Effect of Extracted Tempered Glass from End-of-Life Solar Panels on Mechanical Properties of Mortar (사용수명이 종료된 태양광 패널에서 분리된 강화유리가 모르타르의 역학적 특성에 미치는 영향)

  • So Yeong Choi;Sang Woo Kim;Il Sun Kim;Eun Ik Yang
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.27 no.2
    • /
    • pp.77-84
    • /
    • 2023
  • As the installation of solar panel accelerates, so does the number of solar panels reaching their end-of-life (EOL). However, the EOL solar panels is becoming a concern, as they contain potentially hazardous materials and are not easily recycled. Coping strategies such as effective collection, disposal, and recycling methods will be important to manage the growing number of EOL solar panels in the coming years.Therefore, many studies have focused on the development of EOL solar panel recycling technology. One recycling technology for EOL solar panels applicable to the construction field is the application of extracted tempered glass from EOL solar panels as construction materials. This study summarized the EOL solar panel disassembly technology and evaluated the mechanical properties of mortar using extracted tempered glass as fine aggregate. The results showed that when tempered glass was used as a fine aggregate in mortar, the compressive strength, flexural strength, and macro pores in the 1-3 ㎛ with 200-300 ㎛ range were affected, regardless of the disassembly technology of EOL solar panels. Especially, we found that the mechanical performance of mortar using chemically treated tempered glass was noticeably decreased due to changes in the chemical composition of the extracted tempered glass resulting from the removal of K2O and CuO due to chemical reactions. Meanwhile, it was found that when fly ash was used as a binder, the reduction of mechanical performance could be alleviated.

Carbonation Evaluation After CO2 Curing of Concrete Bricks Using Industrial by-products (산업부산물을 사용한 콘크리트 벽돌의 CO2 양생 후 탄산화 평가 )

  • Hoon Moon;Namkon Lee;Jung-Jun Park;Gum-Sung Ryu;Gi-Joon Park;Indong Jang
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.11 no.4
    • /
    • pp.373-380
    • /
    • 2023
  • This study investigated the carbonation of concrete brick cured in a CO2 environment for the utilization of CO2 captured in power plants. Concrete brick specimens were produced with electric arc furnace reducing slag (ERS) and electric arc furnace oxidizing slag (EOS), and cured for 3 days in a CO2 chamber with a concentration of 20 % or in a constant temperature and humidity chamber. The weight change, compressive strength, flexural strength and carbonation depth of concrete bricks were measured. From the results, it was found that when subjected to CO2 curing, CO2 was absorbed at the level of 2.4 % of the weight of the specimen. The specimen incorporating ERS showed the highest carbonation depth, and satisfied KS F4004 standards for the concrete brick. Therefore, it is expected that the captured CO2 can be utilized in the CO2 curing process of concrete brick.

The Time Dependent Deflection Characteristics and Evaluation of Reinforced Recycled Aggregate Concrete Beams (순환골재를 사용한 철근콘크리트 보의 장기 처짐 특성 및 평가)

  • Ji, Sang-Kyu;Yun, Hyun-Do;Kim, Sun-Woo;Lee, Eon-Young
    • Journal of the Korea Concrete Institute
    • /
    • v.20 no.1
    • /
    • pp.43-50
    • /
    • 2008
  • This paper presents experimental and analytical results on the long-term behavior of the reinforced recycled aggregate concrete beams under sustained loading. In this experimental program, three beams with different conditions of aggregates replacement (natural aggregate 100%, recycled coarse aggregate 100%, recycled fine aggregate 50%) were subjected to the sustained flexural loading that was a half of the nominal flexural capacity over a period of 1 year. The beam were designed with net span of 2,000 mm and rectangular cross-section of 170 mm width and 170 mm effective depth. The beams were instrumented and monitored to observe the change in the long-term behavior due to creep and shrinkage of concrete under sustained loading. The predictions of long-term deflection by ACI code, Branson, Mayer, Neville, EMM and AEMM were compared with the experimental results. From the experimental results, the reinforced concrete beams with recycled aggregates showed the same performance as that of a beam with natural aggregate. The proposed method to predict the long-term deflections of reinforced recycled aggregate concrete beams gives a good estimation for experimental results.

Properties of Non-Sintered Cement Mortar using Alkali and Sulfate Mixed Stimulants Accroding to Curing Method (양생방법에 따른 알칼리 및 황산염 복합자극제를 사용한 비소성 시멘트 모르타르의 특성)

  • Park, Sung-Joon;Kim, Ji-Hoon;Hyung, Won-Gil
    • Journal of the Korea Concrete Institute
    • /
    • v.27 no.3
    • /
    • pp.237-244
    • /
    • 2015
  • Entering the 20th century since the industrial revolution, the cement has been widely used in the field of construction and civil engineering due to the remarkable development of construction industry. However, result from that development, each kind of industrial by-products and waste and the carbon dioxide generated in the process of cement production cause air pollution and environmental damage so earth is getting sick now slowly. Therefore, we have to recognize importance about this. It means that the time taking specific and long-term measures have come. In this research paper, as substitution of the cement generating environmental pollution, we investigate the hydration reaction of non-Sintered Cement mortar mixed with GBFS, active stimulant of alkaline and sulphate series by using SEM and XRD, mechanical and chemical properties according to the curing method. As a result of this experiment, NSC realized outstanding strength for water curing and steam curing. It means that it has a good possibility as substitution of cement. From now on, it can be used for structure satisfying specific standard. We expect to find a substitution of outstanding cement by progressing continuous research making the best use of pros and cons according to the curing method.

Ground Vibration Reduction Technology Using High Damping Polymer Concrete (고 감쇠 폴리머 콘크리트를 활용한 지반진동 저감기술에 대한 연구)

  • Kim, Jeong-Jin;Seok, Won-Gyun;We, Joon-Woo;Ahn, So-Hee
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.25 no.6
    • /
    • pp.154-160
    • /
    • 2021
  • Recently, there have been increasing construction works carried out in urban centers, which are inducing frequent artificial vibration in the vicinity of existing structures due to such construction works. moreover, in case of industrial estates, vibration is induced due to operation of machines in the surrounding areas, thereby causing problems. meanwhile, in case of ordinary concrete that compose structure has low level of damping capability for vibration. accordingly, there are difficulties in blocking a wide range of vibrations delivered to the structures from outside including not only vibrations generated in the structures themselves but also ground vibration. recently, numerous studies are being carried out actively on high-damping system that markedly enhanced the damping performances of structures by utilizing polymer concrete in order to block the vibrations delivered to the structures through ground. therefore, this study compared the performances of polymer concrete with those of ordinary concrete, polyurethane pad and foamed rubber pad in order to review its performances in reducing ground vibration. for this purpose, review of FRF and vibration acceleration as dynamic characteristics was made. after comparative verification on the dynamic characteristics is made when polymer concrete and other aforementioned materials are applied to underground structures, the possibility of application of polymer concrete to structures is reviewed.

Effects of Boliing, Steaming, and Chemical Treatment on Solid Wood Bending of Quercus acutissima Carr. and Pinus densiflora S. et. Z. (자비(煮沸), 증자(蒸煮) 및 약제처리(藥劑處理)가 상수리나무와 소나무의 휨가공성(加工性)에 미치는 영향(影響))

  • So, Won-Tek
    • Journal of the Korean Wood Science and Technology
    • /
    • v.13 no.1
    • /
    • pp.19-62
    • /
    • 1985
  • This study was performed to investigate: (i) the bending processing properties of silk worm oak (Quercus acutissima Carr.) and Korean red pine (Pinus densiflora S. et Z.) by boiling and steaming treatments; (ii) the effects of interrelated factors - sapwood and heartwood, annual ring placement, softening temperature and time, moisture content. and wood defects on bending processing properties; (iii) the changing rates of bending radii after release from a tension strap, and (iv) the improving methods of bending process by treatment with chemicals. The size of specimens tested was $15{\times}15{\times}350mm$ for boiling and steaming treatments and $5{\times}10{\times}200mm$ for treatments with chemicals. The specimens were green for boiling treatments and dried to 15 percent for steaming treatments. The specimens for treatments with chemicals were soaked in saturated urea solution, 35 percent formaldehyde solution, 25 percent polyethylene glycol -400 solution, and 25 percent ammonium hydroxide solution for 5 days and immediately followed the bending process, respectively. The results obtained were as follows: 1. The internal temperature of silk worm oak and Korean red pine by boiling and steaming time was raised slowly to $30^{\circ}C$ but rapidly from $30^{\circ}C$ to $80-90^{\circ}C$ and then slowly from $80-90^{\circ}C$ to $100^{\circ}C$. 2. The softening time required to the final temperature was directly proportional to the thickness of specimen. The time required from $25^{\circ}C$ to $100^{\circ}C$ for 15mm-squared specimen was 9.6-11.2 minutes in silk worm oak and 7.6-8.1 minutes in Korean red pine. 3. The moisture content (M.C.) of specimen by steaming time was increased rapidly first 4 minutes in the both species, and moderately from 4 to 20 minutes and then slowly and constantly in silk worm oak, and moderately from 4 to 15 minutes and then slowly and constantly in Korean red pine. The M.C. of 15mm-squared specimen in 50 minutes of steaming was increased to 18.0 percent in the oak and 22.4 percent in the pine from the initial conditioned M.C. of 15 percent The rate of moisture adsorption measured was therefore faster in the pine than in the oak. 4. The mechanical properties of the both species were decreased significantly with the increase of boiling rime. The decrement by the boiling treatment for 60 minutes was measured to 36.6-45.0 percent in compressive strength, 12.5-17.5 percent in tensile strength, 31.6-40.9 percent in modulus of rupture, and 23.3-34.6 percent in modulus of elasticity. 5. The minimum bending radius (M.B.R.) of sapwood and heartwood was 60-80 mm and 90 mm in silk worm oak, and 260 - 300 mm and 280 - 300 mm in Korean red pine, respectively. Therefore, the both species showed better bending processing properties in sapwood than in heartwood. 6. The M.B.R. of edge-grained and flat-grained specimen in suk worm oak was 60-80 mm, but the M.B.R. in Korean red pine was 240-280 mm and 260-360 mm, respectively. Comparing the M.B.R. of edge-grained with flat-grained specimen, in the pine the edge-grained showed better bending processing property than the flat-grained. 7. The bending processing properties of the both species were improved by the rising of softening temperature from $40^{\circ}C$ to $100^{\circ}C$. The minimum softening temperature for bending was $90^{\circ}C$ in silk worm oak and $80^{\circ}C$ in Korean red pine, and the dependency of softening temperature for bending was therefore higher in the oak than in the pine. 8. The bending processing properties of the both species were improved by the increase of softening time as well as temperature, but even after the internal temperature of specimen reaching to the final temperature, somewhat prolonged softening was required to obtain the best plastic conditions. The minimum softening time for bending of 15 mm-squared silk worm oak and Korean red pine specimen was 15 and 10 minutes in the boiling treatment, and 30 and 20 minutes in the steaming treatment, respectively. 9. The optimum M.C. for bending of silk worm oak was 20 percent, and the M.C. above fiber saturation point rather degraded the bending processing property, whereas the optimum M.C. of Korean red pine needed to be above 30 percent. 10. The bending works in the optimum conditions obtained as seen in Table 24 showed that the M.B.R. of silk worm oak and Korean red pine was 80 mm and 240 mm in the boiling treatment, and 50 mm and 280 mm in the steaming treatment, respectively. Therefore, the bending processing property of the oak was better in the steaming than in the boiling treatment, but that of the pine better in the boiling than in the steaming treatment. 11. In the bending without a tension strap, the radio r/t of the minimum bending radius t to the thickness t of silk worm oak and Korean red pine specimen amounted to 16.0 and 21.3 in the boiling treatment, and 17.3 and 24.0 in the steaming treatment, respectively. But in the bending with a tension strap, the r/t of the oak and the pine specimen decreased to 5.3 and 16.0 in t he boiling treatment, and 3.3 and 18.7 in the steaming treatment, respectively. Therefore, the bending processing properties of the both species were significantly improved by the strap. 12. The effect of pin knot on the degradation of bending processing property was very severe in silk worm oak by side, e.g. 90 percent of the oak specimens with pin knot on the concave side were ruptured when bent to a 100 mm radius but only 10 percent of the other specimens with pin knot on the convex side were ruptured. 13. The changing rate in the bending radius of specimen bent to a 300 mm radius after 30 days of exposure to room temperature conditions was measured to 4.0-10.3 percent in the boiling treatment and 13,0-15.0 percent in the steaming treatment. Therefore, the degree of spring back after release was higher in the steaming than in the boiling treatment. And the changing rate of moisture-proofing treated specimen by expoxy resin coating was only -1.0.0 percent. 14. Formaldehyde, 35 percent solution, and 25 percent polyethylene glycol-400 solution found no effect on the plasticization of the both species, but saturated urea solution and 25 percent ammonium hydroxide solution found significant effect in comparison to non-treated specimen. But the effect of the treatment with chemicals alone was inferior to that of the steaming treatment, and the steaming treatment after the treatment with chemicals improved 10-24 percent over the bending processing property of steam-bent specimen. 15. Three plasticity coefficients - load-strain coefficient, strain coefficient, and energy coefficient - were evaluated to be appropriate for the index of bending processing property because the coefficients had highly significant correlation with the bending radius. The fitness of the coefficients as the index was good at load-strain coefficient, energy coefficient, and strain coefficient, in order.

  • PDF