저탄소강의 고출력 $CO_2$ 레이저 빔 용접 (High power $CO_2$ laser beam welding for low carbon steels)

  • 김재도
    • Journal of Welding and Joining
    • /
    • 제7권4호
    • /
    • pp.12-21
    • /
    • 1989
  • Laser beam welding parameters have experimentally investigated, using a continuous wave 3kW $CO_2$ laser with the various travel speeds, beam mode and laser beam power in low carbon steels. An optimum position of focus and the effect of shielding gas on penetration depth with varying the flow range of 0.5 to 5.1m/min have been combined to investigate the effect of laser power and travel speed on penetration depth and bead width. It is found that the optimum position of focus in 3kW class laser is 0.5 to 1.5mm below the surface of the material. The flow rate of shielding gas affects the penetration depth and He is more effective than Ar. The penetration depth in laser welds of low carbon steels is between two and four times of the bead width. Laser beam welding of butt joints in 2mm thick carbon steel has been carried out to establish a weldability lobe. The lobe indicating acceptable welding conditions is introduced.

  • PDF

레이저 빔에 의한 철강재의 Ti 표면합금화에 미치는 C함량의 영향 (Effect of C-Content for Ti Surface-Alloying Treatment on Steel by $CO_2$ Laser Beam)

  • 최준영;김도훈
    • 한국재료학회지
    • /
    • 제2권6호
    • /
    • pp.436-442
    • /
    • 1992
  • 레이저빔에 의한 철강재의 Ti 표면합금화에 미치는 C함량의 영향을 관찰하였다. 철강재상에 Ti 코팅 후 레이저빔 조사시 질소를 취입가스로 사용하면 부분적으로 TiN과 F$e_2$Ti가 형성된다. 저탄소강의 경우 Ti함량의 증가에 따라 임계냉각 속도의 증가로 마르텐사이트화가 억제된다. 고탄소강의 경우 Ti의 함량이 1.5%정도 임에도 훼라이트 조직이 형성되지 않고 마르텐사이트 조직이 형성되어 경화된다. 그리고 고탄소강의 Ti 표면합금층 형성에 부분적인 TiC의 석출이 있어 더욱 경도를 증가시키는 것으로 생각된다.

  • PDF

강재보와 합성기둥에 사용된 새로운 반강접 접합부의 설계 (Design of Innovative SMA PR Connections Between Steel Beams and Composite Columns)

  • 손홍민;;허종완
    • 복합신소재구조학회 논문집
    • /
    • 제5권1호
    • /
    • pp.28-36
    • /
    • 2014
  • This study describes the development of innovative connections between steel beams and concrete-filled tube columns that utilize a combination of low-carbon steel and super-elastic shape memory alloy components. The intent is to combine the recentering behavior provided by the shape memory alloys to reduce building damage and residual drift after a major earthquake with the excellent energy dissipation of the low-carbon steel. The analysis and design of structures requires that simple yet accurate models for the connection behavior be developed. The development of a simplified 2D spring connection model for cyclic loads from advanced 3D FE monotonic studies is described. The implementation of those models into non-linear frame analyses indicates hat the recentering systems will provide substantial benefits for smaller earthquakes and superior performance to all-welded moment frames for large earthquakes.

$CO_2$레이저빔에 의한 저탄소강판과 아연도금강판의 Tailored Blank 용접에 관한 연구 (A Study of Tailored Blank Welding between Mild Steel and Zn-coated Steel Sheets by $CO_2$ Laser Beam)

  • 서종현;김도훈;유병길;이경돈
    • 한국레이저가공학회지
    • /
    • 제1권1호
    • /
    • pp.4-10
    • /
    • 1998
  • A basic research for tailored blank welding between mild steel and Zn-coated steel was carried out with $CO_2$ laser beam. The materials used in this work were low carbon steel sheet with a thickness of 1.2mm and Zn-coated steel sheet with the same thickness and 6.3$\mu$m Zn coating. Experiments were carried out by applying the Taguchi method in order to obtain optimized conditions for the application of tailored blank laser welding method in practical manufacturing process. Optical microscopy, XRD, SEM and TEM analysis were performed to observe microstructures and to determine the solidification mode of welded zone. Also mechanical properties were measured by microhardness test tensile test and Erichsen test in order to evaluate the formability of welded specimen. There was no trapped Zn in the fusion zone, and the phases in this region consisted of polygonal ferrite, quasi-polygonal ferrite, banitic ferrite and martensite. The elongation value of welded specimen was more than 80% of that value in the substrate and LDH value was more than 90% of that value in the substrate metal.

  • PDF