Dissolution of Pb from the Complex Sulphide Concentrates Containing Galena and Arsenopyrite by Alkaline Oxidative Leaching (황비철광(黃砒鐵鑛)과 방연광(方鉛鑛)의 혼합황화광(混合黃化鑛)의 알카리산화(酸化)에 의한 Pb침출(浸出))

  • Youn, Ki-Byoung
    • Resources Recycling
    • /
    • v.17 no.3
    • /
    • pp.42-47
    • /
    • 2008
  • In this work, the dissolution behavior of Pb from the complex sulphide concentrates containing Galena and Arsenopyrite by alkaline oxidative leaching was studied. The influences of leaching temperature, oxygen partial pressure, leaching time and NaOH concentration of leaching solution were examined at the leaching conditions in the range of $100^{\circ}C{\sim}140^{\circ}C$ temperature, $40psi{\sim}100psi\;PO_2$ and $0.5M{\sim}2M$ NaOH concentration. The optimum result was obtained at the leaching condition of leaching temperature $120^{\circ}C$, 100psi $PO_2$, leaching time 30min. and 2M NaOH concentration of leaching solution.

Removal and Separation of Metallic Constituents from the By-product Recovered from Gold Mine Tailings (금(金) 광산(鑛山) 폐광미(廢鑛尾)로부터 회수(回收)된 금속광물(金屬鑛物) 부산물(副産物) 중의 금속성분(金屬成分) 분리(分離), 제거연구(除去硏究))

  • Youn, Ki-Byoung
    • Resources Recycling
    • /
    • v.19 no.3
    • /
    • pp.9-15
    • /
    • 2010
  • Domestic gold mine tailings, generally, contain a lot of non-metallic silica and clay minerals. These minerals can be separated from the tailings by various physical separation methods and used as raw materials for cements and ceramic products. In these physical separation procedures, metallic complex sulfides, in which Au and metallic constituents such as Pb, As and Fe were concentrated, were obtained as a by-product. These metallic constituents should be removed or separated from the by-product to extract Au efficiently. In this work, removal and separation processes of Pb, As, and Fe from the by-product were investigated. Pb was removed to under 3% by using alkaline oxidative leaching at the leaching condition of $120^{\circ}C$, 2M NaOH, 100psi $Po_2$, 250r.p.m., 4 wt.% solid and 30 min. leaching time. The leached residue was roasted and separated magnetically to obtain a non-magnetic product contained <0.2% As, <3% Fe and high concentrated Au more than 8,000 ppm.