전기화학적 방법에 의한 AISI 304 스테인리스강 용접부의 내식성 평가 (A Corrosion Resistance Evaluation of Welded AISI 304 Stainless Steel by Electrochemical Methods.)

  • 백신영;김관휴
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제14권1호
    • /
    • pp.83-89
    • /
    • 1990
  • Electrochemical methods have been proposed as non-destructive, rapid and quantitative means for determining the degree of sensitization associated with Chromium depleted zones surrounding precipitates of Cr carbide and formation of secondary phase in stainless steel. In this study, the specimen of AISI 304 stainless steel and its welded sections, which welded by TIG, MIG, $CO_2$ and ARC, were tested corrosion resistance by electrochemical methods in 0.5N HCl and 1N $H_2SO_4$ with or without 0.01N KSCN. The results were confirmed that electrochemical methods could be used as a test method of corrosion resistance evaluation for the welded AISI 304 stainless steel.

  • PDF

용접방법에 따른 AISI 304 및 316L스테인리스강 용접부의 틈부식 거동 (The Crevice Corrosion Behavior of AISI 304 & 316L Stainless Steel Welded by TIG, MIG, CO2 and SMA)

  • 백신영
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제15권4호
    • /
    • pp.22-28
    • /
    • 1991
  • The crevice corrosion behavior on austenitic AISI 304 and 316L stainless steel welded by TIG, MIG, $CO_2$ and SMA was studied. The results are as follows : In 10% $FeCl_3$ solution and natural sea water sampled near Mokpo port, the base metal of 304 stainless steel showed small amount corrosion, whereas 316L stainless steel did not showed any corrosion in the test periods. The weight loss caused by crevice corrosion increased with increasing weld heat input and residual .delta. ferrite formed in welded part. The corrosion resistance of the welded part was in the order of TIG, MIG, $CO_2$ and SMA. From this tendency, it is proved that the smaller heat input gives the better corrosion resistance.

  • PDF

Creq/Nieq비에 따른 AISI 304L 및 AISI 316L 스테인리스강 용접부의 미세조직 및 전기화학적 양극분극 평가 (Evaluations of Microstructure and Electrochemical Anodic Polarization of AISI 304L and AISI 316L Stainless Steel Weld Metals with Creq/Nieq Ratio)

  • 김연희;장아영;강동훈;고대은;신용택;이해우
    • 대한금속재료학회지
    • /
    • 제48권12호
    • /
    • pp.1090-1096
    • /
    • 2010
  • This pitting corrosion study of welded joints of austenitic stainless steels (AISI 304L and 316L) has addressed the differentiating solidification mode using three newly introduced filler wires with a flux-cored arc welding process (FCAW). The delta ferrite (${\delta}$-ferrite) content in the welded metals increased with an increasing equivalent weight ratio of chromium/nickel ($Cr_{eq}/Ni_{eq}$). Ductility dip cracking (DDC) was observed in the welded metal containing ferrite with none of AISI 304L and 0.1% of AISI 316L. The potentiodynamic anodic polarization results revealed that the $Cr_{eq}/Ni_{eq}$ ratio in a 3.5% NaCl solution didn't much affect the pitting potential ($E_{pit}$). The AISI 316L welded metals with ${\ddot{a}}$-ferrite content of over 10% had a superior $E_{pit}$ value. Though the AISI 316L welded metal with 0.1% ferrite had larger molybdenum contents than AISI 304L specimens, it showed a similar $E_{pit}$ value because the concentration of chloride ions and the corrosion product induced severe damage near the DDC.

AISI 304 스테인리스강의 동적 재결정립 예측 (Prediction for the Dynamically Recrystallized Grain Size of AISI 304)

  • 김성일;유연철
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.143-146
    • /
    • 2001
  • The evolution of dynamic recrystallization (DRX) was studied with torsion test for AISI 304 stainless steel in the temperature range of $900-1000^{\circ}C$ and strain rate range of 0.05-5/sec. The evolution of DRX was investigated with microstructural analysis and change of flow stress curve slope. The investigation of serrated grain boundaries using electron back scattered diffraction (EBSD) analysis indicated that the nucleated new DRX grain size was similar to the size of bulging part. Before the steady state, the dynamically recrystallizing grains do not remain a constant size and gradually grow to the size of fully DRX grain at steady state. The calculation of grain size was based on $X_{DRX}$ and the assumption, which the nucleated DRX grains are growing to the steady state, continuously. It was found that the calculated results agreed with the microstructure of the alloy.

  • PDF

오스테나이트 스테인리스강 용접부의 응력부식 거동에 미치는 용접 방법의 영향 (The effect of welding methods on the stress corrosion behavior of the welded austenitic stainless steel)

  • 백신영
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제19권4호
    • /
    • pp.42-50
    • /
    • 1995
  • To study the effect of welding methods on the Stress Corrosion Cracking (SCC) behavior of welded AISI type 316L and 304 austenitic stainless steel, the Slow Strain Rate Technique(SSRT) has been adopted in the boiling 45 wt% $MgCl_2$ solution. The results are as follows. 1) Welded sections are more susceptible than base metal in SCC, and the rank of SCC, and the rasistance in welding method is TIG, MIG, $CO_2$ and ARC. 2) The Ultimate tensile strength(UTS) and the strain of both base metal and welded joint are reduced as decreasing extension rate. 3) The SCC resistance of 316L base metal and welded sections are superior than that of 304. 4) The tendency of pitting and the SCC suseptibility are agreed well, and the SCC site is welded deposit section in 316L whereas HAZ in 304.

  • PDF

304L 스테인리스강의 저온 플라즈마질탄화 및 2-step 플라즈마 프로세스 (Low temperature plasma nitricarburizing and 2-step plasma processes of 304L austenitic stainless steels)

  • 이인섭
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2007년도 추계학술대회 논문집
    • /
    • pp.65-68
    • /
    • 2007
  • 저온 플라즈마 기술을 이용하면 오스테나이트계 스테인리스강의 내식성과 표면경도를 동시에 증가 시킬 수 있다. 여러 가지 처리방법 중 질탄화와 2-step 공정으로 처리한 AISI304L강의 표면을 분석하였다. 처리한 모든 시편의 표면은 expanded austenite(${\gamma}_N$)이 형성되었고, 표면 경도도 모재보다 약 4배 이상 증가 하였다. 저온플라즈마 질탄화 공정의 경우 경화층의 두께가 최대 15 ${\mu}m$밖에 형성되지 않았지만 2-step공정의 경우 질탄화 공정보다 짧은 시간으로 약 2배의 경화층을 얻을 수 있었다. 두 가지 공정 모두 온도와 시간이 증가할수록 경화층의 두께가 두꺼워졌지만, 과도하게 높은 온도와 긴 공정시간은 석출물을 형성 시켰다. 석출물이 형성되지 않은 시편의 경우 내식성이 증가하였다.

  • PDF

부식액의 조건 및 주사 속도가 AISI 304 스테인리스강의 전기화학적 부식에 미치는 영향 (Effect of the Corrosive Solution Conditions and Scan Rate to the Electrochemical Corrosion on the AISI 304 Stainless Steel)

  • 나은영;백신영
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제21권5호
    • /
    • pp.535-541
    • /
    • 1997
  • The effect of concentration of each solution( HCI, $H_2SO_4$ and $HNO_3$), scan rate and polished surface condition on the corrosion of AISI 304 Stainless Steel were investigated, utilizing the Method ASTM G5 - 87. It can be concluded that: 1) For the same concentration(i.e. 1N) of each solution the corrosion rate is the highest in HCI and lowest in $HNO_3$. Also, the difference of values of $i_{cirt}$ generated for each solution is significant. 2) As the concentration of the solution $H_2SO_4$ is increased (O.5N, 1N, 2N) the values of $E_{cor}$ $i_{crit}$ and $i_{p}$ are increased. 3) In case of existence of SCN ion of O.OlN, the values of iCTIt and ip generated are approximately 100 times and 1.4 times higher respectively, than in the case of non - existence of $SCN^{-}$. However the existence of $SCN^{-}$ doesn't affect the value of $E_{cor}$ and $E_{p}$. 4) The values of $i_{crit}$ and $i_{p}$ are increased due to the increase of scan rate. But the values of $E_{cor}$ and $E_{p}$ do not depend on the scan rate. 5) The $i_{p}$ value depends greatly on oxygen in the solution, but the changes in values of $E_{cor}$ $i_{crit}$ and $E_{b}$ due to the oxygen are insignificant. 6) If a component is polished using #400, #600 and #800 wet polish paper, the effect of surface condition on variations of values of $i_{crit}$ and $i_{p}$ is slightly significant.

  • PDF