원자력발전소용 316 스테인리스강 배관의 부식특성에 미치는 유도가열벤딩공정의 영향 (Effect of Induction Heat Bending Process on the Corrosion Properties of 316 Stainless Steel Pipes for Nuclear Power Plant)

  • 신민철;김영식;김경수;장현영;박흥배;성기호
    • Corrosion Science and Technology
    • /
    • 제13권3호
    • /
    • pp.87-94
    • /
    • 2014
  • Recently, the application of bending products has been increased since the industries such as automobile, aerospace, ships, and plants greatly need the usage of pipes. For facility fabrication, bending process is one of key technologies for pipings. Induction heat bending process is composed of bending deformation by repeated local heat and cooling. Because of local heating and compressive strain, detrimental phases may be precipitated and microstructural change can be induced. This work focused on the effect of induction heat bending process on the properties of ASME SA312 TP316 stainless steel. Evaluation was done on the base metal and the bended areas before and after heat treatment. Microstructure analysis, intergranular corrosion test including Huey test, double loop electropotentiokinetic reactivation test, oxalic acid etch test, and anodic polarization test were performed. On the base of microstructural analysis, grain boundaries in bended extrados area were zagged by bending process, but there were no precipitates in grain and grain boundary and the intergranular corrosion rate was similar to that of base metal. However, pitting potentials of bended area were lower than that of the base metal and zagged boundaries was one of the pitting initiation sites. By re-annealing treatment, grain boundary was recovered and pitting potential was similar to that of the base metal.

참조응력을 이용한 316LN 스테인리스강의 크리프 해석 (Creep Analysis of Type 316LN Stainless Steel Using Reference Stress)

  • 김우곤;류우석
    • 대한기계학회논문집A
    • /
    • 제26권10호
    • /
    • pp.2122-2129
    • /
    • 2002
  • Creep damage using a reference stress(RS) was analyzed for type 316LN stainless steel. The generalized K-R equation was reconstructed into the RS equation using a critical stress value $\sigma$. The RS equation was derived from the critical stress in failure time $t_f$ instead of material damage parameter $\omega$, which indicates the critical condition of collapse or approach to gross instability of materials during creep. For obtaining the reference stress, a series of creep tests and tensile tests were conducted with at 55$0^{\circ}C$ and $600^{\circ}C$. The stress-time data obtained from creep tests were applied to the RS equations to characterize the creep damage of type 316LN stainless steel. The value of creep constant r with stress levels was about 18 at 55$0^{\circ}C$ and 21 at $600^{\circ}C$. This value was almost similar with r = 24 in the K-R equation, which was obtained by using damage parameter $\omega$. Relationship plots of creep failure strain and life fraction $(t_f /t_r)$ were also obtained with different λ values. The RS equation was therefore more convenient than the generalized K-R equation, because the measuring process to quantify the damage parameter $\omega$ such as voids or micro cracks in crept materials was omitted. The RS method can be easily used by designers and plant operator as a creep design tool.

선택적 레이저 용융법으로 제조한 316L 스테인리스강의 기계적 이방성에 미치는 기공의 영향 (Effect of Porosity on Mechanical Anisotropy of 316L Austenitic Stainless Steel Additively Manufactured by Selective Laser Melting)

  • 박정민;전진명;김정기;성유진;박순홍;김형섭
    • 한국분말재료학회지
    • /
    • 제25권6호
    • /
    • pp.475-481
    • /
    • 2018
  • Selective laser melting (SLM), a type of additive manufacturing (AM) technology, leads a global manufacturing trend by enabling the design of geometrically complex products with topology optimization for optimized performance. Using this method, three-dimensional (3D) computer-aided design (CAD) data components can be built up directly in a layer-by-layer fashion using a high-energy laser beam for the selective melting and rapid solidification of thin layers of metallic powders. Although there are considerable expectations that this novel process will overcome many traditional manufacturing process limits, some issues still exist in applying the SLM process to diverse metallic materials, particularly regarding the formation of porosity. This is a major processing-induced phenomenon, and frequently observed in almost all SLM-processed metallic components. In this study, we investigate the mechanical anisotropy of SLM-produced 316L stainless steel based on microstructural factors and highly-oriented porosity. Tensile tests are performed to investigate the microstructure and porosity effects on mechanical anisotropy in terms of both strength and ductility.

스테인레스와 공구강 위에 스퍼터링된 Zr-ZrN 코팅층의 경도 및 밀착성에 대한 연구 (Hardness and adhesion of the reactively sputtered Zr-ZrN on the stainless steel(SUS304) and tool steel(SKH9))

  • 예길촌;신현준;권식철;백원승
    • 한국표면공학회지
    • /
    • 제26권6호
    • /
    • pp.316-326
    • /
    • 1993
  • Adhesion and hardeness are the most important properties of a hard coated layer which is applied to wear-resistant devices. Zr/ZrN layer was deposited on tool steel(SKH9) and stainless steel(SUS304) by a re-active D.C. magnetron sputtering technique and their microhardness and adhesion strength were measured for the films processed by changing the partial pressures of $N_2$ gas (4~10$\times$$10^{-4}$mbar) and the substrate bias voltage(0~250V). The adhesion strength was evaluated by acoustic signals through the scratch-test with the incremental applied load. As the partial pressure of $N_2$ gas and the substrate bias voltage were increased, the adhesion strength of tool steel was observed to be stronger than that of the stainless steel. The adhesion strength was generally, observed to decrease with the same tendency regardless of the kinds of substrates. The adhesion strength of tool steel was increased more and more strongly than that of stainless steel as heat-treated temperature was increased. The strength of tool steel was appeared to be high adhesion strength at $400^{\circ}C$. From the failure mode of the film during the scratch adhesion test, the cohesive failure was observed to be obvious and the adhesive failure in a minor portion in the Zr/ZrN doublelayer regardless of the kinds of substrates.

  • PDF

최소구속법을 이용한 Type 316LN 강의 크리프 수명 예측 (Creep Life Prediction of Type 316LN Steel Using Minimum Commitment Method)

  • 김우곤;윤송남;류우석;이원
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 추계학술대회 논문집
    • /
    • pp.295-298
    • /
    • 2005
  • A minimum commitment method (MCM) was applied to predict the creep rupture life of type 316LN SS. For this purpose, a number of the creep rupture data for the type 316LN SS were collected through literature survey and experimental data of KAERl, Using the short-term creep rupture data under 2000 hr, the long-term creep rupture life above $10^5$ hour was predicted by means of the MCM. An optimum value of A, P and G function, used in the MCM equation, was determined respectively, and the creep rupture life with the A values in different temperatures was compared with the experimental data and the predicted curves.

  • PDF

태양열 반응로용 나트륨 히트파이프의 열이송 특성에 관한 실험적 연구 (An Experimental Study on the Heat Transport Characteristics of a Sodium Heat Pipe for a Solar Furnace)

  • 부준홍;박철민;김진수;강용혁
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2008년도 춘계학술대회 논문집
    • /
    • pp.178-181
    • /
    • 2008
  • Cylindrical stainless-steel/sodium heat pipe for a high-temperature application was manufactured and tested for transient and steady-state operations. The container material was made of stainless-steel 316, and the working fluid was sodium. Stainless-steel 316 mesh screen was inserted as a capillary structure. The working fluid fill charge ratio was approximately 64 $\sim$ 181% based on the pore space of the wick. The outer diameter of the heat pipe was 12.7 mm and the total length was 250 mm. The evaporator part was 150 mm and the condenser 80 mm. The performance test of the heat pipe has been conducted in the furnace with up to 800 W. The variation of the average heat transfer coefficient was investigated as a function of heat flux and vapor temperature. As input thermal load increased, it was showed that difference of temperatures in evaporator and condenser decreased and that operating section and heat transfer characteristics at the heat pipe increased.

  • PDF

초내식성 스테인레스강의 금속이온용출특성 및 세포적합성 (Metal Ion Release Behaviour and Cytotoxicity of a Super Stainless Steel)

  • 김철생;박진수;허억;강곤
    • 대한의용생체공학회:의공학회지
    • /
    • 제17권1호
    • /
    • pp.11-18
    • /
    • 1996
  • The toxic metal ion release behaviour and the cytotoxicity of a super stainless steel (S.S.S, 22cr-20Ni -6Mo-0.25N) were investigated The measurement of the amount of static and wear- induced trace metal ion released from the steels was conducted in Hank's balanced salt solution using an electrothermal atomic absdrption spectrometry equiped with Uaphite furnace. And the in vitro cytotoxicity of the materials was assesed in cell culture. The static dissolution rates of Fe and Cr ions from the S.S.S were significantly lower than those of 316L SS. However, the Ni ion release from the S.S.S during the first 4 weeks was yester than that from 316L 55 by 15-45%. Also, the wear-in- duces dissolution rates from the steels were not correlated either with their elemental composition rates or with the static metal ion release rates. The S.S.S did not deteriorate the osteoblasts viability. And no toxic response was observed from the macrophages cultured for 7 days in RFMI 1640 medium immersed with the S.S.S specimens.

  • PDF

Corrosion fatigue crack growth behavior of 316LN stainless steel in high-temperature pressurized water

  • Zhang, Ziyu;Tan, Jibo;Wu, Xinqiang;Han, En-Hou;Ke, Wei
    • Nuclear Engineering and Technology
    • /
    • 제53권9호
    • /
    • pp.2977-2981
    • /
    • 2021
  • Corrosion fatigue crack growth (FCG) behavior of 316LN stainless steel was investigated in high-temperature pressurized water at different temperatures, load ratios (R = Kmax/Kmin) and rise times (tR). The environmental assisted effect on FCG rate was observed when both the R and tR exceeded their critical values. The FCG rate showed a linear relation with stress intensity factor range (ΔK) in double logarithmic coordinate. The environmental assisted effect on FCG rate depended on the ΔK and quantitative relations were proposed. Possible mechanisms of environmental assisted FCG rate under different testing conditions are also discussed.

페라이트계 및 오스테나이트계 스테인리스강과 IF강의 이종 접합부의 저항 점 용접성 평가 (Assessment of Resistance Spot Weldability of Dissimilar Joints of Austenitic Stainless Steels/IF Steels and Ferritic Stainless Steels/IF Steels)

  • 이진범;김동철;남대근;강남현;김순국;유지훈;임영목;박영도
    • 대한금속재료학회지
    • /
    • 제49권1호
    • /
    • pp.64-72
    • /
    • 2011
  • The spot weldability of dissimilar metal joints between austenitic stainless steels (STS316)/IF steels and ferritic stainless steels (STS430)/IF steels was investigated. This study was aimed to determine the spot welding parameters for a dissimilar metal joint and to evaluate the dissimilar metal joint's weldability, including its welding nugget shape, tensile-shear strength, hardness, and microstructure. The comparison of these results was described in terms of fracture behavior. Compared with the weld lobe of similar metal joints, dissimilar metal joints (STS430/IF) had reduced weld current range. However, the weld lobe of STS316/IF steel joint showed increased weld current range. This is because the dilution of chemical composition in the molten weld pool suppressed the heat input being caused by Joule heat with current flow through the samples. The microstructure of the fusion zone was fully martensite and mixture of ferrite and martensite for austenitic stainless steel/IF steel and ferritic stainless steel/IF steel combination, respectively. The experimental results showed that the shape of nugget was asymmetric, in which the fusion zone of the austenitic and ferritic stainless steel sheet was larger due to the higher bulk-resistance. The predicted microstructure by using the Schaeffler diagram was well matched with experimental results. After peel test, the fracture was initiated from heat affected zone of ferritic stainless steel sheet side, however the final fracture was propagated into the IF steel sheet side due to its lower strength.

스테인레스강 316L 상의 New Austrian Tunneling Method Coatings의 수지에 관한 기계적 특성 (Mechanical Properties on Resin of New Austrian Tunneling Coatings on Stainless Steel 316L)

  • 이주엽;성완모;김주한;성민정;김기준
    • 한국응용과학기술학회지
    • /
    • 제37권4호
    • /
    • pp.1034-1040
    • /
    • 2020
  • 스테인레스 스틸에 대한 합성된 폴리우레탄-에폭시 수지의 기계적 특성은 SEM, FT-IR, 인장특성, 그리고 EIS에 의한 특정질량손실량, 입도분석 등에 의해 물성을 측정하였다. 친환경적인 NATM 도료에 관한 관심이 고조됨에 따라 스테인레스 등의 금속에 코팅하는 무용제 도료를 합성하였다. 폴리올, IPDI, 충진제, 실리콘 계면활성제, 촉매 등이 함유된 기존 중방식수지보다 폴리올, MDI, 충진제, 실리콘 계면활성제, 촉매가 함유되어 합성된 중방식수지의 도료가 온도변화에 따른 인장강도가 증가하였고, 전해성이 높은 용액 속에서 저헝력이 크게 측정되었으며, 내구력과 강도가 양호하였다. 견고한 NATM 수지의 기계적 특성은 가교와 부식환경의 차단력이 증가함에 따라 강도가 증가하였다. 결론적으로 중방식의 가교된 미세조직은 방청코팅이 어려운 스테인레스 스틸 같은 금속물질 코팅에도 좋은 실험결과를 보여주었다.