)를 이용한 임계응력세기인자($K_{IC}$)를 측정하여 분석하였다. 실험결과, 무전해 니켈도금은 탄소나노튜브의 표면특성의 변화를 가져오며, 니켈도금된 MWCNTs(Ni-MWCNTs)가 들어있는 경우 미처리 MWCNTs와 비교하여 우수한 열전도도 및 파괴인성을 보였다. 이는 Ni-MWCNTs와 에폭시수지와의 분자간 상호작용의 향상 때문이라 판단된다.

상향식 연속주조법에 의한 Al-Cu-Ni 3원합금의 응고조직에 관한 연구 (On the Microstructures of Al-Cu-Ni Ternary Alloys by Upward Continuous Casting)

  • 권기균;이계완
    • 한국주조공학회지
    • /
    • 제10권5호
    • /
    • pp.426-434
    • /
    • 1990
  • Continuous casting of the Al-Cu-Ni ternary eutectic alloys was carried out by the upward continuous casting process. The morphology of the ternary eutectic growth and the stability of solid-liquid interface were investigated under various growth conditions. It was possible to get the planar solid-liquid interface at the condition of $G_L/R=3.59{\times}10^3^{\circ}C\;sec/mm^2$ in Al-Cu-Ni ternary eutectic alloys. In Al-rich, Ni-rich and Cu-rich hypereutectics of Al-Cu-Ni ternary alloys, primary ${\alpha},\;{\tau}\;and\;{\theta}$ dendrites have grown as the leading phase ahead of the ternary eutectic composites.

  • PDF

SiCp입자강화 Al 복합재료의 내열 및 마모특성 (Heat and Wear Resistance Characterization of SiCp Reinforced Al Matrix Composites)

  • 김석원;김완기;우기도;안행근
    • 한국주조공학회지
    • /
    • 제20권6호
    • /
    • pp.377-385
    • /
    • 2000
  • Al matrix composites as the most promising MMCs can be expected to be excellent engineering materials in the nearest future. So as to improve material properties of composite, many manufacturing processes have been developed. Among them, squeeze casting process which offers fine microstructure and near-net-shape is one of the most successful MMCs manufacturing processes. But, in case of with subsieve size particles (under 44 ${\mu}m$), it is very difficult to homogeneously distribute particles in matrix of Al matrix composite by various casting processes, including squeeze casting used so far. Duplex process which was developed in previous study was used to distribute the particle of subsieve size more homogeneously in matrix of Al matrix composite. Microstructures, wear and heat resistance characterization of Al-Si-Cu-Mg-(Ni)/SiCp manufactured by duplex process were examined to clarify the effect of manufacturing conditions, particle size of reinforcement and alloying elements. Al matrix composites reinforced with SiCp(10 ${\mu}m$) have the lowest wear amount among composites reinforced with 3 ${\mu}m$, 5 ${\mu}m$ and 10 ${\mu}m$ SiCp. The wear amount of Al matrix composites with 10 wt.% SiCp(3, 5, 10 ${\mu}m$) was decreased according to the increase of the sliding speed because abrasive wear takes place at high sliding speed of 4m/s and worn debris with block type occurs at low sliding speed of 1m/s. As for heat resistance, it is made clear that remarkable heat resistance property can be obtained by addition of Ni element in Al matrix composites.

  • PDF