  • In this study, a structural concrete square beam was developed using the centrifugal molding technique. In order to secure the bending stiffness of the cross section, the hollow rate of the cross section was set to 10% or less. Instead of using the current poor mixture of concrete and a concrete mixing ratio with a high slump (150-200) and a design strength of 100 MPa or more was developed and applied. In order to investigate the durability of centrifugally formed PSC square beams to be used as the superstructure of the avalanch tunnel or ramen bridge, the durability performance of ultra-high-strength centrifugally formed concrete with a compressive strength of 100 MPa was evaluated in terms of deterioration and chemical resistance properties.Concrete durability tests, including chloride penetration resistance, accelerated carbonation, sulfate erosion resistance, freeze-thaw resistance, and scaling resistance, were performed on centrifugally formed square beam test specimens produced in 2022 and 2023. Considering the information verified in this study, the durability of centrifugally molded concrete, which has increased watertightness in the later manufacturing stage, was found to be superior to that of general concrete.

Impact Resistance Reliability of Sn-1.2Ag-0.5Cu-0.4In Solder Joints (Sn-1.2Ag-0.5Cu-0.4In 조성 솔더 접합부의 내 충격 신뢰성 평가)

  • Yu, A-Mi;Lee, Chang-Woo;Kim, Jeong-Han;Kim, Mok-Soon;Lee, Jong-Hyun
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.226-226
    • /
    • 2008
  • 지난 10여년 동안 Sn-3.0Ag-0.5(wt%)Cu 합금은 대표 무연솔더 조성으로 다양한 전자제품의 실장 및 접합에 적용되어 왔으며, 그 신뢰성 역시 충분히 검증된 바 있다. 그러나 최근 Ag 가격의 급격한 상승과 솔더 접합부의 내 충격 신뢰성을 보다 향상시키고자 하는 업계의 동향은 Ag의 함량이 낮은 무연솔더 조성의 적용 확대를 유도하고 있다. 이에 따라 본 연구자들은 저 Ag 함유 무연슬더로 Sn-1.2Ag-0.5Cu-0.4In 조성을 제안한 바 있는데, 이는 Sn-3.0Ag-0.5Cu 조성 이상의 solderability를 가지면서도 그 금속원료 가격이 약 20% 가량 저렴한 특징을 가진다. 또한 열 싸이클링 (cycling) 테스트를 통한 슬더 조인트의 신뢰성을 평가한 결과, Sn-3.0Ag-0.5Cu에 크게 뒤떨어지지 않는 양호한 특성이 관찰되었다. 따라서 본 연구에서는 열 싸이클링 테스트와 더불어 최근 그 중요성이 지속적으로 커지고 있는 내 충격 신뢰성 평가 시험을 실시하여 개발된 4원계 무연솔더 조성의 기계적 특성을 기존 무연솔더 조성과 비교, 분석해 보았다. 각 솔더 조성은 솔더 볼 형태로 제조되어 CSP(Chip Scale Package) 상에 범핑 (bumping)되었으며, CSP를 PCB(Printed Circuit Board) 상에 실장하는 공정에서도 Sn-3.0Ag-0.5Cu 및 Sn-1.2Ag-0.5Cu-0.4In의 두 종류의 솔더 페이스트가 사용되었다. 본 연구에서의 내 충격 신뢰성 시험에는 자체 제작한 rod drop 시험기를 사용하였는데, 고정된 CSP 실장 board의 후면 부위를 일정한 높이에서 추를 반복적으로 자유 낙하시켜 급격한 충격을 주는 방식으로 실험을 실시하였다. 이 때 추의 무게는 30g, 낙하 높이는 10cm 였으며, 추의 낙하 시 측정된 board 의 휨 변위량은 약 0.7mm로 측정되었다. 사용된 CSP와 PCB 는 모두 daisy chain 방식으로 연결되어 있기 때문에 저항측정기를 사용한 간단한 실시간 저항 측정 방법으로 시험 이력에 따른 파단부의 발생 시점과 대략의 위치를 손쉽게 확인할 수 있었다. 솔더 조인트의 파단 기준 저항값으로 $1000\Omega$을 설정하였으며. 각 조건 당 5 개 이상의 샘플에 대해 평가를 실시한 후 그 평균값을 조사하였다. 시험 결과 제안된 Sn-1.2Ag-0.5Cu-0.4In 조성은 대표적인 저 Ag 함유 조성인 Sn-1.0Ag-0.5Cu에 비해서는 떨어지는 내 충격 신뢰성을 나타내었지만, 우수한 연성에 기인하여 Sn-3.0Ag-0.5Cu 조성에 비해서는 약 2 배 이상 우수한 신뢰성이 관찰되었다. 또한 CSP의 실장 시 Sn-3.0Ag-0.5Cu보다 Sn-1.2Ag-0.5Cu-0.4In 조성 솔더 페이스트를 적용한 경우에서 보다 우수한 내 충격 신뢰성을 나타내어 기본적으로 개발된 Sn-1.2Ag-0.5Cu-0.4In 솔더 페이스트가 Sn-3.0Ag-0.5Cu 조성의 기존 솔더 페이스트 보다 내 충격 신뢰성이 우수함을 검증할 수 있었다. 각 조성의 솔더 조인트를 $150^{\circ}C$ 에서 500시간 aging한 후 실시한 내 충격 신뢰성 평가에서는 모든 조성에서 그 신뢰성이 급감하는 경항을 나타내었으나, Sn-1.2Ag-0.5Cu-0.4In가 Sn-l.0Ag-0.5Cu보다도 그 상대적인 신뢰성이 우수한 것으로 관찰되었다. 이와 같이 aging 후 실시하는 충격시험은 가장 실제적인 상황과 유사한 조건이므로 상기의 실험 결과는 매우 고무적이었으며, 이에 대한 보다 면밀한 분석이 요청되었다. 마지막으로 파면 및 미세조직 관찰을 통하여 각 조성에서의 충격 파단 특성을 비교, 분석해 보았다.

  • PDF

Study on the Physical and Mechanical Properties of Particleboard and Oriented Strandboard Manufactured by Tulliptree (Liriodendron tulipifera L.) (백합나무를 이용하여 제조한 3층 파티클보드와 배향성 스트랜드보드(OSB)의 물성에 관한 연구)

  • Seo, Jun won;Gang, Gil woo;Jo, Gun hee;Park, Heon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.46 no.1
    • /
    • pp.67-72
    • /
    • 2018
  • This study was conducted to investigate a potential of Yellow poplar (Liriodendron tulipifera L.) as a raw material for the manufacturing of particleboard (PB) and oriented strandboard (OSB). PB panels were prepared at the parameters of $0.7g/cm^3$ density, 15 mm thickness, three-layer, $E_1$ grade urea-formaldehyde (UF) resin, emulsion wax, and hardener. OSB panels were manufactured with a density of $0.65g/cm^3$, thickness of 10 mm, and $E_1$ grade of UF resin. Particle size of the face layer of PB was 20~80 mesh with 7~9% moisture content (MC), while that of core-layer was 3~20 mesh with 3~5% MC, which was similar to the production condition of commercial PB. As a result, the manufactured PB panels with 15.8 mm thickness, $0.7g/cm^3$ density, and 5.8% MC satisfied the requirement of bending strength of 15 type PB of Korean Industrial Standard (KS F 3104). Both internal bonding (IB) strength and surface screw withdrawal resistance also satisfied the requirement of 18 type PB of the standard. But, the edge screw withdrawal resistance satisfied the requirement of 15 type PB of the standard. These differences in properties could be due to the slenderness ratio of raw particles. In case of OSB panels with 10.7 mm thickness, $0.68g/cm^3$ density, and 5.8% MC satisfied all the requirements of bending strength, screw withdrawal resistance, and IB strength of 18 type PB of the standard. These results suggest that Yellow poplar wood has a good potential as a raw material for the production of PB and OSB.

Effects of Boliing, Steaming, and Chemical Treatment on Solid Wood Bending of Quercus acutissima Carr. and Pinus densiflora S. et. Z. (자비(煮沸), 증자(蒸煮) 및 약제처리(藥劑處理)가 상수리나무와 소나무의 휨가공성(加工性)에 미치는 영향(影響))

  • So, Won-Tek
    • Journal of the Korean Wood Science and Technology
    • /
    • v.13 no.1
    • /
    • pp.19-62
    • /
    • 1985
  • This study was performed to investigate: (i) the bending processing properties of silk worm oak (Quercus acutissima Carr.) and Korean red pine (Pinus densiflora S. et Z.) by boiling and steaming treatments; (ii) the effects of interrelated factors - sapwood and heartwood, annual ring placement, softening temperature and time, moisture content. and wood defects on bending processing properties; (iii) the changing rates of bending radii after release from a tension strap, and (iv) the improving methods of bending process by treatment with chemicals. The size of specimens tested was $15{\times}15{\times}350mm$ for boiling and steaming treatments and $5{\times}10{\times}200mm$ for treatments with chemicals. The specimens were green for boiling treatments and dried to 15 percent for steaming treatments. The specimens for treatments with chemicals were soaked in saturated urea solution, 35 percent formaldehyde solution, 25 percent polyethylene glycol -400 solution, and 25 percent ammonium hydroxide solution for 5 days and immediately followed the bending process, respectively. The results obtained were as follows: 1. The internal temperature of silk worm oak and Korean red pine by boiling and steaming time was raised slowly to $30^{\circ}C$ but rapidly from $30^{\circ}C$ to $80-90^{\circ}C$ and then slowly from $80-90^{\circ}C$ to $100^{\circ}C$. 2. The softening time required to the final temperature was directly proportional to the thickness of specimen. The time required from $25^{\circ}C$ to $100^{\circ}C$ for 15mm-squared specimen was 9.6-11.2 minutes in silk worm oak and 7.6-8.1 minutes in Korean red pine. 3. The moisture content (M.C.) of specimen by steaming time was increased rapidly first 4 minutes in the both species, and moderately from 4 to 20 minutes and then slowly and constantly in silk worm oak, and moderately from 4 to 15 minutes and then slowly and constantly in Korean red pine. The M.C. of 15mm-squared specimen in 50 minutes of steaming was increased to 18.0 percent in the oak and 22.4 percent in the pine from the initial conditioned M.C. of 15 percent The rate of moisture adsorption measured was therefore faster in the pine than in the oak. 4. The mechanical properties of the both species were decreased significantly with the increase of boiling rime. The decrement by the boiling treatment for 60 minutes was measured to 36.6-45.0 percent in compressive strength, 12.5-17.5 percent in tensile strength, 31.6-40.9 percent in modulus of rupture, and 23.3-34.6 percent in modulus of elasticity. 5. The minimum bending radius (M.B.R.) of sapwood and heartwood was 60-80 mm and 90 mm in silk worm oak, and 260 - 300 mm and 280 - 300 mm in Korean red pine, respectively. Therefore, the both species showed better bending processing properties in sapwood than in heartwood. 6. The M.B.R. of edge-grained and flat-grained specimen in suk worm oak was 60-80 mm, but the M.B.R. in Korean red pine was 240-280 mm and 260-360 mm, respectively. Comparing the M.B.R. of edge-grained with flat-grained specimen, in the pine the edge-grained showed better bending processing property than the flat-grained. 7. The bending processing properties of the both species were improved by the rising of softening temperature from $40^{\circ}C$ to $100^{\circ}C$. The minimum softening temperature for bending was $90^{\circ}C$ in silk worm oak and $80^{\circ}C$ in Korean red pine, and the dependency of softening temperature for bending was therefore higher in the oak than in the pine. 8. The bending processing properties of the both species were improved by the increase of softening time as well as temperature, but even after the internal temperature of specimen reaching to the final temperature, somewhat prolonged softening was required to obtain the best plastic conditions. The minimum softening time for bending of 15 mm-squared silk worm oak and Korean red pine specimen was 15 and 10 minutes in the boiling treatment, and 30 and 20 minutes in the steaming treatment, respectively. 9. The optimum M.C. for bending of silk worm oak was 20 percent, and the M.C. above fiber saturation point rather degraded the bending processing property, whereas the optimum M.C. of Korean red pine needed to be above 30 percent. 10. The bending works in the optimum conditions obtained as seen in Table 24 showed that the M.B.R. of silk worm oak and Korean red pine was 80 mm and 240 mm in the boiling treatment, and 50 mm and 280 mm in the steaming treatment, respectively. Therefore, the bending processing property of the oak was better in the steaming than in the boiling treatment, but that of the pine better in the boiling than in the steaming treatment. 11. In the bending without a tension strap, the radio r/t of the minimum bending radius t to the thickness t of silk worm oak and Korean red pine specimen amounted to 16.0 and 21.3 in the boiling treatment, and 17.3 and 24.0 in the steaming treatment, respectively. But in the bending with a tension strap, the r/t of the oak and the pine specimen decreased to 5.3 and 16.0 in t he boiling treatment, and 3.3 and 18.7 in the steaming treatment, respectively. Therefore, the bending processing properties of the both species were significantly improved by the strap. 12. The effect of pin knot on the degradation of bending processing property was very severe in silk worm oak by side, e.g. 90 percent of the oak specimens with pin knot on the concave side were ruptured when bent to a 100 mm radius but only 10 percent of the other specimens with pin knot on the convex side were ruptured. 13. The changing rate in the bending radius of specimen bent to a 300 mm radius after 30 days of exposure to room temperature conditions was measured to 4.0-10.3 percent in the boiling treatment and 13,0-15.0 percent in the steaming treatment. Therefore, the degree of spring back after release was higher in the steaming than in the boiling treatment. And the changing rate of moisture-proofing treated specimen by expoxy resin coating was only -1.0.0 percent. 14. Formaldehyde, 35 percent solution, and 25 percent polyethylene glycol-400 solution found no effect on the plasticization of the both species, but saturated urea solution and 25 percent ammonium hydroxide solution found significant effect in comparison to non-treated specimen. But the effect of the treatment with chemicals alone was inferior to that of the steaming treatment, and the steaming treatment after the treatment with chemicals improved 10-24 percent over the bending processing property of steam-bent specimen. 15. Three plasticity coefficients - load-strain coefficient, strain coefficient, and energy coefficient - were evaluated to be appropriate for the index of bending processing property because the coefficients had highly significant correlation with the bending radius. The fitness of the coefficients as the index was good at load-strain coefficient, energy coefficient, and strain coefficient, in order.

  • PDF

Evaluation on Performance of Repair Mortar Used for Pre-wetting Spray Method (프리웨팅 스프레이 공법용 모르타르의 성능평가)

  • Nam, Yong-Hyuk;Chung, Young-Jun;Jang, Suk-Hwan;An, Young-Ki;Kim, Sung Chil
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.9 no.4
    • /
    • pp.235-242
    • /
    • 2005
  • This study is on the evaluation of performance of polymer cement mortar which is used for pre-wetting spray method. Pre-wetting spray method is an epoch-making method to repair concrete structures damaged, which is added a small quantity water preciously to dry mortar to reduce dust and rebound and spray mortar mixed with fixed quantity water at nozzle before spray. The result showed that physical performance such like compressive, flexural and adhesive strength of polymer cement mortar, TS 100 used for pre-wetting spray method was superior to other repair mortar. Also durable performance such as resistance on permeability of chloride ion, carbonation, chemical and freezing-thawing was excellent.

An Experimental Study on the Mechanical Behavior of Concrete Using Non-Sintered Cement (비소성 시멘트 콘크리트의 역학적 거동에 대한 실험 연구)

  • Yoo, Sung-Won;Min, Gyeong-Oan
    • Journal of the Korea Institute of Building Construction
    • /
    • v.12 no.1
    • /
    • pp.115-121
    • /
    • 2012
  • If cement could be manufactured with industrial byproducts such as granulated blast furnace slag, phosphogypsum, and waste lime rather than clinker, there would be many advantages, including the maximization of the use of these industrial byproducts for high value-added resources, the conservation of natural resources and energy by omitting the use of clinker, the minimization of environmental pollution problems caused by $CO_2$ discharge, and the reduction of the production cost. For this reason, in this study, mechanical behavior tests of non-sintered cement concrete were performed, and elasticity modulus and stress-strain relationship of non-sintered cement concrete were proposed. Nine test members were manufactured and tested according to reinforcement ratio and concrete compressive strength. According to the test results, there was no difference between general cement concrete and non-sintered cement concrete in terms of flexure and shear behavior.

A Study on the Development of Light Emotion Friendly Concrete Block for Efficient Application of Titan-oxide Photocatalyst (이산화티탄 광촉매의 효율적 적용을 위한 LEFC 블록 제작에 관한 연구)

  • Kim, Byoung-Il;Oh, Sang-Keun;Seo, Seung-Hoon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.6
    • /
    • pp.120-131
    • /
    • 2019
  • Recently, the level of fine dust and ultrafine dust has reached its highest level, threatening the public's health. If the air purifier was not operated indoors, natural ventilation would not be possible. In this study, photocatalyst is applied to building materials to purify air in a passive manner. In order to use photocatalyst for LEFC(Light Emotion Friendly Concrete), it is necessary to secure self-consolidating capability. Therefore, self-consolidating performance was evaluated by slump test, J-ring test and L-box test with UHPC materials applied. Based on these results, the mixture proportion was determined, and the mechanical performance was evaluated by compressive and flexural tests. Concrete blocks were constructed with a fabrication method that improved the existing process of making LEFC. Also, the concrete block was emptied as a way to reduce the use of expensive photocatalyst. Finally, in order to identify the distribution of TiO2, an EDS analysis was performed.

Steel Fiber Reinforcing Effect Analysis of Slab Panel Structure and Assessment Technics of Toughness (강섬유보강 패널구조의 보강효과 분석 및 인성평가 기법)

  • Jeon, Chan-Ki;Park, Sun-Kyu
    • Magazine of the Korea Concrete Institute
    • /
    • v.11 no.2
    • /
    • pp.209-220
    • /
    • 1999
  • This paper is aimed to evaluate the effectiveness of flexural toughness of slab panel structures($60{\times}60{\times}10$) reinforced by steel fiber instead of wire mesh. Steel fiber used in this study is double hooked Dramix type fiber. And the fiber length is 60mm, diameter is 0.8mm, Various assessment methods of toughness index are used to estimate the proper effectiveness. In this experimental study, we find that Johnston, JCI-SF4 and EFNARC method are more effective to assess the flexural toughness of slab panels than the others. And the steel fiber is very effective alternative material to reinforce slab panel structures instead of wire mesh. Fiber volume fraction of 0.5~0.75% is more useful than the others in enhancing the post-peak energy absorption and toughness index by Johnston's $I_{5.5}$ assessment method. And the slab panels reinforcing with steel fiber are more resistant to crack propagation than wire mesh reinforcing slabs.

Comparison on the Behaviors of Inverted Tee and Rectangular Precast Prestressed Concrete Beams Under Combined Bending and Torsion (휨과 비틀림을 받는 프리캐스트 PSC 역T형 보와 직사각형 보의 거동 비교)

  • Seol Dong-Jae;Park Sang-Yeol;Yu Sung-Yong
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.6 s.84
    • /
    • pp.733-740
    • /
    • 2004
  • This study presents the behaviors of the typical architectural precast prestressed concrete beams, inverted tee and rectangular beams, subjected to combined flexural and torsional loads. For this purpose, two inverted-tee beams were designed with a parking live load, $5 kN/m^2$, and a market load $12 kN/m^2$ according to the currently used typical shape in the domestic building site. Also, two rectangular beams were also designed as the same bottom dimension and area, and reinforced for similar strength as in the cases of inverted tee beams. Total of four beams were tested, under combined bending and torsion, analysed and compared. Test results showed that the cracking and ultimate flexural strength of the beams decreased under torsional loading. However, two different shaped-beams had roughly the same load resisting capacity in service and ultimate states.

Failure Mode and Design Guideline for Reinforced Concrete Slab Strengthened Using Carbon FRP Grid (Carbon FRP Grid로 휨 보강한 철근콘크리트 슬래브의 파괴형태와 설계기준)

  • Park Sang-Yeol;Xian Cui
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.5 s.83
    • /
    • pp.667-675
    • /
    • 2004
  • This paper presents the failure mode and strengthening design of reinforced concrete slab strengthened with Carbon Fiber Reinforced Polymer(CFRP) grid. Parameters involved in this experimental study are FRP grid reinforcement quantity, repair mortar thickness, the presence of anchor, and strengthening in compression. In this study, there are different failure types with increasing the CFRP grid strengthening reinforcement. On the low strengthening level, CFRP grid in repair mortar cover ruptures. On the moderate strengthening level, there is a debonding shear failure in the interface of carbon FRP grid because of the excessive shear deformation. On the high strengthening level, diagonal shear failure occurs. With the increasing of FRP grid reinforcement, the strengthening effect increased, but the ductility decreased. By limiting the strengthening level, it can be achieved to prevent shear failure which result in sudden loss in the resisting load capacity. CFRP rupture failure is desirable, because CFRP ruptured concrete slab keeps the same load capacity and ductility haying before strengthening even after failure. Finally, design guideline and procedure are given for strengthening of concrete slab with CFRP grid.