불순 Fe를 함유한 A356 주조합금에서 미세조직 형성에 관한 Mn과 Cr의 효과 (The Effects of Mn and Cr Additions on the Microstructure of A356 Alloys Containing Impure Fe)

  • 한상원
    • 한국주조공학회지
    • /
    • 제25권3호
    • /
    • pp.128-133
    • /
    • 2005
  • The effects of Mn and Cr on the crystallization behaviors of Fe-bearing intennetallics in A356 alloy were studied. Coarse and acicular ${\beta}-Al_{5}$FeSi phase in A356-0.20wt.%Fe alloy was modified into small ${\alpha}$-Al(Fe,Mn)Si and ${\alpha}$-Al(Fe,Cr)Si phases in response to Mn and Cr addition, respectively. Increasing of Mn addition amount elevates the crystallizing temperature of ${\alpha}$-Al(Fe,Mn)Si and the Mn/Fe ratio in the ${\alpha}$-Al(Fe,Mn)Si. Cr is more effective to modify ${\beta}-Al_{5}$FeSi in comparison with Mn. ${\alpha}$-Al(Fe,Mn)Si phase had BCC/SC dual structure.

Al2Ca를 함유한 A356 합금에서의 다양한 열처리 조건에 따른 공정 Si 개량화 거동 (Modification Behavior of Eutectic Si with Varying Heat Treatment Conditions in A356 Alloy with Al2Ca)

  • 김세준;현승균;김세광;윤영옥
    • 한국주조공학회지
    • /
    • 제34권5호
    • /
    • pp.156-161
    • /
    • 2014
  • This study is focused on the effect of $Al_2Ca$ as a modifier on eutectic Si modification of A356 alloy. Microstructural observation was carried out for as-cast, as-solution treated and as-aged samples. Solution treatment and aging were performed for 2, 4, 6 and 10 hrs at $540^{\circ}C$ and $170^{\circ}C$, respectively. Although A356 alloy, which $Al_2Ca$ was added, has no significant difference in as-cast phases with normal A356 alloys, it shows much more modified eutectic Si, grain refinement and improved tensile property both in as-cast and as-heat treated conditions. TGA result shows that $Al_2Ca$ added A356 alloy has a certain improvement in oxidation resistance.

저온 주조법을 응용한 Al-Zn-Mg-Cu 합금의 반응고 성형 (Semi-Solid Forming of Al-Zn-Mg-Cu Alloy Applying Low-Temperature Casting Process)

  • 김정민;김기태;정운재
    • 한국주조공학회지
    • /
    • 제22권2호
    • /
    • pp.82-88
    • /
    • 2002
  • Al-5.5Zn-2.5Mg-l.5Cu semi-solid slurry was prepared by cooling the liquid metal with a low superheat to a solid and liquid co-existing temperature. Relatively round solid particles could be obtained in the slurry through the simple process. The prepared slurry was deformed into the metallic mold by a press and the mechanical properties of obtained specimens were investigated. Mold filling ability of the alloy slurry was also investigated and compared with that of A356 alloy. Al-Zn-Mg-Cu alloy showed lower mold filling ability than A356 alloy probably because small amount of eutectic phase is present and the heat of fusion generated during solidification is smaller than that of A356 alloy.

Sr 개량처리된 사형주조 Al-7Si-0.35Mg 합금의 열처리에 따른 공정 Si상 변화거동 및 특성평가 (Behavior of Eutectic Si and Mechanical Properties of Sr Modified Al-7Si-0.35Mg alloy with Solid Solution Treatment for Sand Casting)

  • 김명균;황석민
    • 한국주조공학회지
    • /
    • 제38권1호
    • /
    • pp.1-8
    • /
    • 2018
  • In this study, we focused on the correlation between the solidification structure, heat treatment and mechanical properties of the A356 alloy according to the conditions of Sr modification. The microstructural evolution of the eutectic Si and ${\alpha}-Al$ phase in the A356 alloy castings depending on the amount of Sr were investigated during solid solution heat treatment using an optical microscope, a scanning electron microscope and an image analyzer. In addition, tensile tests on the heat treated materials examined the relationship between the microstructure and the fracture surface. The as-cast A356 alloys under 40 ppm Sr showed an undermodified microstructure, but that of the added 60-80 ppm Sr had well modified structure of fine fibrous silicon. After solid solution treatment, the microstructure of the undermodified A356 alloy exhibited a partially spheroidized morphology, but the remainder showed the fragmentation of fibrous shaped silicon. The spheroidization of the eutectic silicon in the modified A356 alloys was completed during heat treatment, which was very effective in increasing the elongation. This is supported by the fracture surface in the tensile test.

전자 교반과 결정립 미세화에 의한 반용융 A356 재료의 결정립 크기 비교 (A Comparison of the Grain Size of Semisolid A356 Aluminum Alloy Obtained by EMS Stirring and Grain Refinement)

  • 양자오;서판기;고재홍;정용식;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 추계학술대회논문집
    • /
    • pp.148-151
    • /
    • 2004
  • Different kinds of feedstock of semisolid a356 aluminum alloy manufactured by EMS stirring only, inoculation of Al-5Ti-B only and combination of inoculation and EMS stirring were investigated. It is found that the grain size of these feedstock are $350{\mu}m$ for EMS casting only, $320{\mu}m$ for inoculation by Al-5Ti-B, and $100{\mu}m$ for the combination of EMS stirring and inoculation of Al-5Ti-B master alloys. The microstructure of the sample obtain by combination of inoculation and EMS system show the best homogeneousness and finest grains.

  • PDF

Al alloy와의 경계면을 포함한 A356/SiCw의 충격거동 (Impact behavior of including the boundary between A356/SiCw and Al alloy)

  • 조종인;남현욱;한경섭
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2002년도 춘계학술발표대회 논문집
    • /
    • pp.97-100
    • /
    • 2002
  • In this research, the impact behavior of the boundary between MMC-reinforced SiC whisker and Al alloy were studied. It is known that the resultant of the interfacial reaction between SiC whisker and Al alloy has brittle and low toughness property. In this paper, impact behavior of graded MMC & Al alloy shows the interfacial opening at the boundary. Generally this phenomenon is generated by thermal residual stress, brittle interfacial reaction resultant and difference of the deflection. So, these results may be interpreted as a macroscopic method of measuring the interfacial strength between matrix and reinforcement

  • PDF

나노/마이크로 인덴터와 AFM을 이용한 스퀴즈 캐스트 A356 합금의 시효경화특성 평가 (Evaluation of Age-Hardening Characteristics of Squeeze-Cast A356 Alloy by Using Micro/Nano Indenter with AFM)

  • 윤성원;김현일;강충길
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.1398-1401
    • /
    • 2005
  • The nano/microstructure, the aging response (in T5 heat treatment), and the mechanical/tribological properties of the eutectic regions in squeeze-cast A356 alloy were investigated using nano/micro-indentation and mechanical scratching, combined wit optical microscopy and atomic force microscope(AFM). Most eutectic Si crystals in the A356 alloy showed a modified morphology as fine-fibers. The loading curve for the eutectic region was more irregular than that of the primary Al region due to the presence of various particles of varying strength. In addition, the eutectic region showed lower pile-up and higher elastic recovery than the primary Al region. The aging responses of the eutectic regions in the squeeze-cast A356 alloys aged at $150^{\circ}C$ for different times(0, 2, 4, 8, 10, 16, 24, 36 and 72 h) were investigated. As the aging time increased, acicular Si particles in the eutectic regions gradually came to a fine structure. Both Vickers hardness ($H_V$) and indentation ($H_{IT}$) test results showed almost the same trend of aging curves, and the peak was obtained at the same aging time of 10 h. A remarkable size-dependence of the tests was found. The friction coefficient for the eutectic region was lower than that for the primary Al region.

  • PDF

Al-Si-Mg계 주조용 알루미늄 합금의 고주기 피로 거동에 미치는 기공의 영향 (Effect of Porosity on the High-Cycle Fatigue Behavior of Al-Si-Mg Casting Alloy)

  • 이영재;강원국;어광준;조규상;이기안
    • 소성∙가공
    • /
    • 제18권4호
    • /
    • pp.296-303
    • /
    • 2009
  • The effect of porosity on the high-cycle fatigue properties of Al-Si-Mg casting aluminum alloys was investigated in this study. Microstructure examination, tensile and high-cycle fatigue test were conducted on both Al-Si-Mg casted (F) and heat-treated (T6) conditions. Porosity characteristics on the fracture surfaces of fatigue-tested samples were examined using SEM and image analysis. The microstructure observation results showed that eutectic Si particles were homogeneously dispersed in the matrix of the Al-Si-Mg casting alloys, but there were porosities formed as cast defects. The high-cycle fatigue results indicated that the fatigue strength of the 356-T6 alloy was higher than that of the 356-F alloys because of the significant reduction in volume fraction of pores by heat treatment. The SEM fractography results showed that porosity affected detrimental effect on the fatigue life: 80% of all tested samples fractured as a result of porosity which acted as the main crack initiation site. It was found that fatigue life decreased as the size of the surface pore increased. A comparison was made between surface pore and inner pore for its effect on the fatigue behavior. The results showed that the fatigue strength with the inner pores was higher than that of the surface pore.

Al-Si-Mg계 주조용 알루미늄 합금의 고주기 피로 거동에 미치는 기공의 영향 (Effect of Porosity on the High-Cycle Fatigue Behavior of Al-Si-Mg Casting Alloy)

  • 이영재;강원국;어광준;조규상;이기안
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.350-352
    • /
    • 2009
  • The effect of porosity on the high-cycle fatigue properties of Al-Si-Mg casting aluminum alloys was investigated in this study. Microstructure examination, tensile and high-cycle fatigue test were conducted on both Al-Si-Mg casted (F) and heat-treated (T6) conditions. Porosity characteristics on the fracture surfaces of fatigue-tested samples were examined using SEM and image analysis. The microstructure observation results showed that eutectic Si particles were homogeneously dispersed in the matrix of the Al-Si-Mg casting alloys, but there were porosities formed as cast defects. The high-cycle fatigue results indicated that the fatigue strength of the 356-T6 alloy was higher than that of the 356-F alloys because of the significant reduction in volume fraction of pores by heat treatment. The SEM fractography results showed that porosity affected detrimental effect on the fatigue life: 80% of all tested samples fractured as a result of porosity which acted as the main crack initiation site. It was found that fatigue life decreased as the size of the surface pore increased. A comparison was made between surface pore and inner pore fur its effect on the fatigue behavior. The results showed that the fatigue strength with the inner pores was higher than that of the surface pore.

  • PDF

용융금속 교반공정을 통한 고Fe 함유 A356 합금의 미세조직 개질 (Microstructural Modification of High-Fe Containing A356 Alloy by Liquid Metal Shearing Process)

  • 김봉환;이상목
    • 한국주조공학회지
    • /
    • 제31권6호
    • /
    • pp.354-361
    • /
    • 2011
  • The liquid metal shearing device was constructed and assembled with a commercial high-pressure die-caster in order to induce intensive turbulent shearing force on molten aluminum alloys. The effect of the liquid metal shearing on the microstructure and tensile properties of A356 alloys was investigated with the variation of iron content. The experimental results show that dendritic primary ${\alpha}$-Al phase was effectively modified into a equiaxed form by the liquid metal shearing. It was also found that the needle-like ${\beta}$-AlFeSi phase in a Fe containing A356 alloy was changed into a blocky shape resulting in the improved mechanical properties. Based on the mechanical properties, it was suggested that the iron content in A356 alloy could be more widely tolerated by utilizing the liquid metal shearing HPDC process.