• 제목/요약/키워드: 접선저항력

검색결과 2건 처리시간 0.022초

레지노이드 본드 CBN 휠의 연삭 특성 (Grinding Characteristics of Resinoid-bond CBN Wheel)

  • 원종호;김건희;박원규;안병민;박순섭;이진오;조주현
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1997년도 추계학술대회 논문집
    • /
    • pp.870-874
    • /
    • 1997
  • Super-abrasives such as diamond and CBN have used to maintain accuracy and form deviation for superalloy etc. This study contains the dry cylindrical grinding of metals with resinoid-bond CBN wheel. For various conditions of grinding speed, workpiece speed, grinding depth and feed speed of table, the grinding resistance and the surface roughness are measured and discussed. The results are as follows.

  • PDF

열압밀화 라디에타 소나무재의 역학적 특성 (The Mechanical Properties of Heat-Compressed Radiata Pine (Pinus radiata D.Don) - Effect of Press Temperature & Time -)

  • 황성욱;이원희
    • Journal of the Korean Wood Science and Technology
    • /
    • 제39권4호
    • /
    • pp.303-310
    • /
    • 2011
  • 본 연구에서는 압체온도와 시간에 따른 열압밀화 라디에타 소나무재의 역학적 특성을 조사하였다. 종압축강도와 휨강도는 압체온도와 시간의 증가와 함께 증가하였다. 그러나 압체온도 $220^{\circ}C$에서는 열화로 인해 오히려 감소된 값을 나타내었다. 표면경도는 압체온도의 증가와 함께 증가하였으며, 압체시간이 표면경도에 미치는 영향은 미약하였다. 못뽑기저항의 경우 접선단면의 저항력이 가장 높았으며, 압체온도와 시간에 의한 영향은 거의 나타나지 않았다.