압흔가공위치에 따른 피로균열 전파거동 (The Behavior of Fatigue Crack Propagation by Position of Indentations)

  • 송삼홍;최진호
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1995년도 춘계학술대회 논문집
    • /
    • pp.28-32
    • /
    • 1995
  • This effective way for repairing a fatigue crack is making indetations around fatigue crack tip. In this paper, we performed fatigue test to investigate the optimal position of the indentations, and observed crack opening behavior at the same time. The indentation positions of specimens were on the crack tip, front and back of the crack tip. The results of the experiment showed taht it was veryeffective way to increase fatigue life that making indentations on the crack tip, and it was the optimal position that making indentations on the crack tip.

  • PDF

수정 Forman 모델을 이용한 고성능 강재의 피로균열전파와 피로수명평가 (Fatigue Crack Propagation and Fatigue Life Evaluation of High-Performance Steel using Modified Forman Model)

  • 최성원;강동환;이종관;김태원
    • 대한기계학회논문집A
    • /
    • 제35권11호
    • /
    • pp.1361-1368
    • /
    • 2011
  • 응력확대계수비와 하중 주파수가 각각 'R=0.1, f=0.1 Hz', 'R=0.3, f=0.3 Hz' 및 'R=0.5, f=0.5 Hz'인 세가지 하중 조건에서 피로균열전파 실험을 하였으며 이를 바탕으로 고성능 강재의 피로균열전파거동 분석과 피로수명평가를 수행하였다. 하중 조건에 따른 피로균열전파거동을 모사하기 위해 수정된 Forman 모델을 제안하였으며 제안된 모델은 하한 응력확대계수폭과 균열 닫힘 현상에 의한 유효 응력확대계수폭을 고려함으로써 거동의 전 영역을 모사할 수 있었다. 응력확대계수비와 하중 주파수가 0.1 인 경우, 균열이 약 5.0 mm 전파될 때 피로수명을 평가한 결과, Forman 모델은 8,814 cycles, 수정된 모델은 12,292 cycles 의 계산결과를 얻었으며, 이를 12,774 cycles 의 실제 실험결과와 비교할 때 수정된 Forman 모델이 실제 피로균열전파거동을 보다 효과적으로 모사하고 있음을 확인할 수 있었다.