• Title/Summary/Keyword: Acetylated wood

Search Result 20, Processing Time 0.029 seconds

Total Utilization of Woody Biomass by Steam Explosion (III) - The Preparation of Acetate from Pine and Oak Exploded Wood - (폭쇄법을 이용한 목질계 바이오매스의 종합적 이용 (III) - 소나무와 신갈나무 폭쇄재로부터 셀룰로오스 아세테이트의 제조 -)

  • Lee, Jong-Yoon;Chang, Jun-Pok;Yang, Jae-Kyung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.23 no.2
    • /
    • pp.26-31
    • /
    • 1995
  • Acetylcellulose(AC) was prepared with steam exploded wood(EXW) and EXW after delignification with sodium chlorite, pine (Pinus densiflora) and oak (Quercus mongolica) woods. The color of acetylated pine and oak exploded wood was brown, degree of substitution(D.S) of pine was 1.47~2.09, and this of oak was 1.49~2.29. The hemicellulose content of acetylated pine and oak exploded wood was 0~3.4% and 1.49~11.3%, individually. The degree of substitution of acetylated wood prepared from delignified EXW in the pine and oak wood was 0.50~0.71 and 0.70~0.88, individually. Hemicellulose content of acetylated EXW with sodium chlorite after delignification in the pine and oak wood was less than 1% and 0.6~2.5%. The color of acetylated wood after delignification was white. IR-spectra of acetylated pine and oak EXW after delignification were found that peaks at around 1740$cm^{-1}$ and 1200$cm^{-1}$ increase markedly, due to ester carbonyl group.

  • PDF

Dimensional Change of Acetylated Hardwood (아세틸화 활엽수재의 치수변화 특성)

  • 한규성
    • Journal of the Korea Furniture Society
    • /
    • v.11 no.2
    • /
    • pp.79-84
    • /
    • 2000
  • It is well-known fact that dimensional stability of wood is greatly enhanced by acetylation of wood. This dimensional stability results from bulking of the reacted acetate within the cell wall, which reduces further swelling when the modified woods come into contact with water or water vapor. The purpose of this research was to determine the water absorption and dimensional stability of the acetylated solid wood in liquid water and in humidity tests. Beech and red oak were acetylated. Moisture and water absorption of acetylated wood were quite dependent on weight percent gain(WPG). Antiswelling efficiency(ASE) was quite dependent on WPG, but was not dependent on species.

  • PDF

Decay Resistance of the Acetylated Tropical Hardwood Species

  • Grace, Adebawo Funke;Yekeen, Ogunsanwo Olukayode;Olalekan, Olajuyigbe Samuel
    • Journal of Forest and Environmental Science
    • /
    • v.36 no.3
    • /
    • pp.225-232
    • /
    • 2020
  • Chemical modification of wood is an effective method to enhance the biological durability of wood with no toxic effect on the environment. In this study, wood of Triplochiton scleroxylon was modified using acetylation techniques. A total of one hundred wood blocks, (each 20×20×60 mm) obtained from a 22-year old T. scleroxylon tree were conditioned and acetylated at 120℃ in a bioreactor containing acetic anhydride for 60, 120, 180, 240 and 300 minutes. The percentage weight gain of acetylated wood was determined. The untreated (control) and treated blocks were exposed to Pleurotus ostreatus (white rot fungus) and Fibroporia vaillanti (brown rot fungus) after which moisture content (MC) and weight loss (WL) was monitored for 16 weeks. Data were analysed using descriptive and inferential statistics at p<0.05 level of significance. The percentage weight gain of acetylated wood samples increased with time from 10.4% (60 minutes) to 22.7% (300 minutes). MC of untreated blocks inoculated with Pleurotus ostreatus was significantly higher than those of Fibroporia vaillantii after 16 weeks exposure. There was no significant difference in the MC of the of the acetylated samples for the two fungi after 300 minutes reaction time. The WL of untreated blocks inoculated with Fibroporia vaillantii was higher than those of Pleurotus ostreatus, however, the two fungi showed no significant difference in the WL for the acetylated samples after 16 weeks exposure. Acetylation prevents moisture absorption and inhibition of fungi growth in acetylated wood compared to untreated wood, thereby enhancing the durability of Triplochiton scleroxylon.

The Laccase Activity of Trametes versicolor during Cultivation on Acetylated Wood and 13C-CP/MAS NMR Study (아세틸화 처리 목재에 배양시킨 Trametes versicolor의 Laccase활성과 13C-CP/MAS NMR 분석)

  • Son, Dong-Won;Lee, Dong-Heub
    • Journal of the Korean Wood Science and Technology
    • /
    • v.29 no.4
    • /
    • pp.60-66
    • /
    • 2001
  • For examine anti-degradation factors of acetylated wood, acetylated wood was incubated on Trametes versicolor. The laccase activity was examined in broth culture and solid fermentation that contain acetylated chips. The change of acetyl groups and chemical composition in the acetylated wood having massloss analysed by $^{13}C$-CP/MAS NMR. The laccase activity was detected in broth culture. When the T. versicolor contact to acetylated wood directly, the laccase activity was very low and couldn't maintain during test periods. Through the analysing of $^{13}C$-CP/MAS NMR, the acetylation took place carbohydrates as well as lignin and hydroxyl group of amorphous region was more easily substituted that of crystalline region The spectral analyses of $^{13}C$-CP/MAS NMR were shown that introduced acetyl bond was stable against fungal attack.

  • PDF

Dimensional Change of Acetylated Softwood (아세틸화 침엽수재의 치수변화 특성)

  • Han, Gyu-Seong;Cho, Nam-Seok
    • Journal of the Korean Wood Science and Technology
    • /
    • v.24 no.4
    • /
    • pp.40-46
    • /
    • 1996
  • It is well-known fact that dimensional stability of wood is greatly enhanced by acetylation of wood. This dimensional stability results from bulking of the reacted acetate within the cell wall, which reduces further swelling when the modified woods corne into contact with water or water vapor. The purpose of this research was to determine the water absorption and dimensional stability of the acetylated solid wood in liquid water and in humidity tests. Radiata pine, Siberian larch, and Japanese larch were acetylated. Antiswelling efficiency(ASE) and equilibrium moisture content(EMC) of acetylated wood, at 95% RH and $20^{\circ}C$ after 4weeks, was quite dependent on WPG, but was not dependent on species.

  • PDF

Acetylation of Papermaking Pulp Fiber and its Application (제지용(製紙用) 펄프 섬유(纖維)의 아세틸화(化)와 응용(應用))

  • Won, Jong-Myoung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.20 no.1
    • /
    • pp.51-59
    • /
    • 1992
  • The acetylation of papermaking pulp fiber(SwBKP, SwUKP, HwBKP and HwBCTMF) is carried out to modify the characteristics of pulp and paper. The effects of the addition of acetylated pulp on the filler retention and paper properties were investigated. The acetylation depended upon pulp type and the content of short fiber and fines. The addition of acetylated SwBKP did not deteriorate the retention of clay, talc and calcium carbonate, while the retention of titanium dioxide was increased with the addition of 20% and above. The brightness opacity, air permeability and tear strength were improved, but water resistance, burst strength and folding endurance were decreased by the addition of acetylated SwBKP and SwUKP. The tensile strength of SwBKP was increased until 20% of acetylated pulp is added, and then decreased. The tensile strength of SwUKP, however, was not changed until the acetylated pulp of 25% is added. The dimensional stability was improved by the addition of acetylated pulp and showed the different response to SwBKP and SwUKP.

  • PDF

Structure Determination of Sucrose by Acetylation and Acid Hydrolysis

  • Min, Hee-Jeong;Lee, Tae-Seong;Bae, Young-Soo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.42 no.2
    • /
    • pp.183-192
    • /
    • 2014
  • For the structure determination of D-(+)-sucrose, which consists of ${\alpha}$-D-(+)-glucose and ${\beta}$-D-(+)-fructose, it was acetylated with acetic anhydride and triethyl amine, pyridine, zinc chloride, and sodium acetate as catalysts. The acetylated D-(+)-sucrose was acid-hydrolyzed using sulfuric acid and sodium chloride in methanolic solution. The structures of the reaction products were determined by $^1H$-NMR and $^{13}C$-NMR spectra. The yield of the acetylation indicated the high value in zinc chloride as 70% in zinc chloride catalyst. The acid-hydrolyzed product of the acetylated D-(+)-sucrose, 2,3,4,6,1',3',4',6'-octa-O-acetyl-D-(+)-sucrose, gave 2,3,4,6-tetra-O-acetyl-${\beta}$-D-(+)-glucose and it suggests that the acetylated D-(+)-sucrose was rearranged through the formation of oxonium ion by mutarotation in the 2,3,4,6-tetra-O-acetyl-${\alpha}$-D-(+)-glucose moiety and through the ring opening in the 1',3',4',6'-tetra-O-acetyl-${\beta}$-D-(+)-fructose moiety.

Evaluation of Material Properties of Acetylated Medium Density Fiberboard (MDF) (아세틸화 처리 중밀도 섬유판(MDF)의 재질 평가)

  • LEE, Jong Shin;KIM, Soung Joon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.48 no.3
    • /
    • pp.393-404
    • /
    • 2020
  • This study examined the material properties of MDF manufactured using acetylated pinus radiata fibers against moisture and compared the properties with the fiberboard quality standards of KS F 3200. Since acetylated MDF shows very low moisture content, water absorption and thickness swelling than the quality standards, it is expected to have an excellent dimensional stability. The bending strength in wetting condition of the acetylated MDF reached approximately 70% of the bending strength in dry condition, making it suitable for the quality standards. The internal bond of the acetylated MDF in the wetting condition was higher than the minimum internal bond of the quality standards in the dry condition, showing a good water resistance. Since the water droplet contact angle of the acetylated MDF is larger than that of untreated MDF, it is determined that it contributes in improving the water resistance due to the low wettability.

Investigation on the Dimensional Stability of Acetylated Larch (Larix kaempferi) Small Square (아세틸화처리 낙엽송(Larix kaempferi) 소형 각재의 치수안정성 조사)

  • Lee, Won-Hee;Kang, Ho-Yang
    • Journal of the Korea Furniture Society
    • /
    • v.27 no.4
    • /
    • pp.302-308
    • /
    • 2016
  • It has been known that acetylation improves the dimensional stability of wood. Liquid phase acetylation is more popular than gas-phase acetylation for the effectiveness of weight gain of wood. In this study the specimens of domestic red and Korean pines are acetylated in liquid phase and their physical properties, such as density, bending strength, anti-hygroscopicity etc., are analyzed. Acetylation increases the average weights and volume of larch specimens by 11.4% and 3.4%, respectively, and their average oven-dry densities are increased by $0.03g/cm^3$. Acetylation does not influence on Modulus of Rupture (MOR) and Modulus of Elasticity (MOE). The average Percentage Reduction in Hygroscopicity (PRH) and average Percentage Reduction in Water soaking (PRW) of larch specimens are respectively 20.2% and 20.8%. Thus it can be concluded that acetylation improves the dimensional stability of larch specimens.

Current Research Trends in Wood Preservatives for Enhancing Durability - A Literature Review on Non-Copper Wood Preservatives - (옥외 내구성 향상을 위한 목재보존제의 최근 연구 동향 -비 구리계 약제를 중심으로-)

  • Kim, Yeong-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.41 no.3
    • /
    • pp.187-200
    • /
    • 2013
  • Current research trends of non-copper wood preservatives for enhancing durability was reviewed; as a follow-up of the review in 2012 on copper-based wood preservatives. Main environmental friendly non-copper wood preservatives studied by many scientists were boron-based compounds, synthetic compounds from natural products, and pyrethroids family of chemicals, etc. The critical issue regarding treated woods with boron-based compounds used outdoors was the leaching of boron. Many studies mainly focused on boron fixation improvement using variety of polymers. Moreover, the studies showed notable increases in attempts to use natural products used commonly in the medical fields as wood preservatives as well as outdoor use of chemical modified such as acetylated wood developed in purpose of stabilizing dimension.