Amorphous FeCoSiB films with high saturation magnetostriction and excellent soft magnetic properties have been studied to evaluate their strain sensitivity. Films were subjected to a strain by bending of their substrates, which caused a change in the magnetic anisotropy of films via magnetoelastic coupling. Films were exhibited a figure of merit $F=({\Delta}{\mu}/{\mu})/{\varepsilon}$ (change in film permeability $\mu$ per unit strain $\varepsilon$) of $1.2{\times}10^5$, which is comparable with that of amorphous ribbons. To make a study of application of magnetostrictive films as strain sensor elements, we have prepared a micro-patterned film by means of the photolithography and ion milling processes. Impedance change in the patterned films, when strain was applied, was measured over the frequency range from 1 MHz to 1 GHz. Reflecting a large value of figure of merit F, a variation of 46% impedance of films was shown at 100 MHz frequency when a strain of $300{\times}10^{-6}$ was applied.
A high efficiency small electromagnet (22 mm air gap and $40{\times}25mm^{2}$ core's cross section) suitable for measuring magnetostriction and magnetic anisotropy was biult. The magnet could be minaturized by reducing the measuring space and time. The excitation current of the electromagnet was supplied for only a few second of measuring time. Cooling system of the electromagnet could be eliminated since the dissipation energy was very small. An 0.5 T magnetic field was generated with 180 W power consumption. The values of magnetostriction and magnetic anisotropy were measured with a very sensitive capacitance cell with resolution of $10^{-8}$ and 1 nJ. The torque was calibrated using a soft magnetic ribbon's shape anisotropy.
This paper describes the mathematical modeling method for the static magnetic field signature generated by a magnetic scale model. we proposed the equivalent dipole modeling method utilizing a singular value decomposition technique from magnetic field signatures by magnetic sensors are located special depths below the scale model. The proposed dipole modeling method was successfully verified through comparisons with the real measured values in our non-magnetic laboratory. Using the proposed method, it is possible to predict and analyze static magnetic field distributions at any difference depths generated from the real ships as well as a scale model ship.
Two-layered ferromagnetic alloy films (NiFe, CoFe) with a Conetic (NiFeCuMo) intermediately soft magnetic layer of different thickness were investigated to correlate the coercivity values and magnetization process with the strength of saturation field of hard axis. Thickness dependence of the $H_{EC}$ (coercivity of easy axis), $H_{HS}$ (saturation field of hard axis.), and X (susceptibility) of NiFe and NiFeCuMo thin films for the glass/Ta(5 nm)/[CoFe or NiFe(5 nm-t/2)]/NiFeCuMo(t = 0, 4, 6, 8, 10 nm)/[CoFe or NiFe(5 nm-t/2)]/Ta(5 nm) films prepared by the ion beam deposition method was measured. The magnetic properties $H_{EC}$, $H_{HS}$, and X of two-layered ferromagnetic CoFe, NiFe films with a NiFeCuMo intermediately super-soft magnetic layer were strongly depended on the thickness of NiFeCuMo layer. The value of the coercivity and magnetic susceptibility of the NiFeCuMo film decreased by 25% and doubled relative to that of the NiFe film.
The ${\mu}$-turn coil having a width of ${\mu}m$ on the GMR-SV (giant magnetoresistance-spin valve) device based on the antiferromagnetic IrMn layer was fabricated by using the optical lithography process. In the case of GMR-SV film and GMR-SV device, the magnetoresistance ratios and the magnetic sensitivities are 4.4%, 2.0%/Oe and 1.6 %, 0.1%/Oe, respectively. In the y-z plane the distribution of magnetic field of GMR-SV device and $10{\mu}$-turns coil which put under the several magnetic bead(MB)s with a diameter of $1{\mu}m$ attached to RBC (red blood cell) was analyzed by the computer simulation using the finite element method. When the AC currents of 20 kHz from 0.1 mA to 10.0 mA flow to the 10 turns ${\mu}$-coil, the magnetic field at the position of $z=0{\mu}m$ at the center of coil was calculated from $30.1{\mu}T$ to $3060{\mu}T$ in proportion to the current. The magnetic field at the position of $z=10{\mu}m$ was decreased to one-sixth of that of $z=0{\mu}m$. It was confirmed that the $10{\mu}$-turn coil having enough magnitude of magnetic field for the capture of RBC is possible to use as a biosensor for the detection of magnetic beads attached to RBC.
This paper introduces the eddy current signal characteristic of magnetic and non-magnetic gas turbine rotor. In the past, Magnetic particle inspection method was used in magnetic material for qualitative defect evaluation and the ultrasonic test method was used for quantitative evaluation. Nowadays, eddy current method is used in magnetic gas turbine rotor inspection due to advanced sensor design technology. We are studying on the magnetic gas turbine rotor by using eddy current method. We prepared diverse depth specimens made by magnetic and non-magnetic materials. We select optimum frequency according to material standard penetration data and experiment results. We got the signal on magnetic and non-magnetic material about 0.2 mm, 05 mm, 1.0 mm, 1.5 mm 2.0 mm and 2.5 mm depth defects and compare the signal amplitude and signal trend according to defect depth and frequency. The results show that signal amplitudes of magnetic are bigger than non-magnetic material and the trends are similar on every defect depth and frequency. The detection and resolution capabilities of eddy current are more effective in magnetic material than in non-magnetic materials. So, the eddy current method is effective inspection method on magnetic gas turbine rotor. And it has the merits of time saving and simple procedure by elimination of the ultrasonic inspection in traditional inspection method.
Proceedings of the Korean Vacuum Society Conference
/
2011.08a
/
pp.308-308
/
2011
6.48 ${\AA}$의 격자 상수를 갖는 InSb 물질은 0.17 eV의 낮은 에너지 밴드갭과 78,000 cm2/Vs의 전자 이동도를 갖는 물질로서 고속의 자성 센서소자, 장파장의 광 검출기 그리고 고속 전자소자 등의 분야에서 많은 주목을 받고 있다. 그러나, 전기적 특성이 우수한 InSb 물질을 소자로 구현하는데 있어서 큰 어려움이 있다. InSb와 격자 크기가 잘 맞으면서 절연이 우수한 기판의 부재가 가장 큰 문제가 되는 부분이다. 즉, 격자 부정합을 최소화하며 동시에 절연기판을 사용함으로써 소자의 특성을 잘 살려야 하는 것이다. 이러한 이유로 인하여 InSb 기반의 소자가 널리 사용되지 못하고 있는 것이다. 현재 범용으로 사용하고 있는 기판은 격자 부정합이 14%인 GaAs, 11%의 InP 그리고 18%의 Si 등이 있다. 이번 발표에서는 GaAs 기판 위에 격자 부정합을 최소화하여 InSb 박막을 최적화 시켜 성장하는 방법에 대해서 소개하고자 한다. InSb 박막 성장하는데 있어 논문으로 보고된 여러 가지 방법들이 있다. 기판과의 격자 부정합을 줄이기 위하여 저온-고온 (L-T)의 의한 메타몰픽(metamorphic) buffer 층을 성장 후 InSb 박막을 성장하는 방법[1] 그리고 단계별 buffer를 성장하는 방법[2] 등을 통해서 많은 진보가 있었다. 하지만, 우리는 GaAs 기판 위에 AlSb 박막을 성장 하면서 동시에 In과 Al의 양을 서서히 변화시키는 grading 기술을 사용하였다. 즉, 물질 각각의 격자상수를 고려하여 GaAs (기판)-AlSb-InAlSb-InSb로 변화를 주어 격자 부정합이 최소가 되도록 하여 만들어진 buffer 위에 InSb 층이 만들어 지도록 하여 GaAs 기판 위에 InSb 박막을 성장 할 수 있었다. grading 기술을 이용하여 만들어진 buffer 위에 성장된 0.3 um의 InSb 박막 층은 상온에서 전자 이동도가 약 38,000 cm2/Vs에 이르는 것을 확인하였다. InSb 박막의 두께가 약 1 um 되어야 30,000 cm2/Vs 이상의 전자 이동도를 얻을 수 있다고 많은 논문을 통해서 보고 되고 있으나 우리는 단지 0.3 um의 InSb 박막두께에서 이와 같은 전기적인 특성을 확인하였기에 이상과 같이 보고 하고자 한다.
Homegeneous feedstock is necessary to make plastic magents with uniform magnetic properties, therefore the optrimized mixing route and the homogeneity evaluation method are demanded. In this paper, method of homogeneity evaluation and effect of homogeneity on the magnetic prperites were investigated using Sr-ferrite /EVA plastic magnets. The feedstocks with different homogeneity were prepared using batch mixer and single screw extruder. The homogeneities of feedstocks were tested by torgue sensor, capilary rheometer, and measurement of magnetic properties. Mixing torque measurement using torque sensor was an effective method to determine the critical powder loading, but it was nor suitable to suitable to determine the feedstock mixing quality. Particle alignment measurement of a plastic magent was very accurate to evaluate the homogeneity, but expensive equipments were required to make and measure the samples. Pressure measurement using capillary rheometer was a very effective and easy method with high accuracy. Homogeneous feedstock increased the particle alignment of plastic magnet. Remanet flux density and maximum energy product increased linearly and quadratically with increasing particle alignment, respectively.
We investigated that the fabrication and reproducing signal characteristics of tri-layered magnetoresistance (MR) element for the high density magnetic thin film heads and sensors. Magnetoresistance curve of tri-layered MR element predicted by computer modeling was saturated above external field of -15 Oe~+22 Oe, and it was shifted to linearized region as large as 4 Oe. In the case of fabricated real device, magnetoresistance curve was saturated above external field of $\pm$15 Oe, and it was shifted to linearized region as large as 4 Oe. As shown in real device, MR response curve was in good agreement with the simulation results. As a result of experimental data of reproducing output signal in real device, it retained normal sinusoidal waveforms in 1~4 Oe external magnetic field. In this magnetic field region, the fabricated heads with tri-layered MR element can be operated with good reproduced characteristics. This will be beneficial to the use of efficient processes of manufacturing elements and the vacuum deposition techniques which control thin film properties.
The external magnetic field dependency of the impedance, resistance, and inductance of the meander pattern fabricated by using Co-base amorphous ribbon has been investigated in the frequency range of 300 ㎑∼1 ㎓. The amorphous ribbon was patterned to the meander pattern through conventional photolithography and wet etching process. The extremely high sensitivity in impedance changing ratio by external magnetic field was observed. This is due to the transverse magnetic anisotropy the pattern which was induced by magnetic field annealing. The impedance had peak value at the external field of -13 Oe and the impedance changing ratio 100 ${\times}$ (Z$\_$13/-Z$\_$0/)/Z$\_$0/) was about 210% at the frequency of 50 MHz.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.