• Title/Summary/Keyword: 접착부착

Search Result 214, Processing Time 0.028 seconds

Pressure Sensitive Adhesives for Transdermal Drug Delivery System(TDDS) (경피흡수제제용 점착제)

  • Kim, Birm-June;Kim, Hyun-Joong
    • Journal of Adhesion and Interface
    • /
    • v.4 no.1
    • /
    • pp.43-50
    • /
    • 2003
  • 점착제는 경피흡수제제(transdermal drug delivery system, TDDS)의 중요한 구성요소 중의 하나이다. TDDS용 점착제는 일반적인 점착제의 역할 외에도 부착되는 피부에 적합해야 하고, 이것에 포함되는 약물 및 첨가제들과 양립하면서 약물의 전달을 효과적으로 지속해야한다. 본 총설에서는 흔히 사용되는 TDDS용 점착제인 polyisobutylenes, polyacrylates, silicones와 최근에 개발된 제품들을 소개한다.

  • PDF

Comparison between Shear and Tensile Adhesion Strength of Cement for Ceramic Tiles and an Experimental Evaluation on the Cutting Effect of Tile for Tensile Adhesion Strength (타일 시멘트 전단접착강도와 인장부착강도 비교 및 인발부착강도 타일커팅 영향에 관한 실험적 평가)

  • Lee, Sang-Hyun;Ki, Jun-Do;Cho, Hong-Bum;Kim, Young-Sun;Moon, Hyung-Jae;Jeon, Hyun-Su
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2021.05a
    • /
    • pp.181-182
    • /
    • 2021
  • Selecting a proper tile cement for ceramic tile is important to secure tile construction quality. But there is some ambiguity in standards about evaluating adhesion test such as using KS L 1593 in Lab test but using KS L 1592 in site. So, this study aims to how to select proper tile cement for securing adhesion strength in site considering both tensile and shear adhesion strength of cement for ceramic tile. Also, when doing tensile adhesion test in site, there may be adhesion drop because of cutting tile with grinder. As a result, drop of adhesion strength is about 9% ans quality manager consider these factor and should select proper tile cement.

  • PDF

Effects of conventional and self-etching adhesive systems on bond strength of orthodontic attachments bonded to erupted and unerupted teeth (치아 맹출 유무에 대한 자가부식 접착제에 의한 교정용 부착장치의 접착강도)

  • Nur, Metin;Uysal, Tancan;Yesilyurt, Cemal;Bayram, Mehmet
    • The korean journal of orthodontics
    • /
    • v.40 no.4
    • /
    • pp.267-275
    • /
    • 2010
  • Objective: The aim of this study was to evaluate and compare the shear bond strength (SBS) and failure-mode of orthodontic buttons bonded to erupted and unerupted teeth with conventional and self-etching adhesive systems. Methods: Eighty-four erupted and 84 unerupted, human third-molar teeth were used. For both groups, the buccal surfaces of each tooth were assigned one of the following type of adhesive systems (n = 12). A, Conventional systems: 1, Transbond XT (3M Unitek, Monrovia, CA, USA); 2, Prime & Bond NT (Dentsply/Caulk, Milford, USA); 3, Single Bond (3M ESPE, Minnesota, USA); and B, Self-etching adhesives; 4, Clearfil SE Bond (Kuraray, Okayama, Japan); 5, Transbond Plus (3M Unitek, Monrovia, CA, USA); 6, Clearfil S3 (Kuraray, Tokyo, Japan); 7, G Bond (GC, Tokyo, Japan). The SBSs of the attachments and the adhesive remnant index (ARI) scores were recorded. Data were analyzed with analysis of variance (ANOVA), independent-sample t-test and chi-square tests. Results: When the SBSs of erupted and unerupted teeth were compared, only the Clearfil-SE Bond and G-Bond were significantly different. Bond strengths of all adhesive systems were higher in unerupted teeth than erupted teeth, except the Single-Bond system. Conclusions: When using conventional adhesives, bonding to erupted and unerupted teeth may not be significantly different. However, clinicians need to take into consideration the types of self-etching systems before usage.

Interaction of Schwann Cells with Various Protein- or Polypeptide-Coated PLGA Surfaces (다양한 단백질과 폴리펩타이드로 코팅된 PLGA 표면과 슈반세포와의 상호관계)

  • Park Ki-Suk;Kim Su-Mi;Kim Moon-Suk;Lee Il-Woo;Rhee John-M.;Lee Hai-Bang;Khang Gil-Son
    • Polymer(Korea)
    • /
    • v.30 no.5
    • /
    • pp.445-452
    • /
    • 2006
  • In this study, we investigated interaction of Schwann cells (SCs) with various cell-adhesive coated polymer surface. We used cell-adhesives that like a fibronectin (FN), fibrinogen(FG), laminin(LM), vitronectin (VN), poly-D-Iysine (PDL), and poly-L-Iysine (PLL) to coat PLGA film surface and evaluated the surface property of coated or not PLGA films by measurement of water contact angle and ESCA. SCs were cultured on coated or non-coated PLGA film surface, and then examined the cell adhesion and proliferation by cell count and SEM observation. Cell count results revealed initial cell adhesion related to protein adsorption on PLGA surface. In addition, serum content in media related to cell proliferation rate. In this result, we recognized that adhesion and proliferation of SCs were affected by specific cell-adhesives. In these results, we recognized that is important to provide the suitable surface environment according to cell types and culture condition for improvement of cell adhesion and proliferation.

Evaluation of Slant Shear Strength of Recycled Asphalt Mixture with Different Tack Coat Applications (Tack Coat 使用條件에 따른 再活用 아스팔트 混合物의 附着剪斷 性能評價)

  • 김낙석
    • Resources Recycling
    • /
    • v.10 no.1
    • /
    • pp.32-41
    • /
    • 2001
  • Bond shear strengths of recycled asphalt concrete were evaluated under different tack coat applications. Regardless of the new and old mixtures, the bond shear strengths at $30^{\circ}C$ were increased by 10-20% than those at 1$0^{\circ}C$. The bond shear strengths of recycled asphalt concrete without tack coat showed very low ones. These are the main reasons for the frequent longitudinal interface crack in the field. The effect of tack coat curing time on bond shear strengths was inferior to the tack coat construction temperature.

  • PDF

Synthesis and Characterization of Catechol-Containing Biomimetic Mucoadhesive Polymers (카테콜 함유 생체모방 점막접착형 고분자의 합성 및 특성 연구)

  • Park, Dong Jin;Lee, Sang Jin;Lee, Sang Cheon
    • Polymer(Korea)
    • /
    • v.37 no.5
    • /
    • pp.625-631
    • /
    • 2013
  • Mucoadhesive property is the major function as an adhesive for medical devices, and therefore, these days many researches have conducted to develop polymers having this property. Recently, biomimetic technology has been used for developing mucoadhesive polymers. Among many technologies, mussel-inspired approaches have received noticeable attention because of its thread's strong adhesive characteristics. In this study, we synthesized mucoadhesive biomimetic polymers employing catechol structures which are abundant in mussel adhesive proteins, and their structures and molecular weights were characterized by using nuclear magnetic resonance spectroscopy and gel permeation chromatography. To evaluate in vitro mucoadhesive strength, the sheet type of the small intestinal porcine submucosa was prepared. Compared to commercial fibrin glue adhesives, catechol-containing mucoadhesive polymers showed enhanced adhesive strength. The study of adhesive strength with considering diverse factors, such as temperature, pressure, and oxidant amount indicated that mussel-inspired mucoadhesive polymer could be a promising candidate for an adhesive in various biomedical applications.

A COMPARATIVE STUDY OF THE SHEAR BOND STRENGTH AND ADHESIVE FAILURE PATTERN OF METAL BRACKETS BONDED ON NATURAL TEETH AND PORCELAIN TEETH (자연 치관과 포세린 치관상에서 교정용 브라켓 부착시 전단 결합 강도와 파절 양상에 관한 비교 연구)

  • Lee, Hyun-Sun;Kim, Jong-Soo;Yoo, Seung-Hoon
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.35 no.2
    • /
    • pp.195-204
    • /
    • 2008
  • Orthodontic brackets often need to be bonded to porcelain such as porcelain fused to metal crowns and porcelain jacket crowns. The purpose of this study was to evaluate the clinical usability of direct bonding system on porcelain teeth by measuring shear bond strength according to various conditions and observing adhesive failure patterns. The specimens, 20 maxillary premolars and 80 porcelain teeth that were produced by duplication of the labial surface of a maxillary first premolar were used and randomly divided into four groups of twenty teeth each. The 5 different preparation procedures tested: (1) application of 37% phosphoric acid on natural teeth, (2) sandblasting on porcelain surfaces, (3) sandblasting and application of 9.6% hydrofluoric acid on porcelain surfaces, (4) sandblasting and application of silane on porcelain surface, (5) sandblasting and application of 9.6% hydrofluoric acid and silane on porcelain surfaces. The metal brackets were bonded with Transbond $XT^{(R)}$ bonding material. The shear bond strength was tested by the micro universal testing machine(Kyung-Sung, Korea) and the amount of residual adhesive on the tooth surface after debonding was examined by stereoscope and assessed with an adhesive remnant index. The results of this study suggest that the direct bonding system on porcelain teeth with sandblasting, HF and porcelain primer is clinically useful.

  • PDF

Effect of thermocycling on shear bond strength and mode of failure of ceramic orthodontic brackets bonded to different porcelain restorations (수 종의 도재 수복물에 부착된 세라믹 브라켓의 전단접착강도와 파절양상에 열순환이 미치는 영향)

  • Kang, Sang-Wook;Son, Woo-Sung;Park, Soo-Byung;Kim, Seong-Sik
    • The korean journal of orthodontics
    • /
    • v.39 no.4
    • /
    • pp.225-233
    • /
    • 2009
  • Objective: The purpose of this study was to investigate the effect of thermocycling and type of porcelain restoration on shear bond strength (SBS) and mode of failure of monocrystalline ceramic brackets. Methods: A total of 60 porcelain discs were made and divided into three equal groups as follows: Ceramco 3, IPS Empress II, Zi-ceram/Vintage ZR. ceramic brackets were bonded to the prepared porcelain surfaces in the same manner. Each group was divided randomly into two subgroups: thermocycled group and non-thermocycled group (control). All samples were tested in shear mode on an universal testing machine. Results: SBS of the non-thermocycled group was clinically acceptable (Ceramco 3: $7.06\;{\pm}\;1.76\;MPa$, IPS Empress II: $7.55\;{\pm}\;2.38\;MPa$, Zi-ceram/Vintage ZR: $7.19\;{\pm}\;1.38\;MPa$). But, SBS of the thermocycled group was significantly reduced (Ceramco 3: $4.88\;{\pm}\;1.00\;MPa$, IPS Empress II: $5.46\;{\pm}\;1.35\;MPa$, Zi-ceram/Vintage ZR: $4.84\;{\pm}\;1.01\;MPa$, p < 0.05). There was no difference between the shear bond strength by type of porcelain restoration. All bonding failure occurred between bracket base and adhesive, except for 2 samples. Conclusions: The results of this study suggest that the type of porcelain restoration did not affect SBS, but thermocycling weakened SBS. Therefore, the effect of thermocycling should be considered when using ceramic brackets in practice.

Shear bond strength and adhesive failure pattern in bracket bonding with plasma arc light (Plasma arc light를 이용한 bracket 부착시의 전단결합강도와 파절양상의 유형)

  • Yoo, Hyung-Seok;Oh, Young-Geun;Lee, Seung-Yeon;Park, Young-Chel
    • The korean journal of orthodontics
    • /
    • v.31 no.2 s.85
    • /
    • pp.261-270
    • /
    • 2001
  • The purpose of this study was to evaluate the clinical usefulness of plasma arc light which can reduce the curing time dramatically compared by shear bond strengths and failure patterns of the brackets bonded with visible light in direct bracket bonding. Some kinds of brackets were bonded with the Transbond$^{\circledR}$ to the human premolars which were embedded in the resin blocks according to the various conditions. After bonding, the shear bond strength was tested by Instron universal testing machine and in addition , the amount of residual adhesive remaining on the tooth after debonding was measured by the stereoscope and assessed with adhesive remnant index(ARI). The results were as follows : 1. When plasma arc light was used for bonding the brackets, the shear bond strength was clinically sufficient in both metal and ceramic brackets, but resin brackets showed significantly lower bond strength but which was clinically useful. 2. When metal brackets were bonded using visible light, there was no significant difference in shear bond strength due to the light-curing time and the bond strength was clinically sufficient. 3. When the adhesive failure patterns of brackets bonded with plasma arc light were observed by using the adhesive remnant index, the bond failure of the metal and resin bracket occurred more frequently at bracket-adhesive interface but the failure of the ceramic bracket occurred more frequently at enamel-adhesive interface. 4. There was no statistically significant difference of the shear bond strength and adhesive failure pattern between metal bracket bonded for 2 seconds by curing with plasma arc light and 10 seconds by curing with visible light. 6. When metal brackets were bonded using plasma arc light, the shear bond strength decreased as the distance from the light source increased. The above results suggest that plasma arc light can be clinically useful for bonding the brackets without fear of the decrease of the shear bond strength.

  • PDF

Clinical Usefulness of Denture Adhesives (의치접착제의 임상적 효용성)

  • Lee, Jin-Han;Lim, Young-Jun;Lee, Seok-Hyung;Lee, Joon-Seok
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.28 no.2
    • /
    • pp.163-169
    • /
    • 2012
  • Denture adhesive is the material using for enhancing retention and function of the denture. For a long time, denture adhesive was regarded as a repulsive material for dentist. However, it seems that the needs for using this is increasing. This study was planned to recognize the denture adhesive about kinds, components, and action mechanisms through literature review, and also evaluate its clinical effects and implications.