  • The experimental study with the prototype provides more acceptable data than the others. But there are so many limited conditions to perform the experimental study with the prototype. So the theoretical similitude with the scaled model and the numerical study with the CFD method have been chosen alternatively to analysis the fume movement. In this study, the ventilation was estimated from the results of the numerical study based on the experimental results as the boundary conditions. The grid A and B were same size and shape with the models which was used in the experimental study and consisted with 163,839, 122,965 cells respectively. The height of the fume layer was estimated form the mole fraction of fume components and the ventilation was determined by the velocity and temperature of the fume. The results of this study showed that the fume movements estimated from the numerical study are enough to apply to the prototype if there are proper heat loss correction factors. The numerical study is easier to change study conditions and faster to get results from the study than the experimental study. So if we find some proper heat loss correction factors, it's possible to execute the various and advanced study with the numerical study.

The Corrosion Behavior of Cold-Rolled 304 Stainless Steel In Salt Spray Environments (염분분사환경에서 냉연 304 스테인레스강의 부식거동)

  • Chiang, M.F.;Young, M.C.;Huang, J.Y.
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.9 no.2
    • /
    • pp.93-98
    • /
    • 2011
  • Saline corrosion is one of the major degradation mechanisms for stainless steel type 304 (SS304) dry storage cask during the spent fuel interim storage period. Slow strain rate test (SSRT) and neutral salt spray test (NSS) were performed at $85^{\circ}C$ and $200^{\circ}C$ with 0.5 wt% sodium chloride mist sprayed on the cold-rolled SS304 specimens of different degrees of reduction in this study. The weight changes of the NSS specimens tested at $85^{\circ}C$ for 2000 hours differed greatly from those at $200^{\circ}C$. The weight loss of NSS specimens was not significant at $85^{\circ}C$ but the weight gain decreased gradually with increasing the cold-rolled reduction. The yield strength (YS) and ultimate tensile stress (UTS) values obtained from the SSRT tests for lightly cold-rolled specimens in the salt spray environment at $85^{\circ}C$ and $200^{\circ}C$ are slightly lower than in air. But for those with 20% reductions, the specimen strengths were no longer changed by the saline corrosion. The preliminary results demonstrated that the quality and performance of cold-rolled SS304 is acceptable for fabrication of dry storage casks. However, more work on the corrosion behavior of cold-rolled stainless steel in the saline atmosphere is needed to better understand its long-term performance.