현장재생골재를 사용한 포장용 콘크리트의 기본 물성실험 (Evaluation of Concrete Material Properties for Pavement Using Job-site Processed Recycled Aggregates)

  • 양성철;김남호
    • 한국도로학회논문집
    • /
    • 제15권2호
    • /
    • pp.57-63
    • /
    • 2013
  • PURPOSES : This study was performed to investigate a feasibility of job-site use of recycled concrete aggregate exceeding 3% of absorption rate. Test variables are coarse aggregate types such as natural aggregate, job-site processed recycled aggregate, and recycled aggregate processed from the intermediate waste treatment company. METHODS : First, aggregate properties such as gradation, specific gravity and absorption rate were determined. Next a basic series of mechanical properties of concrete was tested. RESULTS : All strength test results such as compression, flexure and modulus were satisfied for the minimum requirements. Finally up to first 48 elapsed days the shrinkage strains of concretes made from both recycled aggregates (in case of volume-surface ratio of 300) appeared to be greater than 26% of the companion concretes made from natural aggregates. CONCLUSIONS : Drying shrinkage result is ascribed to greater absorption rate and specific gravity of those specimens made from recycled aggregate. This may be reduced with an addition of admixtures.

No-fines Concrete의 공학적 특성 (Engineering Properties of No-fines Concrete)

  • 민정기;성찬용;김성완
    • 한국농공학회지
    • /
    • 제37권1호
    • /
    • pp.73-80
    • /
    • 1995
  • This study was carried out to investigate the engineering properties of no-fines con- crete, consisting only of coarse aggregate, cement and water. The used coarse aggregates were two, one is natural coarse aggregate grading 4.75~ lOmm, the other is synthetic lightweight coarse aggregate grading 3~8mm. The results of this study are summarized as follows; 1. The W/C ratio of each type was increased with increase of additional amount of coarse aggregate. 2. The unit weight of used ndtural coarse aggregate was shown 1.762~2.184g/cm$^3$, and synthetic lightweight coarse aggregate was shown 0.756 ~ 1 .348g/cm$^3$. 3. The ahsorption rate of used natural coarse aggregate was shown 8.4 ~ 9.4 %, and synthetic lightweight coarse aggregate was shown 17.0~42.4%. 4. The compressive, tensile and hending strength was decreased with increase of coarse aggregate, respectively. The compressive strength of natural coarse aggregate 1:3 was shown 309kg/cm$^2$. 5. The ultrasonic pulse velocity and dynamic medulus of elasticity of each type was de- creased with increase coarse aggregate, respectively. Also, the decreasing rate of the natural aggregate was larger than that of the synthetic lightweight coarse ag- gregate.

  • PDF

골재-모르타르 경계면의 부착강도 특성 (Bond Strength Characteristics Between Aggregate and Mortar)

  • 박연동;양주경;임희철;김진근;장정수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1991년도 가을 학술발표회 논문집
    • /
    • pp.129-134
    • /
    • 1991
  • The effects of water-cement ratio, age, and admixture such as fly ash, silica fume on the bond strength between aggregate and mortar were investigated. As the result, with increasing of water-cement ratio, the bond strength was slightly decreased while the compressive strengths of mortar and concrete were seriously decreased. The rate of strength gain of bond strength was not decreased with increasing of water-cement ratio while that of compressive strength was gradually decreased.

  • PDF

낮은 W/C비를 갖는 콘크리트 제품에 대한 폐주물사의 적용 (Application of Waste Foundry Sand to Concrete-Based Product Having Low Water Cement Ratio)

  • 이대경;김동주;조홍준;김진만
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 가을 학술발표회 논문집
    • /
    • pp.79-84
    • /
    • 2001
  • Because the WFS(Waste Foundry Sand), by-product of a casting factory, is generally a smaller particle than a fine aggregate, it has a bad influence on quality of concrete. Especially, the grading of aggregate is a very important factor in the case of concrete-based products having low water cement ratio manufactured by vibration and pressing method. Therefore, it is necessary to use WFS with the suitable grading of aggregate that it don't has a bad Influence on the quality of concrete-based products. This study investigated the suitable using proportion of WFS by means of the composition method of aggregate suggested by Driscoll. The results showed that it was desirable to use 10% of WFS since higher strength was developed with that amount.

  • PDF

산업부산물을 이용한 포러스콘크리트의 식생능력평가에 관한 연구 (An Experimental Study on the Evaluation of Porous Concrete using Industrial By-products of Planting Factory)

  • 박승범;권혁준;서대석;윤덕열
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 봄 학술발표회 논문집
    • /
    • pp.779-784
    • /
    • 2002
  • Porous concrete with a great deal of continuous porosity enables to contain water and to pass air freely through firmly hardened material, and allow necessary nutrients to reach roots of vegetation. Therefore, this paper deals with the voluntary properties and efficiency for planting of plant porous concrete. The results of experiment showed that void volumes were 17% to 31%, and compressive strength ranged between 80kgf/cm$^2$ and 180kgf/cm$^2$ when the ratio of the paste to aggregate was 0.3-0.5 When the aggregate size are 20-30mm, the paste to aggregate ratio is 0.3, and the length of Paranial Ryegress came up as 32cm. Ut supra the efficiency of planting goes through Paranial Ryegrass in result the length of plant are in compliance with void volume and aggregate size.

  • PDF

Engineering Properties of Permeable Polymer Concrete Using Bottom Ash and Recycled Coarse Aggregate

  • Sung, Chan-Yong;Kim, Jong-Hyouk
    • 한국농공학회논문집
    • /
    • 제48권7호
    • /
    • pp.25-31
    • /
    • 2006
  • Permeable polymer concretes can be applied to roads, sidewalks, river embankment, drain pipes, conduits, retaining walls, yards, parking lots, plazas, interlocking blocks, etc. This study was to explore a possibility of using bottom ash as filler and recycled coarse aggregate of industrial by-products for permeable polymer concrete. The tests carried out at $20{\pm}1^{\circ}C$ and $60{\pm}2%$ relative humidity. At 7 days of curing, unit weight, void ratio, compressive and flexural strength and coefficient of permeability ranged between $1,652{\sim}1,828kgf/m^{3},\;15{\sim}29+%,\;18.2{\sim}24.5\;MPa,\;6.4{\sim}8.4\;MPa\;and\;6.8{\times}10^{-2}{\sim}1.7{\times}10^{-1}\;cm/s$, respectively. It was concluded that the bottom ash and recycled coarse .aggregate can be used in the permeable polymer concrete.

Fresh and hardened properties of concrete containing cold bonded aggregates

  • Thomas, Job;B., Harilal
    • Advances in concrete construction
    • /
    • 제2권2호
    • /
    • pp.77-89
    • /
    • 2014
  • The properties of fresh and hardened concrete made using three types of artificial cold bonded aggregates are determined. The properties, namely, slump, water absorption, compressive strength and splitting tensile strength of concrete containing artificial aggregate are reported. The variables considered are aggregate type and water-to-cement ratio. Three types of cold bonded aggregates are prepared using fly ash and quarry dust. The water-to-cement ratio of 0.35, 0.45, 0.55 and 0.65 is used. The test result indicates that artificial aggregates can be recommended for making the concrete up to a strength grade of 38 MPa. The use of quarry dust in the production of artificial aggregate mitigates environmental concerns on disposal problems of the dust. Hence, the alternate material proposed in this study is a green technology in concrete production.

이론공극율, 골재입도 및 양생방법이 포러스콘크리트의 강도 및 투수성능에 미치는 영향 (Influence of Theoretical Void Ratio, Grading of Aggregate and Curing Method on Strength and Water Permeability of Porous Concrete)

  • 김재환;유범재;최세진;백용관;박정호;김무한
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.373-378
    • /
    • 2000
  • The objective of this study was to investigate the influence the influence of theoretical void ratio(T.V.R), grading of aggregate and curing method on the strength and water permeability of porous concrete, and the reduction proportion of water permeability by these factors. The results of the study showed that its strength and water permeability were greatly depended on the T.V.R and grading of aggregate, but didn't on the curing method. And, when the T.V.R and grading of aggregate were increased, the reduction proportion of water permeability was small. As the relation ship between its physical properties and non-destruction test values was very high, its use for the estimation of the physical properties will be useful.

  • PDF

잔골재 종류 및 치환율에 따른 저탄소 무기결합재의 유동 및 강도특성 (Flowing and Strength Properties of Low Carbon Inorganic Composite Depending to Fine Aggregate Types and Replacement Ratio)

  • 박종필;배상우;이윤성;이강필;이상수;송하영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2011년도 추계 학술논문 발표대회
    • /
    • pp.235-236
    • /
    • 2011
  • This study analyzed flowing and strength properties of mortar depending to fine aggregate types and replacement ratio by using blast furnace slag, red mud, and silica fume that are industrial by products. The findings showed that higher replacement level of fine aggregate increased air content while decreased table flow. In addition, compressive strength showed that the higher replacement level was regardless of fine aggregate types, the lower strength became. Mortar substituted by the dredged sand showed high strength.

  • PDF

괴상석탄재와 폐주물사를 혼입한 경량모르터의 특성에 관한 기초적 연구 (A Fundamental Study on the Properties of Lightweight Mortar Mixed with Bottom ash and Waste Foundry Sand)

  • 이승한;한형섭;정용욱
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 가을 학술발표회 논문집
    • /
    • pp.223-228
    • /
    • 1997
  • In this study, bottom ash, lightweight aggregate, and Expanded Polystyrene was used to lighten the mortar. In order to compensate the reduction of strength caused by lightening, the waste foundry sand produced as solid waste was substituted for fine aggregate. As the device of reducing the ratio of absorption, the procedure of mixture was altered to check the effectiveness of surface coating of porous lightweight aggregate. It was observed over 170kg/$\textrm{cm}^2$ compressive strength at gravity about 1.3, an over 380kg/$\textrm{cm}^2$ at gravity about 1.7. the maximum strength was occurred when 30% of fine aggregate was replaced was replaced with waste foundry sand, and the ratio of absorption was decreased over 10% by changing the procedure of mixture.

  • PDF