• Title/Summary/Keyword: API 5L X65

Search Result 36, Processing Time 0.023 seconds

Hydrogen Diffusion in APX X65 Grade Linepipe Steels

  • Park, Gyu Tae;Koh, Seong Ung;Kim, Kyoo Young;Jung, Hwan Gyo
    • Corrosion Science and Technology
    • /
    • v.5 no.4
    • /
    • pp.117-122
    • /
    • 2006
  • Hydrogen permeation measurements have been carried out on API X65 grade linepipe steel. In order to study the effect of steel microstructure on hydrogen diffusion behavior in linepipe steel, the accelerated cooling condition was applied and then three different kinds of microstructures were obtained. Hydrogen permeation measurement has been performed in reference to modified ISO17081 (2004) and ZIS Z3113 method. Hydrogen trapping parameters in these steels were evaluated in terms of the effective diffusivity ($D_{eff}$), permeability ($J_{ss}L$) and the amount of diffusible hydrogen. In this study, microstructures which affect both hydrogen trapping and diffusion were degenerated pearlite (DP), acicular ferrite (AF), bainite and martensite/austenite constituents (MA). The low $D_{eff}$ and $J_{ss}L$ mean that more hydrogen can be trapped reversibly or irreversibly and the corresponding steel microstructure is dominant hydrogen trapping site. The large amount of diffusible hydrogen means that corresponding steel microstructure is predominantly reversible. The results of this study suggest that the hydrogen trapping efficiency increases in the order of DP, bainite and AF, while AF is the most efficient reversible trap.

Effect of Bacteria in Soil on Microbiologically Influenced Corrosion Behavior of Underground X65 Pipeline (토양 속 박테리아가 지하매설 X65 배관의 미생물 부식 거동에 미치는 영향)

  • Choe, Byung Hak;Han, Sung Hee;Kim, Dae Hyun;Kim, Woosik;Kim, Cheolman;Choi, Kwang Su
    • Korean Journal of Materials Research
    • /
    • v.32 no.3
    • /
    • pp.168-179
    • /
    • 2022
  • Microbiologically Influenced Corrosion (MIC) occurring in underground buried pipes of API 5L X65 steel was investigated. MIC is a corrosion phenomenon caused by microorganisms in soil; it affects steel materials in wet atmosphere. The microstructure and mechanical properties resulting from MIC were analyzed by OM, SEM/EDS, and mapping. Corrosion of pipe cross section was composed of ① surface film, ② iron oxide, and ③ surface/internal microbial corrosive by-product similar to surface corrosion pattern. The surface film is an area where concentrations of C/O components are on average 65 %/16 %; the main components of Fe Oxide were measured and found to be 48Fe-42O. The MIC area is divided into surface and inner areas, where high concentrations of N of 6 %/5 % are detected, respectively, in addition to the C/O component. The high concentration of C/O components observed on pipe surfaces and cross sections is considered to be MIC due to the various bacteria present. It is assumed that this is related to the heat-shrinkable sheet, which is a corrosion-resistant coating layer that becomes the MIC by-product component. The MIC generated on the pipe surface and cross section is inferred to have a high concentration of N components. High concentrations of N components occur frequently on surface and inner regions; these regions were investigated and Na/Mg/Ca basic substances were found to have accumulated as well. Therefore, it is presumed that the corrosion of buried pipes is due to the MIC of the NRB (nitrate reducing bacteria) reaction in the soil.

Analysis of offshore pipeline laid on 3D seabed configuration by Abaqus

  • Moghaddam, Ali Shaghaghi;Mohammadnia, Saeid;Sagharichiha, Mohammad
    • Ocean Systems Engineering
    • /
    • v.5 no.1
    • /
    • pp.31-40
    • /
    • 2015
  • Three dimensional (3D) non-linear finite element analysis of offshore pipeline is investigated in this work with the help of general purpose software Abaqus. The general algorithm for the finite element approach is introduced. The 3D seabed mesh, limited to a corridor along the pipeline, is extracted from survey data via Fledermous software. Moreover soil bearing capacity and coefficient of frictions, obtained from the field survey report, and are introduced into the finite element model through the interaction module. For a case of study, a 32inch pipeline with API 5L X65 material grade subjected to high pressure and high temperature loading is investigated in more details.

The Evaluation of Burst Pressure for Corroded Weld in Gas Pipeline (가스배관에서 원주 및 심 용접부의 부식손상 부위에 대한 파열압력 평가)

  • Kim Yeong Pyo;Kim U Sik;O Gyu Hwan
    • Proceedings of the KWS Conference
    • /
    • v.43
    • /
    • pp.165-167
    • /
    • 2004
  • The failure pressure for corroded pipeline was measured by burst testing and classified with respect to corrosion sizes and corroded regions - the body, the girth weld and the seam weld of pipe. A series of finite element analyses were performed to obtain a limit load solution for corrosion defects on the basis of burst test. As a result, the criteria for failure assessment of corrosion defect within the body, the girth weld and the seam weld of API 5L X65 gas pipeline were proposed.

  • PDF

Evaluation of weld joint properties with length of inserted short pipe at the time of pipeline welding (배관용접시 단관삽입길이에 따른 용접부 특성 평가)

  • Kim Cheol-man;Kim Woo-sik;Kim Young-seob;Kwon Jeong-rock
    • 한국가스학회:학술대회논문집
    • /
    • 2003.10a
    • /
    • pp.53-58
    • /
    • 2003
  • API 5L X65 배관에 50mm이상의 단관을 삽입하여 용접하였을 경우, 삽입된 단관 길이 변화에 따른 용접부 기계적 특성 평가 결과를 요약하면 다음과 같다. 1. 단관삽입 용접부위의 거시적 조직관찰, 미소경도측정, 인장시험, 굽힘시험을 수행한 결과, 단관삽입 용접부의 건전성에는 문제가 없는 것으로 평가되었다. 2. 단관삽입 용접부의 원주방향 최대 인장 잔류응력의 크기는 단관 삽입 길이에 관계없이 약 150MPa로서 그리고 최대 압축 잔류응축은 약 300MPa로 측정되었다. 모재의 항복강도가 492MPa인 것과 비교하여보면 단관 삽입 용접에 의한 잔류응력의 영향은 매우 작은 것으로 평가되었다.

  • PDF

THE EFFECTS OF HEAT INPUT AND GAS FLOW RATE ON WELD INTEGRITY FOR SLEEVE REPAIR WELDING OF IN-SERVICE GAS PIPELINES

  • Kim, Young-pyo;Kim, Woo-sik;Bani, In-wan;Oh, Kyu-Hwan
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.390-395
    • /
    • 2002
  • The experimental and numerical study has been conducted on the sleeve repair welding of API 5L X65 pipeline. SMA W and GTAW were applied to weld the sleeve. The macrostructure and hardness of repair welds have been examined. The [mite element analysis of the multi-pass sleeve-fillet welding has been conducted to validate the experiment and investigate the effects of in-service welding conditions. The effect of gas flow rate on the hydrogen cracking was investigated. The effect of internal pressure on residual stresses and plastic strain was investigated. The allowable heat input was predicted considering the maximum temperature of inner surface of pipe and cooling rate at CGHAZ.

  • PDF

Fracture Toughness Evaluation of Natural Gas Pipeline under the Cathodic Protection

  • Kim, Cheol-Man;Baek, Jong-Hyun;Kim, Young-Pyo;Kim, Woo-Sik
    • Corrosion Science and Technology
    • /
    • v.8 no.4
    • /
    • pp.133-138
    • /
    • 2009
  • For the corrosion protection of the natural gas transmission pipelines, two methods are used, cathodic protection and coating technique. In the case of cathodic protection, defects are embrittled by occurring hydrogen at the crack tip or material surface. It is however very important to evaluate whether cracks in the embrittled area can grow or not, especially in weld metal. In this work, on the basis of elastic plastic fracture mechanics, we performed the CTOD testing with various test conditions, such as testing rate and potential. The CTOD of the base metal and the weld metal showed a strong dependence of the test conditions. The CTOD decreased with decreasing testing rate and with increasing cathodic potential. The morphology of the fracture surface showed the quasi-cleavage at low testing rate and cathodic overprotection. The low CTOD was caused by hydrogen embrittlement at crack tip.

The Effects of Heat Input and Gas Flow Rate on Weld Integrity for Sleeve Repair Welding of In-Service Gas Pipelines

  • Kim, Y.P.;Kim, W.S.;Bang, I.W.;Oh, K.H.
    • International Journal of Korean Welding Society
    • /
    • v.2 no.2
    • /
    • pp.36-41
    • /
    • 2002
  • The experimental and numerical study has been conducted on the sleeve repair welding of API 5L X65 pipeline. SMAW and GTAW were applied to weld the sleeve. The macrostructure and hardness of repair welds have been examined. The finite element analysis of the multi-pass sleeve-fillet welding has been conducted to validate the experiment and investigate the effects of in-service welding conditions. The effect of gas flow rate on the hydrogen cracking was investigated. The effect of internal pressure on residual stresses and plastic strain was investigated. The allowable heat input was predicted considering the maximum temperature of inner surface of pipe and cooling rate at CGHAZ.

  • PDF

A Study on the Deformation Characteristics of Gas Pipeline under Internal Pressure and In-Plane Bending Load (내압과 굽힘하중을 받는 가스배관의 변형특성에 관한 연구)

  • Jang, Yun-Chan;Kim, Ik-Joong;Kim, Cheol-Man;Jeon, Bub-Gyu;Chang, Sung-Jin;Kim, Young-Pyo
    • Transactions of the Korean Society of Pressure Vessels and Piping
    • /
    • v.15 no.2
    • /
    • pp.50-57
    • /
    • 2019
  • This paper investigates deformation characteristics of gas pipeline using the in-plane bending experiment and finite element analysis of a pipe bend. The effect of the bending angle and internal pressure on the deformation characteristics is analyzed. The pipe bend used in this study is API 5L X65 (out diameter: 20 inch) material with the thickness of 11.9 mm. The maximum load, displacement at maximum load, angle and local strain of 90° pipe bend are obtained from the in-plane bending experiment. Comparison between FE results and experimental data shows overall good agreements. In addition, the deformation characteristics of 22.5° and 45° pipe bend are calculated using the finite element analysis. As a result, the effect of the bend angle on the deformation characteristics is discussed.

Load-Bearing Capacity of Subsea Pipeline with Variation of Sea Water Depth and Buried Depth (수심과 퇴적 깊이 변화에 따른 해저배관의 하중지지능력 평가)

  • Baek, Jong-Hyun;Kim, Young-Pyo;Kim, Woo-Sik
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.36 no.10
    • /
    • pp.1131-1137
    • /
    • 2012
  • Subsea pipelines have been operated with buried depths of 1.2-4m underneath the seabed to prevent buoyancy and external impacts. Therefore, they have to show resistance to both the soil load and the hydrostatic pressure. In this study, the structural integrity of a subsea pipeline subjected to soil load and hydrostatic pressure was evaluated by using FE analyses. A parametric study showed that the internal pressure increased the plastic collapse depth by increasing the resistance to plastic collapse. The hoop stress increased with an increase in the buried depth for the same water depth; however, the hoop stress decreased with an increase in the water depth for the same buried depth.