• 제목/요약/키워드: Abrasive wear

검색결과 286건 처리시간 0.024초

Tribological performance of the laser surface treated CrZrSiN thin films

  • Kim, DongJun;La, JoungHyun;Lee, SangYul
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2012년도 춘계학술발표회 논문집
    • /
    • pp.141-142
    • /
    • 2012
  • Recently, surface texturing by atmospheric laser processing has been received lots of attention to improve the tribological performance of various surfaces and this laser texturing of surfaces could be considered in a large extent to improve tribological performance of PVD coated surface. Surface texturing could be performed by various manufacturing techniques such as indentation with hard materials, ion etching, abrasive jet machining, lithography, and Laser Surface Texturing (LST). Out of all these techniques, however it is generally accepted that laser surface texturing (LST) by atmospheric laser processing offers the most promising process as LST is very fast, environmentally-friendly, easy to control the shape and size of the microdimples. In this work various preliminary experimental results from the laser texturing on the PVD-coated steel substrate will be presented. Our results indicated that laser texturing definitely affect the tribological performance of the surfaces and the size as well as pattern type of laser texturing are one of the key factors. From the wear tests against an alumina counterpart ball at room temperature under oil-lubricated condition, laser surface texturing on the CrZrSiN films reduced the friction coefficients by approximately more than 5 times in the case of narrow patterned surfaces.

  • PDF

크로마이징 처리 된 철계 소결 부품의 내식성 및 저 마찰특성 (Corrosion Resistance and Low Friction Property of Sintered Steel Parts via Chromizing Treatment)

  • 김상권;박용진;여국현;이재훈
    • 대한금속재료학회지
    • /
    • 제50권11호
    • /
    • pp.809-815
    • /
    • 2012
  • Recently, as the interest in improving energy efficiency has grown, the demand for vehicle and machine parts that are resistant in high temperature corrosive conditions and abrasive environments has increased. Pack chromizing treatment of sintered steels is a profitable method that satisfies both corrosion resistance and low friction properties. Since austenitic stainless steels have good corrosion resistance but low mechanical hardness, if they are replaced by sintered steel parts with pack chromizing treatment, all the desirable properties such as low price, easy molding, high hardness, low frictional coefficient, and high corrosion resistance, can be obtained. The higher corrosion resistance of the chromized parts over that of the austenitic stainless steels was acquired by coating chromium carbides and a thin chromium oxides layer on the surface. Moreover, the surface morphology of chromized parts, which were composed of chromium rich phases and hardened chromium carbides by diffusing and alloying, had a peak-and-valley shape so that the dimple effect by the wrinkled morphology and high hardness induced a low friction coefficient.

그루브의 Trap 효과에 대한 CFD 해석: 제2부 - 그루브 모서리의 곡률반경 변화 (CFD Analysis of Trap Effect of Groove in Lubricating Systems: Part II - Variation in Radius of Curvature of Groove Edge)

  • 홍성호
    • Tribology and Lubricants
    • /
    • 제36권6호
    • /
    • pp.359-364
    • /
    • 2020
  • Numerical investigation of the groove trap effect with variation in the groove-edge radius of curvature is presented here. The trap effect is evaluated in a two-dimensional sliding bearing using computational fluid dynamics (CFD). This simulation is based on the discrete phase model (DPM) and standard k - ε turbulence model using commercial CFD software, FLUENT. The numerical results are evaluated by comparisons with streamlines and particle trajectories in the grooves. Grooves are applied to various lubrication systems to improve their lubrication characteristics, such as load carrying capacity increment, leakage reduction, frictional loss reduction, and preventing three-body abrasive wear due to trapping effect. This study investigates the grove trapping effect for various groove-edge radius of curvature values and Reynolds numbers. The particle is assumed to be made of steel, with a circular shape, and is injected as a single particle in various positions. One-way coupling is used in the DPM model because the single particle injection condition is applied. Further, the "reflect" condition is applied to the wall boundary and "escape" condition is used for the "pressure inlet" and "pressure outlet" boundaries. From the numerical results, the groove edge radius is found to influence the groove trap effect. Moreover, the groove trap effect is more effective when applying the groove edge radius.

자동차 제동시 나타나는 마찰특성에 관한 연구(I. 고체 윤활제($Sb_2S_3$)와 연마제($ZrSiO_4$)의 함량에 따른 영향 (Effect of the Amount of a Lubricant and an Abrasive in the Friction Material on Friction Characteristics)

  • 장호
    • Tribology and Lubricants
    • /
    • 제13권1호
    • /
    • pp.34-41
    • /
    • 1997
  • Frictional behavior of three automotive friction materials (brake pads) containing different amounts of antimony trisulfide ($Sb_2S_3$) and zirconium silicate ($ZRSiO_4$) were investigated using a front brake system. The friction materials were tested on a brake dynamometer (dyno) with gray cast iron rotors. The dynamometer(dyno) test simulated the dragging of a ehicle maintaining 70 km/h and vehicle stops from 100 km/h using 20 different combinations of initial brake temperature (IBT) and input pressure (IP). The results showed a strong influence of the relative amount of $Sb_2S_3$ and $ZrSiO_4$ in friction materials on friction characteristics. Friction stability was improved with the higher concentration of $Sb_2S_3$ in the friction material. Torque variation during drag cycle was increased with an increase of the $ZrSiO_4$ concentration in the friction material. Average friction coefficient and the wear rate of the friction material increased by using more aggressive friction materials containing more $ZrSiO_4$ and less $Sb_2S_3$. Generation of the disk thickness variation (DTV) increased when friction materials with higher concentration of $ZrSiO_4$ were used Careful examination of DTV change showed that aggressiveness of the friction material played an important role in determining torque variation.

THE EFFECTS OF SEALING ON THE PLASMA-SPRAYED OXIDE-BASED COATINGS

  • Kim, Hyung-Jun;Sidoine Odoul;Kweon, Young-Gak
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.53-58
    • /
    • 2002
  • Electrical insulation and mechanical properties of the plasma sprayed oxide ceramic coatings were studied before and after the sealing treatment of the ceramic coatings. Plasma sprayed A1$_2$O$_3$-TiO$_2$ coating as the reference coating was sealed using three commercial sealants based on polymer. Penetration depth of the sealants to the ceramic coating was evaluated directly from the optical microscope using a fluorescent dye. It is estimated that the penetration depth of the sealants to the ceramic coating is from 0.2 to 0.5 mm depending on the sealants used. The preliminary test results with a DC puncture tester imply that the dielectric breakdown voltage mechanism of plasma sprayed ceramic coatings has been determined to be a corona mechanism. Dielectric breakdown voltage of the as-sprayed and as-ground samples have shown a linear trend with regard to the thickness showing an average dielectric strength of 20 kV/mm for the thickness scale studied. It is also shown that grinding the coating before sealing and adding fluorescent dye do not agent the penetration depth of sealants. All of the microhardness, two-body abrasive wear resistance, bond strength, and surface roughness of the ceramic coating after the sealing treatment are improved. The extent of improvement is different from the sealants used. However, three-point bending stress of the ceramic coating after the sealing treatment is decreased. This is attributed to the reduced micro-crack toughening effect since the cracks propagate easily through the lamellar of the coating without crack deflection and/or branching after the sealing treatment.

  • PDF

시일과 스틸면 사이에 구형입자가 있는 접촉문제의 해석 (Contact Analysis of a Spherical Particle Between Elastomeric Seal and Steel Surface)

  • 박태조;조현동
    • 대한기계학회논문집A
    • /
    • 제34권2호
    • /
    • pp.161-166
    • /
    • 2010
  • 본 논문에서는 시일 설치면에서의 마멸발생기구를 정확하게 조사하기 위한 연구의 일환으로 미세입자가 시일과 스틸면 사이에 존재하는 경우의 접촉문제를 비선형문제해석 프로그램인 MARC를 사용하여 해석하였다. 이 결과, 시일의 재질은 스틸면에서의 응력분포와 변형형상에 아주 큰 영향을 미쳤다. 특히, PTFE와 같이 탄성계수가 높은 시일인 경우에 스틸 표면은 국부적으로 항복상태에 도달할 뿐만 아니라 시일을 제거한 후에도 영구변형과 함께 상당한 크기의 압축/인장 잔류응력이 존재하였다. 따라서, 시일과 스틸면 사이에 경질입자가 존재할 경우에는 연삭마멸과 함께 피로마멸이 발생할 수 있음을 확인하였으며, 다양한 설계변수에 대한 추가연구가 요구된다.

표면탄성파를 이용한 마모 표면부의 평가 (Evaluation of Abrasive Wear Face Using SAW)

  • 권성덕;윤석수;송성진;이영제
    • 비파괴검사학회지
    • /
    • 제22권2호
    • /
    • pp.193-197
    • /
    • 2002
  • 레일리 (Rayleigh) 표면탄성파의 속도와 산란의 주파수 의존성을 이용하여 마모로 인해 열화된 AISI 1045강 사편의 깊이방향 잔류응력 분포 (열화 기울기)의 비파괴적인 평가가 시도되었다. 액체/고체 경계면에 초음파가 특정각도로 입사할 때 발생한 표면탄성파의 산란과 복사로 인해 나타나는 후방복사 프로파일의 오른쪽 반치폭과 크기 그리고 발생각으로 잔류응력 분포의 해석도 가능하였으며 평균법에 의한 복사파의 세기 및 스펙트럼의 변화는 잔류응력 분포와 열화로 인해 발생한 미세 결함 밀도과의 연관성을 보여주었다.

Nano-sized TiCxNy를 함유한 STS 복합체의 특성 (Characteristics of Stainless Steel Composites with Nano-sized TiCxNy)

  • 반태호;박성범;조수정;이동원;;박용일;김성진
    • 한국분말재료학회지
    • /
    • 제18권3호
    • /
    • pp.290-296
    • /
    • 2011
  • Titanium carbonitride is more perspective materials compared to titanium carbide. It can be used in tool industry and special products because of its higher strength, abrasive wear-resistance and especially its strong chemical stability at high temperatures. We produced STS+TiCxNy composite by the spark plasma sintering for higher strength and studied the characteristics. The planar and cross-sectional microstructures of the specimens were observed by scanning electron microscopy. Characterizations of the carbon and nitride phases on the surface of composite were carried out using an X-ray diffractometer. During annealing TiCxNy particles diffusion into STS 430 was observed. After annealing, sintering isolations between particles were formed. It causes decreasing of mechanical strength. In addition when annealing temperature was increased hardness increased. Heterogeneous distribution of alloying elements particles was observed. After annealing composites, highest value of hardness was 738.1 MHV.

유한요소해석에 의한 코팅면의 브리넬 경도 평가: 제2보 - 모재와 코팅두께의 영향 (Evaluation of Brinell Hardness of Coated Surface by Finite Element Analysis: Part 2 - Influence of Substrate and Coating Thickness)

  • 박태조;강정국
    • Tribology and Lubricants
    • /
    • 제37권4호
    • /
    • pp.144-150
    • /
    • 2021
  • The most cost-effective method of reducing abrasive wear in mechanical parts is increasing their hardness with thin hard coatings. In practice, the composite hardness of the coated substrate is more important than that of the substrate or coating. After full unloading of the load applied to an indenter, its indentation hardness evaluated based on the dent created on the test piece was almost dependent on plastic deformation of the substrate. Following the first part of this study, which proposes a new Brinell hardness test method for a coated surface, the remainder of the study is focused on practical application of the method. Indentation analyses of a rigid sphere and elastic-perfect plastic materials were performed using finite element analysis software. The maximum principal stress and plastic strain distributions as well as the dent shapes according to the substrate yield stress and coating thickness were compared. The substrate yield stress had a significant effect on the dent size, which in turn determines the Brinell hardness. In particular, plastic deformation of the substrate produced dents regardless of the state of the coating layer. The hardness increase by coating behaved differently depending on the substrate yield stress, coating thickness, and indentation load. These results are expected to be useful when evaluating the composite hardness values of various coated friction surfaces.

다이아몬드 피복공구에 의한 SiC 강화 복합재료의 절삭특성 (Machining Characteristics of SiC reinforced Composite by multiple diamond-coated drills)

  • M. Chen;Lee, Y. M.;S. H. Yang;S. I. Jang
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2003년도 춘계학술대회 논문집
    • /
    • pp.533-537
    • /
    • 2003
  • Compared to sintered polycrystalline diamond (PCD), the deposited thin film diamond has a great advantage on the fabrication of cutting tools with complex geometries such as drills. Because of high performance in high speed machining non-ferrous difficult-to-cut materials in the field of automobiles industry, aeronautics and astronautics industry, diamond-coated drills find large potentialities in commercial applications. However, the poor adhesion of the diamond film on the substrate and high surface roughness of the drill flute adversely affect the tool lift and machining quality and they become the main technical barriers for the successful development and commercialization of diamond-coated drills. In this paper, diamond thin films were deposited on the commercial WC-Co based drills by the electron aided hot filament chemical vapor deposition (EACVD). A new multiple coating technology based on changing gas pressure in different process stages was developed. The large triangular faceted diamond grains may have great contribution to the adhesive strength between the film and the substrate, and the overlapping ball like blocks consisted of nanometer sized diamond crystals may contribute much to the very low roughness of diamond film. Adhesive strength and quality of diamond film were evaluated by scanning electron microscope (SEM), atomic force microscope (AFM), Raman spectrum and drilling experiments. The ring-block tribological experiments were also conducted and the results revealed that the friction coefficient increased with the surface roughness of the diamond film. From a practical viewpoint, the cutting performances of diamond-coated drills were studied by drilling the SiC particles reinforced aluminum-matrix composite. The good adhesive strength and low surface roughness of flute were proved to be beneficial to the good chip evacuation and the decrease of thrust and consequently led to a prolonged tool lift and an improved machining quality. The wear mechanism of diamond-coated drills is the abrasive mechanical attrition.

  • PDF