The prediction for drying shrinkage of self-consolidating concrete using lightweight aggregate (경량골재를 사용한 자기충전 콘크리트의 건조수축률 예측)

  • Kim, Yong-Jic;Choi, Yun-Wang;Kim, Young-Jin
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.11a
    • /
    • pp.341-344
    • /
    • 2008
  • Lightweight concrete is known for its advantage of reducing the self-weight of the structures, reducing the areas of sectional members as well as making the construction convenient. Thus the construction cost can be saved when applied to structures such as long-span bridge and high rise building. However, the lightweight concrete requires specific mix design method that is quite different from the typical concrete, since using the typical mix method would give rise the material segregation as well as lower the strength by the reduced weight of the aggregate. In order to avoid such problems, it is recommended to apply the mix design method of self-consolidating concrete for the lightweight concrete. Therefore experimental tests were performed as such mechanical properties(compressive strength, dry density and structural efficiency) of concrete and dry shrinkage according to ACI committee 209.

  • PDF

A Study in order to Utilize Waste Glasses Powder as Admixtures of Self-Compacting Concrete (폐유리(廢琉璃) 미분용(微粉用)을 보수용(補修用) 모르타르 및 자기충전(自己充塡)콘크리트의 혼화재료(混和材料)로 활용(活用)하기 위한 연구(硏究))

  • Choi, Yun-Wang;Jung, Jea-Gwone;Kang, Hyun-Jin
    • Resources Recycling
    • /
    • v.17 no.1
    • /
    • pp.29-37
    • /
    • 2008
  • Recently, domestically and internationally, the occurrences of Waste Glass are on the increase. Most of scrap glass are either reused of recycled. However, glass not recycled is buriedand is causing secondary environmental problem. With 5% mixture of Waste Glass, the average paste viscosity (rheology) decreased by 22.3% and 28-day compressive strength of mortar's flow and aging decreased by 1.5% and 6% respectively. Also, as Waste Glass mixture ratio of un-hardened elf-compacting concrete increased, fluidity increased and compressive strength decreased. In consideration of adequate compressive strength and fluidity that meets the 2nd class JSCE regulations; optimum mixture ratio of Waste Glass can be concluded as 20%.

An Experimental Study on the Construction Performances and Economical Evaluation of the Self-compacting Concrete by Cementitious Materials (결합재에 따른 자기충전 콘크리트의 시공성 및 경제성 평가에 관한 실험적 연구)

  • Kwon, Yeong-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.29 no.3
    • /
    • pp.315-322
    • /
    • 2017
  • The purpose of this study is to investigate experimentally the construction performances and economical evaluation of the self-compacting concrete in actual site work after selecting the optimum mix proportions according to cementitious materials. Slag cement type of 46.5% slag powder and belite cement of 51.4% $C_2S$ content, lime stone powder as binders are selected for site experiment including water cement ratio. Also, test items for optimum mix proportion are as followings ; (1) Slump flow, 500 mm reaching time, V-type flowing time and U-box height (2) Setting time, bleeding, shortening depth and adiabatic temperature rising (3) Mixing time in plant (4) Concrete quantity and cost, quality control in actual concrete work. As test results, (4) Optimum water-cement ratio ; Slag cement type 41.0% and belite cement 51.0% (2) Setting time and bleeding finishing time of slag cement are faster, bleeding content of slag cement is higher, shortening depth and adiabatic temperature rising of belite cement type are lower (3) Optimum mixing time in batcher plant is 75 seconds and concrete productive capacity is about $100{\sim}110m^3/hr$. (4) Belite cement type is lower than slag cement type in material cost 14.0%, and concrete quantity in actual concreting work save 3.3% in case of belite cement type. Therefore, self-compacting concrete of belite cement type is definitely superior to that of slag cement type in various test items without compressive strength development.

Muti-Objective Design Optimization of Self-Compacting Concrete using CCD Experimental Design and Weighted Multiple Objectives Considering Cost-Effectiveness (비용효율을 고려한 자기 충전형 콘크리트의 CCD 실험설계법 및 가중 다목적성 기반 다목적설계최적화(MODO))

  • Do, Jeongyun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.24 no.3
    • /
    • pp.26-38
    • /
    • 2020
  • Mixture design of self-compacting concrete is a typical multi-criteria decision making problem and conventional mixture designs are based on the low level engineering method like trials and errors through iteration method to satisfy the various requirements. This study concerns with performing the straightforward multiobjective design optimization of economic SCC mixture considering relative importances of the various requirements and cost-effectives of SCC. Total five requirements of 28day compressive strength, filling ability, segregation stability, material cost and mass were taken into consideration to prepare the objective function to be formulated in form of the weighted-multiobjective mixture design optimization problem. Economic SCC mixture computational design can be given in a rational way which considering material costs and the relative importances of the requiremets and from the result of this study it is expected that the development of SCC mixtue computational design and the consequent univeral concrete material design optimization methodology can be advanced.

Development of a Prediction Model for Formwork Pressure Exerted by Self-Compacting Concrete (자기충전 콘크리트의 거푸집 측압 예측 모델 개발)

  • Kwon, Seung-Hee
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.453-456
    • /
    • 2008
  • This study is underway to develop a prediction model for formwork pressure exerted by self-compacting concrete(SCC). Three major mechanisms related to formwork evolution over time were found, and mathematical modelling of each mechanism was made. A calculation method for real formwork pressure by using the mathematical formulae was also established. To verify predictive capability of the prediction model, a parametric study on parameters used in the model was performed. It was confirmed that the proposed model include the essential parameters that can simulate the real formwork pressure evolution over time.

  • PDF

Effect of Hollow Glass Powder on the Self-Compacting Concrete (유공 유리분말이 자기충전 콘크리트의 특성에 미치는 영향)

  • Yoon, Seob;Han, Min-Cheol
    • Journal of the Korea Institute of Building Construction
    • /
    • v.18 no.2
    • /
    • pp.141-149
    • /
    • 2018
  • In this study, compacting, passing performance, segregation resistance and rheological properties were tested to improve the stability of fresh concrete in the production and construction of self-compacting concrete (SCC) using hollow glass powder(GB). As a result, T50 reaching time was shortened up to amount of GB $2.0kg/m^3$. The compacting according to the amount of GB was improved by ball bearing effect of GB. However, T50 reaching time was slightly increased at $4.0kg/m^3$. In the case of passing performance, the result showed that plain was Class 1, GB $0.5{\sim}2.0kg/m^3$ was Class 0, GB $4.0kg/m^3$ was Class 1. Therefore, the passing performance was improved with 'No blocking' up to amount of GB $2.0kg/m^3$. Passing performance Block step (PJ) number by J-ring method was also best at GB $1.0kg/m^3$. In the case of segregation resistance according to the amount of GB, dynamic segregation resistance was increased compared to plain regardless of the amount of GB. And static segregation resistance showed 2.5% of segregation rate at GB $1.0kg/m^3$. Therefore, it was greatly improved compared to plain (12.5%). In the case of rheology property according to the amount of GB, plastic consistency by increasing of GB content didn't show big difference. However, yield stress by increasing of GB content was decreased with GB $1.0kg/m^3$. In conclusion, GB $1.0kg/m^3$ was effective for improvement of compacting, passing performance and yield stress. Also, it will be useful for stability of SCC by improving segregation.