• Title/Summary/Keyword: 탄소섬유 메트

Search Result 5, Processing Time 0.024 seconds

Effect of Various Sizing Agents on the Properties of Nylon6/Carbon Fiber Composites Prepared by Reactive Process (다양한 사이징제가 반응중합에 의해 제조된 나일론 6/탄소섬유 복합체의 물성에 미치는 영향)

  • Park, Ha-Neul;Lee, Hak Sung;Huh, Mongyoung
    • Composites Research
    • /
    • v.31 no.6
    • /
    • pp.299-303
    • /
    • 2018
  • In order to improve the interfacial bonding force and reaction polymerization degree of the carbon fiber reinforced nylon 6 composite material, the surface of the existing epoxy-sizing carbon fiber was desized to remove the epoxy and treated with urethane, nylon and phenoxy sizing agent, was observed. The interfacial bond strength of the resized carbon fiber was confirmed by IFSS (Interfacial Shear Strength) and the fracture surface was observed by scanning electron microscope. The results showed that the interfacial bonding strength of the carbon fiber treated with nylon and phenoxy sizing agents was higher than that of urethane - based sizing. It has been found that the urethane - type resizing carbon fiber has lower interfacial bonding strength than the conventional epoxy - sizing carbon fiber. This result shows that the interfacial bonding between carbon fiber and nylon 6 is improved by removing low activity and smoothness of existing carbon fiber.

메탈파우더/섬유강화 복합재료의 전자파 차폐효과

  • 한길영;안동규;이상훈;김민수
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2004.05a
    • /
    • pp.55-55
    • /
    • 2004
  • 최근 전기 전자 장치의 사용이 급속하게 증가하고 있다. AC모터, 프린터, 디지털 컴퓨터, 계산기, 핸드폰 등과 같은 장비들은 많은 전자파를 방출하고 있다. 이러한 전자파에 노출로 암과 같은 질병이 발생할 수도 있다는 논란이 전 세계적으로 관심이 집중되고 있으며, 전자파에너지를 차패할 수 있는 재료 개발의 필요성이 절실히 요구되고 있는 실정이다. 일반적으로 금속과 합금이 전자파 차폐목적으로 사용되었다 그러나 이러한 재료들은 중량이 무겁고 가요성이 떨어지는 단점이 있다.(중략)

  • PDF

Statistical Analysis of Interfacial Shear Strength on Fiber-Matrix (섬유-Matrix의 계면전단강도에 관한 통계적고찰)

  • 문창권;남기우;엄윤성
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.16 no.2
    • /
    • pp.200-206
    • /
    • 1992
  • The effect of fiber diameter and gauge length on pull-out test for the interfacial properties in fiber reinforced resin composites have been investigated and these results have been arranged as statistical analysis. The fiber and matrix resins used for this study were stainless steel fiber (SUS316) and carbon fiber (high strength type), epoxy and high density polyethylene resin. From this study, it has been found that shear strength are constant regardless of gauge length of pull-out test and coefficient of variation depend on fiber diameter. In addition, it has been found that the interfacial shear strength decreased with the increasing fiber diameter, and in all case, Weibull parameter (m) has approximately 1.2/C.O.V.

A Viscoelastic Study of Glass Transition and Degradation Processes of Phenolic Resin/Carbon Fiber Composites (페놀수지/탄소섬유 열경화성 복합재료의 유리전이와 고온 분해과정에서 관찰되는 점탄성 특성 연구)

  • ;J. C. Seferis
    • The Korean Journal of Rheology
    • /
    • v.11 no.1
    • /
    • pp.9-17
    • /
    • 1999
  • Viscoelastic characteristics of cured phenolic resin/carbon fiber composite materials were investigated through glass transition and degradation reaction processes in the high temperature region up to $400^{\circ}C$. A typical glass transition of the cross-linked thermoset polymer was followed by irreversible degradation reactions, which were exhibited by the increasing storage modulus and loss modulus peak. A degradation master curve was constructed by using the vertical and horizontal shift factors, both of which complied well with the Arrhenius equation in light of the kinetic expression of degradation rate constants. Using an analogy to the Havriliak-Negami equation in dielectric relaxation phenomena, a viscoelastic modeling methodology was developed to characterize the frequency- and temperature-dependent complex moduli of the degrading thermoset polymer composite systems. The temperature-dependent relaxation time of the degrading composites was determined in a continuous fashion and showed a minimum relaxation time between the glass transition and degradation reaction regions. The capability of the developed modeling methodology was demonstrated by describing the complex behavior of the viscoelastic complex moduli of reacting phenolic resin composite systems.

  • PDF

The Effects of Insoluble Polymers on Water Stability of Carbon Fiber Reinforced Polymer-MDF Cementitious Composites (불용성 폴리머가 탄소섬유 보강 Polymer-MDF 시멘트 복합재료의 기계적 특성에 미치는 영향)

  • 김태진;박춘근
    • Composites Research
    • /
    • v.12 no.3
    • /
    • pp.84-90
    • /
    • 1999
  • High alumina cement(HAC) and polyvinyl alcohol(PVA) based macro-defect-free(MDF) cement composites were reinforced using short carbon fibers, 3mm in length, 1-4% in weight fraction and insoluble polymers such as polyurethane, epoxy, phenol resin, in order to increase mechanical properties and water stability. The specimens were manufactured by the low heat-press(warmpress) method. In addition, the interface and the cross-linking reaction of cement and polymers was also studied by the SEM and TEM. Flexural strength of HAC/PVA based MDF cementitious composites was proportionally decreased with increasing fiber contents due to the undensified structure around fibers. The flexural strength of insoluble polymer added specimen was decreased with increasing fiber contents, while water stability was dramatically improved. Epoxy resin added specimen showed the highest strength with increasing fiber contents, compared with other specimens. The water stability of fiber content 4% added specimen immersed in water presented about 95%, 87% at 3 and 7 days immersed in water, respectively. The interfacial adhesive strength of fiber-matrix was very much improved due to cross linking reaction of polymer and metal ions of cement. Tensile strength of insoluble polymers added composites as linearly increased with increasing the fiber contents. The epoxy resin added specimen also showed highest tensile strength. The 4% fiber added specimen presented 30~80% higher strength than controlled specimen.

  • PDF