• 제목/요약/키워드: 천이크리프

검색결과 14건 처리시간 0.017초

화력 발전용 로터강의 초기 변형율이 CYCLIC 크리프 특성에 미치는 영향에 관한 연구 (A Study on the Effect of Initial Strain on Cyclic Creep Properties of Steam Turbine Rotor Steel)

  • 오세규;정순억;한상덕
    • 한국해양공학회지
    • /
    • 제6권1호
    • /
    • pp.78-86
    • /
    • 1992
  • The creep behaviors of 1%Cr-Mo-V and 12%Cr steam turbine rotor steels under static or cyclic load were examined at 600 and $700^{\circ}C$. The relationship between these two kinds of phenomena was studied and the experimental results were summarized as follows: 1) It is confirmed that the cyclic creep strain dependent on time is more available for creep, behavior analysis according to frequency change than that dependent on number of cycles, and the static creep, the special case of cyclic creep with stress ratio of 1 can be also more effectively analyzed by time-dependence. 2) The steady cyclic creep rate vs. the steady static creep rate, increases according to the increase of stress ratio, and this phenomena may occur on occasion of the decrease of the internal stress. 3) The initial strain affects on all the creep properties of the transient region, the steady state region and the rupture time in cyclic creep as well as static creep, and the quantitative relationships among them exist.

  • PDF

12% Cr 로터강의 강도 개선에 관한 연구 (Study on the Improvement of Strength for 12% Chromium Steel Rotor)

  • 장윤석;오세욱
    • 한국해양공학회지
    • /
    • 제3권2호
    • /
    • pp.125-137
    • /
    • 1989
  • To check technical improvement in the soundness and strength of 12% Cr steel rotor, a 25 tons of rotor with 65 tons of ingot was made in real size and was cut to pieces to take test samples, and the various mechanical tests such as impact, tensile, creep, and fatigue were carried out. The strengths are compared with those of 1% Cr-Mo-V rotor of same size. Microstructures of the samples are examined and reviewed. The results can be summarized as follows. 1) Fracture appearance transition temperatures are 80.deg. C at the center part and 60.deg. C near surface of 12% Cr rotor, and 8.deg. C near surface of 1% Cr-Mo-V rotor. 2) Comparative rapid softening occurs at higher temperatures above 600.deg. C for 12% Cr steel and 550.deg. C for 1% Cr-Mo-V steel in tension tests. 3) Fatigue crack propagation rate of 12% Cr steel is almost same as that of 1% Cr-Mo-V steel at the same corresponding surface part of the rotors. The crack growth rate of center part of 12% Cr rotor is faster than near surface part of the rotor, and the crack growth rate at the load condition of R=0.04 is slower than that of the load condition of R=0.5 for both 12% Cr steel and 1% Cr-Mo-V steel. 4) Crack growth rate of radial direction near surface of 12% Cr rotor is faster than that of transverse direction at the same part because of the difference in residual stresses. 5) Both creep and fatigue strengths of 12% Cr steel are superior to those of 1% Cr-Mo-V steel and the difference is thought the effect of climb and glide controlled creep by solid solution of alloying elements and dispersion of carbides.

  • PDF

12% Cr 로터강의 강도 개선에 관한 연구 (Study on the Improvement of Strength for 12% Chromium Steel Rotor)

  • 장윤석;오세욱
    • 한국해양공학회지
    • /
    • 제3권2호
    • /
    • pp.625-625
    • /
    • 1989
  • To check technical improvement in the soundness and strength of 12% Cr steel rotor, a 25 tons of rotor with 65 tons of ingot was made in real size and was cut to pieces to take test samples, and the various mechanical tests such as impact, tensile, creep, and fatigue were carried out. The strengths are compared with those of 1% Cr-Mo-V rotor of same size. Microstructures of the samples are examined and reviewed. The results can be summarized as follows. 1) Fracture appearance transition temperatures are 80.deg. C at the center part and 60.deg. C near surface of 12% Cr rotor, and 8.deg. C near surface of 1% Cr-Mo-V rotor. 2) Comparative rapid softening occurs at higher temperatures above 600.deg. C for 12% Cr steel and 550.deg. C for 1% Cr-Mo-V steel in tension tests. 3) Fatigue crack propagation rate of 12% Cr steel is almost same as that of 1% Cr-Mo-V steel at the same corresponding surface part of the rotors. The crack growth rate of center part of 12% Cr rotor is faster than near surface part of the rotor, and the crack growth rate at the load condition of R=0.04 is slower than that of the load condition of R=0.5 for both 12% Cr steel and 1% Cr-Mo-V steel. 4) Crack growth rate of radial direction near surface of 12% Cr rotor is faster than that of transverse direction at the same part because of the difference in residual stresses. 5) Both creep and fatigue strengths of 12% Cr steel are superior to those of 1% Cr-Mo-V steel and the difference is thought the effect of climb and glide controlled creep by solid solution of alloying elements and dispersion of carbides.

화력발전소 보일러 고온헤더의 실시간 수명 감시시스템 개발 (Development of On-Line Life Monitoring System for high-Temperature Header of Fossile Powder Plant Boiler)

  • 윤필기;정동관;윤기봉
    • 에너지공학
    • /
    • 제8권4호
    • /
    • pp.605-611
    • /
    • 1999
  • 화력발전설비 고온요소의 잔여수명평가는 주로 비파괴검사 및 검사결과의 파괴역학적 해석등으로 행해졌다. 그러나 기존 방법은가동중에는 적용되기 어렵고 급작스런 운전이력에 대한 정량적인 손상을 평가할 수 없었다. 따라서 구조물의 형상, 운전이력 및 재료물성에 근거하여 실시간 수명소비율 및 잔여수명을 평가하는 기술의 개발이 요구되고 있다. 본 연구에서는 고온 증기헤더의 수명을 실시간으로 평가하는 감시시스템 소프트웨어를 개발하였다. 고온헤더에 대하여 해석된 온도, 응력, 그린함수를 이용하여 취약부위의 실시간 응력을 계산하고 천이 사이클을 카운트하여 크리프 및, 피로수명을 계산하였다. 본 소프트웨어를 개발함으로써 운전이력에 따른 소비수명을 실시간으로 평가하고 운전정보를 기록하여 향후 운전계획, 보수주기 및 교체시기를 결정하는데 지침이 되도록 하였다.

  • PDF