• Title/Summary/Keyword: 이온 현미경

Search Result 381, Processing Time 0.017 seconds

EFFECT OF BENZALKONIUM CHLORIDE ON DENTIN BONDING WITH NTG-GMA/BPDM AND DSDM SYSTEM (Benzalkonium Chloride가 NTG-GMA/BPDM계 및 DSDM계 상아질접착제의 접착성능에 미치는 영향)

  • Shin, Il;Park, Jin-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • v.20 no.2
    • /
    • pp.699-720
    • /
    • 1995
  • This study was conducted to evaluate the effect of benzalkonium chloride solution as a wetting agent instead of water on dentin bonding with NTG-GMA/BPDM system (All-bond 2, Bisco.) and DSDM system (Aelitebond, Bisco.). Benzalkonium chloride solution is a chemical disinfectant widely used in medical and dental clinics for preoperative preparation of skin and mucosa due to its strong effect of cationic surface active detergent. Eighty freshly extracted bovine lower incisor were grinded labially to expose flat dentin surface, and then were acid-etched with 10 % phosphoric acid for 15 second, water-rinsed, and dried for 10 second with air syringe. The specimens were randomly divided into 8 groups of 10 teeth. The specimens of control group were remoistured with water and the specimens of experimental groups were remoistured with 0.1 %, 0.5 %, and 1.0 % benzalkonium chloride solution respectively. And then, the Aelitefil composite resin was bonded to the pretreated surface of the specimens by use of All-bond 2 dentin bonding system or Aelitebond dentin bonding system in equal number of the specimens. The bonded specimens were stored in $37^{\circ}C$ distilled water for 24 hours, then the tensile bond strength was measured, the mode of failure was observed, the fractured dentin surface were examined under scanning electron microscopy, and FT-IR spectroscopy was taken for the purpose of investigating the changes of the dentin surface pretreated with benzal konium chloride solution followed by each primer of the dentin bonding systems. The results were as follows : In the group of bonding with NTG-GMA/BPDM dentin bonding agent(All-bond 2), higher tensile bond strength was only seen in the experimental group remoistured with 0.1 % benzal konium chloride solution than that in water-remoistured control group(p<0.05). In the group of bonding with DSDM dentin bonding agent (Aelitebond), no significant differences were seen between the control and each one of the experimental group(p<0.05). Higher tensile bond strength were seen in NTG-GMAIBPDM dentin bonding agent group than in DSDM dentin bonding agent group regardless of remoistur ization with benzal konium chloride solution. On the examination of failure mode, cohesive and mixed failure were predominantly seen in the group of bonding with NTG-GMAIBPDM dentin bonding agent, while adhesive failure was predominantly seen in the group of bonding with DSDM dentin bonding agent. On SEM examination of fractured surfaces, no differences of findings of primed dentin surface between the groups with and without remoisturization with benzal konium chloride solution. FT-IR spectroscopy taken from the control and the experimental group reve::.led that some higher absorbance derived from the primers binding to dentin surface was seen at the group pretreated with 0.1 % benzal konium chloride solution than at the control group of remoisturizing with water.

  • PDF