AZ31 마그네슘합금판의 온간 디프드로잉 성형성해석 (The Simulations on the Formability of AZ31 Magnesium Alloy Sheet in Warm Deep Drawing)

  • 강대민;황종관
    • 한국기계가공학회지
    • /
    • 제3권1호
    • /
    • pp.52-58
    • /
    • 2004
  • The material used is a commercial magnesium based alloy AZ31(Mg-3Al-1Zn)sheet with a thickness of 1.0mm. Uniaxial tension tests at warm temperature were carried out to investigate the material characteristics of K, m, and n. A warm drawing process with a local heating and cooling technique was developed to improve formability in this study with results of uniaxial tension tests because it is very difficult for Mg alloy to deform at room temperature by the conventional method. The die and blank holder were heated up, while the punch was water-cooled during deformation. FE simulations considering heat transfer were executed with Mg alloy to investigate the Improvement of deep drawability. For the assessment of improvement those were compare with the results of no considering heat transfer and room temperature.

  • PDF

AZ31B 판재의 온간 디프드로잉 성형성 극대화를 위한 금형 온도 (Tool Temperatures to Maximize the Warm Deep-drawability of AZ31B Sheets)

  • 최선철;김형종;김헌영;홍석무;신용승
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 추계학술대회 논문집
    • /
    • pp.66-70
    • /
    • 2008
  • In this study, the formability of AZ31B magnesium alloy sheets was investigated by the analytical and experimental approaches. Tensile tests and limit dome height tests were rallied out at several temperatures between $25^{\circ}C$ and $300^{\circ}C$ to obtain the mechanical properties and forming limit diagram (FLD). The FLD-based criterion considering the strain-path and the blank temperature was used to predict the forming limit in a deep-drawing process of cross-shaped cup by finite element analysis. This criterion proved to be very useful in determining the optimal process conditions such as blank shape, punch velocity, minimum comer radius, fillet size, and so on, through the comparison between FEA and experimental data. In particular, the temperature of each tool that provided the best formability of the blank was determined by coupled temperature-deformation analyses. A practical method that can greatly reduce the forming time by increasing the punch speed during the forming process was suggested.

  • PDF

고온상태에서 마그네슘 합금의 디프드로잉 성형성에 관한 연구 (A Study on the Formability of Magnesium Alloy in Warm Temperature)

  • 강대민;황종관
    • 한국기계가공학회지
    • /
    • 제2권2호
    • /
    • pp.84-90
    • /
    • 2003
  • Magnesium alloys have been paid attention In automotive and industries as lightweight materials, and with these materials it has been attempted at deep drawing process for assessment of formability of sheet metal. For warm deep drawing process with a local heating and cooling technique, both die and blank holder were heated at warm temperature while the punch was kept at room temperature by cooling water. Warm deep-drawing process with considering heat transfer was simulated by finite element method to investigate the improvement of deep-drawability and temperature distribution of Mg alloy sheet. The effect of sham rate sensitivity index on the deformation profile was considered in this work and the simulation results revealed that considering heat transfer is very effective for deep-drawability of Mg alloy. The deformed blank In considering heat transfer was drawn successfully without any localized thinning and the cup height is higher in contrast to results of simulations in considering no heat transfer.

  • PDF

마그네슘합금 판재의 온간 디프 드로잉성에 관한 연구 (A Study on the Warm Deep Drawability of Mg- Alloy Sheet Metal)

  • 이용길;김종호;이종섭
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 추계학술대회논문집
    • /
    • pp.117-120
    • /
    • 2003
  • Warm deep drawing which is one of the new forming technologies to improve formability of sheet metal is applied to the cylindrical cup drawing of Mg-alloy sheet metal. In experiments the temperature of die and blank holder is varied from room temperature to $300^{\circ}C$, while the punch is cooled by circulation of coolant to increase the fracture strength of workpiece on the punch corner area. Test material chosen for experiments is AZ31 magnesium sheet metal. Teflon film as a lubricant is used on both sides of a workpiece. The limit drawing ratio as well as thickness distributions of drawn cups are investigated and validity of warm deep drawing process is also discussed.

  • PDF

알루미늄 합금박판 비등온 성형공정의 유한요소해석 및 실험적 연구(제1부. 실험) (Finite Element Analysis and Experimental Investigation of Non-isothermal Forming Processes for Aluminum-Alloy Sheet Metals. (Part 1. Experiment))

  • 류호연;배원택;김종호;김성민;구본영;금영탁
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1998년도 춘계학술대회논문집
    • /
    • pp.45-52
    • /
    • 1998
  • This study is to investigate the effects of warm deep drawing with aluminum sheets of A1050-H16 and A5052-H32 for improving deep drawability. Experiments for procucing circular cups and square cups were carried out for various working conditions, such as forming temperature and blank shape. The limit drawing ratio(LDR) of 2.63 in warm deep drawing of circular cups in case of A5052-H32 sheet, whereas LDR of A1050-H16 is 2.25, could be obtained and the former was 8 times higher than the value at room temperature. The maximum relative drawing depth for square cups of A5052-H32 material was also about 2 times deeper than the depth drawn at room temperature. The effects of blank shape, and temperature on drawability of aluminum materials as well as thickness distribution of drawn cups were examined and discussed.

  • PDF

금형의 국부적인 가열에 의한 사각통의 온간 디프로드로잉 성형성에 미치는 온도의 효과 (Temperature Effect On Warm Deep Drawability of Rectangular Cup Using Local Heating of Dies)

  • 김창호;박동환;강성수
    • 한국정밀공학회지
    • /
    • 제13권5호
    • /
    • pp.53-59
    • /
    • 1996
  • Warm deep drawing of single-action dies using local heating has appeared to be an alternative attractive production method of multi-operation die sets generally used at room temperature in deep drawing of rectangular cup. Uniaxial tensile tests and deep drawing tests of various materials are carried out and the effect of temperature on tensile properties and drawability are examined at temperatures up to 200 .deg. C under three kinds of lubricants of teflon film, vinyl film and drawing oil. Good formability is achieved when punch and die temperature were differentiated intentionally in order to get large tensile strength(TS) at punch shoulder protion and small TS at die side. Throughout the experiments, it has been shown that the limiting drawing height of STS316L was increased with heating die and blank holder at 100 .deg. C, but that of STS430 wasn't. When vinyl or teflon film was attached on the plates, the drawability was increased considerably.

  • PDF

AZ3l 판재의 온간 사각컵 디프드로잉에서 금형 설계에 대한 성형성 민감도의 평가 (Evaluation of Formability Sensitivity to Die Design in Warm Square Cup Deep Drawing of AZ31 Sheet)

  • 김기덕;김흥규
    • 소성∙가공
    • /
    • 제16권2호
    • /
    • pp.120-125
    • /
    • 2007
  • Magnesium alloy has low formability at room temperature and therefore, in many cases, forming at elevated temperatures is necessary to obtain the required material flow without failure. Tn the present study, square cup deep drawing tests using the magnesium alloy AE31 sheet were experimentally conducted using the porches and dies with different edge radius to evaluate the formability sensitivity to the die design variables. The experimental results showed that the fracture position over the cup wall moved from the punch nose to the flange as the die temperature increased, and that the drawing depth change was more affected by the punch radius than the die radius.

가공유기변태 강판의 온간 디프드로잉 성형 특성 (Characteristics on the Warm Deep Drawability of Transformation-Induced Plasticity Steel Sheet)

  • 공경환;최치수;최이천;서대교
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2000년도 추계학술대회 논문집
    • /
    • pp.162-167
    • /
    • 2000
  • The warm deep drawability in square cup drawing is investigated about a newly developed high-strength steel sheet with retained austenite which is transformed into martensite during forming. For this investigation, six steps of temperature ranges, from room temperature to $250^{\circ}C$, and five kinds of drawing ratio, from 2.2 to 2.6 were adopted. As a result the maximum drawing force and the maximum drawing depth were affected by the elevated temperatures, and the more stable thickness strain distribution was observed to the elevated temperatures. But blue shortness happened over $200^{\circ}C$. The FEM analysis using the LS-DYNA code is adopted to compare the experimental results with the analytical results for thickness strain distribution.

  • PDF

합금화 용융 아연 도금강판의 온간 디프드로잉 성형성에 관한 연구 (A Study on the Warm Beep Drawabilities of Galvannealed Steel Sheet)

  • 장성호;최치수;최이천;서대교
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2000년도 추계학술대회 논문집
    • /
    • pp.168-173
    • /
    • 2000
  • The limiting drawing ratio (LDR) under uniform heating of blanks was measured at the various temperature ranges between 25 and $250^{\circ}C$ by using two different blank shapes, square and circular blanks, and six different blank sizes with the drawing ratios(DR) of 2.4 to 2.9. The galvannealed steel sheet (SCP3CM 60/60) of 0.7mm thickness was used. The LDR at warm forming condition reached 1.2 times of that at room temperature, and the maximum drawing depth reached 1.9 times. The higher temperature was adopted, the more stable and uniform thickness strain distribution was observed.

  • PDF

Mg 합금 온간 판재 성형시 공정 변수의 영향에 관한 연구 (An Effect on the Process Parameter of Mg Alloy at Warm Sheet Forming)

  • 이영선;권용남;김민철;최상운;이정환
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.43-47
    • /
    • 2006
  • Since the sheet metal forming of Mg alloy is performing at elevated temperature, the effect of process conditions related with the forming temperature is very important factor. Therefore, the investigation for process variables is necessary to design the tools and process conditions. In this study, the effects of process variables were studied by the experimental and FE analysis using the square cup deep drawing. The temperature, forming speed, and lubricant condition were investigated. When forming temperature was $250^{\circ}C$, speed forming was low, and teflon sheet was used as lubricant, the formed parts were good without defects.