플라스마 이온증착 기술을 이용한 스테인리스강의 질화처리에 관한 연구 (Research of Nitriding Process on Austenite Stainless Steel with Plasma Immersion Ion Beam)

  • 김재돌;박일수;옥철호
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제32권2호
    • /
    • pp.262-267
    • /
    • 2008
  • Plasma immersion ion beam (PIIB) nitriding process is an environmentally benign and cost-effective process, and offers the potential of producing high dose of nitrogen ions in a way of simple, fast and economic technique for the high plasma flux treatment of large surface area with nitrogen ion source gas. In this report PIIB nitriding technique was used for nitriding on austenite stainless steel of AISI304 with plasma treatment at $250{\sim}500^{\circ}C$ for 4 hours, and with the working gas pressure of $2.67{\times}10^{-1}$ Pa in vacuum condition. This PIIB process might prove the advantage of the low energy high flux of ion bombardment and enhance the tribological or mechanical properties of austenite stainless steel by nitriding, Furthermore, PIIB showed a useful surface modification technique for the nitriding an irregularly shaped three dimensional workpiece of austenite stainless steel and for the improvement of surface properties of AISI 304, such as hardness and strength

오스테나이트 스테인리스강 용접부의 응력부식 거동에 미치는 용접 방법의 영향 (The effect of welding methods on the stress corrosion behavior of the welded austenitic stainless steel)

  • 백신영
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제19권4호
    • /
    • pp.42-50
    • /
    • 1995
  • To study the effect of welding methods on the Stress Corrosion Cracking (SCC) behavior of welded AISI type 316L and 304 austenitic stainless steel, the Slow Strain Rate Technique(SSRT) has been adopted in the boiling 45 wt% $MgCl_2$ solution. The results are as follows. 1) Welded sections are more susceptible than base metal in SCC, and the rank of SCC, and the rasistance in welding method is TIG, MIG, $CO_2$ and ARC. 2) The Ultimate tensile strength(UTS) and the strain of both base metal and welded joint are reduced as decreasing extension rate. 3) The SCC resistance of 316L base metal and welded sections are superior than that of 304. 4) The tendency of pitting and the SCC suseptibility are agreed well, and the SCC site is welded deposit section in 316L whereas HAZ in 304.

  • PDF

AISI304L stainless steel에 저온 플라즈마 침탄처리 후 질화처리 시 Ar의 영향 (Effect of Ar addition on the surface properties of AISI304L stainless steel during low temperature plasma nitriding after low temperature plasma carburizing)

  • 정광호;이인섭
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2007년도 춘계학술발표회 초록집
    • /
    • pp.120-121
    • /
    • 2007
  • 스테인리스강을 침탄 또는 질화처리 하면 내식성이 크게 떨어진다. 하지만 처리 온도를 충분히 낮게 하면 내식성의 저하 없이 표면 경도를 증가시킬 수 있다. 침탄처리 후 질화 처리를 연속적으로 수행하면, 두꺼운 경화층을 가지고, 침탄처리한 표면보다 높은 경도를 가질 수 있다. 이 논문에서는 침탄처리 후 질화 처리시, Ar을 주입하여 질화층 형성에 주는 영향을 조사 하였다. Ar의 양이 20%보다 낮은 경우 석출물이 거의 형성되지 않았으며, Ar의 양이 증가할수록 표면경도도 증가하였다.

  • PDF

부식액의 조건 및 주사 속도가 AISI 304 스테인리스강의 전기화학적 부식에 미치는 영향 (Effect of the Corrosive Solution Conditions and Scan Rate to the Electrochemical Corrosion on the AISI 304 Stainless Steel)

  • 나은영;백신영
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제21권5호
    • /
    • pp.535-541
    • /
    • 1997
  • The effect of concentration of each solution( HCI, $H_2SO_4$ and $HNO_3$), scan rate and polished surface condition on the corrosion of AISI 304 Stainless Steel were investigated, utilizing the Method ASTM G5 - 87. It can be concluded that: 1) For the same concentration(i.e. 1N) of each solution the corrosion rate is the highest in HCI and lowest in $HNO_3$. Also, the difference of values of $i_{cirt}$ generated for each solution is significant. 2) As the concentration of the solution $H_2SO_4$ is increased (O.5N, 1N, 2N) the values of $E_{cor}$ $i_{crit}$ and $i_{p}$ are increased. 3) In case of existence of SCN ion of O.OlN, the values of iCTIt and ip generated are approximately 100 times and 1.4 times higher respectively, than in the case of non - existence of $SCN^{-}$. However the existence of $SCN^{-}$ doesn't affect the value of $E_{cor}$ and $E_{p}$. 4) The values of $i_{crit}$ and $i_{p}$ are increased due to the increase of scan rate. But the values of $E_{cor}$ and $E_{p}$ do not depend on the scan rate. 5) The $i_{p}$ value depends greatly on oxygen in the solution, but the changes in values of $E_{cor}$ $i_{crit}$ and $E_{b}$ due to the oxygen are insignificant. 6) If a component is polished using #400, #600 and #800 wet polish paper, the effect of surface condition on variations of values of $i_{crit}$ and $i_{p}$ is slightly significant.

  • PDF

Lubricating Effect of Water-soluble Hexagonal Boron Nitride Nanolubricants on AISI 304 Steel Sliding Pair

  • Gowtham Balasubramaniam;Dae-Hyun Cho
    • Tribology and Lubricants
    • /
    • 제39권2호
    • /
    • pp.43-48
    • /
    • 2023
  • In this study, we investigate the tribological behavior of AISI 304 stainless steel pairs under deionized water and hexagonal boron nitride (h-BN) water dispersion lubrication. The specimen friction and wear properties are evaluated using a reciprocating ball-on-flat tribometer. The coefficient of friction remains nearly constant throughout the test under both lubricant conditions. The wear depth of the specimens under h-BN lubrication is smaller than that under deionized water lubrication, indicating the inhibition behavior of h-BN nanolubricants on direct metal-metal contacts. Optical micrographs and stylus profilometer measurements are performed to evaluate the severity of damage caused by the sliding motion and to determine the wear morphology of the specimens, respectively. The results show that h-BN nanolubricants does not have a significant effect on the friction behavior but demonstrates reduced wear owing to their trapping effect between the sliding interfaces. Moreover, scanning electron microscopy and energy-dispersive X-ray spectroscopy images of the specimens were acquired to confirm the trapping effect of h-BN between the sliding interfaces. The results also suggest that the trapped lubricants can distribute the contact pressure, reducing the wear damage caused by the metal-metal contact at the interface. In conclusion, h-BN nanolubricants have potential as an anti-wear additive for lubrication applications. Further investigation is needed to provide direct evidence of the trapping effect of h-BN nanoparticles between the sliding interfaces. These findings could lead to the development of more efficient and effective lubricants for various industrial applications.

AISI 304 스테인리스강의 동적 재결정립 예측 (Prediction for the Dynamically Recrystallized Grain Size of AISI 304)

  • 김성일;유연철
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.143-146
    • /
    • 2001
  • The evolution of dynamic recrystallization (DRX) was studied with torsion test for AISI 304 stainless steel in the temperature range of $900-1000^{\circ}C$ and strain rate range of 0.05-5/sec. The evolution of DRX was investigated with microstructural analysis and change of flow stress curve slope. The investigation of serrated grain boundaries using electron back scattered diffraction (EBSD) analysis indicated that the nucleated new DRX grain size was similar to the size of bulging part. Before the steady state, the dynamically recrystallizing grains do not remain a constant size and gradually grow to the size of fully DRX grain at steady state. The calculation of grain size was based on $X_{DRX}$ and the assumption, which the nucleated DRX grains are growing to the steady state, continuously. It was found that the calculated results agreed with the microstructure of the alloy.

  • PDF

신뢰성기법을 이용한 항공구조재의 열기계적 특성 연구 (A Study on Thermo Mechanical Properties for a Airframe Structural Material by using Reliability Methods)

  • 박성호;박노석;김재훈
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 2008년도 제30회 춘계학술대회논문집
    • /
    • pp.40-45
    • /
    • 2008
  • 본 연구는 항공구조재로 널리 사용되고 있는 AISI 304강에 대한 상온 및 고온 인장특성을 신뢰성 기법을 이용하여 실험한 결과를 정리한 것이다. 인장실험은 ASTM 규정에 의하여 수행하였고, 정규확률지를 이용하여 항공구조설계 시 적용할 수 있는 A-Basis 및 B-Basis 강도를 평가하는 신뢰성 해석을 수행하였다.

  • PDF

3 차원 유한요소법을 이용한 AISI 304 표면용접평판의 잔류응력해석 (Residual Stress Analysis of AISI 304 Surface Welding Plate by 3D Finite Element Method)

  • 이경수;김태룡;김만원;박재학
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2008년도 추계학술대회A
    • /
    • pp.390-395
    • /
    • 2008
  • This study is performed to understand three dimensional characteristics of weld residual stress for the surface weld on the stainless steel plate. AISI 304 plate with one path weld on the surface was used as a test specimen. Finite element analysis was done to analyze thermal transient and residual stress due to weld. The result of finite element analysis was validated by previous paper and measurement data. Among various techniques for residual stress measurement, instrumented ball indentation method was applied. The calculated residual stresses by finite element analysis showed good agreement with the measured results.

  • PDF

오스테나이트계 스테인레스 강관에서의 손상해석에 관한 연구 (Failure Analysis of Austenitic Stainless Steel Pipe)

  • 이상율;이종오;이주석;조경식;조종춘;이보영
    • Journal of Welding and Joining
    • /
    • 제11권1호
    • /
    • pp.21-32
    • /
    • 1993
  • A cracking failure of a austenitic stainless steel elbow in a naphtha cracking line in a petrochenmical plant occurred, resulting in leakage of organic compound flowing inside the elbow. Due to the failure, emergency shutdown of the plant was enforced to repair the troubled part of the line. The repair cost as well as production loss during the unscheduled plant shutdown has cost the company a great amount of financial loss. In this studies, a failure analysis of the cracked elbow was performed using NDT, chemical analysis, microstructural analysis including optical microscopy as well as scanning electron microscopy with EPMA, mechanical testings such as tensile testing, hardness testing and Charphy impact test fractography. The results indicated that several problems such as a welding defect and presence of a detrimental phase which was found to be relate to improper postforming heat treatment process was identified and the failure was concluded to be due to a low temperature embrittlement of the defect-containing elbows.

  • PDF