This paper reports the test results for shrinkage properties of low shrinkage high performance concrete developed by the authors depending on specimen size and constraint of reinforcing bar. As properties in fresh concrete low shrinkage high performance concrete(LSHPC) combined with expansive additives and shrinkage reducing admixture resulted in increase SP dosage due to loss of fluidity compared with that of control mixture concrete, while the dosage of AE agent was decreased. LSHPC exhibited higher compressive and tensile strength than control mixture concrete. For the effect of specimen size, an increase in specimen size led to a reduction of drying shrinkage. However, it was found that the autogenous shrinkage was not affected by the specimen size and measuring method. For constraint condition, an increase in the ratio of reinforcing bar caused the slight reduction in the strain of reinforcing bar, while it increased the autogenous shrinkage stress. It was seen that LSHPC was effective to reduce autogenous shrinkage by as much as 70% compared with control mixture high performance concrete.
In this study, corrosion resistance of palm oil fuel ash (POFA) concrete as a blended concrete is evaluated by using electrochemical technique. The POFA is an industrial byproduct obtained from fuel ash after extracting palm oil from palm-tree. In order to obtain basic material characteristics of the POFA concrete, tests on compressive strength, slump, weight loss, bleeding and expansion ratio were carried out the early-aged POFA concrete. On the other hand, durability characteristics, both chloride penetration and carbonation depth test, were also conducted. Finally, corrosion resistance were evaluated by applying electro-chemical artificial crack healing technique, and the tests on the impressed voltage characteristic, galvanic current and linear polarization resistance. From the experimental results, it was found that long-term strength, bleeding, lower slump ratio, expansion ratio, chloride penetration, carbonation and corrosion resistance were improved by using the POFA due to activated pozzolanic reaction. It can be also mentioned that POFA concrete has a potential to be used as a cementitious binder for green-recycling resources.
This study examines setting shrinkage, coefficient of thermal expansion, and elastic modulus of unsaturated polyester( UP)-methyl methacrylate(MMA) polymer concrete, which is generally used for repair of portland cement concrete pavement and manufacturing of precast products. In this study, a series of laboratory test were conducted with variables such as UP-MMA ratio, shrinkage reducing agent (SRA) content, and test temperature. The results showed that the setting shrinkage ranged from 29.2 to $82.6{\times}10^{-4}$, which was significantly affected by test temperature. Moreover, the findings revealed that the coefficient of thermal expansion, elastic modulus and ultimate strain of UP-MMA based polymer concrete ranged from 21.6 to $31.2{\times}10^{-6}/^{\circ}C$, 2.8 to $3.3{\times}10^4$ MPa, and 0.00381 to 0.00418, respectively. The results of this study will be used as important data for design and application of UP-MMA based polymer concrete.
This study was focused on the improvement of production techniques of small crucibles in relation with the appropriate selection of raw materials, various batch compositions and physical and chemical characteristics of the crucibles. Various tests gave the optimum batch composition for the carbon bond graphite cructble as follows: Pyontaek graphite flake (refractory aggregate) : 40Part Silicon carbide: 15Part Tar pitch (binder) : 11Part Inorganic additives (to improve the oxidation resistance) : 15 Part Cryolite : 3 Part Ferro manganese : 2 Part Ferrosilicon : 25 Part Crucibles pressed with 400kg/$\textrm{cm}^2$ at 12$0^{\circ}C$. and fired in reducing atmosphere at 120$0^{\circ}C$ brought the most favorable results as follows: Bulk density : 2.31 Apparent density : 2.58 Porosity : 15.2% Oxidation loss at 1, 50$0^{\circ}C$. for 3 hrs : below 3.77% Water absorption : 6.01% Compressive strength : 438kg/$\textrm{cm}^2$ Tensile strength : 256kg/$\textrm{cm}^2$.
An OWC-type Wave Energy Conversion passes through 3 steps energy conversion process. This paper deal with the impulse turbine with staggered blade to improved performance by numerical analysis using commercial CFD code, FLUENT Maximum value of axial airflow velocity during exhalation is higher than that during inhalation This paper deal with special-type of Impulse Turbine so-called "Staggered Blade" for more efficiency to making air flow direct to on pressure side. Also, this paper has proposed special-type turbine with self-pitched blade more efficient.
It has been pointed out that the collapses of unsaturated road embankments caused by earthquake are attributed to high water content caused by the seepage of the underground water and/or the rainfall infiltration. Hence, it is important to study influences of water content on the dynamic stability and deformation mode of unsaturated road embankments for development of a proper design scheme including an effective reinforcement to prevent severe damage. This study demonstrates dynamic centrifugal model tests with different water contents to investigate the effect of water content on deformation and failure behaviors of unsaturated road embankments. Based on the measurement of displacement, the pore water pressure and the acceleration during dynamic loading, dynamic behavior of the unsaturated road embankments with about optimum water content and the higher water content than the optimum one have been examined. In addition, an image analysis has revealed the displacement field and the distributions of strains in the road embankment, by which deformation mode of the road embankment with higher water content has been clarified. It has been confirmed that in the case of higher water content the settlement of the crown is large mainly owing to the volume compression underneath the crown, while the small confining pressure at the toe and near the slope surface induces large shear deformation with volume expansion.
Transactions of the Korean Society of Mechanical Engineers
/
v.16
no.8
/
pp.1552-1565
/
1992
Three dimensional numerical calculations were carried out for two different combustion chambers with the offset valve in order to investigate the swirl and the squish effects on the flow fields. The modified K-.epsilon. turbulence model considering the change of the density under the condition of the rapid compression and expansion of the pistion was used. During the compression process, it was found that the squish flow which controls the subsequent combustion process was produced due to the piston bowl in the bowl piston type combustion chambers but not for the flat piston type. The swirl velocity close to the solid body rotation was maintained in the flat piston type combustion chambers, but for the bowl piston type a resulting from the change of the solid body rotation was generated in the radial-circumferential plane. For the swirl ratio effect, as the swirl ratio increases, it was found that a large and strong vortex was generated in the radial-circumferential plane of bowl piston type combustion chambers because of the strong inward flows from the combustion chamber wall. These computational results were compared with the results of LDA measurement.
Only a few studies have been conducted using reduced slag as recycled material. The reduced slag in electric furnace is produced as a by-product in making a steel and a few applications of the reduced slag as expensive additives and bonding materials or as the stabilized soils was reported. The purpose of this study is to present the feasibility of the reduced slag as recycled material, especially, in a field of civil engineering. In order to achieve the purpose experiments such as SEM and XRF analysis was conducted for the reduced slag in electric furnace. Based on the results various geotechnical experiments were conducted to know engineering properties of slag-soil mixtures. Weathered soils and clay are mixed with reduced slag for various ratios. As the ratio of reduced slag to weathered soil increases, the maximum dry unit weight of the mixture decreased with increasing optimum moisture content. The results indicates that there is no effect on a reduced slag by compaction efforts. The shear strengths of the weathered soil-slag mixtures are slightly higher or similar to those of weathered soils. The permeability of the weathered soil-slag mixtures is similar to that of silty or sandy soils. Therefore, it is possible to use the mixtures as embankment or backfill materials in the fields. The unconfined strength of the mixtures of reduced slag and clay is higher than that of clay and it tends to increase with the curing time. Therefore it can be used to improve the soft ground.
We could say that the concrete filled steel tube structure is superior in the vlew of various
structure properties as to promote improvement of structural capacity to dtmonstrate heterogeneous material properties interdependently.
The compressive strength is increased by putting to tri axial stress because lateral expansion
of concrete 1s confined by the steel tube, when concrete conflned by steel tube fall under centric
axial load. Also, it have an advantage that decreasr of load carrying capacity 1s small, not
occuring section deficiency due to protect falling piienornonon by co~nprrssion fallurc of concrete.
So this study investigated for structural behaviors yroprrtiex of concwir. confined by steel
tube throughout a series of experlmerit with kcy parxncter, such as diameter-to-thickness(D / t)
ratio, strength of concrete as a study on properties of structural behaviors of confined concrete
confined by circular steel tube( tri axial stress). Frorn the expcrment results, the obtained
results, are surnrnarised as foliow.
(1) The restraint effect of concrete by steel tube was presented significantly as the D /t ratio
of steel tube and the strength of filled concrete decrease, and the confined concrete by circular
steel tube was increased respectively twice as much as 4-7 in deformation capacity at the ultimate
strength ,compared with those of non-confined concrete, so expected to increase flexible
effect of concrete.
(2) The emprical formula to predict the ultimate capacity of confined concrete by steel tube
and concrete filled steel tube column using restraint coefficient of concrete were proposed.
Magazine of the Korean Society of Agricultural Engineers
/
v.39
no.1
/
pp.75-82
/
1997
건설기술과 산업의 발전에 따라 구조물은 대형화되어 가고, 건설공사의 급격한 팽창으로 골재 수용량이 급증함에 따라 천연골재자원은 점차 부족현상을 면치 못할 처지에 있다. 또한, 무리한 천연골재의 채취는 자연환경을 훼손시킬 뿐만 아니라 자연보호 측면에서도 심각한 공해문제로 대두되고 있어 공급량 부족현상은 날로 심화되고 있다. 이에 세계 몇몇 나라에세는 산업부산물을 이용한 골재 생산으로 공해예방과 폐기물 활용방법을 연구하고 있다. 산업부산물중 플라이 애쉬 생산량은 전 세계적으로 매년 약 2억여톤에 달하고 있으나 이중 일부만 활용되고 있는 실정이다. 이와같은 부산물을 활용하기 위한 일환으로 산업부산물인 PFA(Pulverized Fuel Ash)로 만든 인공경량골재의 년생산량이 영국은 600,000$m^3$, 미국은 300,000$m^3$이며, 매년 증가주세에 있다. 고성능 경량골재 콘크리트는 단위중량의 증가없이 내구성과 강도를 향상시켜 실용화 측면에서 경제적인 효과가 있으며, 플라이 애쉬로 만든 경량골재는 시멘트와의 친화력이나 접착면에서 우수한 것으로 알려져 있다. 본 시험에 사용한 골재는 플라이 애쉬로 만든 인공경량 조골재와 강모래이고, 결합제로서 프틀랜드 시멘트를 사용하였다. 부수적인 결합재로서는 플라이 애쉬, 슬래그, 실리카 흄을 사용하였으며, 고성능 경량골재 콘크리트를 개발코자 재령 28일과 180일의 압축강도가 각각 50MPa와 60MPa가 되도록 배합설계를 하였다. 본 연구에서는 플라이 애쉬, 슬래그, 시리카 흄과 같은 산업부산물을 혼입했을때 경량골재 콘크리트의 압축강도, 휨강도, 동탄성계수, 공극체적, 공극률, 단위중량, 공극 크기별 분포등의 변화를 실험적으로 구명하여 재반 구조용 콘크리트에 활용하기 위한 기초자료를 마련코저 한다.있어 특정한 발육단계의 난포 사망기전을 연구하기 어렵다. 또한 난포는 생체 내에서 다양한 호르몬을 동시에 분비하기 때문에 특정한 난소국부호르몬이 사망기전에 미치는 영향을 조사하기 힘든 점이 있다. 최근 들어 난포체외배양이 다양하게 개발되면서, 이러한 어려운 점을 극복할 수 있게 되었다. 본 논문은 각 발육단계의 난포를 절단해 체외배양하면서, apoptosis DNA 절단 현상을 이용하여 각종 난소국부 호르몬들이 난포발육단계별로 사망기전에 미치는 영향을 요약해 보였다. 난포는 발육하면서 점차 복잡한 호르몬 경로를 생존을 위해 필요로 한다. Prevulatory난포생존에 필요한 난소국부호르몬들은 early antral 단계의 난포에서는 그 미치는 영향이 감소되다가 preantral단계의 난포에서는 영향을 전혀 미치지 못했다. 단지 예외는 cGMP처리로써, 세포내 cGMP수준을 일정하게 유지시켜주는 것이 난포발육단계에 무관하게 생존에 중요한 인자로, 장래 연구는 난포 세포내의 cGMP수준을 조절하는 기작을 규명하는데 있을 것이다.인정되지 않았다. 7. 농지보전 처리구인 배수구와 초생수로구는 비처리구에 비해 낮은 침두 유출량과 낮은 토양유실량을 나타내었다.구보다 14% 절감되는 것으로 나타났다.작용하는 것으로 사료된다.된다.정량 분석한 결과이다. 시편의 조성은 33.6 at% U, 66.4 at% O의 결과를 얻었다. 산화물 핵연료의 표면 관찰 및 정량 분석 시험시 시편 표면을 전도성 물질로 증착시키지 않고, Silver Paint 에 시편을 접착하는 방법으로도 만족한 시험 결과를 얻을 수 있었다.째, 회복기 중에 일어나는 입자들의 유입은 자기폭풍의 지속시간을 연장시키는 경향을 보이며 큰 자기폭풍일수록 현저했다. 주상에서 관측된 이러한 특성은 서브스톰 확장기 활동이 자기폭풍의 발달과 밀접한 관계가
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.