작은 표면균열의 성장특성에 의한 수명예측 (A Fatigue Life Prediction by Growth Characteristics of a Small Surface Crack)

  • 서창민;임창순;강용구
    • 한국해양공학회지
    • /
    • 제3권2호
    • /
    • pp.617-617
    • /
    • 1989
  • This paper deals with a fatigue life prediction of a surface crack based on the experimentally obtained relationship between surface crack length ratio $a/a_{f}$ and cycle ratio $N/N_{f}$ using micro computer. Firstly $a/a_{f}$-$N/N_{f}$ curves obtained from experimental tests, were assumed as three curves UC(the upper limit curve), LC(the lower limit curve) and MC(the middle curve), and these were utilized to predict the fatigue life. Comparing the calculated values which represent the characteristics of crack growth behaviors from the three assumed curves with the experimental ones, it has been found that in the stable crack growth region, they coincide reasonably well each other. And the differences between the fatigue lives obtained from the assumed curves and the experimental fatigue life did not exceed 20%. Using the characteristics of $a/a_{f}$-$N/N_{f}$ curves, it is possible to predict the da/dN-Kmax curves and the S-$N_{f}$ curves.

작은 표면균열의 성장특성에 의한 수명예측 (A Fatigue Life Prediction by Growth Characteristics of a Small Surface Crack)

  • 서창민;임창순;강용구
    • 한국해양공학회지
    • /
    • 제3권2호
    • /
    • pp.108-117
    • /
    • 1989
  • This paper deals with a fatigue life prediction of a surface crack based on the experimentally obtained relationship between surface crack length ratio $a/a_{f}$ and cycle ratio $N/N_{f}$ using micro computer. Firstly $a/a_{f}$-$N/N_{f}$ curves obtained from experimental tests, were assumed as three curves UC(the upper limit curve), LC(the lower limit curve) and MC(the middle curve), and these were utilized to predict the fatigue life. Comparing the calculated values which represent the characteristics of crack growth behaviors from the three assumed curves with the experimental ones, it has been found that in the stable crack growth region, they coincide reasonably well each other. And the differences between the fatigue lives obtained from the assumed curves and the experimental fatigue life did not exceed 20%. Using the characteristics of $a/a_{f}$-$N/N_{f}$ curves, it is possible to predict the da/dN-Kmax curves and the S-$N_{f}$ curves.

  • PDF

2024-T3 및 황동의 작은 표면결함재의 피로균열 성장특성에 관한 연구 (A study on the growth behaviors of surface fatigue crack initiated from a small-surface defect of 2024-T3 and brass)

  • 서창민;오명석
    • 한국해양공학회지
    • /
    • 제10권1호
    • /
    • pp.53-64
    • /
    • 1996
  • In this paper, rotating bending fatigue tests have been carried out to investigate the growth behabiors of surface fatigue crack initiated from a small artificial surface defect, that might exist in real structures, on 2024-T3 and 6:4 brass. The test results are analysed in the viewpoints of both strength of materials and fracture mechanics, it can be concluded as follows. The effect of a small artificial surface defect upon the fatigue strength is very large. The sensitivity of 2024-T3 on the defect is higher than that of 6:4 brass. The growth behavior of the surface fatigue crack of 2024-T3 is different from that of 6:4 brass. The growth rate of the surface fatigue crack of 2024-T3 is considerably rapid in the early stage of the fatigue life and apt to decrease in the later stage. It was impossible to establish a unifying approach in the analysis of crack growth begabior of 2024-T3 and 6:4 brass using the maximum stress intensity factor because of their dependence on stress level. But if the elastic strain and cyclic total strain intensity factor range were applied to obtain the growth rate of surface fatigue cracks of the materials, the data were found to be nearly coincided.

  • PDF

작은 表面缺陷에서 發생.成長하는 表面疲勞균열의 成長特性에 관한 硏究 (Crack growth behavior of fatigue surface crack initiated from a small surface defect)

  • 서창민;권오헌;이정주
    • 대한기계학회논문집
    • /
    • 제11권2호
    • /
    • pp.191-197
    • /
    • 1987
  • 본 논문에서는 이상과 같이 그 중요성이 인정되는 작은 표면피로균열의 성장 특성을 조사하기 위하여 연강과 중탄소강에 두 종류의 작은 표면결함을 가공한 네가지 종류의 시험편을 제작하고, 응력비 R=-1인 소야식 회전굽힘 피로시험을 통하여 작은 표면결함이 피로강도에 미치는 영향과 그 성장특성을 조사한 후 응력확대계수 K를 사 용하는 방법과 반복전스트레인 확대계수범위 .DELTA. $K_{\epsilon}$t/를 비교 검토하여 그 유효성 을 조사하고 이를 파괴역학적 측면에서 고찰하였다.다.

표면균열의 거동과 피로수명예측에 관한 연구 (Surface Crack Behavior and the Fatigue Life Prediction of Notched Specimens)

  • 서창민;이정주;정은화;박희범
    • 대한기계학회논문집
    • /
    • 제12권5호
    • /
    • pp.1097-1103
    • /
    • 1988
  • 본 연구에서는 이 좁은 벤트내에 자료가 모이는 피로균열의 특성을 이용하여 표면피로균열의 성장거동을 파괴역학적으로 해석, 연구하여 균열의 성장특성과 $S-N_{f}$ 곡선의 추정을 마이크로 컴퓨터로 계산하였다.