• 제목/요약/키워드: Al 2024

검색결과 249건 처리시간 0.025초

Al 2024를 이용한 Conflat Flange Gasket의 특성 (Characteristics of Al 2024 Conflat Flange Gaskets)

  • 이철로;박재홍;홍승수;임재영;신용현;정광화
    • 한국진공학회지
    • /
    • 제1권2호
    • /
    • pp.237-243
    • /
    • 1992
  • Two gaskets of Al 2024-T4 and annealed al 2024-T4 were made. We had acquired 2 $\times$ 10-12torr in a chamber using them. Microstructures, hardness and stress concentration of the gaskets were examined before and after baking. Knife edge damages such as decrease of edge height(H) and increase of edge angle() were found on knife edges when the Al 2024-T4 gasket was used. But no damage was found with the annealed Al 2024 gasket.

  • PDF

소형펀치 시험법을 이용한 Al 2024 ECAP 재료의 강도특성 평가 (Assessment of Strength Characteristics of Al 2024 ECAP Metal Using Small Punch Testing)

  • 마영화;최정우;김선화;윤기봉
    • 대한기계학회논문집A
    • /
    • 제30권1호
    • /
    • pp.8-17
    • /
    • 2006
  • When subjected to severe shear deformation by ECAP, microstructure of Al2024 becomes extremely refined. To measure the strength of that, small punch(SP) testing method was adopted as a substitute for the conventional uniaxial tensile testing because the size of material processed by ECAP were limited to ${\psi}12\;mm$ in transverse direction. SP tests were performed with specimens in longitudinal and transverse directions of Al2024 ECAP metal. For comparing the strength values with those assessed by SP tests, uniaxial tensile tests were also conducted with specimens in longitudinal direction. Failure surfaces of the tested SP specimens showed that failure mode was shear deformation and Al 2024 ECAP metal has an anisotropy in strength. Thus, conventional equations proposed for assessing the strength characteristics were improper to assess those of Al2024 ECAP metal. In this paper a way of assessing the strength of Al 2024 ECAP metal was proposed and was proven to be effective.

ECAP Al 2024 합금의 소성변형량에 따른 강도 특성 및 이방성 연구 (A Study on Strength Characteristic Variation as amount of Plastic Deformation and Strength Anisotrophy for ECAP Al 2024 Alloy)

  • 최정우;마영화;윤기봉
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 추계학술대회 논문집
    • /
    • pp.283-286
    • /
    • 2005
  • When subjected to severe shear deformation by ECAP, microstructure of Al2024 becomes nanocrystalline grained texture material. To measure the strength of that, small punch (SP) testing method was adopted as a substitute for the conventional uniaxial tensile testing because the size of material processed by ECAP were limited to $\varphi12mm$ in transverse direction. SP tests were performed with specimens in longitudinal and transverse directions of Al 2024 ECAP metal. For comparing the strength values with those assessed by SP tests, uniaxial tensile tests were also conducted with specimens in longitudinal direction. Failure surfaces of the tested SP specimens showed that failure mode was shear deformation and Al 2024 ECAP metal has an anisotropy in strength. Thus, conventional equations proposed for assessing the strength characteristics were improper to assess those of Al2024 ECAP metal. In this paper a way of assessing the strength of Al 2024 ECAP metal was proposed and was proven to be effective.

  • PDF

2024 알루미늄의 마찰용접에 관한 연구 (A study on friction welding of 2024 aluminium)

  • 송오성;강춘식
    • Journal of Welding and Joining
    • /
    • 제8권3호
    • /
    • pp.24-30
    • /
    • 1990
  • 2024 Aluminium was welded by domestic manufactured continuous type friction welder. The problems and optimum condition were studied in 2024 Al-2024 Al cases. Mechanical tests and microstructure analysis were studeid. Interfacial temperature of welding was predicted by FDM. The obtained results are as follows: 1) In case of Al-Al, the optimum condition range was wide. 2) At the boundary zone, fine recrystallized zone was not harmful to the mechanical property and no growth of precipitation was observed. 3) In case of Al-Al, temperature gradient can be predictedby FDM and heat input can be taken as weld parameter.

  • PDF

Al2024의 고속 정면밀링 가공에서 표면 거칠기에 관한 연구 (A Study on Surface roughness in High speed face milling machining of Al2024)

  • 장성민
    • 한국산학기술학회논문지
    • /
    • 제15권2호
    • /
    • pp.603-608
    • /
    • 2014
  • 항공기와 자동차 부품과 관련된 많은 제조업에서, 낮은 비중과 높은 강도에서 뛰어난 알루미늄 합금(Al2024)은 효과적으로 사용되었다. 가공소재의 표면거칠기 품위를 위한 정면밀링 가공기술은 이들 분야에서 적용되어 왔다. 챔퍼된 드로우 어웨이 타입의 인서트를 갖는 정면밀링 가공은 단지 이론적으로 완전한 평면을 생산할 수 있다. 그러나 그것은 절삭온도, 소성변형, 동적효과 등으로 인하여 불가능하다. 본 논문에서 실험적 연구는 검증된 고속가공이 가능한 정면밀링커터 바디를 사용하여 Al2024의 고속가공 후 표면거칠기를 개선하기 위하여 수행되었다.

Rheo-compocasting법으로 제조된 알루미나 입자강화 Al합금 복합재료의 계면반응 (Interfacial Characteristics of $Al-2024/Al_2O_{3p}$ Composite Fabricated by Rheo-compocasting)

  • 현석종;예병준
    • 한국주조공학회지
    • /
    • 제13권3호
    • /
    • pp.285-294
    • /
    • 1993
  • Aluminum alloy 2024 matrix composites reinforced with $Al_2O_3$ particles, were prepared by rheo-compocasting, a process which consists of the incoporation distribution of reinforcement by stirring within a semi-solid alloy. The microstructures and characteristics of the interfaces have been studied using optical microscope and scanning electon microscope in 2024 aluminum alloy composites reinforced with $Al_2O_3$ particles. The main results are as follows: (1) $Al_2O_3$ particles were well distributed in composites by using rheo-compocasting. (2) As the addition of $Al_2O_3$ particle increases, the average dendrite numbers and the hardness were increased. (3) Interaction between $Al_2O_3$ particles and alloy 2024 resulted in the formation of Mg and Cu element rich region around the $Al_2O_3$ particles.

  • PDF

자전연소법으로 제조한 Al2O3.SiC 입자로 보강된2024/(Al2O3.SiC)p 복합재료의 기계적특성 (Mechanical Properties of 2024/(Al2O3.SiC)p Composite Reinforced with Al2O3.SiC Particle Prepared by SHS Process)

  • 맹덕영
    • 한국분말재료학회지
    • /
    • 제7권1호
    • /
    • pp.35-41
    • /
    • 2000
  • Al2O3$.$SiC particle was prepared was prepared by the self-propagting high temperature sYthesis(SHS) process from a mixture of SiO2, Al and C powders, The fabricated Al2O3$.$SiC particle was applied to 2024Al/(Al2O3$.$SiC)pcomposite as a reinforcement. Aluminum matix composites were fabricares by the powder extrusion method using the synthesized Al2O3$.$SiC particle and commercial 2024Al powder. Theoptimum preparation conditions for Al2O3$.$SiC partticle by SHS process were described. The influence of the Al2O3$.$SiC voiume fraction on the mechanical was composite was also discussed. Despite adiabatic temperature was about 2367K, SHs reaction was completed not by itself, but by using pre-heating. Mean particle size of final particle synthesized was 0.73 ${\mu}$m and most of the particle was smaller than 2${\mu}$m. Elastic modulus and tensile strength of the composite increased with increase the volume fraction of reinforcement but, tensile strength depreciated at 30 vol% of reinforcement.

  • PDF

In-situ Vacuum Hot Press 공정을 이용한 SiCp/Al 복합재료의 제조 (Fabrication of SiCp/Al Alloy Composites by In-situ Vacuum Hot Press Process)

  • 최세원;홍성길;김영만;장시영;강창석
    • 한국재료학회지
    • /
    • 제11권7호
    • /
    • pp.590-598
    • /
    • 2001
  • 본 연구에서는 특별하게 고안된 In-situ VHP 제조 공정을 이용하여 상온에서 $500^{\circ}C$까지의 진공 열간 압축과 canning 작업 없이 $520^{\circ}C$에서 연속 압출옳 하여 Sicp/pure Al과 SiCp/2024Al MMCs를 제조하였다. 복합재료의 인장강도와 미세구조에 영향을 주는 SiC 입자크기, 체적률, 압출비에 대해서 조사하였다. 압출비 10:1의 경우에는 SiCp/pure Al과 SiCp/2024Al 복합재료 둘 다 건전한 외형과 SiCp의 일정한 분산을 가지면서 SiCp의 균열이 없는 좋은 미세 구조를 가지고 있었다. 그러나 압출비 16:1의 경우에는 체적률이 증가할수록 파괴된 SiC 입자의 수가 증가하였으며 2024Al 기지내의 복합재료와 순수한 Al 기지재 복합재료를 서로 비교하였다. 동일한 체적률과 압출비의 경우에는 SiCp의 크기가 작은 복합재료가 SiCp가 큰 복합재료보다 인장강도가 더 높았다.

  • PDF

고온 프레스법에 의한 TiNi/Al2024 복합재료의 제조 및 기계적 특성평가 (Fabrication and Mechanical Properties of TiNi/Al2024 Composites by Hot-Press Method)

  • 손용규;배동수;박영철;이규창
    • 소성∙가공
    • /
    • 제18권1호
    • /
    • pp.45-51
    • /
    • 2009
  • Shape memory alloy has been used to improve the tensile strength of composite by the occurrence of compressive residual stress in matrix using its shape memory effect. In order to fabricate shape memory alloy composite, TiNi alloy fiber and Al2024 sheets were used as reinforcing material and matrix, respectively. In this study, TiNi/Al2024 shape memory alloy composite was made by using hot press method. In order to investigate bonding condition between TiNi reinforcement and Al matrix, the micro-structure of interface was observed by using optical microscope and diffusion layer of interface was measured by using Electron Probe Micro Analyser. And the mechanical properties of composite with three parameters(volume fraction of fiber, cold rolling amount and test temperature) were obtained by tensile test. The most optimum bonding condition for fabrication the TiNi/Al2024 composite material was obtained as holding for 30min. under the pressure of 60MPa at 793K. The strength of composite material increased considerably with the volume fraction of fiber up to 7.0%. And the tensile strength of this composite increased with the reduction ratio and it also depends on the volume fraction of fiber.