• 제목/요약/키워드: Adhesive strength

검색결과 1,542건 처리시간 0.03초

EXPERIMENTAL STUDY ON PROBABILITY OF STRENGTH FOR EPOXY ADHESIVE-BONDED METALS

  • Seo, Do-Won;Lim, Jae-Kyoo;Jeon, Yang-Bae;Yoon, Ho-Cheol
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.688-693
    • /
    • 2002
  • Adhesive bonding is becoming one of the popular joining techniques in metal industries, since it has some advantages over other techniques such as welding and diffusion bonding, e.g., any dissimilar metals are easily adhesive-bonded together. In this study, the experiments were carried out in order to provide the statistical data with strength evaluation methods: tension, shear and four-point bending tests for thermoplastic epoxy resin based adhesive-bonded metal joints. We should certificate on the probability of the adhesive strength that has the tendency of brittle fracture, the adhesive bonding strength between metals with thermoplastic adhesive has the best probability at four-point bending test. The strength testing method that has higher probability is four-point bending test, shear test and tensile test in order.

  • PDF

압연강판 접착제 접합부의 환경 접합강도에 미치는 온도 및 침수시간의 영향 (Effect of Temperature and Immersion Time on the Environmental Adhesive Strength of Adhesively Bonded Joints of Rolled Steel Sheet)

  • 송준희;이희제;임재규
    • 대한기계학회논문집A
    • /
    • 제26권12호
    • /
    • pp.2662-2669
    • /
    • 2002
  • Recently structural applications of adhesive bonding method have been increased extensively in automobile industry. Adhesively-bonded joints which are used in automobile field are exposed to various environmental conditions. In this study, several environmental factors were concerned to evaluate their effects on the adhesive strength such as air temperature, water temperature, exposed time in water. The specimens are exposed for 1, 10 and 100 hours at various air temperatures to evaluate the effects of the air and water temperature on the adhesive strength. It is proved that the adhesive strength decrease with rising the air and water temperature, and the adhesive strength decrease steeply at the higher temperature with increasing the exposure time in water.

Compressive Shear and Bending Performance of Compressed Laminated Wood after Microwave Heating

  • Park, Cheul-Woo;Lim, Nam-Gi
    • 한국건축시공학회지
    • /
    • 제12권5호
    • /
    • pp.539-547
    • /
    • 2012
  • To manufacture laminated wood with improved mechanical properties by providing uniform adhesiveness, the adhesive was applied and the plate adhesive was laminated on the wood surface. Then, after laminating the wood on the top part of the adhesivebond, it was heated and dried while the adhesive was stiffened using microwaves, and the test piece was manufactured by compressing it with the press machine for thirty minutes. The temperature and the water content were examined according to the heating time of the wood heated with the microwave, and testing was conducted on the shear strength and flexural strength of the wood. In addition, the microstructure of the adhesive bond between the wood was recorded to confirm the penetrabilityinto the wood structure for the adhesive. After the test was conducted, it was found that the test piece manufactured with wood that has its water content leveled with the microwave heating showed improved shear strength and bending strength compared to the standard test piece. With regard to adhesives, liquefied polyvinyl acetate resin and plate's PVB resin were found to have superior adhesive strength. Also, after filming the cellular microstructure, it was found that when the laminated wood is heated with microwaves, the infiltration of the adhesive into the inside of the wood becomes easy, which makes it effective for improving adhesiveness.

Preparation of Stick Type Solid Glue as Paper Adhesive Using Mixed Seaweed Extract

  • Oh, Seung-Jun;Han, Won-Sik;Wi, Koang-Chul
    • 보존과학회지
    • /
    • 제35권4호
    • /
    • pp.269-277
    • /
    • 2019
  • Seaweed extracts, namely carrageenan obtained from Grateloupia elliptica and algin obtained from Laminaria, were employed as adhesive agents to synthesize solid adhesives for paper. Carrageenan from Grateloupia elliptica with the highest adhesive strength and lgin from Laminaria with the highest compressive strength was selected. The selected carrageenan and algin were mixed in a ratio of 7:3, and the mixture was employed as an adhesive agent. At a high temperature, sodium stearate(used as a solidifying material) oxidized the seaweed extracts. Consequently, carrageenan and algin were added to the final manufacturing process. The adhesive strength of the final synthesized solid adhesive is found to be 3.02 MPa and the compressive strength is found to be 30.5 N. Compared to the adhesive strength (2.95 MPa) and compressive strength (30.11 N) of commercial solid adhesives, the obtained results indicate superior adhesion characteristics. Furthermore, the proposed adhesive is environment-friendly because the presence of volatile organic compounds, formaldehyde, and heavy metals(such as chromium, lead, and cadmium) were not detected. Moreover, when used, the flatness of paper was twice that of commercial solid paper adhesives. Hence, the proposed adhesive can provide excellent adhesion, stability, and usability.

접착제 접합된 자연섬유강화 복합재료의 파괴강도 특성에 미치는 섬유 방향의 영향 (Effect of Fiber Orientation on Failure Strength Properties of Natural Fiber Reinforced Composites including Adhesive Bonded Joint)

  • 윤호철
    • Journal of Welding and Joining
    • /
    • 제24권5호
    • /
    • pp.43-48
    • /
    • 2006
  • This paper is concerned with a fracture strength study of composite adhesive lap joints. The tests were carried out on specimen joints manufactured hybrid stacked composites such as the polyester and bamboo natural fiber layer. The main objective of the work was to test the fracture strength using hybrid stacked composites with a polyester and bamboo natural fiber layer. Tensile and peel strength of hybrid stacked composites are tested before appling adhesive bonding. From results, Natural fiber reinforced composites have lower tensile strength than the original polyester. and The load directional orientation and small amount and low thickness of bamboo natural fiber layer have a good effect on the tensile and peel strength of natural fiber reinforced composites. The failure strength of these materials applied adhesive bonding is also affected by fiber orientation and thickness of bamboo natural fiber layer. There for, Fiber orientation of bamboo natural fiber layer have a great effect on the tensile-shear strength of natural fiber reinforced composites including adhesive bonded joints.

단판(單板)의 PEG 처리조건(處理條件)에 따른 합판(合板)의 성질(性質) (Plywood Properties by PEG Treatment Conditions on Veneer)

  • 서진석;도금현
    • Journal of the Korean Wood Science and Technology
    • /
    • 제17권2호
    • /
    • pp.20-25
    • /
    • 1989
  • This study was carried out in order to investigate the treatment effect of PEG soln which is a common dimensional stabilizer to green log. sawing panel etc, on bonding product including plywood widely-used in secondary processing unit. The 30% concentration of aqueous PEG soln. with molecular weight of 400, 1.000 and 4,000 were prepared respectively, and also dipping the veneer in the PEG soln. spreading the PEG soln. on veneer and mixing the PEG soln. in the adhesive were allowed. Then the ratio of PEG impregnation on veneer, the adhesive strength of plywood were epitomized as follows: The ratio of impregnation by PEG 4,000 at dipping condition was highest. while that by PEG 400 at same condition was lowest. However, the effect of PEG molecular weight on the ratio of impregnation at spreading condition did not occur. 2. The adhesive strength was great in the order of 4,000>400>1,000 in molecular weight of PEG at dipping and spreading conditions. In case of mixing the PEG soln. in the adhesive, the adhesive strength was great in the order of 400>1,000>4,000 in molecular weight of PEG. Throughout three treatment conditions, PEG 400 was relatively favourable with about 10kg/$cm^2$ dry strength. 3. The adhesive strength was great 10 the order of spreading >dipping >mixing condition. 4. Although adhesive strength with the 30% concentration of aqueous PEG soln. was decreased by 35% and over, compared to control (non-treatment) adhesive strength, all types of PEG treatment except mixing the PEG soln. in the adhesive exceeded the standard dry strength for common use panel. 7.5kg/$cm^2$. 5. In warm water-proof test, the adhesive strengths by all PEG treatment conditions were less than the standard wet strength, 7.5kg cot, and also delamination of glue line occured mostly in mixing in the PEG soln. in the adhesive condition.

  • PDF

T형 이음 접합에 의한 경량구조물용 접착이음강도의 평가 (Strength Evaluation of Adhesive Bonded Joint for Light Weight Structure by T-Peel Joint Test)

  • 이강용;공병석;우형표
    • 한국자동차공학회논문집
    • /
    • 제6권4호
    • /
    • pp.56-65
    • /
    • 1998
  • The bonding strength evaluation of the light weight materials for an electrical vehicle has been performed through the T-peel joint test in which the design paramete- rs such as joint style, adherend type, adherend thickness, adhesive thickness, and adhesive type are considered. It is experimentally observed that the peel strength of joint increases with the increase of the adherend thickness. With the increase of the adhesive thickness, however, the peel strength of joint increases a little. Aluminum-FRP adherend combination shows such higher peel strength than that of Aluminum-Aluminum adherend combination. For the adhesive bonded joint, the results of FEM analysis agree with those of experiment. The adhesive bonded joint reinfored with a rivet gives higher peel strength than that of the joint without rivet.

  • PDF

접착이음의 강도평가에 관한 연구 (제1보 겹치기 접착이음의 응력해석과 파괴강도) (A Study on Strength Evaluation of Adhesive Joints(1st Report, Stress Analysis and Fracture Strength of Adhesive Single-Lap Joint))

  • 정남용
    • 대한기계학회논문집
    • /
    • 제16권4호
    • /
    • pp.667-674
    • /
    • 1992
  • 본 연구에서는 복합재료의 접착이음에 대한 강도 평가법을 확립하기 위한 기 초연구로써 접착이음의 가장기본적인 형태의 하나인 겹치기 이음(single-lap joint: SLJ)에 대한 응력해석과 정적 및 피로 강도시험을 실시하고, 종래의 강도평가법의 문 제점을 파악.검토하고 정량적이고 통일적인 접착이음의 강도평가법의 확립 및 설계 기 준의 설정에 대한 새로운 방향을 모색 하고저 한다.

미세-전단 결합 강도 시험을 이용한 상아질 접착제와 수복용 복합 레진의 호환성에 관한 연구 (IN VITRO MICRO-SHEAR BOND STRENGTH OF FIVE COMPOSITE RESINS TO DENTIN WITH FIVE DIFFERENT DENTIN ADHESIVES)

  • 정진호;노병덕
    • Restorative Dentistry and Endodontics
    • /
    • 제29권4호
    • /
    • pp.353-364
    • /
    • 2004
  • The purpose of this study was to compare and to evaluate the combination use of 5 kinds of dentin adhesive systems and 5 kinds of composite resins using micro-shear bond test. Five adhesive systems (Prime & Bond NT (PBN). Onecoat bond (OC), Excite (EX), Syntac (SY), Clearfil SE bond (CS)) and five composite resins (Spectrum (SP), Synergy Compact (SC), Tetric Ceram (TC), Clearfil AP-X (CA), Z100 (Z1)) were used for this study ($5{\;}{\times}{\;}5{\;}={\;}25group$, n =14/group). The slices of horizontally sectioned human tooth were bonded with each bonding system and each composite resin, and tested by a micro-shear bond strength test. These results were analyzed statistically. The mean micro-shear bond strength of dentin adhesive systems were in order of CS (22.642 MPa), SY (18.368 MPa), EX (14.599 MPa). OC (13.702 MPa). PBN (12.762 MPa). The mean bond strength of self-etching primer system group (CS, SY) in dentin was higher than that of self-priming adhesive system groups (PBN, EX, OC) significantly (P<0.05). The mean bond strength of composite resins was in order of SP (19.008 MPa), CA (17.532 MPa). SC (15.787 MPa), TC (15.068 MPa). Z1 (14.678 MPa). Micro-shear bond strength of SP was stronger than those of other composite resins significantly (P < 0.05). And those of TC and Z1 were weaker than other composite resins significantly (P < 0.05). No difference was found in micro-shear bond strength of composite resin in self-etching primer adhesive system groups (CS, SY) statistically. However, there was significant difference of micro-shear bond strength of composite resin groups in self-priming adhesive systems group (PBN, EX, OC). The combination of composite resin and dentin adhesive system recommended by manufacturer did not represent positive correlation. It didn't seem to be a significant factor.

ArF 엑시머 레이저에 의한 가류 고무의 표면처리 (Surface treatment of vulcanized rubber by ArF excimer laser)

  • 이봉주
    • 한국광학회지
    • /
    • 제13권4호
    • /
    • pp.332-335
    • /
    • 2002
  • 가류고무의 접착력을 향상시키기 위해서 엑시머 펄스 레이저 광으로 표면처리를 하였다. 레이저 광 조사 수의 증가에 따라, 접착력은 크게 향상되어, 100회의 조사 수에서 1500 N/m의 가장 큰 값을 얻었다. 또한 에너지 밀도 증가에 대해서도 접착력은 증가하여 에너지 밀도 176 mJ/$cm^{2}$에서 가장 큰 접착력 1500 N/m를 얻게 되었다. 에너지 밀도의 증가에 따라 접착력이 증가하는 것은 표면적의 증가와 관련이 있음을 알았다.